Composite desulphurization agent
A desulfurizing agent, thiourea technology, applied in the separation of dispersed particles, chemical instruments and methods, separation methods, etc., can solve the problems of high operating costs, easy moisture absorption, low desulfurization rate, etc., to reduce operating costs and high utilization value. , the effect is obvious
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0047] The invention includes the following raw materials: lime and thiourea by-products.
[0048] Lime: the chemical symbol is CaO, the chemical composition is CaO content > 95%, and the physical state is 0.5-3mm white granular.
[0049] Thiourea by-product: the main component (weight, the same below) of thiourea by-product is calcium hydroxide Ca(OH) 2 , 68% content, 3.8% magnesium oxide content, 5% activated carbon content, and more than 23% moisture. The physical state is 80 mesh black powder. The thiourea by-product of the present invention is calculated according to the content of 68% of the active ingredient calcium hydroxide as the ratio of raw materials, so as to facilitate the ratio calculation of the raw materials of the thiourea by-product and other raw materials.
[0050] The present invention prepares raw materials by the following weight percentages:
[0051] Lime: 40-80%;
[0052] Thiourea by-product: 20-60%.
[0053] production method:
[0054] Preparati...
Embodiment 2
[0072] The invention includes the following raw materials: lime, thiourea by-product, acidified weathered coal.
[0073] Lime: the chemical symbol is CaO, the chemical composition is CaO content > 95%, and the physical state is 0.5-3mm white granular.
[0074] Thiourea by-product: The main component of thiourea by-product is calcium hydroxide Ca(OH) 2 , 68% content, 3.8% magnesium oxide content, 5% activated carbon content, and more than 23% moisture. The physical state is 80 mesh black powder.
[0075] Acidified weathered coal: The main component of acidified weathered coal is humic acid, which contains a variety of chemical bonds, and its physical state is 120 mesh black powder. Acidified weathered coal contains a variety of chemical bonds and has a strong adsorption capacity. The preparation method of acidified weathered coal: Add the existing product weathered coal into sulfuric acid with a weight of 20% of the weight of the weathered coal and a concentration of 60%, re...
Embodiment 3
[0101] The invention includes the following raw materials: lime, by-products of thiourea, and activated carbon.
[0102] Lime: the chemical symbol is CaO, the chemical composition is CaO content > 95%, and the physical state is 0.5-3mm white granular.
[0103] Thiourea by-product: The main component of thiourea by-product is calcium hydroxide Ca(OH) 2 , 68% content, 3.8% magnesium oxide content, 5% activated carbon content, and more than 23% moisture. The physical state is 80 mesh black powder.
[0104] Activated carbon: The chemical symbol of the activated carbon is C, the chemical composition is activated carbon c, and the physical state is 100 mesh black powder.
[0105] The present invention prepares raw materials by the following weight percentages:
[0106] Lime: 40-70%;
[0107] Thiourea by-product: 20-56%;
[0108] Activated carbon: 3-15%.
[0109] production method
[0110] Raw material preparation: Prepare raw materials according to the formula.
[0111]High-...