Embodiment 1
[0034] Grind a lead-zinc sulfide ore until the content of -0.074mm accounts for 80%, add 400g / t hydrogen peroxide, 500g / t sodium alginate, 120g / t bis(2-methylpropyl)- Sodium dithiophosphonate, 30g / t No. 2 oil, roughing lead sulfide minerals after pulping to obtain lead sulfide roughing concentrate and roughing tailings; add 400g / t seaweed to the lead sulfide roughing concentrate sodium alginate for the first beneficiation, the first beneficiation of the middle ore returns to roughing, the first beneficiation concentrate is then added with 200g / t sodium alginate for the second beneficiation to obtain lead concentrate, the second Return to the first beneficiation in the secondary beneficiation medium ore; add 100g / t bis(2-methylpropyl)-sodium dithiophosphonate to the lead roughing tailings for the first scavenging, and the first scavenging The concentrated ore returns to the rougher, and the scavenging tailings are added with 50g / t bis(2-methylpropyl)-sodium dithiophosphonate fo...
Embodiment 2
[0038]Grind a lead-zinc sulfide ore until the content of -0.074mm accounts for 75%, add 200g / t hydrogen peroxide, 400g / t sodium alginate, 180g / t bis(2-methylpropyl)- Sodium dithiophosphonate, 30g / t No. 2 oil, roughing lead sulfide minerals after pulping to obtain lead sulfide roughing concentrate and roughing tailings; add 200g / t seaweed to the lead sulfide roughing concentrate sodium alginate for the first beneficiation, the first beneficiation of medium ore returns to roughing, the first beneficiation concentrate is added with 100g / t sodium alginate for the second beneficiation to obtain lead concentrate, the second beneficiation Return to the first beneficiation of the middle ore in the beneficiation; add 90g / t bis(2-methylpropyl)-sodium dithiophosphonate to the lead roughing tailings for the first scavenging, the first scavenging The concentrate is returned to the rougher, and 40g / t of bis(2-methylpropyl)-sodium dithiophosphonate is added to the tailings for the second swe...