A technology of sample pads and target objects, which is applied in the field of biochemical testing, can solve the problems that the potential of pretreatment tools has not been brought into play, and achieve the effects of reducing the amount of reagents, improving detection efficiency, and reducing applications
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] Embodiment 1. prepares modified sample pad by immersion physisorption method
[0049] Use tweezers to soak the non-woven fabric sample pad in a methanol solution containing 10 mM 2,2'-(octadecylimino)diethanol for 30 minutes, then place the sample pad in a porous grid rack and dry it at 70°C for 8 Hour. Afterwards, the sample pad is cut into a rectangular block of 4.8×18 mm to obtain a sample pad with long fatty chains on the surface.
Embodiment 2
[0050] Example 2. Preparation of modified sample pads by soaking in situ generation method
[0051] Cut the glass fiber sample pad into small pieces of 4.8×18mm, put them into a Teflon mesh bag, and suspend them in 200mL of a mixture of polystyrene, acrylic acid and potassium persulfate (5g of polystyrene, 5g of acrylic acid and Potassium persulfate (0.625g) in deionized water, after nitrogen exchange, was heated up to 75°C and reacted overnight. After the reaction, the mesh bag was taken out, and the glass fiber was dried at 90° C. for 24 hours to obtain a polystyrene-modified sample pad with carboxyl groups on the surface.
[0052] Cut the non-woven sample pad into small pieces of 4.8×18mm, fix it on the wall of a 500mL beaker with a magnet, add 200mL of 10mM ethanol solution of 2-phenylethyltrichlorosilane into the beaker, heat and stir under magnetic force Stir in a container and heat to 60°C. Then, 7.5 mL of 0.1M ammonia water was added dropwise thereto, keeping 1 drop / ...
Embodiment 3
[0053] Example 3. Preparation of silanol-modified sample pads by coating physical adsorption
[0054] Grind 5g of 300-mesh to 400-mesh silicon dioxide, 30ml of water and 0.5% sodium carboxymethylcellulose in a mortar for 30 minutes, pour it on the glass fiber sample pad, spread it flat with a spreader, and let it air in the air After drying for 48 hours and drying at 60° C. for 2 hours, a sample pad whose surface is modified with silanol can be obtained.
[0055] The preparation method of the non-woven fabric sample pad modified by silanol is similar, the only difference is that the non-woven fabric is used as the sample pad.