A kind of amoled display panel structure and preparation method thereof
A technology for display panels and packaging substrates, used in semiconductor/solid-state device manufacturing, identification devices, instruments, etc., can solve problems such as cracks or fractures, affecting the strength and service life of AMOLED display panels, avoid water vapor intrusion, improve Mechanism strength and service life, the effect of avoiding edge collapse
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0042] Such as figure 2 and image 3 As shown, this embodiment relates to an AMOLED display panel structure, which includes an AMOLED display panel 1 and an outer pin bonding area mechanism 2 arranged on the first side edge of the AMOLED display panel; Adhesive 3 is poured into other side edges other than the edge and the outer lead attaching area mechanism 2, so as to increase the strength of the AMOLED display panel structure.
[0043] In a preferred embodiment of the present invention, the above-mentioned adhesive 3 is ultraviolet glue (UV glue) or silica gel; among them, ultraviolet glue is also called photosensitive glue, ultraviolet light curing glue, and it is a kind of glue that must be irradiated by ultraviolet light to be cured. A type of adhesive that can be used as a bonding agent. Specifically, UV is the abbreviation of Ultraviolet Rays in English, that is, ultraviolet light with a wavelength in the range of 110-400nm. The principle of UV glue curing is that t...
Embodiment 2
[0052] This embodiment relates to a method for preparing an AMOLED display panel structure, and the method specifically includes:
[0053] In step S1, an AMOLED display panel is provided, and the AMOLED display panel includes a package substrate and a polarizer disposed on the package substrate.
[0054] Step S2 , forming an outer pin bonding area mechanism on the first side edge of the AMOLED display panel.
[0055] In a preferred embodiment of the present invention, step S2 specifically includes:
[0056] Step S21 , attaching a protective film on the first side edge of the AMOLED display panel, the protective film fills the height difference between the packaging substrate and the polarizer, and the protective film avoids the bonding area of the touch panel.
[0057] Step S22 , attaching a buffer layer to the side edge of the protective film along the bottom edge of the packaging substrate.
[0058] In a preferred embodiment of the present invention, the buffer layer inc...