[0016] A new type of ink for rotary printing, the ink includes the following components in parts by weight: 8 parts of acrylic emulsion, 5 parts of vinyl acetate-ethylene copolymer emulsion, 4 parts of glycidyl acrylate, hydroxypropyl methylcellulose 3 parts of nitrocellulose, 0.5 parts of nitrocellulose, 0.8 parts of dioctyl phthalate, 3 parts of hydroxypropyl methacrylate, 5 parts of butyl acetate, 3 parts of silicone modified polyester resin, 3 parts of fumaric acid , 5 parts of ethanol, 3 parts of cis-9-octadecenoic acid methyl ester, 1 part of dimethyl siloxane, 3 parts of C9 petroleum resin, 1 part of polyethylene glycol, 0.5 part of preservative, 0.2 part of defoamer 3 parts, dye 3 parts.
[0017] The above components are calculated as 1 kg per part. Stir at 45-50°C at a speed of 300-500r / min. Add the liquid component while stirring. After all the liquid components are added, adjust the speed to 1000-2000r / min and stir. After 30-50 minutes, add preservatives, defoamers...
Embodiment 2
[0019] A new type of ink for rotary printing, the ink includes the following components in parts by weight: 12 parts of acrylic emulsion, 3 parts of vinyl acetate-ethylene copolymer emulsion, 6 parts of glycidyl acrylate, hydroxypropyl methylcellulose 1 part of cellulose, 2 parts of nitrocellulose, 0.2 parts of dioctyl phthalate, 8 parts of hydroxypropyl methacrylate, 2 parts of butyl acetate, 5 parts of silicone modified polyester resin, 1 part of fumaric acid , 8 parts of ethanol, 2 parts of cis-9-octadecenoic acid methyl ester, 3 parts of dimethyl siloxane, 1 part of C9 petroleum resin, 1.5 parts of polyethylene glycol, 0.1 part of preservative, 0.3 part of defoamer 1 part, dye 1 part.
[0020] The above components are calculated as 1 kg per part. Stir at 45-50°C at a speed of 300-500r / min. Add the liquid component while stirring. After all the liquid components are added, adjust the speed to 1000-2000r / min and stir. After 30-50 minutes, add preservatives, defoamers, and o...
Embodiment 3
[0022] A new type of ink for rotary printing, the ink includes the following components in parts by weight: 8 parts of acrylic emulsion, 4 parts of vinyl acetate-ethylene copolymer emulsion, 6 parts of glycidyl acrylate, hydroxypropyl methylcellulose 1 part of cellulose, 1 part of nitrocellulose, 0.8 parts of dioctyl phthalate, 3 parts of hydroxypropyl methacrylate, 3 parts of butyl acetate, 5 parts of silicone modified polyester resin, 1 part of fumaric acid , 6 parts of ethanol, 3 parts of cis-9-octadecenoic acid methyl ester, 1 part of dimethyl siloxane, 2 parts of C9 petroleum resin, 1.5 parts of polyethylene glycol, 0.1 part of preservative, 0.3 part of defoamer 3 parts, 3 parts of dye, 2 parts of 2-methyl-2,4-pentanediol, 3 parts of methyl oleate, 3 parts of vinyl siloxane.
[0023] The above components are calculated as 1 kg per part. Stir at 45-50°C at a speed of 300-500r / min. Add the liquid component while stirring. After all the liquid components are added, adjust th...