A kind of oil agent for fluorine-containing polyester FDY fiber and preparation method thereof
A technology of fluorine-containing polyester and fiber, which is applied in the field of oil agent for fluorine-containing polyester FDY fiber and its preparation, can solve the problems of unsatisfactory adhesion and wetting performance, achieve excellent comprehensive performance and solve the problem of wetting performance Problems, the effect of reducing hair breakage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024]In parts by weight, get 20 parts of polyisomeric decanol polyoxyethylene ether, 10 parts of potassium lauryl phosphate, 16 parts of polyethylene glycol monostearate, 4 parts of sodium lauryl sulfonate and 5 parts of perfluorobutyl ethyl acrylate were mixed at room temperature and stirred for 20 minutes. Add the above mixture to 45 parts of 9 # In mineral oil, the temperature is controlled at 55°C and stirred for 1 hour to obtain FDY oil with excellent performance.
Embodiment 2
[0026] In parts by weight, take 35 parts of isomeric tridecyl alcohol polyoxyethylene ether, 5 parts of isomeric tridecyl alcohol polyoxyethylene ether phosphate potassium salt, 14 parts of polyethylene glycol stearic acid diester, 1 part of pentadecyl alcohol Sodium alkyl sulfonate and 5 parts of perfluorohexyl ethyl acrylate were mixed at room temperature and stirred for 30 minutes. Add the above mixture to 40 parts of 10 # In mineral oil, the temperature is controlled at 40°C and stirred for 0.5h to obtain FDY oil with excellent performance.
Embodiment 3
[0028] In parts by weight, take 25 parts of polyoxyethylene laurate, 7 parts of potassium tetradecyl phosphate, 11 parts of polyethylene glycol monolaurate, 5 parts of sodium cetyl sulfonate, 2 parts of Perfluorooctyl ethyl acrylate was mixed at room temperature and stirred for 20 minutes. Add the above mixture to 50 parts of 11 # In mineral oil, the temperature is controlled at 55°C and stirred for 2 hours to obtain FDY oil with excellent performance.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com