A production method and technology of brown silk, which is applied in the field of microwave composite brown silk cement plate production, can solve the problems of waste of brown silk and damage to cement structure, etc., and achieve the effects of reducing costs, solving environmental pollution, and enhancing strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] A kind of preparation method of microwave composite brown silk cement plate, comprises the following steps:
[0031] 1) The first is microwave irradiation pretreatment: spread bundles of brown silk (Hainan brown silk, YX-401) on the conveyor belt with a thickness of 2cm, enter the microwave drying tunnel at 200°C for pretreatment, and use 2cm / The speed of S advances, and the whole pretreatment time is about 10 minutes. After the treatment, tiny pores and air passages are formed on the surface of the brown silk, such as figure 1 shown;
[0032] 2) The brown silk after microwave pretreatment enters the modified soaking link: the brown silk is soaked in two modified solution pools, each soaked for about 5 minutes, and the interval between two soaks is 3 minutes; the soaking liquid components in the two modified solution pools are the same, The soaking solution is composed of: water 50wt%, industrial sodium silicate solution (modulus 2.2-2.3, Yigao Chemical Industry) 40wt...
Embodiment 2
[0038] A kind of preparation method of microwave composite brown silk cement plate, comprises the following steps:
[0039]1) The first is microwave irradiation pretreatment: spread the bundled brown silk (Hainan brown silk, YX-401) on the conveyor belt with a thickness of 3cm, enter the microwave drying tunnel at 200°C for pretreatment, and heat the / S speed forward, the whole pretreatment time is about 15min.
[0040] 2) The brown silk after microwave pretreatment enters the modified soaking link: the brown silk is soaked in two modified solution pools, each soaked for about 8 minutes, and the interval between two soaks is 5 minutes; the soaking liquid components in the two modified solution pools are the same, The soaking solution is composed of: water 50wt%, industrial sodium silicate solution (modulus 2.2-2.3, Yigao Chemical Industry) 40wt%, silicon micropowder (800 mesh, produced in Donghai County, Lianyungang) 9.75wt%, industrial latex powder (wa Gram industrial latex ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| modulus | aaaaa | aaaaa |