Leather polishing agent
A technology of leather and carnauba, applied in the field of leather care, can solve the problems of wrinkles, cortex mildew, cracking, etc., and achieve the effect of reasonable formula, remarkable effect and convenient use
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] Leather polishing agent, comprising the following components by weight: 20 parts of glazing wax, 4 parts of carnauba wax, 6 parts of beeswax, 10 parts of polyurethane, 10 parts of white oil, 3 parts of methacrylic acid, cetyl trimethyl 10 parts of base, 4 parts of ditetraylaminoethyl methacrylate, 30 parts of isooctyl acrylate, 6 parts of hydroxyethyl methacrylate, 3 parts of glycerin, and 0.4 parts of persulfate.
[0009] Stir methacrylic acid, isooctyl acrylate and hydroxyethyl methacrylate evenly at room temperature, and emulsify for 30 minutes, then raise the temperature to 80°C and add other raw materials, stir evenly, and let it dry to room temperature to be the finished product.
Embodiment 2
[0011] A leather polish, comprising the following components by weight: 25 parts of glazing wax, 7 parts of carnauba wax, 8 parts of beeswax, 15 parts of polyurethane, 15 parts of white oil, 4 parts of methacrylic acid, cetyl trimethyl 13 parts of base, 6 parts of ditetraylaminoethyl methacrylate, 40 parts of isooctyl acrylate, 7 parts of hydroxyethyl methacrylate, 4 parts of glycerol, and 0.6 parts of persulfate.
[0012] Stir methacrylic acid, isooctyl acrylate and hydroxyethyl methacrylate evenly at room temperature, and emulsify for 30 minutes, then raise the temperature to 80°C and add other raw materials, stir evenly, and let it dry to room temperature to be the finished product.
Embodiment 3
[0014] A leather polish, comprising the following components by weight: 30 parts of glazing wax, 10 parts of carnauba wax, 10 parts of beeswax, 20 parts of polyurethane, 20 parts of white oil, 5 parts of methacrylic acid, cetyl trimethyl 16 parts of base, 8 parts of ditetraylaminoethyl methacrylate, 50 parts of isooctyl acrylate, 8 parts of hydroxyethyl methacrylate, 5 parts of glycerin, and 0.8 parts of persulfate.
[0015] Stir methacrylic acid, isooctyl acrylate and hydroxyethyl methacrylate evenly at room temperature, and emulsify for 30 minutes, then raise the temperature to 80°C and add other raw materials, stir evenly, and let it dry to room temperature to be the finished product.