Water cooling wall tube row structure resistant to falling coke impacting and wearing
A water-cooled wall and pipe row technology, applied in the direction of pipeline damage/abrasion prevention, pipe components, pipe supports, etc., can solve problems such as poor wear resistance, and achieve the effects of ensuring wear resistance, impact protection, and increasing bending strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] see Figure 1-Figure 2 , this embodiment provides a water-cooled wall tube row structure resistant to falling coke impact wear, including tube bodies 1 arranged side by side in sequence, and two adjacent tube bodies 1 are connected by welded tubes 2 to form a tube row. The top of the row is provided with a tube row wear-resistant body 3 that protects the upper half of the tube row. The tube row wear-resistant body 3 includes wear-resistant cladding layers 4 that are connected side by side. A trapezoidal connection wear-resistant body 5 is arranged between the cladding layers 4, and wear-resistant sawtooth rows 6 distributed along the outer wall of the wear-resistant cladding are arranged on each wear-resistant cladding layer 4. The wear-resistant cladding The cladding 4 includes a wear-resistant ceramic sheet 4-1 located on the upper surface, a buffer wear-resistant layer 4-2 is arranged on the lower layer of the wear-resistant ceramic sheet 4-1, and a reinforcing rib i...
Embodiment 2
[0021] see image 3 , this embodiment provides a water-cooled wall tube row structure that is resistant to falling coke impact and wear. In order to improve the impact resistance, the number of reinforcing ribs 4-3 is more than one extending along the length direction of the tube body 1. Moreover, a damping layer 9 is arranged between two adjacent reinforcing ribs 4-3, and the impact resistance is improved by arranging multiple reinforcing ribs 4-3.
[0022] In order to improve the wear resistance, the thickness of the buffer wear-resistant layer 4-2 is 0.5-1mm, and the hardness of the wear-resistant cladding layer is between 600-1000HV.
[0023] In order to facilitate processing, the high temperature resistant cushion cushion 4-4 is compounded with the pipe body 1 through compound glue.
Embodiment 3
[0025] see Figure 4 , this embodiment provides a water-cooled wall pipe row structure that is resistant to defocusing impact wear. In order to improve wear resistance, the wear-resistant sawtooth row 6 is changed into a wear-resistant arc-shaped row 10 with a wavy upper surface. The wear-resistant sawtooth row 6 is changed into a wear-resistant arc-shaped row 10 whose upper surface is wavy, so that the wear resistance of the upper surface is better.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Thickness | aaaaa | aaaaa |
| Hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com