Copper-clad aluminum alloy cable
A technology of copper-clad aluminum alloy and copper alloy, which can be applied to insulated cables, metal/alloy conductors, cables, etc., and can solve problems such as reducing the mechanical properties of cables
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] A copper-clad aluminum alloy cable provided in Embodiment 1 of the present invention includes a conductor, the conductor includes an inner core and an outer core, and the inner core and the outer core form a bimetallic concentric circle structure, wherein the inner core is an aluminum alloy , the outer core is a copper alloy; the alloy composition mass fraction ratio of the aluminum alloy inner core is Cu0.10%, B0.15%, Ce0.01%, and the rest are Al and unavoidable impurities; the copper The mass fraction ratio of the alloy composition of the alloy outer core is Al0.08%, Mg0.85%, La0.01%, and the rest is Cu and unavoidable impurities; ℃ for 1 hour; then melt the aluminum alloy, and then pour the aluminum alloy liquid into the tank, so that the aluminum alloy liquid is cooled and formed in the copper alloy tank, and finally the cooled copper alloy skin is covered with shielding layer, insulating layer and resistance A high-temperature layer; wherein, the shielding layer is...
Embodiment 2
[0012] A copper-clad aluminum alloy cable provided in Embodiment 2 of the present invention includes a conductor, the conductor includes an inner core and an outer core, and the inner core and the outer core form a bimetallic concentric circle structure, wherein the inner core is an aluminum alloy , the outer core is a copper alloy; the alloy composition mass fraction ratio of the aluminum alloy inner core is Cu0.85%, B0.25%, 0.03%, and the rest are Al and unavoidable impurities; the outer core of the copper alloy The mass fraction ratio of the alloy composition of the core is Al0.18%, Mg1.15%, La0.02%, and the rest is Cu and unavoidable impurities; firstly, the copper alloy is melted and casted, and then grooved in the center, and kept at 550°C 0.5h; then melt the aluminum alloy, and then inject the aluminum alloy liquid into the tank, so that the aluminum alloy liquid is cooled and formed in the copper alloy tank, and finally the cooled copper alloy skin layer is covered with...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More