[0027] A wood staining method with stable performance, comprising the following steps:
[0028] (1) Preparation of staining agent:
[0029] 1) Weigh 13 parts of aminopropyltrimethoxysilane, 10.5 parts of polyepoxysuccinic acid, 6.5 parts of glyceryl tristearate, 17 parts of modified epoxy resin and 115 parts of sterile water in corresponding weight parts. In the stirring tank, the temperature in the stirring tank is controlled at 210°C, and the stirring process is carried out for 32 minutes;
[0030] 2) Reduce the temperature in the stirring tank in operation 1) to 35°C, and then weigh 42 parts of plant extracts, 5 parts of polyoxyethylene polyoxypropanolamine ether, and 6 parts of nonylphenol polyoxyethylene ether in corresponding weight parts. Put them together in the mixing tank and continue stirring for 2.2 hours;
[0031] (2) Wood pretreatment: the surface of the wood to be dyed is polished, deburred, and then placed in 19% hydrogen peroxide for bleaching treatment, and...
Embodiment 2
[0045] A wood staining method with stable performance, comprising the following steps:
[0046] (1) Preparation of staining agent:
[0047] 1) Weigh 14 parts of aminopropyltrimethoxysilane, 11 parts of polyepoxysuccinic acid, 7 parts of glyceryl tristearate, 18 parts of modified epoxy resin and 120 parts of sterile water in corresponding weight parts. In the stirring tank, the temperature in the stirring tank is controlled at 220°C, and the stirring process is carried out for 35 minutes;
[0048] 2) Reduce the temperature in the stirring tank in operation 1) to 36°C, and then weigh 45 parts of plant extracts, 6 parts of polyoxyethylene polyoxypropanolamine ether, and 7 parts of nonylphenol polyoxyethylene ether in corresponding parts by weight. Put them together in the mixing tank and continue stirring for 2.5 hours;
[0049] (2) Wood pretreatment: the surface of the wood to be dyed is polished, deburred, and then placed in 21% hydrogen peroxide for bleaching treatment, and ...
Embodiment 3
[0063] A wood staining method with stable performance, comprising the following steps:
[0064] (1) Preparation of staining agent:
[0065] 1) Weigh 15 parts of aminopropyltrimethoxysilane, 11.5 parts of polyepoxysuccinic acid, 7.5 parts of glyceryl tristearate, 19 parts of modified epoxy resin and 125 parts of sterile water in corresponding weight parts. In the stirring tank, the temperature in the stirring tank is controlled at 230°C, and the stirring process is carried out for 38 minutes;
[0066] 2) Reduce the temperature in the stirring tank in operation 1) to 37°C, and then weigh 48 parts of plant extracts, 7 parts of polyoxyethylene polyoxypropanolamine ether, and 8 parts of nonylphenol polyoxyethylene ether in corresponding parts by weight. Put them together in the mixing tank and continue stirring for 2.8 hours;
[0067] (2) Wood pretreatment: the surface of the wood to be dyed is polished, deburred, and then placed in 23% hydrogen peroxide for bleaching treatment, ...