Embodiment 1
[0026] A variable color pigment, comprising the following components by weight: 30 parts of kaolin, 5 parts of white carbon black, 8 parts of color-changing fine powder, 5 parts of montmorillonite, 0.5 parts of sodium oleate, 1 part of Aminopropylamine dioleate, 30 parts of ethanol, 3 parts of ethylene glycol and 1 part of water. Wherein the discoloration micropowder is obtained by the following method: dissolving phenolphthalein and carboxymethyl cellulose in 30% ethanol aqueous solution, then adding No. 200 solvent oil, slowly adding absolute ethanol, and obtaining the discoloration micropowder after evaporating the solvent.
Embodiment 2
[0028] A color-changing pigment, comprising the following components by weight: 40 parts of calcium sulfate, 10 parts of talcum powder, 6 parts of color-changing micropowder, 10 parts of montmorillonite, 1 part of aminopropylamine dioleate, 15 parts of acetone, 3 parts of polyethylene glycol, 5 parts of ethylene glycol and 2 parts of water. Wherein the color-changing micropowder is prepared by the following method: dissolving methyl orange and carboxymethyl cellulose in 30% ethanol aqueous solution, then adding No. 200 solvent oil, slowly adding absolute ethanol, and obtaining the color-changing micropowder after evaporating the solvent.
Embodiment 3
[0030] A color-changing pigment, comprising the following components by weight: 40 parts of calcium sulfate, 10 parts of talcum powder, 6 parts of color-changing micropowder, 10 parts of montmorillonite, 1 part of aminopropylamine dioleate, 15 parts of acetone, 3 parts of polyethylene glycol, 5 parts of ethylene glycol and 2 parts of water. Wherein the color-changing micropowder is prepared by the following method: dissolving litmus and carboxymethyl cellulose in 30% ethanol aqueous solution, then adding No. 200 solvent oil, slowly adding absolute ethanol, and obtaining the color-changing micropowder after evaporating the solvent.
PUM
| Property | Measurement | Unit |
|---|---|---|
| flash point | aaaaa | aaaaa |
| surface tension | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com