A kind of asphalt pavement and curing agent technology, which is applied in the direction of roads, roads, on-site paved coagulation pavements, etc., can solve the problems of poor fatigue and durability, insufficient rigidity, and low strength, and achieve excellent fatigue performance and low equipment requirements , Improve the effect of adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039] A kind of asphalt pavement maintenance agent of the present invention, it comprises mutually independent A component and B component, and A component comprises E51 type epoxy resin, S-150 solvent naphtha, carbon black, dispersant, penetrating agent and rare earth, Component B contains cashew oil modified amine, S-150 solvent naphtha, asphalt, asphalt regenerant and rare earth;
[0040] The mass fraction proportioning of above each component is:
[0041] A component
[0042] E51 type epoxy resin 25%
[0043] S-150 solvent oil 15%
[0044] Carbon black 3%
[0045] Dispersant 2%
[0046] Penetrant 2%
[0047] Heat Stabilizer A 3%
[0048] B component
[0049] Cashew oil modified amine MK-C6040 25%
[0050] S-150 solvent oil 10%
[0052] Asphalt rejuvenator 5% and
[0053] Heat Stabilizer B 3%.
[0054] The dispersant used in this example is a mixture of dispersants Silok®7050 and Silok®7160 (the ratio of the two is 1:1, both are prod...
Embodiment 2
[0062] A kind of asphalt pavement maintenance agent of the present invention, it comprises mutually independent A component and B component, and A component comprises E51 type epoxy resin, S-150 solvent naphtha, carbon black, dispersant, penetrating agent and rare earth, Component B contains cashew oil modified amine, S-150 solvent naphtha, asphalt, asphalt regenerant and rare earth;
[0063] The mass fraction proportioning of above each component is:
[0064] A component
[0065] E51 type epoxy resin 25%
[0066] S-150 solvent oil 15%
[0067] Carbon black 3%
[0068] Dispersant 2%
[0069] Penetrant 2%
[0070] Heat Stabilizer A 3%
[0071] B component
[0072] Cashew oil modified amine MK-C2016 25%
[0073] S-150 solvent oil 10%
[0074] Modified asphalt 7%
[0075] Asphalt rejuvenator 5% and
[0076] Heat Stabilizer B 3%.
[0077] The dispersant, penetrating agent, heat stabilizer A, heat stabilizer B, and asphalt regenerant used in this example are all the sam...
Embodiment 3
[0085] A kind of asphalt pavement maintenance agent of the present invention, it comprises mutually independent A component and B component, and A component comprises E44 type epoxy resin, S-150 / S-100 solvent oil, carbon black, dispersant, penetrating agent and rare earth, component B contains cashew nut oil modified amine, S-150 / S-100 solvent oil, asphalt, asphalt regenerant and rare earth;
[0086] The mass fraction proportioning of above each component is:
[0087] A component
[0088] E44 type epoxy resin 25%
[0089] S-150 and S-100 solvent oil 15% (mixed according to the mass ratio of 1:1)
[0090] Carbon black 3%
[0091] Dispersant 2%
[0092] Penetrant 2%
[0093] Heat Stabilizer A 3%
[0094] B component
[0095] Cashew oil modified amine MK-C2016 25%
[0096] S-150 and S-100 solvent oil 10% (mixed according to the mass ratio of 1:1)
[0098] Asphalt rejuvenator 5% and
[0099] Heat Stabilizer B 3%.
[0100] The dispersant used...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More