Wet treatment process for laterite-nickel ore

AU2025271102A1Pending Publication Date: 2026-09-10CHINA ENFI ENG CORP +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
AU2025271102
Authority / Receiving Office
AU · AU
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-02-25
Filing Date
2025-04-28
Publication Date
2026-09-10

AI Technical Summary

Technical Problem

The existing high-pressure leaching process for laterite nickel ore has problems such as long process, poor quality of nickel-cobalt hydroxide products, and low overall scandium recovery rate.

Method used

A short-process wet processing technology for laterite nickel ore is adopted, including acid leaching, liquid-solid separation and countercurrent washing. Through one iron and aluminum removal and one nickel and cobalt precipitation treatment, iron and aluminum removal solution and iron and aluminum slag are obtained. The iron and aluminum slag is returned to the acid leaching step. The temperature, time and pH value are optimized to improve the recovery rate of nickel and cobalt and the quality of nickel and cobalt hydroxide products.

Benefits of technology

It shortens the complex process of traditional two-stage iron and aluminum removal and two-stage nickel and cobalt immersion, reduces production costs and energy consumption, and improves the recovery rate of nickel and cobalt, the overall recovery rate of scandium, and the quality of nickel and cobalt oxide products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000035_0000
    Figure 00000035_0000
Patent Text Reader

Abstract

Provided in the present disclosure is a wet treatment process for nickel laterite ore. The wet treatment process comprises: step S1, subjecting nickel laterite ore to an acid leaching treatment with an inorganic acid, so as to obtain a leached ore slurry; step S2, sequentially performing liquid-solid separation and counter-current washing on the leached ore slurry, so as to obtain a washed slurry and a leaching residue; step S3, adding a first oxidant and a first neutralizer to the washed slurry for an iron-aluminum removal treatment, so as to obtain a solution from which iron and aluminum have been removed and an iron-aluminum residue; step S4, performing a nickel-cobalt precipitation treatment on the solution from which iron and aluminum have been removed, so as to obtain a precipitated slurry; step S5, continuously performing a thickening separation treatment on the precipitated slurry, so as to obtain an underflow and an overflow; and step S6, sequentially performing post-washing treatments on the underflow, so as to obtain a nickel-cobalt hydroxide product. The present disclosure provides a short-flow wet treatment process for nickel laterite ore, which reduces production costs and energy consumption, and also improves the recovery rate of nickel and cobalt, the overall recovery rate of scandium and the quality of the nickel-cobalt oxide product.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Process method for recovering aluminum and scandium

    AU2023433480A1

  • Wet treatment process of laterite nickel ore

    CN111424172A

  • A process for the recovery of value metals from material containing base metal oxides