Process for synthesizing polyamine grease coating material
A synthesis process and polyurethane technology, applied in polyurea/polyurethane coatings, coatings, etc., can solve problems such as low production efficiency, easy to cause bad materials, and difficult to master, so as to improve production efficiency, reduce production costs, and improve production efficiency. The effect of technical simplicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0006] Embodiment: A kind of polyurethane paint synthesis technique is characterized in that: it is after being allocated by curing agent and water, is added dropwise in the coating, and the ratio of curing agent and water allocation is 1: 1 to 30 times or 1: 5 to 15 times, and can also be freely allocated, preferably 1: 8 to 10 times, more preferably 1: 8.6 to 9 times, the curing agent is isophorone diamine, water can be purified water or demineralized water, the most The best choice is pure water or demineralized water. The temperature of paint, curing agent and water should be controlled at 35°C-0°C or 20°C-0°C when adding drops, and the best control is at 15°C-0°C. The best solution is to control the temperature at 10°C-0°C. The speed of dropping should be determined by the time of uninterrupted dropping. Its time is 50-100 minutes, the best is 70-90 minutes, and the best choice is 75- 85 minutes, the most appropriate time is about 80 minutes, no more than 3 minutes, the b...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More