A corrugated box and compound adhesive technology, applied in the direction of adhesive types, starch adhesives, adhesive additives, etc., can solve the problems of unstable cardboard performance, low adhesive performance, easy mildew damage, etc., and achieve easy Procurement, simple production process, good film formation and toughness effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] A composite glue for corrugated boxes, the composite glue for corrugated boxes is formed by mixing two components A and B at a weight ratio of 4:1, and the A component includes the following substances in weight percentage: cassava flour 20 %, sodium hydroxide 1%, lignin 1%, potassium permanganate 0.5%, urea-formaldehyde resin 1%, borax 0.1%, tributyl phosphate 1%, glycerol 0.5%, and the balance is water; the B The components include the following substances in terms of weight percentage: 10% of polyvinyl alcohol, 20% of formaldehyde, and the balance is water.
Embodiment 2
[0012] A composite glue for corrugated boxes, the composite glue for corrugated boxes is formed by mixing two components A and B at a weight ratio of 4:1, and the A component includes the following substances in weight percentage: cassava flour 25 %, sodium hydroxide 1%, lignin 1.5%, potassium permanganate 0.5%, urea-formaldehyde resin 2%, borax 0.5%, tributyl phosphate 1%, glycerol 1%, and the balance is water; the B The components include the following substances in terms of weight percentage: 20% of polyvinyl alcohol, 25% of formaldehyde and the balance of water.
Embodiment 3
[0014] A composite glue for corrugated boxes, the composite glue for corrugated boxes is formed by mixing two components A and B at a weight ratio of 4:1, and the A component includes the following substances in weight percentage: cassava flour 30 %, sodium hydroxide 2%, lignin 2%, potassium permanganate 1%, urea-formaldehyde resin 2%, boron 0.5%, tributyl phosphate 2%, glycerol 1%, and the balance is water; the B The components include the following substances in weight percentage: 20% of polyvinyl alcohol, 30% of formaldehyde, and the balance is water.