Closed punching method of TC4 alloy high barrel ring part
An alloy and punching technology, applied in the field of closed punching, achieves the effects of improving dimensional accuracy and batch stability, reducing operation difficulty, and improving appearance quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach
[0015] The main chemical element content (percentage by weight) of the TC4 alloy is: 5.5%-6.8% Al content, 3.5%-4.5% V content, 0.30% Fe content, 0.10% C content, 0.05% N content, The content of H is 0.015%, the content of O is 0.20%, and the balance is Ti.
[0016] The steps of this method are as follows:
[0017] Cut the TC4 alloy into bars according to certain specifications; heat the TC4 alloy bars to 30°C below the phase transition point, and keep warm at 0.6min / mm; The hammer upsets the TC4 alloy bar to a predetermined size; puts the upset TC4 alloy billet 4 into the punching die 1, and puts them together under the press. The outer wall of the punching die 1 has a dovetail groove for fixing , to prevent the punching die 1 and the TC4 alloy blank 4 from moving with the forging hammer, such as figure 1 As shown, the punching die 1 is equipped with a limit pad 2. The pad 2 is designed according to the height of the TC4 alloy blank 4, so that the TC4 alloy blank 4 is flush...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 