Embodiment 1
[0014] The invention is an improved interior wall paint, which is made of the following raw materials in parts by weight: 1.5 parts of nano-titanium oxide, 5 parts of titanium dioxide, 20 parts of white latex, 6 parts of glycerol, 15 parts of deionized water, laurel 2.5 parts of aldehydes, 2.5 parts of 2-octylphenol polyoxyethylene ether, 2.5 parts of methyl methacrylate and 3.5 parts of polyethylene glycol.
[0015] A kind of preparation method of improved interior wall paint, comprises the following steps:
[0016] 1) Put the nano-titanium oxide, titanium dioxide and white latex into the high-speed disperser according to the formula and stir at high speed for 15 minutes, then turn to low-speed stirring for 5 minutes, and vacuumize and exhaust while stirring;
[0017] 2) Stir evenly and disperse at high speed until the fineness is below 15 microns;
[0018] 3) After reducing the stirring speed, add glycerol, deionized water, laurylaldehyde and 2-octylphenol polyoxyethylene e...
Embodiment 2
[0022] The invention is an improved interior wall paint, which is made of the following raw materials in parts by weight: 3.7 parts of nano-titanium oxide, 10 parts of titanium dioxide, 30 parts of white latex, 10 parts of glycerin, 120 parts of deionized water, laurel 6.3 parts of aldehyde, 3.6 parts of 2-octylphenol polyoxyethylene ether, 3.7 parts of methyl methacrylate and 4.2 parts of polyethylene glycol.
[0023] A kind of preparation method of improved interior wall paint, comprises the following steps:
[0024] 1) Put nano-titanium oxide, titanium dioxide and white latex into the high-speed disperser according to the formula and stir at high speed for 20 minutes, then turn to low-speed stirring for 10 minutes, and vacuumize while stirring;
[0025] 2) Stir evenly and disperse at high speed until the fineness is below 15 microns;
[0026] 3) After reducing the stirring speed, add glycerol, deionized water, laurylaldehyde and 2-octylphenol polyoxyethylene ether in turn,...
Embodiment 3
[0030] The invention is an improved interior wall paint, which is made of the following raw materials in parts by weight: 3.1 parts of nano-titanium oxide, 7 parts of titanium dioxide, 23 parts of white latex, 8.5 parts of glycerol, 17.5 parts of deionized water, laurel 4.2 parts of aldehyde, 3 parts of 2-octylphenol polyoxyethylene ether, 2.9 parts of methyl methacrylate and 3.9 parts of polyethylene glycol.
[0031] A kind of preparation method of improved interior wall paint, comprises the following steps:
[0032] 1) Put nano-titanium oxide, titanium dioxide and white latex into the high-speed disperser according to the formula and stir at high speed for 18 minutes, then turn to low-speed stirring for 8 minutes, and vacuumize and exhaust while stirring;
[0033] 2) Stir evenly and disperse at high speed until the fineness is below 15 microns;
[0034] 3) After reducing the stirring speed, add glycerol, deionized water, laurylaldehyde and 2-octylphenol polyoxyethylene ethe...
PUM
Login to View More Abstract
Description
Claims