A manufacturing method and anti-chip technology, which is applied in the manufacture of optical record carriers, optical record carriers, etc., can solve the problems of high production cost of optical discs, errors in writing data on optical discs, and cumbersome processing processes, etc., so as to maintain flatness, The effect of ensuring production quality and correctness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] In the overall injection, it contains 60% of acrylate resin, 32% of trimethylolpropane triacrylate (TMPTA) and its EO.PO modified monomer, 5% of Irgacure-184 photosensitizer, and 3% of The wax is in a viscosity state of 40-50cps / 25°. Under the working condition of the surface temperature of the optical disc at 35°C, the injection is applied to the surface of the data reading and writing surface of the optical disc by means of centrifugal coating, and the injection is confirmed. After coating, irradiate the injection with ultraviolet light for 5 seconds, so that the ingredients in the injection can be converted into a light-transmitting film with a film thickness of 0.01±0.002mm with a hardness between 2H-7H , the anti-scratch surface of the optical disc is formed by the light-transmitting film, so as to form an effective anti-scratch effect on the data reading and writing surface of the optical disc, and keep the data reading and writing surface smooth, so as to increase...
Embodiment 2
[0026] The overall injection contains 60% acrylate resin, 24.5% monomer, 12.5% Irgacure-184 sensitizer, and 3% wax to form a viscosity state of 40-50cps / 25°. Under the working condition of 47°C, the injection agent is applied to the surface layer of the data reading and writing surface of the optical disc by means of centrifugal coating, and after the injection agent is coated, the injection agent is irradiated with ultraviolet light for 2.5 seconds.
Embodiment 3
[0028] In the overall injection, it contains 60% of acrylate resin, 17% of trimethylolpropane triacrylate (TMPTA) and its EO.PO modified monomer, 20% of Irgacure-184 photosensitizer, and 3% of Silane has a viscosity state of 40-50cps / 25°. Under the working condition of the surface temperature of the optical disc at 60°C, the injection agent is applied to the surface layer of the data reading and writing surface of the optical disc by means of centrifugal coating, and the injection agent After the application was confirmed, the injection was irradiated with ultraviolet rays for 1 second.
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |