Abstract

The invention discloses a method for manufacturing an archaizing wooden boat. The method comprises the steps that thin willow branches with the even thickness and high tenacity are selected for use, the branches are firstly soaked, so that white thin gentle branch materials are prepared, a boat shape is woven from the gentle branch materials through design and machining, and the archaizing wooden boat is manufactured after archaizing treatment. According to the method, the manufacturing technology is simple, production and machining cost is low, surface layer retro-treatment is vivid, and the archaizing effect is good.

Application Domain

Cane mechanical workingReed/straw treatment

Technology Topic

EngineeringManufacturing engineering +3

Examples

  • Experimental program(1)

Example Embodiment

[0005] The manufacturing process steps of the present invention are as follows
[0006] 1. Material selection: choose willow wood branches with uniform thickness, smooth surface and good toughness, which are soaked, peeled, and rinsed to become white and soft;
[0007] 2. Knitting: Weaving thin flexible strips or rattan into the shape of a boat in accordance with the design graphics. The braided strips or rattans should be evenly arranged, tight and tight;
[0008] 3. Put the woven wooden boat in a humid storage room with a constant temperature of 10 degrees Celsius for old treatment, leave it for 3-7 days until the surface of the wooden boat is all mildewed, take it out, dry it in the sun for 3-5 days, and dry the wooden boat Put it again in a humid warehouse with a constant temperature of 10 degrees for a second mold change for 3-5 days, then take it out and put it in the sun for a second time for 3-5 days;
[0009] 4. Drying: Put the wooden boat that has been air-dried twice in a drying room at 65-70℃ until the water content of the wooden boat is 8-12%℃, and then take it out;
[0010] 5. Fumigation: Put the dried wooden boat into the fumigation room, use 56g/m of methyl bromide 3 , Fumigation and disinfection, room temperature 16-20℃, airtight for 24h, sterilization;
[0011] 6. Attach a waterproof membrane to the processed wooden ship cabin to form an anti-ancient wooden ship.
[0012] The production process of the invention is simple, the production and processing cost is low, the surface layer is treated with vivid retro-looking, and the anti-aging effect is good.

PUM

no PUM

Description & Claims & Application Information

We can also present the details of the Description, Claims and Application information to help users get a comprehensive understanding of the technical details of the patent, such as background art, summary of invention, brief description of drawings, description of embodiments, and other original content. On the other hand, users can also determine the specific scope of protection of the technology through the list of claims; as well as understand the changes in the life cycle of the technology with the presentation of the patent timeline. Login to view more.
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products