Solidification material for non-fired brick containing desert soil or dredged soil as raw material, and method and manual manufacturing apparatus for manufacturing non-fired brick containing desert soil or dredged soil as raw material, using same solidification material

BD1007150BActive Publication Date: 2026-09-06EIKEN CO LTD +1
0 Cites 0 Cited by

Patent Information

Application Number
BD2022120
Authority / Receiving Office
BD · BD
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-03-24
Publication Date
2026-09-06
Estimated Expiration
2038-03-24
Patent Text Reader

Abstract

A manual manufacturing apparatus for manufacturing a non-fired brick containing desert soil or dredged soil as a raw material using an inorganic solidification material, in accordance with a manufacturing method which is a mixing ratio of the desert soil or the dredged soil is 12 parts by mass, in a mixing ratio of a composition included in the kneaded mixture, the sand is 1 part by mass, the cement is 2 parts by mass, the inorganic solidification material is 0.002 parts by mass and the water is 2.6 parts by mass, and a tolerance range of the mixing ratio of the composition is 10%.
Need to check novelty before this filing date? Find Prior Art