A core-shell structure, zinc oxide technology, applied in non-active ingredients medical preparations, active ingredients-containing medical preparations, drug combinations, etc., can solve problems such as environmental pollution, animal intestinal discomfort, pollution of groundwater, etc. The effect of reducing soil environmental pollution, reducing breeding costs, and reducing zinc emissions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Weigh 200g of zinc oxide, spray a small amount of water into the granulation equipment, and bind the zinc oxide into small particles. Weigh 300g of montmorillonite powder, gradually add it to the granulation equipment equipped with zinc oxide particles, start the equipment to make the montmorillonite powder evenly adhere to the surface of zinc oxide particles, and add an appropriate amount of water to promote the adhesion of montmorillonite powder . Then 6g of alginate was dissolved in the mixed solution of alcohol and water, and sprayed onto the surface of zinc oxide / montmorillonite particles to form a layer of gastric protection film. The granules are dried and sieved to obtain the product.
Embodiment 2
[0031] Weigh 300g of zinc oxide, spray a small amount of starch aqueous solution into the granulation equipment, and sterilize the zinc oxide to bond into small particles. Weigh 600g of montmorillonite powder, gradually add it to the granulation equipment equipped with zinc oxide particles, start the equipment to make the montmorillonite powder evenly adhere to the surface of the zinc oxide particles, and add an appropriate amount of water to promote the adhesion of the montmorillonite powder . Then, 10 g of polyvinyl alcohol acetate phthalate was dissolved in an alcohol-water mixed solution, and sprayed onto the surface of the zinc oxide / montmorillonite particles to form a layer of gastric protection film. The granules are dried and sieved to obtain the product.
Embodiment 3
[0033] Weigh 200g of zinc oxide, spray a small amount of starch aqueous solution into the granulation equipment, and sterilize the zinc oxide to bond into small particles. Weigh 200g of zeolite powder and gradually add it to the granulation equipment equipped with zinc oxide particles, start the equipment to make the montmorillonite powder evenly adhere to the surface of the zinc oxide particles, and add an appropriate amount of water to promote the adhesion of the montmorillonite powder. Then the 15 fatty acid is dissolved in the mixed solution of alcohol and water, and sprayed onto the surface of the zinc oxide / montmorillonite particles to form a gastric protection film. The granules are dried and sieved to obtain the product.
[0034] The coated zinc oxide samples of Examples 1, 2, 3 and common zinc oxide were subjected to a comparison test of diarrhea frequency under the same feeding conditions. The calculation method of food diarrhea frequency is:
[0035] Diarrhea freq...