A soybean oil and silicon dioxide technology, applied in coatings, wax coatings, etc., can solve the problems of environmental protection performance, reduced beautification effect, and reduced gloss, so as to achieve the effect of not causing environmental pollution and ensuring the durability of use.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] A wall beautification varnish comprising the following components in parts by mass:
[0022] 8-10 parts of vinyl chloride resin liquid, 6-8 parts of pine resin, 10-12 parts of liquid paraffin, 4-8 parts of polyethylene wax, 3-6 parts of silicon dioxide, 5-10 parts of peanut protein, coating film enhancer 2-4 parts, 40-50 parts of organic solvent, 3-5 parts of soybean oil, 1-3 parts of waterproofing agent.
[0023] The preparation method of above-mentioned formula:
[0024] 1), mix 8-10 parts of vinyl chloride resin liquid, 6-8 parts of pine resin, 10-12 parts of liquid paraffin, 4-8 parts of polyethylene wax, 3-6 parts of silicon dioxide, 5-10 parts of peanut protein, 2-4 parts of coating film enhancer, 40-50 parts of organic solvent, 3-5 parts of soybean oil, 1-3 parts of water repellent, add water and mix until liquid, and fully stir to prepare mixture A;
[0025] 2) Stir the mixture A prepared in step 1, put it in a heater, and continue heating for 24-30 minutes, s...
Embodiment 2
[0027] A wall beautification varnish comprises the following components in parts by mass:
[0028] 8 parts of vinyl chloride resin solution, 6 parts of pine resin, 10 parts of liquid paraffin, 4 parts of polyethylene wax, 3 parts of silicon dioxide, 5 parts of peanut protein, 2 parts of coating enhancer, 40 parts of organic solvent, 3 parts of soybean oil , 1 part of waterproofing agent.
Embodiment 3
[0030] A wall beautification varnish comprising the following components in parts by mass:
[0031] 9 parts of vinyl acetate resin, 7 parts of pine resin, 11 parts of liquid paraffin, 6 parts of polyethylene wax, 4 parts of silicon dioxide, 7 parts of peanut protein, 3 parts of coating enhancer, 45 parts of organic solvent, 4 parts of soybean oil , 2 parts of waterproofing agent.