Water-based air purification paint and preparation method thereof
A kind of air purification and water-based technology, applied in the direction of coating, etc., can solve the problems of not meeting the requirements of environmental protection, low air quality, serious atmospheric smog, etc., and achieve good cold and heat cycle resistance, convenient use, and good decorative effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Example Embodiment
[0015] Example one
[0016] A water-based air purification paint, comprising the following components in mass percentage: water 25%; dispersant 0.6%; nano anion powder 10%; titanium dioxide: 26%; activated carbon 2%; acrylic emulsion: 35%; additives: 1.4%. Wherein, the auxiliary agent is a mixture composed of a film-forming auxiliary agent, a defoamer, an antiseptic and antifungal agent, and a thickener with a mass ratio of 1.5:0.1:0.25:0.5.
[0017] The preparation method of the above water-based air purification paint includes the following steps: at room temperature, add water and titanium dioxide into the container, use a disperser to disperse at a speed greater than 500r / min for 30 minutes, and then add dispersant, nano anion powder, and activated carbon , Acrylic emulsion and additives, continue to disperse until evenly mixed, and grind with a sand mill to a fineness of less than 20 microns to obtain water-based air purification paint.
Example Embodiment
[0018] Example two
[0019] A water-based air purification paint, including the following components in mass percentage: water 25%; dispersant 0.5%; nano anion powder 10%; wollastonite powder: 27%; bamboo charcoal powder 3%; acrylic emulsion: 33%; Agent: 1.5%. Wherein, the auxiliary agent is a mixture of a film-forming auxiliary agent, a defoamer, an antiseptic and antifungal agent, and a thickening agent with a mass ratio of 2:0.1:0.3:0.5.
[0020] The preparation method of water-based air purification paint includes the following steps: at room temperature, add water and wollastonite powder into the container, use a disperser to disperse at a speed greater than 500r / min for 30 minutes, and then add dispersant, nano anion powder, bamboo charcoal Powder, acrylic emulsion and additives, continue to be dispersed until they are evenly mixed, and then grind with a sand mill to a fineness of less than 20 microns to obtain water-based air purification paint.
Example Embodiment
[0021] Example three
[0022] A water-based air purification paint, including the following components in mass percentages: water 26%; dispersant 1%; nano anion powder 10%; titanium dioxide: 29%; activated carbon 1%; acrylic emulsion: 30%; additives: 1%. Wherein, the auxiliary agent is a mixture of a film-forming auxiliary agent, an antifoaming agent, an antiseptic and antifungal agent, and a thickening agent with a mass ratio of 1.3:0.1:0.24:0.5.
[0023] The preparation method of water-based air purification paint includes the following steps: at room temperature, add water and titanium dioxide into a container, use a disperser to disperse at a speed greater than 500r / min for 30 minutes, and then add dispersant, nano anion powder, activated carbon, Acrylic emulsion and additives, continue to be dispersed until they are evenly mixed, and then grind with a sand mill to a fineness of less than 20 microns to obtain water-based air purification paint.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap