Preparation process of rolling brush
A preparation process, rolling brush technology, applied in the direction of rayon manufacturing, conjugated rayon, fiber chemical characteristics, etc., to achieve the effect of good adsorption, small bristles, and simple preparation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A kind of preparation process of rolling brush, described rolling brush comprises inner tube and bristle, and described inner tube is made of modified ore material; The preparation process of described rolling brush comprises the following steps:
[0020] (1) Prepare the inner tube; the modified ore material is made of the following raw materials in parts by weight: 10 parts of fly ash, 15 parts of epoxy resin, 5 parts of diatomite, 4 parts of zinc octadecanoate, glass powder 3 parts, 2 parts of melamine, 4 parts of kaolin, 4 parts of paraffin oil, 2 parts of molybdenum oxide, 2 parts of crosslinking agent, 2 parts of isomeric tridecanol; The preparation method of the modified ore material comprises the following steps: Under the protection of dry nitrogen, put fly ash, epoxy resin, diatomite, glass powder, molybdenum oxide, kaolin and melamine into the closed reaction kettle equipped with thermometer, stirring device and reflux condenser, and add a certain amount of eth...
Embodiment 2
[0024] A kind of preparation process of rolling brush, described rolling brush comprises inner tube and bristle, and described inner tube is made of modified ore material; The preparation process of described rolling brush comprises the following steps:
[0025] (1) Prepare the inner tube; the modified ore material is made of the following raw materials in parts by weight: 17 parts of fly ash, 28 parts of epoxy resin, 11 parts of diatomite, 8 parts of zinc octadecanoate, glass powder 6 parts, 8 parts of melamine, 8 parts of kaolin, 7 parts of paraffin oil, 7 parts of molybdenum oxide, 4 parts of crosslinking agent, 5 parts of isomeric tridecanol; The preparation method of described modified ore material comprises the following steps: Under the protection of dry nitrogen, put fly ash, epoxy resin, diatomite, glass powder, molybdenum oxide, kaolin and melamine into the closed reaction kettle equipped with thermometer, stirring device and reflux condenser, and add a certain amount...
Embodiment 3
[0029] A kind of preparation process of rolling brush, described rolling brush comprises inner tube and bristle, and described inner tube is made of modified ore material; The preparation process of described rolling brush comprises the following steps:
[0030] (1) Prepare the inner tube; the modified ore material is made of the following raw materials in parts by weight: 14 parts of fly ash, 22 parts of epoxy resin, 7 parts of diatomite, 6 parts of zinc octadecanoate, glass powder 4 parts, 5 parts of melamine, 7 parts of kaolin, 5 parts of paraffin oil, 6 parts of molybdenum oxide, 3 parts of crosslinking agent, 4 parts of isomeric tridecanol. The preparation method of the modified ore material comprises the following steps: under the protection of dry nitrogen, put fly ash, epoxy resin, diatomite, glass powder, molybdenum oxide, kaolin and melamine, add a certain amount of ethanol solution, heat up to 95°C for 1 hour, cool down to 48°C, add zinc octadecanoate, paraffin oil,...