METHOD FOR THE RECOVERY OF INDIUM FROM A SUBSTRATE CONTAINING INDIUM TIN OXIDE AND A METAL LAYER BY METHOD OF A GREEN CHEMICAL PROCESS

DE602023025952T2Active Publication Date: 2026-11-18COMMISSARIAT A LENERGIE ATOMIQUE ET AUX ENERGIES ALTERNATIVES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602023025952
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-03-24
Filing Date
2023-03-24
Publication Date
2026-11-18
Estimated Expiration
2043-03-24
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD

[0001] The present invention relates to the general field of photovoltaic panel recycling.

[0002] The invention relates more particularly to a method of recovering silver from a photovoltaic panel, containing for example crystalline silicon photovoltaic cells.

[0003] The invention is particularly interesting because it allows the indium present in photovoltaic cells to be recovered through green chemistry. PREVIOUS STATE OF THE ART

[0004] The recycling of photovoltaic (PV) panels has become a major issue since August 13, 2012, when the Waste Electrical and Electronic Equipment (WEEE) Directive was extended to photovoltaic (PV) panels.

[0005] Photovoltaic panels typically comprise several photovoltaic cells embedded in a polymer, arranged between two plates, for example, made of glass. Existing photovoltaic cells can, for example, be made of silicon. By way of illustration and not limitation, a silicon heterojunction cell (HJT) can comprise a monocrystalline silicon substrate coated on both sides with layers of amorphous silicon (P and N+). These layers are themselves covered with a transparent conductive oxide (OTC) film and then with a conductive grid.

[0006] Thus, a photovoltaic module with silicon photovoltaic cells is primarily composed of glass (74% of the total weight), aluminum (10%), polymer (approximately 6.5%), and silicon (approximately 3%). Metals (zinc, lead, copper, and silver) represent only a negligible portion of the total mass of the photovoltaic panel.

[0007] The minimum objectives for recovery and recycling of photovoltaic systems are therefore easily achieved by simply recovering the glass and the aluminum frame.

[0008] Current processes focus on dismantling modules by chemical or thermal means and then recycling the different elements through specialized reprocessing methods.

[0009] Silver represents the metal with the highest added value (nearly 90% of the cell's value). Therefore, silver recovery is a major challenge for ensuring the sustainability of the recycling sector.

[0010] It is also of interest to recover the silicon wafers and metals from the conductive transparent oxide layers.

[0011] Typically, the photovoltaic cells in photovoltaic modules are chemically treated by completely dissolving the metallic elements (Cu, Ag, Sn, Pb, Al, etc.), the anti-reflective coatings, and the n-doped layer to recover the silicon. Dissolution can be carried out in treatment baths composed of various acids (e.g., HF, HNO3, H2SO4) concentrated alone or in mixtures, and often brought to a boil.

[0012] For example, CN 102 343 352 A describes a multi-step process for recovering silicon wafers without damaging the antireflective coating or the PN junction. The process is divided into several steps. First, organic solvents such as ethanol, acetone, or isopropyl alcohol are used to dissolve the organic portion of the metallization and thus separate it from the silicon wafer. This step can be carried out using ultrasound. Next, nitric acid (50–65 wt.) or sulfuric acid (70–98 wt.) is used to remove any remaining metal and glass residues. Then, hydrochloric acid is used to remove metal ions. Finally, a final cleaning with hydrofluoric acid removes any remaining silicon oxide. Between each step, the cells are rinsed with water. Thus, the silicon wafer can be recycled.

[0013] US Patent 2011 / 0083972 A1 describes an electrolytic process for recycling active elements, specifically aimed at removing the transparent conductive oxide coating, for example, indium tin oxide (ITO). The substrate is immersed in an acidic (hydrochloric or sulfuric acid) or basic (sodium or potassium hydroxide) bath. It is connected to a DC power source, to which a voltage is applied so that it acts as a cathode (negative electrode). The cathodic potential generates protons that cause the coating to dissolve. The system is closed with an anode immersed in the solution and connected to the power source. This electrolytic process does not address silver recovery. US Patent 2015 / 233004 A1 discloses a process for the selective recovery of indium and tin from ITO waste by sequential dissolution and deposition.

[0014] However, these processes have many disadvantages, particularly due to the nature of the chemical baths and the complexity of the processes (numerous steps).

[0015] This is why the most recent work uses ionic liquids to dissolve and / or recover the elements.

[0016] Recently, it has been demonstrated that the chemical dissolution and electrochemical recovery of silver from ionic liquids in the presence of a redox mediator can be achieved using a two-step process (EP 3178576 A1). In the first step, silver is dissolved in a solution comprising an ionic liquid and a redox mediator. This solution ensures the chemical dissolution of silver under atmospheric conditions (air). In the second step, the silver is recovered by electrolysis in metallic form. Simultaneously with the silver deposition, the redox mediator is regenerated in the ionic liquid medium.

[0017] However, the process uses ionic liquids that are expensive and not biodegradable. Furthermore, this process does not disclose the recovery and valorization of indium.

[0018] Currently, the processes used for silver recovery are complex, costly, reagent-intensive and / or dangerous, and therefore entail a significant economic and environmental cost.

[0019] Thus, none of the current processes allow for the satisfactory recovery of silver and indium. DESCRIPTION OF THE INVENTION

[0020] One aim of the present invention is to propose a process for recovering indium present in a substrate containing indium tin oxide and a metallic layer of a platinum group metal or silver, the substrate originating for example from a photovoltaic module to be recycled, the process being simple to implement, inexpensive and not requiring the use of any product toxic to the environment and / or to the health of the people implementing the process.

[0021] To this end, the present invention as defined by claim 1 proposes a method for recovering indium contained in a substrate comprising an indium-tin oxide film locally covered by a metallic layer, in silver or in a metal of the platinum group, the method comprising a dissolution step during which the substrate is immersed in a dissolution solution comprising a deep eutectic solvent selected from relin, malin and oxalin, thereby selectively dissolving the indium-tin oxide, the dissolution of the indium-tin oxide leading to the release of the metallic layer.

[0022] The invention differs fundamentally from the prior art by its use of deep eutectic solvents (DES). DES are solvents formed by mixing two or more compounds in a precise proportion that corresponds to the eutectic point. Most of these solvents are liquid at room temperature, which facilitates their use. DES are non-volatile, non-flammable, and chemically stable at temperatures up to 200 °C.

[0023] The synthesis of DESs is easy and clean compared to that of ionic liquids, which require several steps of chemical synthesis and purification. DESs are obtained by simply mixing the components in the correct proportions, possibly with heating the mixture, until a homogeneous and transparent liquid is obtained. DESs are composed of a pair consisting of a hydrogen bond donor and a hydrogen bond acceptor.

[0024] The preparation of the solvents requires no chemical reaction and, therefore, the production yield is 100%. It is a simple mixing of the DES component products in the correct proportions with heating, until a homogeneous and transparent liquid is obtained.

[0025] DES allows the indium-tin oxide layer to be dissolved and the metallic layer to be recovered in solid form by way of green chemistry, unlike processes using ionic liquids.

[0026] According to a particularly advantageous embodiment, the deep eutectic solvent is oxaline.

[0027] Advantageously, the dissolution step is carried out at a temperature between 20°C and 120°C, and preferably between 50°C and 80°C.

[0028] Advantageously, the solid-liquid ratio is between 1 and 40%, and preferably between 10% and 20%.

[0029] Advantageously, the dissolution solution further comprises water, the molar percentage of water relative to the deep eutectic solvent being preferably less than 50%.

[0030] According to a particularly advantageous embodiment, the metallic layer is made of silver.

[0031] Advantageously, the substrate further comprises a support, the indium-tin oxide film being disposed between the support and the metallic layer, the support containing silicon or copper, indium, gallium selenide (CIGS).

[0032] Advantageously, the substrate is a photovoltaic cell or photovoltaic cell waste, for example, a heterojunction cell or a CIGS cell. The metallic layer, preferably silver, forms the current collectors. The process allows for the selective dissolution of the ITO layer of the photovoltaic cell, for example, a silicon heterojunction (HJT) cell, thereby decoupling the collectors from the silicon cell body without dissolving any elements other than the transparent conductive indium tin oxide layer.

[0033] The process avoids the non-selective dissolution of elements and the use of concentrated and hazardous acids. Furthermore, this dissolution is carried out in a green solvent that can withstand numerous treatment cycles, increasing both economic and environmental benefits. This approach limits reagent consumption, eliminates the need for various concentrated acids, and reduces the number of steps.

[0034] According to an advantageous embodiment, the process comprises the following steps: a) supply a photovoltaic panel including cables, a junction box, a metal frame, photovoltaic cells encapsulated in a polymer layer and electrical connectors, b) remove the cables, the junction box and the metal frame from the photovoltaic panel, c) carry out a thermal, chemical and / or mechanical treatment to remove the polymer layer encapsulating the photovoltaic cells, d) recover the photovoltaic cells, the photovoltaic cells forming a substrate containing an indium tin oxide film locally covered by a metallic layer, preferably silver, e) implement the indium recovery step as defined above.

[0035] Advantageously, after the dissolution step, the process includes a subsequent step in which the tin is recovered by, for example, implementing a first tin electrodeposition step and then the indium is recovered by, for example, implementing a second indium electrodeposition step.

[0036] The process offers numerous advantages: The process does not require the use of acidic solutions or ionic liquids; the use of DES (and its potential reuse) eliminates solvent preparation steps, thus reducing costs; DES are biodegradable, which reduces constraints related to safety and / or environmental standards; the process does not release harmful gases and does not degrade the reaction medium; the process can be carried out under atmospheric conditions (in air); the process can be carried out at ambient temperature (typically 25°C), thus avoiding the input of thermal energy; DES are inexpensive solvents, which reduces process costs; DES are easy to prepare and can therefore be prepared in situ, The money is not dissolved and is therefore easily recoverable.

[0037] Other features and advantages of the invention will become apparent from the supplementary description that follows.

[0038] It goes without saying that this additional description is given only as an illustration of the object of the invention and should in no way be interpreted as a limitation of this object. BRIEF DESCRIPTION OF THE DRAWINGS

[0039] The present invention will be better understood upon reading the description of exemplary embodiments given by way of illustration only and in no way limiting, with reference to the accompanying drawings in which: THE figures 1A, 1B and 1C are photographic images of a heterojunction cell (HJT) plate, respectively, before, during, and after treatment in Oxaline according to a particular embodiment of the invention. figure 2 This is an image obtained using a scanning electron microscope on a plate of an HJT photovoltaic cell, before treatment in Oxaline. figure 3This is the EDX spectrum obtained on a plate of an HJT photovoltaic cell, before treatment in Oxaline; the EDX spectrum was obtained within the frame of the figure 2 . There figure 4 is an image obtained by scanning electron microscopy on a plate of an HJT photovoltaic cell, after treatment in Oxalin, according to another particular embodiment of the invention. figure 5 is an EDX spectrum obtained on a plate of an HJT photovoltaic cell, after treatment in Oxaline, according to another particular embodiment of the invention; the EDX spectrum was obtained at the level of the area framed in the figure 4 . DETAILED DESCRIPTION OF SPECIFIC METHODS OF IMPLEMENTATION

[0040] Subsequently, even though the description refers to the valorization of photovoltaic panels or modules; the invention is transferable to other substrates containing indium tin oxide and a metallic layer of silver or a platinum group metal (PGM).

[0041] The process of recycling a photovoltaic panel to recover indium includes the following steps: a) supply a photovoltaic panel, b) remove the cables, junction box and metal frame from the photovoltaic panel, c) carry out a thermal, chemical and / or mechanical treatment to remove the polymer layer encapsulating the photovoltaic cells and electrical connectors, d) recover the photovoltaic cells, the photovoltaic cells forming a substrate containing an indium-tin oxide film locally covered by a metallic layer, and more particularly by a layer containing silver, e) implement an indium recovery step.

[0042] The photovoltaic panel to be recycled includes cables, a junction box and a metal frame, a polymer layer (typically ethyl vinyl acetate (EVA)), electrical connectors and photovoltaic cells.

[0043] The process is described more specifically for a photovoltaic panel, but several photovoltaic panels could be treated simultaneously.

[0044] The photovoltaic cell comprises a substrate with various valuable components. In particular, the substrate may consist successively of a support, a transparent conductive oxide (TCO) film, and a metallization layer partially covering the TCO. The TCO film is thus accessible for etching.

[0045] Subsequently, we will describe in more detail a substrate comprising a support, a transparent conductive oxide film, and a metallic layer. However, the process can also be implemented for a substrate consisting of a transparent conductive film and a metallic layer.

[0046] Photovoltaic cells can be made of crystalline silicon, polycrystalline silicon, CIGS or perovskite.

[0047] A Heterojunction (HJT) cell will be chosen, preferably.

[0048] By way of illustration and not limitation, the HJT cell may comprise a monocrystalline silicon substrate coated on both sides with layers of amorphous silicon (P and N+). The amorphous silicon layers may be approximately ten nanometers thick. These layers are themselves coated with a transparent conductive oxide film and then with a conductive grid.

[0049] In the context of the invention, the TCO film is an indium tin oxide film (or ITO for "Indium Tin Oxide"). The ITO comprises, for example, 97% indium oxide (In2O3) and 3% tin oxide SnO2.

[0050] The metallization layer forms a conductive grid.

[0051] The metallization layer is a metallic layer made of a platinum group metal or silver.

[0052] The platinum group metal is chosen from ruthenium, rhodium, palladium, osmium, iridium, and platinum. Preferably, it is platinum.

[0053] Preferably, the metallic layer is silver. The metallic layer contains at least 0.01% silver by mass of the total mass, and preferably at least 0.035% silver by mass.

[0054] The metallic layer can be made of pure silver (i.e., the layer contains at least 99% silver). It is, for example, made with a silver metallizing paste.

[0055] Alternatively, it may contain one or more other elements, for example, chosen from lead, tin, and copper. The connectors, for example, are formed of a copper core coated with Sn62Pb36Ag2.

[0056] Steps b) and c) allow the photovoltaic cells and the silver-containing electrical connectors to be separated and decoupled from the other components of the photovoltaic panel. Once the photovoltaic cells are decoupled, they are advantageously disconnected from each other and, if necessary, from the non-silver-containing electrical connectors.

[0057] At the end of steps b) and c), the elements of interest of the photovoltaic panel were separated.

[0058] This is how we recover the photovoltaic cells (step d).

[0059] Each photovoltaic cell represents a substrate containing indium and silver to be recovered during step e).

[0060] In step e), a dissolution step is carried out in which the substrate is immersed in a dissolution solution. The dissolution solution comprises a deep eutectic solvent chosen from relin, maline, and oxaline.

[0061] In general, DESs can be grouped into four different families: Type I: Quaternary salt + Metal chloride Type II: Quaternary salt + Hydrated metal chloride Type III: Quaternary salt + Hydrogen bond donor Type IV: Hydrated metal chloride + Hydrogen bond donor

[0062] Deep eutectic solvents are, for example, based on mixtures of quaternary ammonium salts with hydrogen bond donors such as amines and carboxylic acids.

[0063] Advantageously, DES is choline chloride in association with a very low toxicity hydrogen bond donor, such as glycerol, ethylene glycol or urea, which guarantees a non-toxic and very low-cost DES.

[0064] Preferably, DES meets the requirements for thermal stability (> 200 °C) and chemical stability (no hydrolysis). It is liquid at or near room temperature (< 100 °C) and forms numerous associations.

[0065] According to an advantageous embodiment, DES is a natural deep eutectic solvent (or NADES for "Natural Deep Eutectic Solvents"). It is a subcategory of DES based on natural products that can be established; they are named for being prepared by mixing natural constituents. These mixtures include organic acids, sugars, choline, urea, and amino acids.

[0066] Preferred hydrogen bond donors (HBDs) include acids such as oxalic, carboxylic, malonic, urea, and phenylpropionic acid. These are advantageously combined with a hydrogen bond acceptor (HBD), which can be a quaternary ammonium compound and, more commonly, choline chloride (ChCl). The Oxaline system, a 1:1 mixture of ChCl and oxalic acid, is preferred. This system exhibits excellent solubility for ITO.

[0067] The introduction of the substrate into the DES results in the immediate dissolution of the transparent conductive oxide.

[0068] This step prevents the emission of gas (flammability, volatility) and / or the degradation of the solution.

[0069] The dissolution step is carried out at a temperature between 15°C and 80°C, and preferably between 15°C and 40°C, for example at room temperature, i.e., around 25°C. Advantageously, no thermal energy input is required to dissolve the TCO. However, increasing the temperature can advantageously improve the dissolution rate without degrading the medium (for temperatures between 15 and 80°C).

[0070] The solid-to-liquid ratio is between 1% and 45%, and preferably between 1% and 30%. This ratio is denoted S / L. Preferably, the S / L ratio is around 10%. By 10%, we mean 10% ± 1%. The solid phase corresponds to the quantity of material used in step e). The liquid phase corresponds to the deep eutectic solvent. This ratio corresponds to the mass of solid, in grams, divided by the volume of the solution, in milliliters. Thus, an S / L ratio between 1% and 30% corresponds to a mass concentration of the metal oxide in the acidic solution between 0.01 g / mL and 0.3 g / mL. For S / L values ​​below 1%, the dissolution yield is also high. However, the amount of acid used is considerably high compared to the amount of metal to be dissolved, and the amount of reagents lost is significant.

[0071] Silver is not dissolved, or only very slightly dissolved, in the dissolving solution. The dissolution of silver is considered negligible at this stage. The same applies to a platinum group metal.

[0072] Optionally, the solution may also include an additive. For example, this could be a drying agent, and / or an agent that promotes mass transport (viscosity, ionic conductivity).

[0073] For example, the agent facilitating mass transport can be water. The percentage of water relative to the DES is advantageously less than 50% molar, and preferably on the order of 10% molar.

[0074] According to another embodiment, the additive can be gamma-butyrolactone.

[0075] The dissolution step can be carried out under agitation.

[0076] After the indium is dissolved, the silver layer, in solid form, can also be easily extracted from the dissolution solution.

[0077] The tin dissolved in solution can be recovered, for example by a first electrodeposition step.

[0078] Indium dissolved in solution can be recovered by a second electrodeposition step.

[0079] Advantageously, tin will be recovered first, then indium.

[0080] A person skilled in the art can choose different separation / recovery techniques depending on the elements. For example, they can choose to implement: an ion flotation step, sieving, electrostatic separation, sieving, liquid / liquid extraction using a DES-insoluble solvent, more specifically solvents with low polarities, precipitation, or even a zinc cementation step.

[0081] The dissolution solution can then be used for a new treatment cycle.

[0082] Alternatively, several substrates can be successively treated in the dissolution solution before implementing the electrodeposition steps. Illustrative and non-limiting examples of embodiments : Test 1: Dissolution of ITO in DES medium :

[0083] Dissolution tests were performed for four DESs: Relin, Maline, Ethalin, and Oxalin. Dissolution was carried out at 70 °C. Unlike acidic aqueous media, this temperature does not pose a problem with regard to the release of harmful species. The treatment duration was 24 hours with a solid / liquid ratio of 10%, using a mass of ITO (In₂O₃, SnO₂) powder of 543 mg.

[0084] The following table lists the maximum concentrations of indium and tin dissolved from ITO for different DES. The target concentration is a theoretical goal that assumes treatment of HJT cells with a 15% ratio.

[0085] We observe a very significant dissolution in Reline medium, in Maline medium and in Oxaline medium.

[0086] However, no dissolution of indium was observed for the Ethaline medium.

[0087] These results demonstrate the excellent solubility of the transparent layer in certain DES. The results with oxaline are remarkable.

[0088] It was possible to achieve: in Reline medium, successive treatment of 10 batches of HJT cells, in Maline medium, successive treatment of 45 batches of HJT cells, in Oxaline medium, successive treatment of 149 batches of HJT cells. [Table 1] Nature of the DES Dissolved concentration (g / L) Target concentration for an HJT cell with S / L=15% (g / L) In Sn In Sn Reline (ChCl / Urea) 1:2 4,2 8,7 0,420 0,167 Ethaline(ChCl / EthyleneGlycol)1:2 0 8,5 0,420 0,167 Maline (ChCl / Malonic acid)1:1 19,3 8,6 0,420 0,167 Oxalin (ChCl / Oxalic acid) 1:1 62,7 8,6 0,420 0,167 Test 2 : Treatment of an HJT cell in DES-Oxaline medium :

[0089] The selective dissolution of ITO located between the silicon and silver connectors of HJT cells was investigated. The treatment was carried out in Oxaline medium at 70 °C for 4 hours, with a volume of 10 mL of DES. A piece of HJT cell was immersed in the DES bath under agitation at 300 rpm. Before treatment, the piece was intact ( Figure 1A ), during the treatment, the detachment of the silver collectors is observed ( figure 1B ), and after treatment the absence of collectors ( figure 1C ). The dissolution of the layer on which the silver rests causes the physical separation of the silver and silicon. SEM-EDX measurements were performed before and after the treatment ( Figures 2 to 4 Before treatment, the presence of indium is measured ( figures 2 and 3 ), and its absence after treatment ( Figures 4 and 5 ), which confirms the dissolution of ITO on the surface.

Claims

1. Method for recovering indium contained in a substrate comprising an indium tin oxide film locally covered with a metal layer of silver or a metal of the platinum group, the method comprising a dissolving step during which the substrate is immersed in a dissolving solution comprising a deep eutectic solvent selected from among reline, maline and oxaline, whereby the indium tin oxide is selectively dissolved, the dissolving of the indium tin oxide leading to the release of the metal layer.

2. Method according to claim 1, characterised in that the deep eutectic solvent is oxaline.

3. Method according to either of claims 1 and 2, characterised in that the dissolving step is carried out at a temperature of between 20°C and 120°C and preferably between 50°C and 80°C.

4. Method according to any one of the preceding claims, characterised in that the solid to liquid ratio is between 1 and 40% and preferably between 10% and 20%.

5. Method according to any one of the preceding claims, characterised in that the dissolving solution further comprises water, the molar percentage of water with respect to the deep eutectic solvent preferably being less than 50%.

6. Method according to any one of the preceding claims, characterised in that the metal layer is made of silver.

7. Method according to any one of the preceding claims, characterised in that the substrate further comprises a carrier, the indium tin oxide film being disposed between the carrier and the metal layer, the carrier further containing silicon or copper indium gallium selenide (CIGS).

8. Method according to any one of the preceding claims, characterised in that the substrate is a photovoltaic cell or photovoltaic cell waste, for example a heterojunction cell or a CIGS cell.

9. Method according to any one of the preceding claims, characterised in that it comprises the following steps: a) providing a photovoltaic panel comprising cables, a junction box, a metal frame, photovoltaic cells encapsulated in a polymer layer and electrical connectors, b) removing the cables, junction box and metal frame from the photovoltaic panel, c) carrying out a thermal, chemical and / or mechanical treatment to take off the polymer layer encapsulating the photovoltaic cells, d) recovering the photovoltaic cells, the photovoltaic cells forming a substrate containing an indium tin oxide film locally covered with a metal layer, preferably of silver, e) performing the method for recovering indium as defined in one of claims 1 to 8.

10. Method according to any one of the preceding claims, characterised in that after the dissolving step, the method comprises a subsequent step during which the tin is recovered by performing for example a first step of electrochemically depositing tin, then the indium is recovered by performing for example a second step of electrochemically depositing indium.