A technology for hydrogenation catalysts and catalyst carriers, which is applied in chemical instruments and methods, preparation of hydroxyl compounds, metal/metal oxide/metal hydroxide catalysts, etc., and can solve the problem of lack of research on bifunctional catalysts, uneven dispersion, and easy production Agglomeration and other problems, to achieve the effect of high alcohol selectivity, high conversion rate of raw materials, good catalyst activity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0018] The preparation method of hydrogenation catalyst provided by the invention comprises the following steps:
[0019] (1) contacting the catalyst carrier with a solution containing a surfactant with an amine group, so that the surfactant is loaded on the catalyst carrier, and then dried to obtain a catalyst carrier solidly loaded with a surfactant;
[0020] (2) The catalyst carrier solidly loaded with surfactant is sequentially immersed in an impregnating solution containing chloroplatinic acid, an impregnating solution containing a water-soluble copper salt, and an impregnating solution containing an auxiliary compound, and drying after each immersion , and the last dried product is roasted, so that the surfactant is decomposed and the chloroplatinic acid, water-soluble copper salt and auxiliary agent compound are converted into platinum oxide, copper oxide and auxiliary agent, respectively.
[0021] The type of the catalyst carrier is not particularly limited in the pres...
Embodiment 1
[0048] This embodiment is used to illustrate the hydrogenation catalyst provided by the present invention, its preparation method and application, and the method of hydrogenation reaction.
[0049]1 g of bis(aminoethylacylmethylethyl) octadecylamine (C18N3, according to literature Wang, W.; Lu, W.S.; Jiang, L. Influence of pH on the aggregation morphology of a novel surfactant with single hydrocarbon chain and multi -amine headgroups.J.Phys.Chem.B.2008,112,1409-1413 prepared by the method disclosed, the same below) was added to 150mL deionized water and stirred evenly to obtain a solution containing surfactant. Add 15g of silicon dioxide to the above-mentioned surfactant-containing solution at a temperature of 40°C and stir for 20 hours, then use a Buchner funnel to carry out suction filtration, and the isolated solid product is rinsed with deionized water, and then at 50 and drying at ℃ for 5 hours to obtain a catalyst carrier solidly loaded with surfactant. Prepare a chloro...
Embodiment 2
[0052] This embodiment is used to illustrate the hydrogenation catalyst provided by the present invention, its preparation method and application, and the method of hydrogenation reaction.
[0053] Add 1 g of bis(aminoethylacylmethylethyl) octadecylamine (C18N3) into 150 mL of deionized water and stir evenly to obtain a solution containing a surfactant. Add 10g of silicon dioxide to the above surfactant solution at 40°C and stir for 20 hours, then use a Buchner funnel to carry out suction filtration, and rinse the isolated solid product with deionized water, then place it at 50°C Drying for 5 hours under the hood to obtain a catalyst carrier solidly loaded with surfactant. Prepare a chloroplatinic acid solution with a concentration of 0.00086mol / L. The above-mentioned catalyst carrier immobilized with surfactant was immersed in the above-mentioned chloroplatinic acid solution with an equal volume for 5 hours, and then dried overnight at 120° C. to obtain Sample 1. Add sample...