A processing technology and technology for gold ore, which is applied in the field of gold ore beneficiation and smelting technology, can solve the problems of large consumption, increased metal loss, and reduced concentrate quality, etc., to achieve good economic benefits and improve the effect of resource utilization.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] An ore body in the Nibao Gold Mine in Guizhou contains 3.25g / t of gold and 5.90% of sulfur. The sulfide is mainly pyrite. The distribution rate of gold in pyrite is 42.1%, and the content of pyrite is 10.85%. In the ore, calcite and dolomite account for 0.55%, and clay minerals account for 30.21%. The ore contains 5.64% water. The particle size analysis shows that when the particle size is controlled at -12mm after crushing, the ore slime of -0.074mm accounts for 19.89%. The process of the present invention is suitable for this ore.
[0030] Such as figure 1 The raw ore shown is crushed by the crushing system. After the ore is crushed to -12mm, the ore is washed twice with a trough washing machine. The gold content in the slime is 0.98g / t, and the removal rate of the slime reaches 86.73%. Add PAM flocculant to the mud after ore washing. The amount of flocculant is 600g / ton. After 20 minutes of sludge sedimentation and separation, the separated ore slime is sent to t...
Embodiment 2
[0035] A certain ore body in Henan Niutougou Gold Mine contains 3.36g / t of gold and 3.01% of sulfur. The sulfide is mainly pyrite. The distribution rate of gold in pyrite is 37.3%, and the content of pyrite is 5.60%. In the ore, feldspar alterations accounted for 52%, chlorite and hornblende accounted for 7.5%, calcite and dolomite accounted for 6%, muscovite and sericite accounted for 2.5%, kaolin accounted for 1.5%, and clay minerals accounted for 3%. The ore contains 5.36% water. The particle size analysis shows that when the particle size is controlled at -15mm after crushing, the ore slime of -0.074mm accounts for 18.45%. The process of the present invention is suitable for this ore.
[0036] Such as figure 1 The raw ore shown is crushed by the crushing system. After the ore is crushed to -15mm, the ore is washed twice with a trough washing machine. The gold content in the slime is 1.23g / t, and the removal rate of the slime reaches 87.13%. PAM flocculant is added to t...