Embodiment 1
[0020] The overturning mold of the present embodiment comprises an upper mold base 10, a punch insert 9, a die template, and a lower die base 1, and the punch insert 9 is fixed on the punch body of the upper die base 10, and the die template and the lower die base The mold base 1 is connected, the die template includes a bottom plate 11 and two side plates 13, the bottom plate 11 is set between the side plates 13, the two side plates 13 and the bottom plate 11 are arranged on the same horizontal line, and the side plate 13 and the bottom plate 11 are movable connect. The movable connection between the side plate 13 and the bottom plate 11 is configured as a hinged connection. The hinges 4 and 6 are arranged at both ends of the side plate 13 . On the lower die base 1, at the contact of the side plate 13 and the lower die base 1 cavity, rollers 14 are set and the rollers 14 are fixed on the lower die base by the mounting bracket 2. Roller 14 is provided with three groups at le...
Embodiment 2
[0025] The difference between the overturning mold of this embodiment and Embodiment 1 is that the hinges of this embodiment are arranged in the middle of the bottom plate in two groups, and the rollers are arranged in two groups.
Embodiment 3
[0027] The difference between this embodiment and Embodiment 1 is that the hinges of this embodiment are provided at both ends and in the middle, one set is set in the middle, one set is set at both ends, and one set of rollers is set in the middle of the side plate.
[0028] The flip-type mold structure of the present invention reduces the load of the mold when the sheet is formed, and reduces the friction between the mold and the sheet, so that no stretch marks will be formed on the outer surface of the formed part, which improves the surface quality of the formed part and prolongs the The service life of the mold is greatly reduced.