Embodiment 1
[0027] Under the condition of 300r / min stirring, firstly add 25kg water-based polyurethane resin into the mixer, start stirring; then add 0.2kg defoamer, 25kg slow drying agent, 0.5kg wetting agent, 1kg penetrating agent, 4kg thickening agent and 44.3kg of water was fully stirred evenly to prepare the water-based color-matching treasure base material.
[0028] Among them, the slow drying agent includes glycerol, film-forming accelerator OE300 and alcohol fat 12, and the weight ratio of glycerol, film-forming accelerator OE300 and alcohol fat 12 is 8:3:2.
Embodiment 2
[0030] Under the stirring condition of 300r / min, first add 25kg of water-based polyurethane resin into the mixer, start stirring; then add 0.2kg of defoamer, 30kg of slow drying agent, 0.5kg of wetting agent, 1kg of penetrant, 4kg of thickener and 39.3kg water,
[0031] Stir fully and evenly to prepare the water-based triser base material.
[0032] Among them, the slow drying agent includes glycerol, film-forming accelerator OE300 and alcohol fat 12, and the weight ratio of glycerol, film-forming accelerator OE300 and alcohol fat 12 is 8:3:2.
Embodiment 3
[0034] Under the condition of stirring at 300r / min, first add 25kg of water-based polyurethane resin into the mixer, start stirring; then add 0.2kg of defoamer, 35kg of slow drying agent, 0.5kg of wetting agent, 1kg of penetrating agent, 4kg of thickener and 34.3kg water,
[0035] Stir fully and evenly to prepare the water-based triser base material.
[0036] Among them, the slow drying agent includes glycerol, film-forming accelerator OE300 and alcohol fat 12, and the weight ratio of glycerol, film-forming accelerator OE300 and alcohol fat 12 is 8:3:2.