Phenolic foaming resin toughened with hydroxyl-terminated nitrile rubber

A technology for toughening hydroxy-terminated nitrile and rubber, which is applied in the field of phenolic foamed resin toughened by hydroxy-terminated nitrile rubber, can solve the problems of poor stability of phenolic resin, inability to achieve homogeneous blending, and uneven rubber distribution. To achieve the effect of short reaction cycle, appropriate hardness and reduced embrittlement

Inactive Publication Date: 2017-05-24
SHENYANG INSTITUTE OF CHEMICAL TECHNOLOGY
View PDF5 Cites 6 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, since the rubber emulsion is a metastable system, homogeneous blending cannot be achieved in the phenolic resin aqueous solution, so the phenolic resin modified by this method has poor stability and is prone to phase separation during use.
In addition, due to the simple physical blending, when the adhesive is cured, the distribution of rubber is not uniform, resulting in poor toughening effect

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] The present invention is a kind of toughened phenolic resin of hydroxy-terminated nitrile rubber, comprising the following steps:

[0028] Set the temperature of the water bath at about 60°C, add 65g of phenol solution into a three-necked flask equipped with a stirring paddle, then add 0.65g of sodium hydroxide and stir evenly for about 5 minutes, and react for half an hour to activate the phenol and separate Add 35g of paraformaldehyde in batches, control the temperature at 60°C within half an hour, keep warm for half an hour after adding all the paraformaldehyde to fully react, then add 5.2g of hydroxy-terminated nitrile rubber, stir magnetically for 10 minutes, and pass N2 protection , slowly raise the temperature to 90°C at a heating rate of 3°C / min, react at constant temperature for about one and a half hours, cool down to 75°C, adjust the pH to 7-8 with acetic acid, dehydrate, and cool the synthesized phenolic resin for 24 hours to obtain modification The target p...

Embodiment 2

[0030] The present invention is a kind of toughened phenolic resin of hydroxy-terminated nitrile rubber, comprising the following steps:

[0031] Set the temperature of the water bath at about 60°C, add 65g of phenol solution into a three-necked flask equipped with a stirring paddle, then add 0.65g of sodium hydroxide and stir evenly for about 5 minutes, and react for half an hour to activate the phenol and separate Add 35g of paraformaldehyde in batches, control the temperature at 60°C within half an hour, keep warm for half an hour to fully react the paraformaldehyde, then add 6.5g of hydroxy-terminated nitrile rubber, stir magnetically for 10 minutes, and pass N2 protection , slowly raise the temperature to 90°C at a heating rate of 3°C / min, react at constant temperature for about one and a half hours, cool down to 75°C, adjust the pH to 7-8 with acetic acid, dehydrate, and cool the synthesized phenolic resin for 24 hours to obtain modification The target phenolic resin.

Embodiment 3

[0033] The present invention is a kind of toughened phenolic resin of hydroxy-terminated nitrile rubber, comprising the following steps:

[0034] Set the temperature of the water bath at about 60°C, add 65g of phenol solution into a three-necked flask equipped with a stirring paddle, then add 0.65g of sodium hydroxide and stir evenly for about 5 minutes, and react for half an hour to activate the phenol and separate Add 35g of paraformaldehyde in batches, control the temperature at 60°C within half an hour, keep warm for half an hour to fully react the paraformaldehyde, then add 9.75g of hydroxy-terminated nitrile rubber, stir magnetically for 10 minutes, and pass N2 protection , slowly raise the temperature to 90°C at a heating rate of 3°C / min, react at constant temperature for about one and a half hours, cool down to 75°C, adjust the pH to 7-8 with acetic acid, dehydrate, and cool the synthesized phenolic resin for 24 hours to obtain modification The target phenolic resin. ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides phenolic foaming resin toughened with hydroxyl-terminated nitrile rubber and relates to phenolic foaming resin. The phenolic foaming resin is prepared from components a follows: phenolic compounds, aldehyde compounds, a modifier and a catalyst. The phenolic foaming resin is prepared through steps as follows: (1), the fused phenolic compounds and the basic catalyst are mixed, put in a water bath kettle and heated to 60 DEG C; (2), the aldehyde compounds are added in batches, and the addition is controlled to be finished within half an hour; (3), heat is preserved for half an hour after the aldehyde compounds are added completely, and the aldehyde compounds are enabled to react completely; (4), the modifier is added, a mixture is put in a magnetic stirrer, stirred for 10 min, heated, subjected to a reaction at the constant temperature for an hour and a half and cooled, PH is regulated to be 7-8 with a PH regulator, dehydration and cooling are performed for 24 h, and the modified target phenolic resin can be obtained. The modified phenolic resin has good mechanical properties and overall performance.

Description

technical field [0001] The invention relates to a phenolic foaming resin, in particular to a phenolic foaming resin toughened by hydroxy-terminated nitrile rubber. Background technique [0002] Phenolic resin is formed by polycondensation of phenol formaldehyde or its derivatives. It has excellent properties such as high bonding strength, high carbon residue rate, low smoke and low toxicity, and various processing forms. It has become an indispensable raw material in contemporary industry. It has a wide range of applications in the fields of electronics, construction, printing, and aerospace. However, traditional phenolic resins still have shortcomings such as insufficient heat resistance, poor toughness, and easy absorption of water and moisture. [0003] Patent CN 200810060760 adopts the rubber toughening method to modify the phenolic resin, and also achieves the toughening effect to a certain extent. The specific technical route is to improve the toughness of the phenol...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C08G8/28
CPCC08G8/28
Inventor 葛铁军王成城王佳唐恺鸿徐志华
Owner SHENYANG INSTITUTE OF CHEMICAL TECHNOLOGY
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products