A technology of wire-covered paint and synthetic paint, applied in the field of enameled wire paint, can solve the problems of heat resistance level lower than 120℃, difficult to meet different environments, insufficient strength, etc., achieve good freezing resistance, solve the problem of substandard pressure resistance and cost low effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0013] The synthetic wire enamel is made from the following raw materials in parts by weight (kg): 10 trimethylolpropane triacrylate, 10 trimellitic anhydride, 5 maleic anhydride, 4 tetraethyleneimine, 8 titanium dioxide, precipitate Barium sulfate 3, nylon 12 10, polyacrylate 20, diethylenetriamine 1, ceramic slag powder 5, zinc oxide 4, aluminum hydroxide 1, microcrystalline wax 13, additive 9, m-p-cresol 90, xylene 100;
[0014] The auxiliary agent is made of the following raw materials in parts by weight (kg): 0.2 nanometer mica powder, silane coupling agent KH550 2, hydroquinone 1, dipentaerythritol hexaacrylate 5, crosslinking agent TAC3, polyisobutylene 2, Dimethylaminoethyl methacrylate 10, butyl ethyl methacrylate 4, propyl gallate 2, coix seed oil 2; the preparation method is to mix the materials, heat to 60-70°C, and stir for 30-40 minutes to react, that is have to.
[0015] The preparation method comprises the following steps:
[0016] (1) Weigh xylene and m-p-c...