A production process, fog white technology, applied to the surface coating liquid device, coating, pretreatment surface, etc., can solve the economic loss, the transparent paint film of the coating is prone to obvious whitening, and affects the coated object Appearance decoration effect and other problems, to achieve the effect of accelerating volatilization and reducing whitening
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] Embodiment 1: the varnish construction technology of solid wood wooden box surface
[0027] (1) Clean the surface of the sample: clean the dust and dirt on the surface of the wooden box;
[0028] (2) Sanding: Use sandpaper to polish the burrs and protrusions of the wooden box to obtain a smooth and flat surface;
[0029] (3) Apply the polyurethane transparent primer by spraying. After the coating is completed, quickly put the object into the vacuum box, start the vacuum pump to vacuum for 60 seconds, then take it out and dry it. After it is completely dry, sand it with sandpaper to make it smooth;
[0030] (4) Repeat step (3) twice;
[0031] (5) Apply polyurethane transparent topcoat by spraying. After the coating is completed, quickly put the object into the vacuum box, start the vacuum pump to vacuum for 120 seconds, and then take it out to dry in the natural environment.
Embodiment 2
[0032] Embodiment 2: the coating construction technology of aluminum alloy handicraft.
[0033] (1) Clean the dirt on the surface: first use an organic solvent to remove the dirt such as oil stains attached to the surface of the aluminum alloy;
[0034] (2) Surface activation treatment: Use phosphating solution or phosphating primer to treat the surface of aluminum alloy, and after reacting with aluminum alloy, form an aluminum phosphide film that paint is easy to adhere to, clean and dry;
[0035] (3) Dust, oil, water vapor and other dirt are not allowed on the treated surface. After the surface treatment meets the coating requirements, immediately use the spraying method to coat the aluminum alloy transparent primer. After the coating is completed, quickly put the object into the vacuum Start the vacuum pump to evacuate the box for 60 seconds, then take it out and dry it;
[0036] (4) After drying, use the method of spraying to apply transparent color paint. After the coati...