Optoelectronic devices and methods of making and using thereof

HK40137479APending Publication Date: 2026-09-11YALE UNIVERSITY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
HK62026126330
Authority / Receiving Office
HK · HK
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-06-22
Filing Date
2026-07-17
Publication Date
2026-09-11

Smart Images

  • Figure 00000079_0000
    Figure 00000079_0000
  • Figure 00000079_0001
    Figure 00000079_0001
  • Figure 00000080_0000
    Figure 00000080_0000
Patent Text Reader

Abstract

Various semiconductor structures including buried tunnel junctions or hole regions are described. Further disclosed are methods of making and using such semiconductor structures, e.g., useful in optoelectronic devices, such as vertical cavity surface emitting lasers (VCSEL), that are capable of emitting light at long wavelengths.
Need to check novelty before this filing date? Find Prior Art

Description

(19) State Intellectual Property Office (12) Invention Patent Application (10) Application Publication Number (43) Application Publication Date (21) Application Number 202480041504.X (22) Application Date 2024.06.24 (30) Priority Data 63 / 509,683 2023.06.22 US (85) PCT International Application Entering National Phase Date 2025.12.19 (86) PCT International Application Application Data PCT / US2024 / 035236 2024.06.24 (87) PCT International Application Publication Data WO2024 / 264039 EN 2024.12.26 (71) Applicant Yale University Address Connecticut, USA (72) Inventors Han Zhong, Li Bingjun, Mi Chen Ziyi (74) Patent Agency Beijing Gewen Law Firm 16168 Patent Attorneys Wang Xinhua and Jia Yafei (51) Int.Cl. H01S 5 / 183 (2006.01) H01S 5 / 30 (2006.01) (54) Invention Title: Optoelectronic Device and Method of Manufacturing and Using Therewith (57) Abstract: This invention describes various semiconductor structures including buried tunnel junctions or via regions. Methods for preparing and using such semiconductor structures are further disclosed, for example, for use in optoelectronic devices (such as vertical-cavity surface-emitting lasers, VCSELs) capable of emitting light at long wavelengths. Claims 11 pages, Description 31 pages, Drawings 15 pages, CN 121532916 A 2026.02.13 CN 1 21 53 29 16 A 1. A semiconductor structure including a buried tunnel junction (BTJ), the semiconductor structure comprising: a bottom structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; an n-type doped first semiconductor layer located on top of the bottom structure; a light-emitting structure comprising multiple quantum wells (MQWs) located on top of the n-type doped first semiconductor layer; a p-type doped first semiconductor layer located on top of the light-emitting structure; and a buried tunnel junction (BTJ) present on the p-type doped first semiconductor layer, wherein the buried tunnel junction comprises: a p-type doped second semiconductor layer having a p-type doping level greater than about 1 × 10¹⁸ cm⁻³; An n-type doped second semiconductor layer is located on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having an n-type doping level greater than about 1 × 10¹⁸ cm⁻³; wherein at least the n-type doped second semiconductor layer has a surface area smaller than the surface area of ​​the p-type doped first semiconductor layer; optionally, wherein the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer;An n-type doped current diffusion layer, the n-type doped current diffusion layer encapsulating at least a portion of the n-type doped second semiconductor layer, and optionally also encapsulating at least a portion of the p-type doped second semiconductor layer; wherein the current diffusion layer, excluding the portion having the n-type doped second semiconductor layer thereon, contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and wherein the surface of the current diffusion layer optionally includes a region above the buried tunnel junction, the region being raised and forming a stepped feature to provide an optical confinement effect. 2. The semiconductor structure of claim 1, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide. 3. The semiconductor structure of any one of claims 1-2, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness. 4. The semiconductor structure of any one of claims 1 to 3, wherein the alternating layers of the bottom structure comprise a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, and gallium antimonide; and wherein the alternating layers are lattice-matched to the semiconductor substrate. 5. The semiconductor structure of any one of claims 1 to 4, wherein the alternating layers of the bottom structure comprise a ternary semiconductor material lattice-matched to the semiconductor substrate. 6. The semiconductor structure of any one of claims 1 to 4, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material lattice-matched to the semiconductor substrate. 7. The semiconductor structure of any one of claims 1 to 6, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer comprise one or more semiconductor materials lattice-matched to the semiconductor substrate. 8. The semiconductor structure of claim 7, wherein the one or more semiconductor materials are lattice-matched with the indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the semiconductor material is lattice-matched with the gallium arsenide semiconductor substrate and is selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the semiconductor material is lattice-matched with the gallium antimonide semiconductor substrate and is selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb. 9. The semiconductor structure of any one of claims 1 to 6, wherein the light-emitting structure, the p-type doped second semiconductor layer, and the n-type doped second semiconductor layer each comprise one or more semiconductor materials that are lattice-mismatched with the semiconductor substrate.10. The semiconductor structure of claim 9, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb. 11. A method of fabricating a semiconductor structure including a buried tunnel junction (BTJ), the method comprising the steps of: (i) forming a bottom structure on a semiconductor substrate, the bottom structure including alternating n-type doped layers and undoped or lightly doped semiconductor layers; (ii) depositing an n-type doped first semiconductor layer on top of the bottom structure; (iii) depositing or forming a light-emitting structure including multiple quantum wells (MQWs) on top of the first semiconductor layer; (iv) depositing a p-type doped first semiconductor layer on top of the light-emitting structure; (v) depositing a p-type doped second semiconductor layer on top of the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; (vi) depositing an n-type doped second semiconductor layer on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; (vii) forming or patterning a mask material over a top surface region of the n-type doped second semiconductor layer; (viii) Removing at least the n-type doped second semiconductor layer by etching, and optionally removing the p-type doped second semiconductor layer thereon except for the surface portion having the mask material; (ix) Removing the mask material; and (x) Depositing an n-type doped current diffusion layer, the n-type doped current diffusion layer at least partially enclosing the n-type doped second semiconductor layer, optionally enclosing a portion of the p-type doped second semiconductor layer, and wherein the current diffusion layer outside the surface portion contacts the p-type doped second semiconductor layer or the p-type doped first semiconductor layer. 12. The method of claim 11, wherein any structure or layer can be independently formed or deposited by metal-organic vapor deposition (MOCVD), molecular beam epitaxy (MBE), or liquid phase epitaxy (LPE). 13. The method of any one of claims 11-12, wherein the mask material is selected from the group consisting of dielectric materials and / or photoresists, such as silicon dioxide, silicon nitride, and aluminum oxide. 14. The method of any one of claims 11-13, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide.15. The method of any one of claims 11-14, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness. 16. The method of any one of claims 11-15, wherein the alternating layers of the bottom structure comprise a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, or gallium antimonide; and the alternating layers are lattice-matched with the semiconductor substrate. 17. The method of any one of claims 11-15, wherein the alternating layers of the bottom structure comprise a ternary semiconductor material lattice-matched with the semiconductor substrate. 18. The method of any one of claims 11-15, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material lattice-matched with the semiconductor substrate. 19. The method of any one of claims 11-18, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer comprise one or more semiconductor materials lattice-matched with the semiconductor substrate. 20. The method of claim 19, wherein the one or more semiconductor materials are lattice-matched with an indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the semiconductor material is lattice-matched with a gallium arsenide semiconductor substrate and is selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the semiconductor material is lattice-matched with a gallium antimonide semiconductor substrate and is selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb. 21. The method of any one of claims 11-18, wherein the light-emitting structure, the p-type doped second semiconductor layer, and the n-type doped second semiconductor layer each comprise one or more semiconductor materials that are lattice-mismatched with the semiconductor substrate. 22. The method of claim 21, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb. 23. A light-emitting structure comprising a buried tunnel junction (BTJ), the light-emitting structure comprising:A bottom reflector structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; wherein the n-type doped layers are porous and include multiple pores; and wherein the undoped or lightly doped semiconductor layers are non-porous or substantially non-porous; an n-type doped first semiconductor layer disposed on top of the bottom structure; a light-emitting structure comprising a multiple quantum well (MQW) located on top of the semiconductor layers; a p-type doped first semiconductor layer located on top of the light-emitting structure; and a buried tunnel junction (BTJ) present on a portion of the p-type doped first semiconductor layer, wherein the buried tunnel junction defines a hole region and comprises: a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; and an n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³, located on top of the p-type doped second semiconductor layer. At least the n-type doped second semiconductor layer has a surface area smaller than that of the p-type doped first semiconductor layer; optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; an n-type doped current diffusion layer, the n-type doped current diffusion layer encapsulating at least a portion of the n-type doped second semiconductor layer, optionally encapsulating at least a portion of the p-type doped second semiconductor layer; wherein the current diffusion layer, excluding the portion on which the n-type doped second semiconductor layer is located, contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and wherein the surface of the current diffusion layer optionally includes a region above the buried tunnel junction, the region being raised and forming a stepped feature, thereby producing an optical confinement effect. 24. The light-emitting structure of claim 23, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide. 25. The light-emitting structure of any one of claims 23-24, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness. 26. The light-emitting structure of any one of claims 23-25, wherein the alternating layers of the bottom structure comprise a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, or gallium antimonide; and the alternating layers are lattice-matched with the semiconductor substrate. 27. The light-emitting structure of any one of claims 23-25, wherein the alternating layers of the bottom structure comprise a ternary semiconductor material lattice-matched with the semiconductor substrate.28. The light-emitting structure of any one of claims 23 to 25, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material lattice-matched with the semiconductor substrate. 29. The light-emitting structure of any one of claims 23 to 28, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer comprise one or more semiconductor materials lattice-matched with the semiconductor substrate. 30. The light-emitting structure of claim 29, wherein the one or more semiconductor materials are lattice-matched with the indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the semiconductor material is lattice-matched with the gallium arsenide semiconductor substrate and is selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the semiconductor material is lattice-matched with the gallium antimonide semiconductor substrate and is selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb. 31. The light-emitting structure of any one of claims 23-28, wherein the light-emitting structure, the p-type doped second semiconductor layer, and the n-type doped second semiconductor layer each comprise one or more semiconductor materials that are lattice mismatched with the semiconductor substrate. 32. The light-emitting structure of claim 31, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb. 33. The light-emitting structure of any one of claims 23-32, wherein the porosity is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%. 34. The light-emitting structure according to any one of claims 23-33, wherein there is a refractive index contrast (Δn) between the alternating layers, which ranges from about 0.1 to 2 or about 0.1 to 2.5. 35. A method of forming a light-emitting structure, comprising the steps of: (i') setting or forming a structure including a buried tunnel junction (BTJ), the structure comprising: a bottom structure, the bottom structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; an n-type doped first semiconductor layer located on top of the bottom structure;A light-emitting structure includes a multiple quantum well (MQW) on top of an n-type doped first semiconductor layer; a p-type doped first semiconductor layer on top of the light-emitting structure; and a buried tunnel junction (BTJ) on the p-type doped first semiconductor layer, wherein the buried tunnel junction includes: a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; an n-type doped second semiconductor layer on top of the p-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; wherein at least the surface area of ​​the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer; optionally, wherein the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; and an n-type doped current diffusion layer that encloses at least a portion of the n-type doped second semiconductor layer and optionally encloses at least a portion of the p-type doped second semiconductor layer. The current diffusion layer, excluding the portion having the n-type doped second semiconductor layer thereon, contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and wherein the surface of the current diffusion layer optionally includes a region above the buried tunnel junction, the region being raised and forming a stepped feature to produce an optical confinement effect; (ii') forming a mesa structure by etching the current diffusion layer, the light-emitting structure, the p-type doped first semiconductor layer, and optionally a portion of the p-type doped second semiconductor layer; (iii') depositing a silicon dioxide layer over the mesa structure, wherein at least a portion of the n-type doped first semiconductor layer is not covered by the silicon dioxide layer; (iv') etching the portion not covered by the silicon dioxide layer to form a trench thereby exposing the sidewalls of the alternating layers of the bottom structure; (v') selectively porosilicated the n-type doped semiconductor layers in the alternating layers of the bottom structure, wherein a plurality of pores are formed, and wherein the undoped or low-doped semiconductor layers remain non-porous or substantially non-porous; (vi') depositing one or more materials to cover the trench, the sidewalls, and the sidewalls of the mesa structure; (vii') Selectively remove the one or more materials to expose at least a portion of the top of the mesa structure, and optionally expose a portion of the n-type doped first semiconductor covered by the one or more materials; and (viii') form metal contacts on a portion of the top of the mesa structure and optionally on a portion of the n-type doped first semiconductor. 36. The method of claim 35, wherein the porosity formed in step (v') is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%.37. The method of any one of claims 35-36, wherein step (v') is performed by electrochemical etching in an electrolyte solution and under an applied bias voltage. 38. The method of claim 37, wherein the electrolyte solution comprises halide ions, hydrochloric acid (HCl), sulfuric acid (H2SO4), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)2, Ca(OH)2, Sr(OH)2, NH4OH, NaCl, NaF, nitric acid (HNO3), organic acids and their salts (such as oxalic acid and citric acid), and mixtures thereof. 39. The method of any one of claims 35-38, wherein the one or more materials are selected from the group consisting of silicon dioxide, alumina, silicon nitride, and spin-coated glass; and / or the one or more materials are organic materials selected from the group consisting of benzocyclobutene (BCB), polyimide, and photoresist; and combinations thereof. 40. The method of any one of claims 35-39, wherein the metal contact formed in step (viii') comprises a metal selected from Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof. 41. An optoelectronic device comprising: a light-emitting structure according to any one of claims 23-34; a top distributed Bragg reflector; and metal contacts. 42. The optoelectronic device of claim 41, wherein the top distributed Bragg reflector comprises alternating layers of any one of: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof. 43. The optoelectronic device of any one of claims 41-42, wherein the metal contact comprises one or more metals selected from the group consisting of Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof. 44. The optoelectronic device of any one of claims 41-43, wherein the optoelectronic device is a vertical-cavity surface-emitting laser (VCSEL). 45. The optoelectronic device of claim 44, wherein the VCSEL operates in continuous-wave mode at room temperature (about 25°C). 46. The optoelectronic device of claim 44, wherein the VCSEL operates at a temperature below about 0°C, above about 25°C, or above about 85°C. 47. The optoelectronic device of claim 44, wherein the VCSEL operates in pulsed mode. 48. The optoelectronic device of claim 44, wherein the VCSEL emits in the infrared wavelength region. 49. The optoelectronic device of claim 44, wherein the power conversion efficiency of the VCSEL is...At least approximately 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 7.5%, or 10%. 50. A method of manufacturing an optoelectronic device, comprising the steps of: (i”) setting or forming a light-emitting structure, the light-emitting structure comprising: a bottom mirror structure, the bottom mirror structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; wherein the n-type doped layers are porous structures and include a plurality of pores; and wherein the undoped or lightly doped semiconductor layers are non-porous or substantially non-porous structures; an n-type doped first semiconductor layer located on top of the bottom structure; a light-emitting structure comprising multiple quantum wells (MQWs) located on top of the semiconductor layers; a p-type doped first semiconductor layer located on top of the light-emitting structure; and a buried tunnel junction (BTJ) present on a portion of the p-type doped first semiconductor layer, wherein the buried tunnel junction defines a hole region and comprises: a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; Claims 6 / 11 pages 7 CN 121532916 A An n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³ is located on top of a p-type doped second semiconductor layer; wherein at least the surface area of ​​the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer; optionally, wherein the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; an n-type doped current diffusion layer encapsulates at least a portion of the n-type doped second semiconductor layer, and optionally also encapsulates at least a portion of the p-type doped second semiconductor layer; wherein the current diffusion layer, excluding the portion on which the n-type doped second semiconductor layer is located, covers and contacts the p-type doped second semiconductor layer or the p-type doped first semiconductor layer; and wherein the surface of the current diffusion layer optionally includes a region above the buried tunnel junction, the region being raised and forming a stepped feature to produce an optical confinement effect; (ii”) a top distributed Bragg reflector is disposed or formed on the light-emitting structure; and (iii”) a metal contact is disposed or formed on the optoelectronic device. 51. The method of claim 50, wherein the top distributed Bragg reflector in step (ii”) comprises alternating layers of any of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof.52. The method of any one of claims 50-51, wherein the metal contact in step (iii”) comprises one or more metals selected from the group consisting of Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof. 53. The method of any one of claims 50 to 52, wherein the optoelectronic device is a vertical-cavity surface-emitting laser (VCSEL). 54. A light-emitting structure comprising: a bottom mirror structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; wherein the n-type doped semiconductor layers are porous and include a plurality of pores; and wherein the undoped or lightly doped semiconductor layers are non-porous or substantially non-porous; an n-type doped first semiconductor layer located on top of the bottom structure; a light-emitting structure comprising multiple quantum wells (MQWs) located on top of the semiconductor layers; and a p-type doped first semiconductor layer located on top of the light-emitting structure. A p-type doped second semiconductor layer is located on top of the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; an n-type doped second semiconductor layer is located on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; an n-type doped current diffusion layer is located on top of the n-type doped second semiconductor layer; wherein a hole region exists, wherein the conductivity of the p-type doped first semiconductor layer within the hole region is greater than the conductivity of the p-type doped first semiconductor layer outside the hole region; wherein the resistivity of the p-type doped first semiconductor layer, and optionally the p-type doped second semiconductor layer and optionally the n-type doped semiconductor layer outside the hole region is higher than that within the hole region; wherein the current diffusion layer is conductive both inside and outside the hole; and wherein the current diffusion layer optionally includes a region on a top surface located above the hole region, the region being raised and forming a stepped feature to provide an optical confinement effect. 55. The light-emitting structure of claim 54, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide. 56. The light-emitting structure of any one of claims 54-55, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness. 57. The light-emitting structure of claim 54, wherein the alternating layers of the bottom structure comprise a binary semiconductor material lattice-matched to the semiconductor substrate. 58. The light-emitting structure of claim 54, wherein the alternating layers of the bottom structure comprise a ternary semiconductor material lattice-matched to the semiconductor substrate.59. The light-emitting structure of claim 54, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material lattice-matched to the semiconductor substrate. 60. The light-emitting structure of any one of claims 54 to 59, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer each independently comprise one or more materials lattice-matched to the semiconductor substrate. 61. The light-emitting structure of claim 60, wherein the one or more materials are lattice-matched to the indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the one or more semiconductor materials are lattice-matched to the gallium arsenide semiconductor substrate and are selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the one or more semiconductor materials are lattice-matched to the gallium arsenide semiconductor substrate and are selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb. 62. The light-emitting structure of claims 54-59, wherein the light-emitting structure, the p-type doped second semiconductor, and the n-type doped second semiconductor each independently comprise one or more materials that are lattice mismatched with the indium phosphide semiconductor substrate. 63. The light-emitting structure of claim 62, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb. 64. The light-emitting structure of any one of claims 54-63, wherein the conductivity of the p-type doped first semiconductor layer outside the aperture region, and optionally the p-type doped second semiconductor layer and optionally the n-type doped second semiconductor layer, is about 1-4 orders of magnitude lower than that within the aperture region. 65. The light-emitting structure of any one of claims 54-64, wherein the porosity is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%. 66. The light-emitting structure of any one of claims 54-65, wherein the refractive index contrast (Δn) between alternating layers in the bottom reflector structure is about 0.1 to 2 or 0.1 to 2.5. 67. A method of forming a light-emitting structure, comprising the steps of: (a) setting or forming a structure comprising:A bottom structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; an n-type doped first semiconductor layer on top of the bottom structure; a light-emitting structure comprising multiple quantum wells (MQWs) on top of the first semiconductor layer; a p-type doped first semiconductor layer on top of the light-emitting structure; a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³ on top of the p-type doped first semiconductor layer; an n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³ on top of the p-type doped second semiconductor layer; and an n-type doped current diffusion layer on top of the n-type doped second semiconductor layer; (b) placing a mask material over the top surface region of the current diffusion layer of the structure; (c) performing ion implantation to reduce the conductivity of at least the p-type doped first semiconductor layer not covered by the mask material. (d) Etching a portion of the current diffusion layer, wherein the etching does not remove the current diffusion layer beneath the mask material; (e) Removing the mask material; (f) Depositing a first layer of silicon dioxide over a portion of the current diffusion layer to cover the area where at least the mask material is present; (g) Annealing the structure to improve the conductivity of the top layer of the current diffusion layer; (h) Forming a mesa structure by etching the current diffusion layer, the n-type doped second semiconductor, the p-type doped second semiconductor, the p-type doped first semiconductor, and the portion of the light-emitting structure not covered by the first silicon dioxide; (i) Depositing a second layer of silicon dioxide over the mesa structure, wherein at least a portion of the n-type doped first semiconductor is not covered by the second layer of silicon dioxide; (j) Etching the structure not covered by the second layer of silicon dioxide to form trenches exposing the sidewalls of the alternating layers of the bottom structure; (k) Selectively porosizing the n-type doped semiconductor layers in the alternating layers of the bottom structure, wherein the formed pores include air, and wherein the undoped or low-doped semiconductor layers remain non-porous or substantially non-porous. (l) depositing one or more materials to cover the trench, the sidewalls of the trench, and the sidewalls of the mesa structure; (m) selectively removing the one or more materials to expose at least a portion of the top of the mesa structure and optionally expose a portion of the semiconductor layer covered by the one or more materials; and (n) forming metal contacts on a portion of the top of the mesa structure and optionally a portion of the semiconductor layer. 68. The method of claim 67, wherein the mask material is selected from the group consisting of silicon dioxide, aluminum oxide, and silicon nitride.The method comprises the group consisting of insulating materials; or organic materials (such as photoresist); or metals (such as nickel); or combinations thereof. 69. The method of any one of claims 67-68, wherein the porosity formed in step (k) is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%. 70. The method of any one of claims 67-69, wherein step (k) is achieved by electrochemical etching in an electrolyte solution and under an applied bias voltage. 71. The method of claim 70, wherein the electrolyte solution comprises halide ions, hydrochloric acid (HCl), sulfuric acid (H2SO4), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)2, Ca(OH)2, Sr(OH)2, NH4OH, NaCl, NaF, nitric acid (HNO3), organic acids and their salts (such as oxalic acid and citric acid), and mixtures thereof. 72. The method of any one of claims 67-71, wherein the one or more materials are selected from the group consisting of silicon dioxide, aluminum oxide, and silicon nitride; and / or the one or more materials are organic materials selected from the group consisting of benzocyclobutene (BCB), polyimide, and photoresist; and combinations thereof. Claims 9 / 11, page 10, CN 121532916 A 73. The method of any one of claims 67-72, wherein the metal contact comprises a metal selected from Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof. 74. An optoelectronic device comprising: a light-emitting structure according to any one of claims 54-66; a top distributed Bragg reflector; and metal contacts. 75. The optoelectronic device of claim 74, wherein the top distributed Bragg reflector comprises alternating layers of any one of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof. 76. The optoelectronic device of any one of claims 74-75, wherein the metal contacts comprise a metal selected from Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof. 77. The optoelectronic device of any one of claims 74-76, wherein the optoelectronic device is a vertical-cavity surface-emitting laser (VCSEL). 78. The optoelectronic device of claim 77, wherein the vertical-cavity surface-emitting laser operates in continuous-wave mode at room temperature (about 25°C). 79. The optoelectronic device of claim 77, wherein the vertical-cavity surface-emitting laser operates at a temperature below about 0°C, above about 25°C, or above about 85°C.80. The optoelectronic device of claim 77, wherein the vertical-cavity surface-emitting laser operates in pulsed mode. 81. The optoelectronic device of claim 77, wherein the vertical-cavity surface-emitting laser emits in the infrared and / or red wavelength region. 82. The optoelectronic device of claim 77, wherein the power conversion efficiency of the vertical-cavity surface-emitting laser is at least about 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 7.5%, or 10%. 83. A method of manufacturing an optoelectronic device, comprising the steps of: (a') setting or forming a light-emitting structure, comprising: a bottom mirror structure, the bottom mirror structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; wherein the n-type doped semiconductor layers are porous structures and include a plurality of pores; and the undoped or lightly doped semiconductor layers are non-porous or substantially non-porous structures; an n-type doped first semiconductor layer located on top of the bottom structure; a light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the semiconductor layers; a p-type doped first semiconductor layer located on top of the light-emitting structure; a p-type doped second semiconductor layer located on top of the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; an n-type doped second semiconductor layer located on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; An n-type doped current diffusion layer is located on top of the n-type doped second semiconductor layer; wherein a hole region exists, wherein the conductivity of the p-type doped first semiconductor layer within the hole region is greater than the conductivity of the p-type doped first semiconductor layer outside the hole region; wherein the p-type doped first semiconductor layer, and optionally the p-type doped second semiconductor layer and optionally the n-type doped second semiconductor layer have a higher resistivity outside the hole region than inside the hole region; (Claims 10 / 11, page 11, CN 121532916 A) wherein the current diffusion layer is conductive both inside and outside the hole region; and wherein the current diffusion layer optionally includes a region on a top surface above the hole region, the region being raised and forming a stepped feature to provide an optical confinement effect; (b') a top distributed Bragg reflector is disposed or formed on the light-emitting structure; and (c') a metal contact is disposed or formed on the optoelectronic device. 84. The method of claim 83, wherein the top distributed Bragg reflector in step (b') comprises alternating layers consisting of any one of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof. 85. The method of any one of claims 83-84, wherein the metal contact in step (c') comprises one or more metals selected from the group consisting of Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof. 86. The method of any one of claims 83-85, wherein the optoelectronic device is a vertical-cavity surface-emitting laser (VCSEL). Claims 11 / 11 pages 12 CN 121532916 A Cross-Reference to Related Applications for Optoelectronic Devices and Methods of Manufacturing and Using Them

[0001] This application claims priority to U.S. Provisional Application No. 63 / 509,683, filed June 22, 2023, the entire contents of which are incorporated herein by reference. Technical Field

[0002] The present invention relates to the field of optoelectronic devices, such as vertical-cavity surface-emitting lasers operating in long-wavelength continuous-wave (CW) mode at room temperature (RT). Background Art

[0003] From the late 1990s to the early 21st century, driven by high-bandwidth optical network applications and fueled by the so-called "telecom bubble," the industry invested heavily in R&D and commercialization efforts to develop long-wavelength (LW) vertical-cavity surface-emitting lasers (VCSELs). Unfortunately, these efforts failed to achieve the expected results. With the collapse of the overheated optical communications market in 2001, progress in this field stagnated. The 1,200 nm to 2,400 nm wavelength range is crucial, as it has traditionally been the optical transmission band for silicon fibers in long-distance single-mode communications. Due to various application requirements, there is renewed interest in long-wavelength vertical-cavity surface-emitting lasers (LW-VCSELs) that can operate within this wavelength range: 1) the demand for low-power on-chip laser sources in optoelectronic integrated circuits; 2) the growing market for eye-friendly optical sensing systems based on VCSELs and VCSEL arrays; 3) the emerging market for low-cost optical links over distances exceeding 1km based on single-mode fiber; 4) free-space (last mile or indoor personal network) optical communication for 6G mobile networks and optical wireless networks; 5) Internet of Things (IoT) applications; 6) low-cost optical detection and ranging systems; and 7) biomedical sensing and diagnostic equipment and systems. In short, mass-producible 1,550nm VCSELs will provide technical support for numerous sensing and communication applications.

[0004] However, one of the challenges in developing near-infrared to mid-infrared VCSELs is the need to combine semiconductor active regions that provide high optical gain in the 1,200-2,400nm band with mirrors that combine high reflectivity, low optical absorptivity, and high thermal conductivity. Ideal semiconductor active regions include InAlGaAs quantum wells grown on InP substrates, while...The previously reported best reflector is the AlAs-GaAs dual-sided reflector (DBR) grown on a GaAs substrate. However, InP and GaAs-based structures are generally incompatible at the epitaxial growth level, making the realization of such VCSELs almost impossible. Although there are various methods for manufacturing near-infrared-mid-infrared VCSELs, and even small-scale commercialization has been achieved, cost-effective mass production has not yet been achieved.

[0005] Therefore, manufacturing VCSELs capable of emitting light in the long wavelength range still faces significant challenges. It is evident that there are still core needs to be addressed in the field of long-wavelength emitting VCSELs.

[0006] Therefore, there is an urgent need to develop various structures that can be used as reflectors, which can be manufactured through simplified processes and can be used to prepare vertical-cavity surface-emitting lasers (VCSELs) with a target emission wavelength. Summary of the Invention

[0007] The object of the present invention is to provide such structures to solve and overcome known problems in the prior art when manufacturing devices such as VCSELs.

[0008] Another object of the present invention is to provide a novel method for preparing such structures. Specification 1 / 31 pages 13 CN 121532916 A

[0009] A further object of the present invention is to provide a method of using the said structure, for example, for VCSELs.

[0010] This document describes various semiconductor structures including buried tunnel junctions (BTJs). Such semiconductor structures can be used to fabricate optoelectronic devices, including vertical-cavity surface-emitting lasers (VCSELs). This document elaborates on semiconductor structures including BTJs and optoelectronic devices made therefrom.

[0011] In addition, this document also describes various light-emitting structures including ion-implanted aperture regions. Such light-emitting structures can be used to fabricate optoelectronic devices, such as vertical-cavity surface-emitting lasers (VCSELs). This document further elaborates on various light-emitting structures including ion-implanted aperture regions and optoelectronic devices made therefrom.

[0012] The above-described various semiconductor structures, light-emitting structures, and optoelectronic devices (such as VCSELs) can be applied to a wide range of fields such as electronics, photonics, and optoelectronics. In particular, the VCSEL can achieve long-wavelength emission (i.e., emission in the red, near-red, or infrared bands in the 900 to 3,000 nm range, covering sub-bands and specific wavelengths within this range). Furthermore, compared to more common laser diodes, the VCSEL offers significant advantages in optical and electrical performance, such as superior beam quality, compact form factor, low-power operation, cost-effective wafer-level testing, higher yield, and lower manufacturing costs. Brief Description of the Drawings

[0013] Non-limiting embodiments are illustrated with reference to the accompanying drawings, which are schematic and not drawn to scale. In the drawings, each identical or similar component is typically identified by a single number. For clarity, not every component is shown in every drawing.The drawings are not labeled, and not all components are labeled where they are not required to be shown, so that those skilled in the art can understand the relevant drawings.

[0014] FIG1A is a non-limiting cross-sectional schematic diagram showing an epitaxial semiconductor structure 100 constructed from bottom to top: (1) a stack 110 composed of 12 pairs of alternating layers, including n+ type indium phosphide (InP) and n- type InP; (2) a thick n-type InP layer 120; (3) a light-emitting structure layer 130 composed of InAlGaAs, which forms an active region with a target emission wavelength of 1550nm; (4) a p-type InP layer 140; (5) a buried tunnel junction composed of the following structures: p++ type InGaAs layer 150 and n++ type InGaAs layer 160; wherein (6) a current diffusion layer 170 encloses the buried tunnel junction; optionally (7) the surface of the current diffusion layer has a non-planar structure, forming a stepped feature (180) and providing an optical confinement effect.

[0015] Figure 1B shows a non-limiting cross-sectional schematic diagram depicting an epitaxial semiconductor structure 100' constructed from bottom to top: (1) a stack 110' composed of 12 pairs of alternating layers, including an n+ type indium phosphide (InP) layer and an n- type InP layer; (2) a thick n-type InP layer 120'; (3) a light-emitting structure layer 130' composed of InAlGaAs, which forms an active region with a target emission wavelength of 1550nm; (4) a p-type InP layer 140'; (5) a p++ type InGaAs layer 150'; (6) a buried tunnel junction composed of an n++ type InGaAs layer 160'; wherein (7) a current diffusion layer 170' encloses the buried tunnel junction; optionally, (7) the surface of the current diffusion layer has a non-planar structure, forming a stepped feature (180') and producing an optical confinement effect.

[0016] Figure 1C shows a non-limiting cross-sectional schematic diagram of the epitaxial semiconductor structure 100”, wherein the p-type doped second semiconductor layer 150'' is partially etched, such that the thickness of the 150” layer below the n-type doped second semiconductor layer 160” is greater than that of the other 150'' layers. For simplicity, other layers and structures are not labeled.

[0017] Figure 1D shows a non-limiting cross-sectional schematic diagram of the epitaxial semiconductor structure 100”', wherein the p-type doped second semiconductor layer 150''' is partially and completely etched, such that the thickness of the 150'' layer below the n-type doped second semiconductor layer 160''' is greater than that of the other 150'' layers, and part of the original layer has been completely etched away. For simplicity, other layers and structures are not labeled.

[0018] Figure 1E shows a non-limiting cross-sectional schematic diagram of the epitaxial semiconductor structure 100””, wherein the p-type doped second semiconductor layer 150”” has a uniform thickness, and part of the original layer has been completely etched away. It is also evident that the n-type doped current-diffusion layer 170" may include additional non-planar regions, with parts of the layer being locally etched away. For simplicity, other layers and structures are not described.Page 2 / 31 of the specification, CN 121532916 A, is not labeled.

[0019] Figure 1f shows a non-limiting cross-sectional schematic diagram of the epitaxial semiconductor structure 100””’, in which the p-type doped second semiconductor layer 150”” is etched to a smaller area than the n-type doped second semiconductor layer 160””” above it. For simplicity, other layers and structures are not labeled.

[0020] Figure 2 shows a non-limiting process flow for manufacturing a structure (e.g., semiconductor structure 100) with a buried tunnel junction (BTJ).

[0021] Figure 3 shows a non-limiting cross-sectional schematic diagram of a light-emitting structure 200 including a distributed Bragg reflector (DBR) and a buried tunnel junction (BTJ), which, from bottom to top, consists of: (1) a bottom structure 210 composed of 12 pairs of alternating layers, including alternating layers of n+ type InP and n- type InP, wherein the n+ type InP layer is electrochemically etched to form a porous structure (as shown in the dark band); (2) a thick n-type InP layer 220; (3) a frustum structure, from bottom to top including: an InAlGaAs layer 230, a p-type InAlAs layer 240; a BJT formed by a p++ type InAlAs layer 250 and an n++ type InP layer; and a top n-type InP current diffusion layer 270 with a stepped feature 280 on its surface. The Al2O3 layer (295) and SiO2 layer (290) shown in the figure are present due to the fabrication process.

[0022] Figure 4 illustrates a non-limiting manufacturing process for creating a light-emitting structure 200 including a distributed Bragg reflector (DBR) and a buried tunnel junction (BTJ).

[0023] Figure 5 shows a non-limiting cross-sectional schematic diagram of a vertical-cavity surface-emitting laser (VCSEL) 300, which is composed of a light-emitting structure 200, including a bottom DBR reflector, a top dielectric DBR reflector 310 located on top of the mesa structure of the light-emitting structure 200, and a metal electrode 320.

[0024] Figure 6 shows a non-limiting process flow for manufacturing a vertical-cavity surface-emitting laser (such as VCSEL 300).

[0025] Figure 7 is an I-V graph of a DBR device with a 10 μm diameter buried tunnel junction (BTJ) (solid line) and a DBR device without a BTJ (dashed line).

[0026] Figure 8A is an L-I or L-J relationship diagram of an NP-type InP VCSEL with a 6 μm aperture region.

[0027] Figure 8B is a single-mode laser spectrum of an NP-type InP VCSEL with a 6μm aperture region.

[0028] Figure 9 shows a non-restrictive cross-sectional schematic diagram of a heteroepitaxial structure 400 formed from bottom to top, which includes: (1) a stack 410 composed of 12 pairs of alternating n+ type InP layers and n type InP layers; (2) a thick n type InP layer 420; and (3) a light-emitting structure 430.Composed of InAlGaAs, providing an active region with a target emission wavelength of 1550 nm; (4) p-type InAlAs layer 440; (5) p++ type InAlAs layer 450; (6) n++ type InP layer 460; and (7) n-type InP layer 470.

[0029] Figure 10 shows a non-limiting fabrication process for fabricating a light-emitting structure 600 including a distributed Bragg reflector (DBR) and a hole region.

[0030] Figure 11 is a doping-induced defect distribution curve simulated using SRIM, with the layer boundaries marked by black dashed lines.

[0031] Figure 12 shows a non-limiting cross-sectional schematic diagram of a light-emitting structure 600 including a distributed Bragg reflector (DBR) and an aperture region, which, from bottom to top, includes: (1) a bottom structure 610 composed of a stack of layers including 12 pairs of alternating n+ type InP and n type InP layers, wherein the n+ type InP layers are electrochemically etched to form a selective porous structure, as shown in the dark band; (2) a thick n type InP layer 620; (3) a frustum structure from bottom to top including: an active region providing a target emission wavelength of 1,550 nm—an InAlGaAs layer 630; a p-type InAlAs layer 640; a p-type InAlAs layer 650; an n++ type InP layer 660; and a current diffusion layer 670 on top, wherein the top surface of the current diffusion layer 670 includes a stepped feature 680. The mesa structure includes a hole region composed of p-type InAlAs, p++ type InAlAs, n++ type InP, and n-type InP portions, partially shown as regions 645, 655, and 665 below the step feature 680. The p-type InAlAs, p++ type InAlAs, n++ type InP, and n-type InP regions outside the hole region are ion-implanted to reduce conductivity, and subsequent annealing restores the conductivity of at least the n-type InP current diffusion layer covering the hole region. Furthermore, the figure also shows a SiO2 layer (690) generated by the manufacturing process. Specification 3 / 31 pages 15 CN 121532916 A

[0032] Figure 13 shows a non-limiting cross-sectional schematic diagram of a vertical cavity surface-emitting laser (VCSEL) 700, which is composed of a light-emitting structure 600, including a bottom dual reflector (DBR), a top dielectric dual reflector mirror 710 located on top of the mesa structure of the light-emitting structure 600, and a metal electrode 720.

[0033] Figure 14 shows a non-limiting process flow for manufacturing a vertical-cavity surface-emitting laser (such as VCSEL700).

[0034] Figure 15 shows the I-V curves for two types of light-emitting devices: the solid line represents the device with a 10 μm diameter hole formed by ion implantation, and the dashed line represents the device without a hole.

[0035] Figure 16A shows the L-I or L-J relationship curves for a 1,380 nm NP-type InP VCSEL with a 7 μm hole region, and its threshold...The current is 0.5 mA.

[0036] Figure 16B shows the single-mode laser spectrum of a 1,380 nm NP-type InP vertical-cavity surface-emitting laser with a 7 μm aperture region at an injection current of 8 mA, with a side-mode suppression ratio exceeding 30 dB.

[0037] Figure 17A shows the L-I or L-J relationship curves of a 1550 nm NP-type InP VCSEL with a 7 μm aperture region and a threshold current of 0.67 mA.

[0038] Figure 17B shows the single-mode laser spectrum of a 1550 nm NP-type InP vertical-cavity surface-emitting laser (VCSEL) with a 7 μm aperture region at an injection current of 7 mA, where the side-mode suppression ratio exceeds 30 dB. Detailed Description

[0039] This document describes various semiconductor structures and their fabrication and use methods. For example, these semiconductor structures can be used to fabricate high-performance VCSEL light-emitting structures including distributed Bragg mirrors, which can emit light at long wavelengths.

[0040] I. Definitions In this specification, “porosity” refers to the percentage of air volume in a porous medium (such as an InP, GaAs, or GaSb layer).

[0041] “Electropolishing” refers to the complete or substantial removal of n-type doped indium phosphide or gallium arsenide through etching (where “substantial removal” means an etching depth exceeding 95%, 96%, 97%, 98%, or 99%), forming a cavity at the original n-type doped material location. This cavity represents a low-refractive-index medium (i.e., air). The refractive index of air is typically about 1.

[0042] “Refractive index” and “refractive index” are used interchangeably, referring to the ratio of the speed of light in a vacuum to the speed of light in a specific medium (such as an InP, GaAs, or GaSb layer), calculated using the formula n = c / v, where c is the speed of light in a vacuum and v is the phase velocity of light in the medium.

[0043] The term “refractive index contrast” as used herein specifically refers to the difference in relative refractive indices between two media with different refractive indices when they come into contact to form an interface.

[0044] Numerical ranges include thickness ranges, doping concentration ranges, integer ranges, time ranges, voltage ranges, length ranges, diameter ranges, concentration ranges, etc. These ranges respectively reveal all possible values ​​reasonably covered by the range, as well as any sub-ranges and combinations thereof included therein. For example, a layer thickness range is approximately 1 nm to 10 nm, which simultaneously covers independently selectable thickness values ​​such as 2, 3, 4, 5, 6, 7, 8, 9 nm, as well as any interval between these values ​​(e.g., 3 nm to 8 nm), and also includes all possible combinations of these values.

[0045] The term "about" is intended to describe a range of approximately ±10% above and below the modified value; in other cases, the value may fluctuate by approximately ±5%. When "about" is placed before a numerical range (e.g., about 1–5) or a sequence (e.g., about 1, 2, 3, 4, etc.), unless otherwise stated, the word is intended to modify both ends of the numerical range and / or each value in the sequence.

[0046] II. Semiconductor Structures and Devices Including Buried Tunnel Junctions (BTJs) This document describes various semiconductor structures including buried tunnel junctions (BTJs). These semiconductor structures can be used to fabricate other optoelectronic devices or form components thereof, such as light-emitting structures including distributed Bragg reflectors (DBRs) and vertical-cavity surface-emitting lasers (VCSELs) as described on page 4 / 31 of this specification (CN 121532916 A). Various BTJ-including semiconductor structures and optoelectronic devices will be described in detail below.

[0047] a. Semiconductor structures including buried tunnel junctions (BTJs) In some cases, non-limiting semiconductor structures including buried tunnel junctions (BTJs) include: a bottom structure comprising alternating n-type doped layers and undoped (or lightly doped) semiconductor layers on a semiconductor substrate; an n-type doped first semiconductor layer on top of the bottom structure; a light-emitting structure comprising multiple quantum wells (MQWs) on top of the n-type doped first semiconductor layer; a p-type doped first semiconductor layer on top of the light-emitting structure; and a buried tunnel junction (BTJ) on top of the p-type doped first semiconductor layer, wherein the buried tunnel junction comprises: a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; an n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; wherein at least the surface area of ​​the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer. Optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; and an n-type doped current diffusion layer that encloses at least a portion of the n-type doped second semiconductor layer, optionally enclosing at least a portion of the p-type doped second semiconductor layer, and wherein the current diffusion layer, excluding the portion having the n-type doped second semiconductor layer, contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and wherein the surface of the current diffusion layer optionally includes a region above the buried tunnel junction that protrudes and forms a stepped feature, thereby producing an optical confinement effect.

[0048] An exemplary non-limiting semiconductor structure including the BTJ is shown in Figures 1a to 1f. The BTJ is constituted by a region buried and located within the current diffusion layer. For example, in semiconductor structure 100, the BTJ is defined by layers 150 and 160, which are enclosed by a current diffusion layer 170 that contacts layer 140. In semiconductor structure 100', the BTJ is defined by layer 160', which is enclosed by current diffusion layer 170', which contacts layer 150'. As described in Embodiment 1, the BTJ defines a current localization that can be generated in devices containing such tunnel junctions.The region of the domain effect. Furthermore, as described above, the top surface of the current diffusion layer of this structure may include a stepped feature (i.e., 180 in FIG. 1b) that covers the BTJ and provides an optical localization effect.

[0049] For specific semiconductor materials constituting the semiconductor structure portion (such as p-type doped second semiconductor layers and n-type doped second semiconductor layers), there are minimum requirements for their doping concentration, as specifically described above. For the remaining p-type or n-type doped layers, there are no particular limitations on their doping concentration levels. In some cases, different p-type or n-type doped layers may each independently have a doping concentration level of at least about 1 × 10¹⁸ cm⁻³ or higher; or be in the range of about 0.1 × 10¹⁹ cm⁻³ to 10 × 10²⁰ cm⁻³. In some cases, high doping concentration levels can be approximately 1 × 10¹⁹ cm⁻³, 2 × 10¹⁹ cm⁻³, 3 × 10¹⁹ cm⁻³, 4 × 10¹⁹ cm⁻³, 5 × 10¹⁹ cm⁻³, 6 × 10¹⁹ cm⁻³, 6 × 10¹⁹ cm⁻³, 8 × 10¹⁹ cm⁻³, 9 × 10¹⁹ cm⁻³, or 10 × 10¹⁹ cm⁻³. In some other cases, different p-type or n-type doped layers can each independently have medium doping concentration levels greater than approximately 1 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 2 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 3 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 4 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, or 5 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³. In some cases, the medium doping concentration ranges from 1 × 10¹⁹ cm⁻³ to less than 1 × 10²⁰ cm⁻³, or from about 0.5 × 10¹⁹ cm⁻³ to less than 10 × 10¹⁹ cm⁻³. In some cases, the medium doping concentration level is approximately 1 × 10¹⁸ cm⁻³, 2 × 10¹⁸ cm⁻³, 3 × 10¹⁸ cm⁻³, 4 × 10¹⁸ cm⁻³, 5 × 10¹⁸ cm⁻³, or 6 × 10¹⁸ cm⁻³, 7 × 10¹⁸ cm⁻³, 8 × 10¹⁸ cm⁻³, 9 × 10¹⁸ cm⁻³, or 10 × 10¹⁸ cm⁻³. However, in other cases, different p-type or n-type doped layers may each have a doping concentration below about 20 × 10¹⁷ cm⁻³ or between about 0.5 × 10¹⁷ cm⁻³ and 10 × 10¹⁷ cm⁻³. In some cases, low doping concentration levels can be approximately 1×10¹⁷ cm⁻³, 2×10¹⁷ cm⁻³, 3×10¹⁷ cm⁻³, 4×10¹⁷ cm⁻³, 5×10¹⁷ cm⁻³, 6×10¹⁷ cm⁻³, 7×10¹⁷ cm⁻³, 8×10¹⁷ cm⁻³, 9×10¹⁷ cm⁻³, or 10×10¹⁷ cm⁻³.

[0050] As described above, the surface area of ​​the n-type doped second semiconductor layer is at least smaller than the surface area of ​​the p-type doped first semiconductor layer. For example, as seen in Figures 1a to 1f, the region or surface area occupied by the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer. In some non-limiting examples, the surface area occupied by the n-type doped second semiconductor layer may be approximately 1% to 30% of the total surface area of ​​the p-type doped first semiconductor layer, or may include sub-ranges and specific values ​​within this range. In some cases (as shown in Figure 1a), the p-type doped second semiconductor layer and the n-type doped second semiconductor layer occupy equal or approximately equal areas on the p-type doped first semiconductor layer, as specifically described below. In other cases, the areas occupied by the two on the p-type doped first semiconductor layer are not equal. For example, as shown in Figure 1b, the surface area of ​​the p-type doped second semiconductor layer may be equal to that of the p-type doped first semiconductor layer, while the surface area of ​​the n-type doped second semiconductor layer is smaller than that of the p-type doped first semiconductor layer.

[0051] In other cases, the p-type doped second semiconductor layer may have any suitable area, may exhibit variable thickness within the same layer, and / or may be completely etched away in specific portions / regions. As shown in FIG1c, the epitaxial semiconductor structure 100” may include a partially etched p-type doped second semiconductor layer 150”, such that the 150” layer below the n-type doped second semiconductor layer 160” is thicker than the remaining 150” layers. However, thickness variations may exist in other forms and locations. As shown in FIG1d, the epitaxial semiconductor structure 100”’ may be partially or completely etched at different locations within the same layer, such that the 150” layer below the n-type doped second semiconductor layer 160” is thicker than the remaining 150” layers, and a portion of the original layer has been completely etched away, as shown. As shown in FIG1e, the epitaxial semiconductor structure 100” may include a uniformly thick p-type doped second semiconductor layer 150”, wherein a portion of the original layer has been completely etched away. FIG1e also shows that the n-type doped current diffusion layer 170” may include additional non-planar features, i.e., portions of the current diffusion layer are locally etched away. Finally, as shown in Figure 1f, the epitaxial semiconductor structure 100””” may include an etched p-type doped second semiconductor layer 150””, the surface area of ​​which is smaller than the surface area of ​​the top n-type doped second semiconductor layer 160”””. This case can be considered as the undercut of the layer.

[0052] In the special case where the areas of the n-type doped second semiconductor layer and the p-type doped second semiconductor layer are equal or approximately equal, it is understood that the two layers are stacked on each other, together forming a double stack existing on the p-type doped first semiconductor layer. See Figure 1a. "Approximately equal" as used herein means that when comparing different regions of the two layers, the area difference is less than about 5%, 4%, 3%, 2%, 1% or less.

[0053] For the semiconductor structure, the semiconductor substrate may be made of indium phosphide, gallium arsenide or gallium antimonide. In some cases,The alternating layers of the bottom structure comprise or are made of a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, or gallium antimonide, whose lattice is matched to a selected semiconductor substrate made of any one of indium phosphide, gallium arsenide, or gallium antimonide. In other cases, the alternating layers of the bottom structure comprise or are made of a ternary semiconductor material that is lattice matched to a selected indium phosphide, gallium arsenide, or gallium antimonide semiconductor substrate. In other cases, the alternating layers of the bottom structure comprise or are made of a quaternary semiconductor material that is lattice matched to a selected indium phosphide, gallium arsenide, or gallium antimonide semiconductor substrate.

[0054] In some cases, for the semiconductor structure, the n-type doped first semiconductor layer, the light-emitting structure, the p-type doped first semiconductor layer, the p-type doped second semiconductor layer, the n-type doped second semiconductor layer, and the current diffusion layer may each independently comprise semiconductor materials selected to be lattice matched to a semiconductor substrate made of indium phosphide, gallium arsenide, or gallium antimonide.

[0055] Without limitation, any suitable semiconductor material that can constitute all or part of the n-type doped first semiconductor layer, the light-emitting structure, the p-type doped first semiconductor layer, the p-type doped second semiconductor layer, the n-type doped second semiconductor layer, and the current diffusion layer can independently include a material that matches the crystal lattice of the indium phosphide semiconductor substrate, selected from, but not limited to, the group consisting of nP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or a semiconductor material that matches the crystal lattice of the gallium arsenide semiconductor substrate, selected from, but not limited to, the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or a semiconductor material that matches the crystal lattice of the gallium arsenide semiconductor substrate, selected from, but not limited to, the group consisting of GaSb, AlAsSb, and AlGaAsSb.

[0056] In some cases, the light-emitting structure, the p-type doped second semiconductor layer, and the n-type doped second semiconductor layer may each independently include a semiconductor material that is lattice-mismatched with a semiconductor substrate made of indium phosphide, gallium arsenide, or gallium antimonide. In such cases, the semiconductor material that is lattice-mismatched with the indium phosphide semiconductor substrate may be selected from, but is not limited to, the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the semiconductor material that is lattice-matched with the gallium arsenide semiconductor substrate may be selected from, but is not limited to, the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the semiconductor material that is lattice-matched with the gallium antimonide semiconductor substrate may be selected from, but is not limited to, the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb.

[0057] In some cases, non-limiting examples of binary semiconductor materials (which may be p-type or n-type doped) may be selected from, but are not limited to, the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb.The group consisting of InP, GaAs, GaSb, and AlAs. In some cases, the non-limiting ternary semiconductor material (which may be p-type or n-type doped) may be selected from the group consisting of InAlAs, InGaAs, AlGaAs, InAlP, InGaP, AlAsSb, and InAsSb. In some cases, the quaternary semiconductor material (which may be p-type or n-type doped) may be selected from the group consisting of InAlGaAs, InGaAsP, and AlGaAsSb. It should be noted that when selecting any binary, ternary, or quaternary semiconductor material for the above single-layer or multi-layer structure, it is advisable to achieve lattice matching between the semiconductor material of each layer of the specific structure and the selected semiconductor substrate (which may be made of InP, GaAs, or GaSb). Those skilled in the art can select suitable materials for each layer that match the lattice of the semiconductor substrate and determine the required doping type and concentration level, as described above.

[0058] The size, shape, and thickness of each of the above layers and structures can be flexibly set according to the actual application requirements. In specific cases, the thickness of different structural layers can be referred to in the following table: Table 1. Thickness

[0059] *The range mentioned above also includes sub-ranges, and any specific thickness within the range listed in Table 1 is included.

[0060] It should be noted that the thickness of the semiconductor structural layers and structural thickness (including bilateral mirrors) used to manufacture the light-emitting structure, and the vertical cavity surface-emitting laser (VCSEL) made from such structure, can also be defined for the thickness of the corresponding layers and structures in the light-emitting structure and VCSEL.

[0061] In some cases, for the bottom structure, the n-type doped semiconductor layers present in the alternating layers have the same thickness as each other, and / or the undoped (or low-doped) semiconductor layers present in the alternating layers have the same thickness as each other. n-type doped and specification 7 / 31 page 19 CN 121532916 A Undoped (or low-doped) semiconductor layers may have the same or different thicknesses. A non-limiting method for fabricating a semiconductor structure including a buried tunnel junction (BTJ) may include the following steps: (i) forming a bottom structure on a semiconductor substrate, the structure including alternating n-type doped layers and undoped (or lightly doped) semiconductor layers; (ii) depositing an n-type doped first semiconductor layer on top of the bottom structure; (iii) a light-emitting structure including the deposition or formation of multiple quantum wells (MQWs) on top of the n-type doped first semiconductor layer; (iv) depositing a p-type doped first semiconductor layer on top of the light-emitting structure; (v) depositing a p-type doped second semiconductor layer over the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; and (vi) depositing an n-type doped semiconductor layer on top of the p-type doped second semiconductor layer, the n-type doped semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁷ cm⁻³.(vii) Forming or patterning a mask material on the top surface region of the n-type doped semiconductor layer; (viii) Etching away at least the n-type doped semiconductor layer and optionally removing the p-type doped second semiconductor layer outside the mask material region; (ix) Removing the mask material; and (x) Depositing an n-type doped current diffusion layer, which at least partially encapsulates the n-type doped second semiconductor layer and optionally encapsulates a portion of the p-type doped second semiconductor layer, wherein the current diffusion layer outside the surface region contacts the p-type doped second semiconductor or the p-type doped first semiconductor.

[0062] Specific fabrication details of the bottom structure are detailed in Section IV below. Figure 2 illustrates an exemplary embodiment of the above method: a tunnel junction is formed by selectively etching layer 160 (optionally etching layer 150), which is then covered with a current diffusion layer. Due to the non-planarity of layer 160 (and optionally layer 150) etched without mask material protection, a stepped feature is formed on top of the current diffusion layer in the BTJ region when the current diffusion layer is deposited.

[0063] The structures and deposited layers formed in the above methods can be independently prepared using existing deposition techniques (including metal-organic chemical vapor deposition, MOCVD). Precursor selection, p / n type dopant configuration, and process conditions for forming and doping such structural layers at specified thicknesses are all well-known techniques.

[0064] Methods for depositing / forming light-emitting structures, including multiple quantum wells (MQWs), are well-known in the prior art.

[0065] In some cases, the mask material is not limited to the group consisting of dielectric materials (such as silicon dioxide, silicon nitride, and alumina) and / or photoresists. Such materials can be formed using plasma-enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), or other well-known techniques.

[0066] For the methods described, any suitable technique (such as wet chemical etching, plasma etching, inductively coupled plasma reactive ion etching (ICP-RIE)) can be used for patterning, etching, or material removal as needed.

[0067] For the method described, the semiconductor substrate may be made of indium phosphide, gallium arsenide, or gallium antimonide. In some cases, the alternating layers of the bottom structure comprise or are made of a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, or gallium antimonide, whose lattice is matched to the selected semiconductor substrate made of indium phosphide, gallium arsenide, or gallium antimonide, respectively. In other cases, the alternating layers of the bottom structure comprise or are made of a ternary semiconductor material, which achieves lattice matching with the selected semiconductor substrate (indium phosphide, gallium arsenide, or gallium antimonide), respectively. In still other cases, the alternating layers of the bottom structure comprise or are made of a quaternary semiconductor material, which achieves lattice matching with the selected indium phosphide, gallium arsenide, or gallium antimonide semiconductor substrate, respectively.

[0068] In some cases, for the semiconductor structure formed according to the method, the n-type doped first semiconductor layer, [details omitted]121532916 A The light structure, the p-type doped first semiconductor layer, the p-type doped second semiconductor layer, the n-type doped second semiconductor layer, and the current diffusion layer may each independently include selected semiconductor materials, which are in conjunction with a semiconductor substrate made of indium phosphide, gallium arsenide, or gallium antimonide.

[0069] Without limitation, suitable semiconductor materials that may constitute all or part of the n-type doped first semiconductor layer, the light-emitting structure, the p-type doped first semiconductor layer, the p-type doped second semiconductor layer, the n-type doped second semiconductor layer, and the current diffusion layer may each independently include a semiconductor material lattice-matched with the indium phosphide semiconductor substrate, selected from, but not limited to, the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or a semiconductor material lattice-matched with the gallium arsenide semiconductor substrate, selected from, but not limited to, the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or a semiconductor material lattice-matched with the gallium arsenide semiconductor substrate, selected from, but not limited to, the group consisting of GaSb, AlAsSb, and AlGaAsSb.

[0070] In some embodiments, the light-emitting structure, the p-type doped second semiconductor layer, and the n-type doped second semiconductor layer may each independently include a semiconductor material that is lattice mismatched with a semiconductor substrate made of indium phosphide, gallium arsenide, or gallium antimonide. In such cases, the semiconductor material is lattice mismatched with the indium phosphide semiconductor substrate and is selected from, but not limited to, the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the semiconductor material is lattice matched with the gallium arsenide semiconductor substrate and is selected from, but not limited to, the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the semiconductor material is lattice matched with the gallium antimonide semiconductor substrate and is selected from, but not limited to, the group consisting of InAl(As)Sb, AlAsSb, AlGaAsSb, etc.

[0071] In some cases, a non-limiting example of a binary semiconductor material (which may be p-type or n-type doped) may be freely selected from the group consisting of InP, GaAs, GaSb, and AlAs. In some cases, the ternary semiconductor material (which may be p-type or n-type doped) in non-limiting examples may be freely selected from the group consisting of InAlAs, InGaAs, AlGaAs, InAlP, InGaP, AlAsSb, and InAsSb. In some cases, the quaternary semiconductor material (which may be p-type or n-type doped) may be freely selected from the group consisting of InAlGaAs, InGaAsP, and AlGaAsSb. It should be noted that when selecting any binary, ternary, or quaternary semiconductor material for the above single-layer or multi-layer structure, it is advisable to achieve lattice matching between the semiconductor material of each layer of the specific structure and the selected semiconductor substrate (which may be made of InP, GaAs, or GaSb). Those skilled in the art can select suitable materials for each layer that are lattice-matched with the semiconductor substrate, andThe required doping type and concentration level are determined as described above.

[0072] For the method described above, the layers, structures and overall semiconductor structure formed according to the method can have any suitable size, shape and thickness. Exemplary (non-limiting) thicknesses of the layers and structures in the overall semiconductor structure are shown in Table 1.

[0073] b. Light-emitting structure containing distributed Bragg reflector (DBR) and buried tunnel junction (BTJ) As described above, the semiconductor structure containing BTJ can be used to manufacture a light-emitting structure including a distributed Bragg reflector and having a buried tunnel junction (BTJ) inside.

[0074] In one embodiment, the light-emitting structure includes a distributed Bragg reflector (DBR) and a buried tunnel junction (BTJ), comprising: a bottom structure comprising alternating n-type doped layers and undoped (or lightly doped) semiconductor layers on a semiconductor substrate, wherein the n-type doped layers are porous and include multiple pores; the undoped (or lightly doped) layers are non-porous or substantially non-porous; an n-type doped first semiconductor layer on top of the bottom structure; a light-emitting structure comprising multiple quantum wells (MQWs) on top of the n-type doped first semiconductor layer; a p-type doped first semiconductor layer on top of the light-emitting structure; and a buried tunnel junction present on a portion (or sub-region) of the p-type doped first semiconductor layer, wherein the buried tunnel junction (BTJ) defines a hole region and includes: a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³. An n-type doped second semiconductor layer is located on top of a p-type doped second semiconductor layer, the n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; wherein at least the surface area of ​​the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer; optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or approximately equal areas on the p-type doped first semiconductor layer; and an n-type doped current diffusion layer, the n-type doped current diffusion layer enclosing at least a portion of the n-type doped second semiconductor layer, optionally enclosing at least a portion of the p-type doped second semiconductor layer, and wherein the current diffusion layer, other than the portion on which the n-type doped second semiconductor layer is located, covers and contacts the p-type doped second semiconductor layer or the p-type doped first semiconductor layer; and wherein the surface of the current diffusion layer optionally includes a raised region covering the buried tunnel junction, the region forming a stepped feature, thereby producing an optical confinement effect.

[0075] FIG3 shows a non-limiting example of a light-emitting structure 200 including the above-described double-layer reflector (DBR), the structure including a DBR and a double-layer tunnel junction (BTJ).

[0076] In some cases, the porosity of the porous n-type doped layer in the bottom structure is at least 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%.

[0077] Due to the porosity of the n-type doped layer in the bottom structure, air can fill multiple pores, resulting in a lower refractive index of the porous n-type doped layer than that of a non-porous or substantially non-porous undoped (or low-doped) layer. In some cases, there is a refractive index contrast (Δn) between the alternating porous layers, ranging from about 0.1 to 2, or about 0.1 to 2.5.

[0078] For the light-emitting structure, the semiconductor substrate may be made of indium phosphide, gallium arsenide, or gallium antimonide. In certain cases, the alternating layers of the bottom structure comprise or are composed of a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, or gallium antimonide, the lattice of which is matched to the selected semiconductor substrate (made of indium phosphide, gallium arsenide, or gallium antimonide). In other cases, the alternating layers of the bottom structure comprise or are composed of ternary semiconductor materials that are lattice-matched to selected indium phosphide, gallium arsenide, or gallium antimonide semiconductor substrates, respectively. In still other cases, the alternating layers of the bottom structure comprise or are composed of quaternary semiconductor materials that are lattice-matched to selected indium phosphide, gallium arsenide, or gallium antimonide semiconductor substrates, respectively.

[0079] In some cases, for the light-emitting structure, the n-type doped first semiconductor layer, the light-emitting structure, the p-type doped first semiconductor layer, the p-type doped second semiconductor layer, the n-type doped second semiconductor layer, and the current diffusion layer may each independently comprise semiconductor materials selected to be used with semiconductor substrates made of indium phosphide, gallium arsenide, or gallium antimonide.

[0080] Without limitation, suitable semiconductor materials that can constitute all or part of the n-type doped first semiconductor layer, the light-emitting structure, the p-type doped first semiconductor layer, the p-type doped second semiconductor layer, the n-type doped second semiconductor layer, and the current diffusion layer can all independently include semiconductor materials that match the crystal lattice of the indium phosphide semiconductor substrate, selected from, but not limited to, the group consisting of InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or semiconductor materials that match the crystal lattice of the gallium arsenide semiconductor substrate, selected from, but not limited to, the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or semiconductor materials that match the crystal lattice of the gallium arsenide semiconductor substrate, selected from, but not limited to, the group consisting of GaSb, AlAsSb, and AlGaAsSb.

[0081] In some cases, the light-emitting structure, the p-type doped second semiconductor layer, and the n-type doped second semiconductor layer can each independently include semiconductor materials that do not match the crystal lattice of the semiconductor substrate made of indium phosphide, gallium arsenide, or gallium antimonide. In such cases, the semiconductor material and the indium phosphide semiconductor substrate are lattice mismatched, and the substrate is selected from, but not limited to, materials such as InAlGaAs, InGaAsP, etc.The group consisting of InGaAs, InAs, and InGaAsSb; or the semiconductor material having lattice matching with the gallium arsenide semiconductor substrate, selected from, but not limited to, the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the semiconductor material having lattice matching with the gallium antimonide semiconductor substrate, selected from, but not limited to, the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb.

[0082] For specific semiconductor materials constituting the light-emitting structure portion (such as p-type doped second semiconductor layers and n-type doped second semiconductor layers), there are minimum requirements for their doping concentration, as specifically described above. For the remaining p-type or n-type doped layers, there are no particular restrictions on their doping concentration levels. In some cases, different p-type or n-type doped layers may each independently have a doping concentration level of at least about 1 × 10¹⁹ cm⁻³ or higher; or in the range of about 0.1 × 10¹⁹ cm⁻³ to 10 × 10²⁰ cm⁻³. In some cases, high doping concentration levels can be approximately 1 × 10¹⁹ cm⁻³, 2 × 10¹⁹ cm⁻³, 3 × 10¹⁹ cm⁻³, 4 × 10¹⁹ cm⁻³, 5 × 10¹⁹ cm⁻³, 6 × 10¹⁹ cm⁻³, 7 × 10¹⁹ cm⁻³, 8 × 10¹⁹ cm⁻³, 9 × 10¹⁹ cm⁻³, or 10 × 10¹⁹ cm⁻³. In some other cases, different p-type or n-type doped layers can each independently have medium doping concentration levels, ranging from approximately 1 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 2 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 3 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 4 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, or 5 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³. In some cases, moderate doping concentration levels range from 1 × 10¹⁹ cm⁻³ to less than 1 × 10²⁰ cm⁻³ or from 0.5 × 0¹⁹ cm⁻³ to less than 1 × 10²⁰ cm⁻³. In other cases, moderate doping concentration levels are approximately 1 × 10¹⁸ cm⁻³, 2 × 10¹⁸ cm⁻³, 3 × 10¹⁸ cm⁻³, 4 × 10¹⁸ cm⁻³, 5 × 10¹⁸ cm⁻³, 6 × 10¹⁸ cm⁻³, 7 × 10¹⁸ cm⁻³, 8 × 10¹⁸ cm⁻³, 9 × 10¹⁸ cm⁻³, or 10 × 10¹⁸ cm⁻³. However, in other cases, different p-type or n-type doped layers may each have a doping concentration below approximately 20 × 10¹⁷ cm⁻³ or between approximately 0.5 × 10¹⁷ cm⁻³ and 10 × 10¹⁷ cm⁻³. In some cases, low doping concentration levels can be approximately 1×10¹⁷ cm⁻³, 2×10¹⁷ cm⁻³, 3×10¹⁷ cm⁻³, 4×10¹⁷ cm⁻³,5×10¹⁷ cm⁻³, 6×10¹⁷ cm⁻³, 7×10¹⁷ cm⁻³, 8×10¹⁷ cm⁻³, 9×10¹⁷ cm⁻³, or 10×10¹⁷ cm⁻³.

[0083] In some cases, non-limiting examples of binary semiconductor materials (which may be p-type or n-type doped) may be selected from the group consisting of InP, GaAs, GaSb, and AlAs. In some cases, non-limiting examples of ternary semiconductor materials (which may be p-type or n-type doped) may be selected from the group consisting of InAlAs, InGaAs, AlGaAs, InAlP, InGaP, AlAsSb, and InAsSb. In some cases, quaternary semiconductor materials (which may be p-type or n-type doped) may be selected from the group consisting of InAlGaAs, InGaAsP, and AlGaAsSb. It should be noted that when selecting any binary, ternary, or quaternary semiconductor material for the above-mentioned single-layer or multi-layer structure, it is advisable to achieve lattice matching between the semiconductor material of each layer of the specific structure and the selected semiconductor substrate (which may be made of InP, GaAs, or GaSb). Those skilled in the art can select suitable materials for each layer that match the lattice of the semiconductor substrate and determine the required doping type and concentration level, as described above.

[0084] For the above-mentioned light-emitting structure, each layer, structure, and overall light-emitting structure can have any suitable size, shape, and thickness. Exemplary (non-limiting) thicknesses of each layer and structure in the overall light-emitting structure are shown in Table 1.

[0085] In some cases, as shown in FIG3, BTJ can constitute part of a mesa structure, the size of which can be selected to be larger than BTJ itself. In other words, the mesa structure encloses BTJ.

[0086] A non-limiting method for fabricating a light-emitting structure including a DBR mirror and a buried tunnel junction (BTJ) may include the following steps: (i') setting or forming a semiconductor structure including a buried tunnel junction (BTJ), the semiconductor structure including: a bottom structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; an n-type doped first semiconductor layer located on top of the bottom structure; a light-emitting structure including a multiple quantum well (MQW) located on top of the n-type doped first semiconductor layer; a p-type doped first semiconductor layer located on top of the light-emitting structure; and a buried tunnel junction (BTJ) located on top of the p-type doped first semiconductor layer, wherein the buried tunnel junction includes: a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; An n-type doped second semiconductor layer is located on top of a p-type doped second semiconductor layer, wherein the n-type doped second semiconductor layer has an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³;The surface area of ​​at least the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer; optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or approximately equal areas on the p-type doped first semiconductor layer; and an n-type doped current diffusion layer, which encapsulates at least a portion of the n-type doped second semiconductor layer, and optionally also encapsulates at least a portion of the p-type doped second semiconductor layer. Wherein, a current diffusion layer, excluding the portion having an n-type doped second semiconductor layer thereon, covers and contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and wherein the surface of the current diffusion layer optionally includes a region above the buried tunnel junction, the region being raised and forming a stepped feature, thereby producing an optical confinement effect; (ii') forming a mesa structure by etching the current diffusion layer, the p-type doped first semiconductor layer, and optionally the p-type doped second semiconductor layer and portions of the light-emitting structure; (iii') depositing a silicon dioxide layer on the mesa structure, wherein at least a portion of the n-type doped first semiconductor layer is not covered by the silicon dioxide layer; (iv') etching the portions not covered by the silicon dioxide layer to form trenches thereby exposing the sidewalls of the alternating layers of the bottom structure; (v') selectively porosilicated the n-type doped semiconductor layer of the bottom structure, wherein multiple pores are formed, and wherein the undoped (or low-doped) semiconductor layers remain in a non-porosilicate or substantially non-porosilicate state; (vi') depositing one or more materials to cover the trenches, sidewalls, and sidewalls of the mesa structure; (vii') Selectively remove one or more of the materials to expose at least a portion of the top of the mesa structure, and optionally expose a portion of the covered n-type doped first semiconductor layer; and (viii') form metal contacts on a portion of the top of the mesa structure and optionally on a portion of the n-type doped first semiconductor layer.

[0087] The above describes a method for forming a structure including a BTJ. Figure 4 shows a non-limiting example of a light-emitting structure including a DBR mirror and a BTJ.

[0088] The structures and layers formed or deposited in the above methods can be independently formed or deposited by existing deposition methods, including metal-organic chemical vapor deposition (MOCVD). The selection of precursors, p-type or n-type dopants, and the process conditions for forming and doping such structures and layers at a specified thickness are well known in the art.

[0089] For the method of fabricating the light-emitting structure, any suitable technique can be used for patterning, etching or removal, such as wet chemical etching, plasma etching, inductively coupled plasma reactive ion etching (ICP-RIE).

[0090] In some embodiments, the one or more materials are selected from the group consisting of silica, alumina, silicon nitride, and spin-coated glass (SOG); and / or the one or more materials are selected from benzocyclobutene (BCB), polyimide, andOrganic materials in the group consisting of photoresists; and combinations thereof. Various types of photoresists are known in the art. For the method described, the deposition of the silicon dioxide layer and one or more materials can be achieved by various methods, such as plasma-enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), or other suitable methods known in the art. Other options for the light-emitting structure and its internal layers have been given in Section IIb above.

[0091] In some embodiments, the porosity formed by step (v') is at least 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%.

[0092] In some embodiments, step (v') is achieved by electrochemical etching in an electrolyte and under an applied bias voltage. In certain cases, the electrolyte may include halide ions, hydrochloric acid (HCl), sulfuric acid (H2SO4), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)2, Ca(OH)2, Sr(OH)2, NH4OH, NaCl, NaF, nitric acid (HNO3), organic acids and their salts (such as oxalic acid and citric acid), and mixtures thereof.

[0093] In some embodiments, the metal contacts formed in step (viii') are composed of one or more of the following metals: Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof. Methods for preparing such metal contacts are well known to those skilled in the art.

[0094] Regarding the mesa structure formed in step (ii'), its size is selected to be larger than the size of BTJ. In other words, the mesa structure completely includes BTJ. This mesa structure can be formed by wet etching or plasma etching (such as RIE etching).

[0095] c. Optoelectronic device with buried tunnel junction (BTJ) As described above, the light-emitting structure including DBR and BTJ can be used to fabricate an optoelectronic device having a buried tunnel junction (BTJ).

[0096] In some cases, the optoelectronic device may include: a light-emitting structure including a bottom distributed Bragg reflector and a buried tunnel junction (BTJ); a top distributed Bragg reflector; and a metal electrode.

[0097] For optoelectronic devices, the light-emitting structure includes a distributed Bragg reflector (DBR) and a bipolar junction (BTJ) as described above. Figure 5 shows a non-limiting example of an optoelectronic device (such as a vertical cavity surface-emitting laser, VCSEL).

[0098] In some cases, the top distributed Bragg reflector is composed of or includes alternating layers of one of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF,a-Si / CaF2 or combinations thereof.

[0099] In some cases, the metal contact layer is made of or includes one or more metals selected from the group consisting of titanium, platinum, gold, germanium, nickel, palladium, indium, and combinations thereof.

[0100] In some cases, the optoelectronic device is a vertical-cavity surface-emitting laser (VCSEL). In some cases, the VCSEL operates in continuous-wave mode at room temperature (about 25°C).

[0101] In other cases, the VCSEL can operate at temperatures below about 0°C, above about 25°C, or above about 85°C. In still other cases, the laser can operate in pulsed mode.

[0102] The VCSEL includes a BTJ structure whose emission wavelength can cover the infrared and / or visible light regions, depending on the choice of the emitting structure material. In some cases, the power conversion efficiency of the VCSEL is at least 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 7.5%, or 10%.

[0103] A non-limiting method for manufacturing an optoelectronic device including a buried tunnel junction (BTJ) may include the following steps: (i”) setting or forming a light-emitting structure including a bottom distributed Bragg reflector and an internal buried tunnel junction (BTJ); (ii”) setting or forming a top distributed Bragg reflector on the light-emitting structure; and (iii”) setting or forming a metal electrode on the optoelectronic device.

[0104] For an optoelectronic device formed according to the above method, its light-emitting structure includes a distributed Bragg reflector (BDR) and a BTJ as described above. Figure 6 shows a non-limiting process flow for manufacturing an optoelectronic device (such as a VCSEL).

[0105] In this method, the top distributed Bragg reflector in step (ii”) may comprise alternating layers of any of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof. Methods for manufacturing such DBRs having the above-described alternating layers are known in the art. The number of alternating layers in such DBRs may depend on the selected material. The top DBR reflector may be deposited using methods in the art and may include annealing to improve reflectivity. In some cases, the reflectivity of the top DBR reflector is at least about 97% or higher.

[0106] For the above method, the metal contact layer in step (iii”) may be composed of the following metals or combinations thereof: titanium (Ti), platinum (Pt), gold (Au), germanium (Ge), nickel (Ni), palladium (Pd), indium (In), and combinations thereof.

[0107] For any of the methods described in Part II, it should be understood that the order of certain steps may be interchanged, provided that it is within permissible limits and does not affect the performance of the resulting structure or device. For example, steps (ii”) and (iii”) in a method for manufacturing an optoelectronic device may be performed in any suitable order.

[0108] III. Light-emitting structures and devices including ion-implanted aperture regions This article describes a variety of light-emitting structures and devices including ion-implanted aperture regions. These light-emitting structures can be used to manufacture other optoelectronic devices or form components thereof, such as light-emitting structures containing distributed Bragg mirrors (DBRs) and vertical-cavity surface-emitting lasers (VCSELs). Various types of light-emitting structures and devices including ion-implanted aperture regions will be described in detail below.

[0109] a. A light-emitting structure including a distributed Bragg reflector (DBR) mirror and an aperture region formed by ion implantation. In one embodiment, the light-emitting structure including a distributed Bragg reflector (DBR) mirror and an aperture region formed by ion implantation comprises: a bottom structure comprising alternating n-type doped layers and undoped (or lightly doped) semiconductor layers on a semiconductor substrate, wherein the n-type doped layers are porous and include a plurality of pores; and wherein the undoped (or lightly doped) layers are non-porous or substantially non-porous; an n-type doped first semiconductor layer located on top of the bottom structure; a light-emitting structure including a multiple quantum well (MQW) located on top of the semiconductor layer; a p-type doped first semiconductor layer located on top of the light-emitting structure; and a p-type doped second semiconductor layer located on top of the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³. An n-type doped second semiconductor layer is located on top of a p-type doped second semiconductor layer, the n-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; an n-type doped current diffusion layer is located on top of the n-type doped second semiconductor layer; wherein a hole region exists, and wherein the conductivity of the p-type doped first semiconductor layer portion within the hole region is greater than the conductivity of the p-type doped first semiconductor layer outside the hole region; wherein the resistivity of the p-type doped first semiconductor layer, and optionally the p-type doped second semiconductor layer and optionally the n-type doped second semiconductor layer outside the hole region is higher than that within the hole region; wherein the current diffusion layer is conductive both inside and outside the hole region; and wherein the current diffusion layer optionally includes a region on the top surface above the hole region, the region being raised and forming a stepped feature, thereby providing an optical confinement effect.

[0110] As shown in FIG12, a non-limiting specification example including the above-described light-emitting structure 600, such as a DBR reflector, is given on page 14 / 31 of CN 121532916 A. As described above and as shown in Figure 12, the aperture region defines a portion of the light-emitting structure composed of a specific layer. This aperture...The region is formed by ion implantation, wherein an ion implantation mask protects specific regions of the structure from conductive damage caused by ion irradiation and implantation. The mask-protected region defines the hole region, as shown in FIG12, which includes at least the 645, 655, and 665 layers that have not been ion implanted. Annealing can restore the conductivity outside the hole region after ion implantation, at least for the n-type doped current diffusion layer. When the light-emitting structure including the DBR mirror and the hole region is used for optoelectronic applications, the hole region can provide a current-limiting effect because the implanted region of the p-type doped first semiconductor remains resistive. In addition, an etching step using the same mask as ion implantation can form an optional stepped structure (680) above the hole region, which can produce an optical confinement effect, allowing for greater overlap between the laser mode and the hole region.

[0111] There are minimum requirements for the doping concentration of the specific semiconductor materials constituting the light-emitting structure (such as the p-type doped semiconductor layer and the n-type doped second semiconductor layer), as described above. There are no particular restrictions on the doping concentration level of the remaining p-type or n-type doped layers mentioned. In some cases, different p-type or n-type doped layers may each independently have a doping concentration level of at least about 1 × 10¹⁹ cm⁻³ or higher; or in the range of about 0.1 × 10¹⁹ cm⁻³ to 10 × 10²⁰ cm⁻³. In some cases, high doping concentration levels may be about 1 × 10¹⁹ cm⁻³, 2 × 10¹⁹ cm⁻³, 3 × 10¹⁹ cm⁻³, 4 × 10¹⁹ cm⁻³, 6 × 10¹⁹ cm⁻³, 7 × 10¹⁹ cm⁻³, 8 × 10¹⁹ cm⁻³, 9 × 10¹⁹ cm⁻³, or 10 × 10¹⁹ cm⁻³. In some other cases, different p-type or n-type doped layers may each independently have a moderate doping concentration level, ranging from about 1 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 2 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 3 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 4 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, or 5 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³. In some cases, the moderate doping concentration ranges from 1 × 10¹⁹ cm⁻³ to less than 1 × 10²⁰ cm⁻³, or from about 0.5 × 10¹⁹ cm⁻³ to less than 1 × 10²⁰ cm⁻³. In some cases, moderate doping concentrations can be approximately 1×10¹⁸ cm⁻³, 2×10¹⁸ cm⁻³, 3×10¹⁸ cm⁻³, 4×10¹⁸ cm⁻³, 6×10¹⁸ cm⁻³, 6×10¹⁸ cm⁻³, 7×10¹⁸ cm⁻³, 8×10¹⁸ cm⁻³, 9×10¹⁸ cm⁻³, or 10×10¹⁸ cm⁻³. However, in other cases, different pThe p-type or n-type doped layers may each have a doping concentration below about 201 × 10¹⁷ cm⁻³ or between about 0.5 × 10¹⁷ cm⁻³ and 10 × 10¹⁷ cm⁻³. In some cases, the low doping concentration level may be about 1 × 10¹⁷ cm⁻³, 2 × 10¹⁷ cm⁻³, 3 × 10¹⁷ cm⁻³, 4 × 10¹⁷ cm⁻³, 5 × 10¹⁷ cm⁻³, 6 × 10¹⁷ cm⁻³, 7 × 10¹⁷ cm⁻³, 8 × 10¹⁷ cm⁻³, 9 × 10¹⁷ cm⁻³, or 10 × 10¹⁷ cm⁻³.

[0112] In some cases, the semiconductor substrate is preferably made of indium phosphide, while the p-type doped first semiconductor layer is composed of p-type doped InAlAs or p-type doped InAlGaAs. In other cases, the semiconductor substrate may also be made of other types of semiconductor materials, such as GaAs or GaSb. The selection of semiconductor materials should ensure lattice matching with the selected semiconductor substrate.

[0113] In some cases, the alternating layers of the bottom structure comprise or are composed of a binary semiconductor material (such as indium phosphide) that matches the lattice of the semiconductor substrate. In other cases, the alternating layers of the bottom structure comprise or are composed of a ternary semiconductor material that matches the lattice of the semiconductor substrate. In still other cases, the alternating layers of the bottom structure comprise or are composed of a quaternary semiconductor material that matches the lattice of the semiconductor substrate.

[0114] In some cases, the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer each independently comprise or are composed of one or more materials that match the lattice of the semiconductor substrate. In some cases, one or more materials match the lattice of, for example, indium phosphide semiconductor substrate and are selected from, but not limited to, the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb.

[0115] In other cases, the light-emitting structure, the p-type doped second semiconductor, and the n-type doped second semiconductor each independently comprise one or more materials that do not match the lattice of the indium phosphide semiconductor substrate. In such cases, the material can be selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb.

[0116] In some cases, a non-limiting example of a binary semiconductor material (which may be p-type or n-type doped) can be selected from the group consisting of InP, GaAs, GaSb, and AlAs. In some cases, a non-limiting example of a ternary semiconductor material (which may be p-type or n-type doped) can be selected from the group consisting of InAlAs, InGaAs, AlGaAs, InAlP, InGaP, AlAsSb, and InAsSb.In some cases, the quaternary semiconductor material (which may be p-type or n-type doped) can be freely selected from the group consisting of InAlGaAs, InGaAsP, and AlGaAsSb. It should be noted that when selecting any binary, ternary, or quaternary semiconductor material for the above single-layer or multi-layer structure, it is advisable to achieve lattice matching between the semiconductor material of each layer of the specific structure and the selected semiconductor substrate (which may be made of InP, GaAs, or GaSb). Those skilled in the art can select a material that matches the lattice of the semiconductor substrate for each layer and determine the required doping type and concentration level, as described above.

[0117] In some cases, the conductivity of the p-type doped first semiconductor layer outside the grating region, and the optional p-type doped second semiconductor layer and the optional n-type doped second semiconductor layer is reduced by about 1-4 orders of magnitude compared to the interior of the grating region. The material constituting the p-type doped first semiconductor layer should preferably be a material whose conductivity decreases (resistance increases) after ion implantation and whose conductivity cannot be recovered or significantly recovered during high-temperature annealing. The term "significant recovery" as used herein refers to a recovery value lower than the original conductivity of the material before ion implantation: approximately 50%, approximately 40%, approximately 30%, approximately 20%, approximately 10%, approximately 5%, and approximately 1%.

[0118] In some cases, the porosity of the n-type doped layer (which is a porous structure) in the bottom structure reaches at least approximately 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%.

[0119] The porous n-type doped semiconductor layer of the bottom structure has multiple pores that can be filled with air, resulting in a refractive index of the porous semiconductor layer that is lower than that of a non-porous or substantially non-porous undoped semiconductor layer. In some cases, there is a refractive index contrast (Δn) between alternating layers after porosification, ranging from approximately 0.1 to 2, or approximately 0.1 to 2.5.

[0120] The size, shape, and thickness of each layer and structure of the above-described light-emitting structure can be flexibly set according to actual application requirements. In some cases, the thicknesses of different structures and layers may be as shown in the table below: Table 2. Thickness

[0121] *The ranges mentioned above also encompass sub-ranges, and any specific thickness within the ranges listed in Table 2 is included.

[0122] It is understood that the thickness of the above-described structures used to fabricate a VCSEL with a DBR light-emitting structure can also define the thickness of these layers.

[0123] In some cases, for the light-emitting structure, the n-type doped semiconductor layers present in the alternating layers have the same thickness as each other, and / or the undoped (or low-doped) semiconductor layers present in the alternating layers have the same thickness as each other. The n-type doped and undoped (or low-doped) semiconductor layers may have the same or different thicknesses.

[0124] In some cases, as shown in FIG12, the aperture region is included in the mesa structure. In this case, the size of the mesa structure is selected to be larger than the size of the aperture region.

[0125] A non-limiting fabrication method for manufacturing a light-emitting structure including a DBR mirror and a aperture region formed by ion implantation (see page 16 / 31, CN 121532916 A). The method may include the following steps: (a) setting or forming a light-emitting structure, comprising: a bottom structure including alternating n-type doped layers and undoped (or lightly doped) semiconductor layers on a semiconductor substrate; an n-type doped first semiconductor layer on top of the bottom structure; a light-emitting structure including multiple quantum wells (MQWs) on top of the first semiconductor layer; a p-type doped first semiconductor layer on top of the light-emitting structure; a p-type doped second semiconductor layer having a p-type doping concentration greater than about 1 × 10¹⁸ cm⁻³, located on top of the p-type doped first semiconductor layer; an n-type doped second semiconductor layer on top of the p-type doped second semiconductor layer having an n-type doping concentration greater than about 1 × 10¹⁸ cm⁻³; and an n-type doped current diffusion layer on top of the n-type doped second semiconductor layer. (b) Placing a mask material over the top surface region of the current diffusion layer of the structure; (c) Performing ion implantation to reduce the conductivity of at least the p-type doped first semiconductor layer not covered by the mask material; (d) Etching a portion of the current diffusion layer, wherein the etching does not remove the current diffusion layer beneath the mask material; (e) Removing the mask material; (f) Depositing a first layer of silicon dioxide over a portion of the current diffusion layer to cover the region where at least the mask material is present; (g) Annealing the structure to improve the conductivity of the current diffusion layer; (h) Forming a mesa structure by etching the current diffusion layer, the n-type doped second semiconductor, the p-type doped second semiconductor, the p-type doped first semiconductor, and the portion of the light-emitting structure not covered by the first layer of silicon dioxide; (i) Depositing a second layer of silicon dioxide on the mesa structure, wherein at least a portion of the n-type doped first semiconductor layer is not covered by the second layer of silicon dioxide; (j) Etching the structure not covered by the second layer of silicon dioxide to form trenches thereby exposing the sidewalls of the alternating layers of the bottom structure; (k) Selectively porosilicate the n-type doped semiconductor layers in the alternating layers of the bottom structure, wherein the formed pores include air, and the undoped semiconductor layers remain porosilicate-free or substantially porosilicate-free; (l) Deposit one or more materials to cover the trenches, sidewalls, and sidewalls of the mesa structure; (m) Selectively remove the one or more materials to expose at least a portion of the top of the mesa structure and optionally expose a portion of the semiconductor layers covered by the one or more materials; and (n) Form metal contacts on a portion of the top of the mesa structure and optionally on a portion of the semiconductor layers.

[0126] Specific fabrication details of the bottom structure are detailed in Section IV below. Figure 10 illustrates an example flow of the above method.The process begins with structure 400 as shown in Figure 9, and Figure 10 illustrates the process of placing a mask material in the top layer to protect the region below it from ion implantation (530). As described in Example 2, the conductivity of the top layer, including at least the n-type doped material, is selectively restored by an annealing process.

[0127] Methods for depositing / forming light-emitting structures, including multiple quantum wells (MQWs), are known in the art.

[0128] The structures and layers formed or deposited in the above methods can all be achieved independently by existing deposition techniques (including metallurgical chemical vapor deposition, page 17 / 31, CN 121532916 A). The selection of precursors, p-type or n-type dopants, and the process conditions for forming and doping such structures and layers at a specified thickness are all well known in the art.

[0129] Regarding the annealing treatment in step (g), it can be carried out under any suitable high temperature conditions, and the annealing time must meet the requirement of improving the conductivity of the current diffusion layer after ion implantation. In some cases, annealing can restore the conductivity of the ion-implanted current-diffusion layer to at least 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, 90%, or higher of the pre-implantation level. In some cases, the annealing temperature range can be set between about 250°C and 450°C, or may include sub-ranges or specific temperature values ​​within this range. The annealing time can be adjusted between about 1 minute and 1 hour or between 1 minute and 30 minutes, also including sub-ranges or specific durations within this range. In some cases, such as when using an n-type indium phosphide current-diffusion layer, the annealing temperature can be set to 350°C, and an annealing time of about 20 minutes can be applied to restore the conductivity of the current-diffusion layer.

[0130] Regarding the mesa structure formed in step (h), its size must be larger than the hole region size. In other words, the mesa structure must completely encompass the hole region. This structure can be formed by wet etching or plasma etching (such as RIE etching).

[0131] For the specific semiconductor materials constituting the light-emitting structure (such as p-type doped second semiconductor layers and n-type doped second semiconductor layers), there are minimum requirements for their doping concentration, as described above. For the remaining p-type or n-type doped layers, there are no particular restrictions on their doping concentration levels. In some cases, different p-type or n-type doped layers may each independently have a doping concentration level of at least about 1 × 10¹⁹ cm⁻³ or higher; or be in the range of about 0.1 × 10¹⁹ cm⁻³ to 10 × 10²⁰ cm⁻³. In some cases, high doping concentration levels may be about 1 × 10¹⁹ cm⁻³, 2 × 10¹⁹ cm⁻³, 3 × 10¹⁹ cm⁻³, 4 × 10¹⁹ cm⁻³, 5 × 10¹⁹ cm⁻³, 6 × 10¹⁹ cm⁻³, 7 × 10¹⁹ cm⁻³, 8 × 10¹⁹ cm⁻³, 9 × 10¹⁹ cm⁻³, or 10 × 10¹⁹ cm⁻³. In some other cases…Different p-type or n-type doped layers can each independently have a medium doping concentration level, ranging from approximately 1 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 2 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 3 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, 4 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³, or 5 × 10¹⁸ cm⁻³ to less than 1 × 10²⁰ cm⁻³. In some cases, the medium doping concentration range is 1 × 10¹⁹ cm⁻³ to less than 1 × 10²⁰ cm⁻³, or approximately 0.5 × 10¹⁹ cm⁻³ to less than 1 × 10²⁰ cm⁻³. In some cases, moderate doping levels are approximately 1×10¹⁸ cm⁻³, 2×10¹⁸ cm⁻³, 3×10¹⁸ cm⁻³, 4×10¹⁸ cm⁻³, 5×10¹⁸ cm⁻³, or 6×10¹⁸ cm⁻³, 7×10¹⁸ cm⁻³, 8×10¹⁸ cm⁻³, 9×10¹⁸ cm⁻³, or 10×10¹⁸ cm⁻³. However, in other cases, different p-type or n-type doped layers may each have a doping concentration below approximately 20×10¹⁷ cm⁻³ or between approximately 0.5×10¹⁷ cm⁻³ and 10×10¹⁷ cm⁻³. In some cases, the low doping concentration level may be about 1×10¹⁷ cm⁻³, 2×10¹⁷ cm⁻³, 3×10¹⁷ cm⁻³, 4×10¹⁷ cm⁻³, 5×10¹⁷ cm⁻³, 6×10¹⁷ cm⁻³, 7×10¹⁷ cm⁻³, 8×10¹⁷ cm⁻³, 9×10¹⁷ cm⁻³, or 10×10¹⁷ cm⁻³.

[0132] In some cases, the mask material in step (b) may be selected from the group including, but not limited to, dielectric materials (such as silicon dioxide, silicon nitride, aluminum oxide), metals (such as nickel), and / or photoresists. Such materials may be formed by a variety of methods, such as plasma-enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), or other suitable methods known in the art.

[0133] For the method described above, any material can be patterned, etched, or removed as needed using any suitable technique (e.g., wet chemical etching, plasma etching, inductively coupled plasma reactive ion etching (ICP-RIE)).

[0134] In some cases, suitable semiconductor materials for the n-type doped first semiconductor layer, p-type doped first semiconductor layer, p-type doped second semiconductor layer, n-type doped second semiconductor layer, and current diffusion layer for the light-emitting structure have been discussed in detail in Section IIIa above.

[0135] For the method described above, the layers, structures, and overall light-emitting structure formed according to the method can have any suitable size, shape, and thickness. Exemplary (non-limiting) thicknesses of the layers and structures in the overall structure are shown in Table 2.

[0136] In some embodiments, the one or more materials are selected from the group consisting of silicon dioxide, alumina, silicon nitride, spin-coated glass, etc.; and / or the one or more materials are selected from organic materials such as benzocyclobutene (BCB), polyimide, photoresist, etc.; and combinations of the above materials. For the method, the deposition of the silicon oxide layer and one or more materials can be achieved by various processes, such as plasma-enhanced chemical vapor deposition (PECVD), atomic layer deposition (ALD), or other known and applicable methods.

[0137] In some embodiments, the porosity formed in step (k) is at least 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%.

[0138] In some embodiments, step (k) is achieved by electrochemical etching in an electrolyte and under an applied bias voltage. In certain cases, the electrolyte may include halide ions, hydrochloric acid (HCl), sulfuric acid (H2SO4), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)2, Ca(OH)2, Sr(OH)2, NH4OH, etc. Sulfuric acid (H2SO4), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)2, Ca(OH)2, Sr(OH)2, NH4OH, NaCl, NaF, nitric acid (HNO3), organic acids and their salts (such as oxalic acid and citric acid), and mixtures thereof.

[0139] In some embodiments, the metal contact formed in step (n) is composed of one or more of the following metals: titanium (Ti), platinum (Pt), gold (Au), germanium (Ge), gallium (Ga), nickel (Ni), palladium (Pd), indium (In), and combinations thereof. Methods for preparing such metal contacts are well known to those skilled in the art.

[0140] i. Ion Implantation Regarding step (c), ion implantation may be carried out according to the following details: The mask material in step (b) may be made of the material specified above. More specifically, the mask material may be considered as an ion implantation mask material, the size, area or shape of which can be arbitrarily set, thereby controllably selecting which areas of the surface are protected from ion implantation.

[0141] Such ion implantation masks may be prepared by a variety of methods. Non-limiting examples include, but are not limited to: (1) Photoresist method: A photoresist layer is spin-coated onto a substrate, and then the mask layer is patterned as required by photolithography, electron beam lithography or imprinting. Depending on the ion source and ion energy used, the mask layer thickness may be adjusted to less than about 1 μm to greater than 10 μm as required.

[0142] (2) Hard mask etching method: A hard mask material layer is deposited, which may be a dielectric (such as silicon dioxide or silicon nitride) or a metal (such as titanium, aluminum, etc.). Different deposition techniques may be used depending on the material properties, such as thermal evaporation, electron beam evaporation, sputtering,Spin coating, chemical vapor deposition, atomic layer deposition, etc. Then spin coating and patterning of photoresist layer on the deposited hard mask layer. Finally, the hard mask layer is removed by chemical or physical etching, and the photoresist pattern is transferred to the bottom layer material.

[0143] (3) Hard mask stripping method: Similar to the above process (hard mask etching method), but the operation order is reversed. First, spin coating of photoresist layer and patterning are formed, and then any of the techniques in (2) above are used to deposit hard mask layer on top of photoresist layer. Then the photoresist is etched to strip the unmasked area in hard mask layer, thereby transferring the pattern to hard mask layer.

[0144] In the ion implantation step, ion implantation is performed only on the exposed area not covered by the mask. Implanted ions can come from a variety of ion sources. A variety of ion types and sources can be selected, such as aluminum, gold, nitrogen, hydrogen, helium, carbon, oxygen, titanium, iron, etc., to change (i.e. damage / reduce) the conductivity of the ion implantation area. In some cases, ions can be selected based on the principle of higher atomic mass. For example, aluminum ions are chosen over hydrogen ions due to their larger atomic mass. The selected energy depends on the desired ion implantation depth and can range from below about 10 keV to above about 1 megaelectron volt, to control the implantation depth within the following ranges: below about 10 nm to above about 1 μm, about 10 nm to about 750 nm, about 10 nm to about 500 nm, about 10 nm to about 250 nm, about 10 nm to about 100 nm, or any suitable sub-range or single depth value within the above ranges. Ion dose can also be used to control the number of implanted ions, thereby modulating conductivity changes. Typical ion implantation dose ranges can cover, but are not limited to, about 10¹² to 10¹⁶ cm⁻³, depending on the ion species and target depth. The energy of the ion implantation source can be used to control the implantation depth of ions in layered structures. Specification 19 / 31 Page 31 CN 121532916 A

[0145] b. Optoelectronic device containing ion implanted aperture region As described above, the light-emitting structure including birefringent lattice (DBR) and aperture region can be used to fabricate optoelectronic devices with aperture region.

[0146] In some cases, the optoelectronic device may include: a light-emitting structure including a bottom distributed Bragg reflector and aperture region; a top distributed Bragg reflector; and a metal electrode.

[0147] For optoelectronic devices, the light-emitting structure includes a bottom distributed Bragg reflector (BDR) reflector and aperture region as described above. Figure 13 shows a non-limiting example of an optoelectronic device (such as a vertical cavity surface-emitting laser VCSEL).

[0148] In some cases, the top distributed Bragg reflector is composed of or includes alternating layers of any of the following: amorphous silicon / silicon dioxide, titanium dioxide / silicon dioxide, tantalum pentoxide / silicon dioxide, niobium pentoxide / silicon dioxide,Zinc selenide / silicon dioxide, amorphous silicon / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof.

[0149] In some cases, the metal contacts are made of or include one or more metals selected from the group consisting of titanium, platinum, gold, germanium, nickel, palladium, indium, and combinations thereof.

[0150] In some cases, the optoelectronic device is a vertical-cavity surface-emitting laser (VCSEL). In some cases, the VCSEL operates in continuous-wave mode at room temperature (about 25°C).

[0151] In other cases, the VCSEL can operate at temperatures below about 0°C, above about 25°C, or above about 85°C. In still other cases, the VCSEL can operate in pulsed mode.

[0152] The VCSEL includes an aperture region that can emit in the infrared and / or red wavelength region, depending on the selection of the emitting structure material. In some cases, the power conversion efficiency of a vertical-cavity surface-emitting laser (VCSEL) reaches at least about 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 7.5%, or 10%.

[0153] A non-limiting method for fabricating an optoelectronic device including an aperture region may include the following steps: (a') setting or forming a light-emitting structure including a bottom distributed Bragg reflector and an aperture region; (b') setting or forming a top distributed Bragg reflector on the light-emitting structure; and (c') setting or forming a metal electrode on the optoelectronic device.

[0154] For an optoelectronic device fabricated according to the above method, its light-emitting structure includes a bottom distributed Bragg reflector (BDR) and an aperture region as described above. Figure 14 shows a non-limiting process flow for fabricating an optoelectronic device (such as a vertical-cavity surface-emitting laser, VCSEL).

[0155] In this method, the top distributed Bragg reflector in step (b') may comprise alternating layers of any of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof. Methods for manufacturing such deep reflective layers having the above-described alternating layers are known in the art. The number of alternating layers in such deep reflective layers may depend on the selected material. The top deep reflective layer mirror may be deposited by methods in the art and may include annealing to improve reflectivity. In some cases, the reflectivity of the top deep reflective layer mirror is at least about 97% or higher.

[0156] For the above method, the metal contacts in step (c') may be made of or include metals selected from titanium (Ti), platinum (Pt), gold (Au), germanium (Ge), nickel (Ni), palladium (Pd), indium (In), and combinations thereof.

[0157] For any of the methods described in Section III, it should be understood that the order of certain steps may be interchanged, provided that it is within permissible limits and does not affect the performance of the resulting structure or device. For example, steps (b') and (c') in the method for manufacturing optoelectronic devices (see page 32 of CN 121532916 A, 20 / 31) may be performed in any suitable order.

[0158] IV. Bottom Structure and its Fabrication and Porosification Methods The various structures (such as semiconductor structures, light-emitting structures) and the bottom structures of the optoelectronic devices described in Sections II and III above will be described in detail below.

[0159] For semiconductor structures 100, 100', 100'', 100''', 10, and 400, each structure includes a bottom structure of alternating doped and undoped (or lightly doped) semiconductor layers on a semiconductor substrate. The semiconductor substrate may be made of materials such as indium phosphide (InP), gallium arsenide (GaAs), or gallium antimonide (GaSb). In these specific structures, the n-type doped semiconductor layer has not undergone selective porosification treatment such as electrochemical etching and remains intact.

[0160] In a non-limiting example, the bottom structure includes multiple undoped or lightly doped (see below) semiconductor layers, which may be composed of indium phosphide, gallium arsenide, or gallium antimonide layers, wherein at least one n-type doped semiconductor layer exists between at least two undoped or lightly doped semiconductor layers, which can be porosified by electrochemical etching (or electropolishing).

[0161] The bottom structure includes alternating semiconductor layers on a semiconductor substrate. In some cases, a semiconductor substrate is selected first, and then a suitable semiconductor material that matches the lattice of the substrate is selected to form alternating n-type doped layers and undoped (or lightly doped) layers. For example, the semiconductor substrate of the bottom structure may be made of indium phosphide (InP), gallium arsenide (GaAs), or gallium antimony arsenide (GaSb). It should be noted that the semiconductor substrate and alternating layers of the bottom structure do not necessarily have to be made of the same material, but it is best to use lattice-matched materials, which is within the scope of choice for those skilled in the art. The size, area, or shape of the semiconductor substrate and its doped or undoped (or lightly doped) layers can be arbitrarily and reasonably set according to specific application requirements. Typically, the semiconductor substrate and all its layers have the same size, area, and shape. In some cases, the overall dimensions (i.e., length and width) of the bottom structure can be approximately 100 micrometers × 100 micrometers, including sub-dimensions therein.

[0162] In some cases, the alternating layers of the bottom structure comprise or are composed of binary semiconductor materials selected from, but not limited to, the group consisting of indium phosphide, gallium arsenide, and gallium antimonide, and are lattice-matched to the semiconductor substrate. In other cases, the alternating layers of the bottom structure comprise or are composed of ternary semiconductor materials that are lattice-matched to the semiconductor substrate. In still other cases, the alternating layers of the bottom structure comprise or are composed of quaternary semiconductor materials that are lattice-matched to the semiconductor substrate.

[0163] In some cases, non-limiting examples of binary semiconductor materials (which may be p-type or n-type doped) can be freely selected from the group consisting of InP, GaAs, GaSb, and AlAs. In some cases, non-limiting examples of ternary semiconductor materials (which may be p-type or n-type doped) can be freely selected from the group consisting of InAlAs, InGaAs, AlGaAs, InAlP, InGaP, AlAsSb, and InAsSb. In some cases, quaternary semiconductor materials (which may be p-type or n-type doped) can be freely selected from the group consisting of InAlGaAs, InGaAsP, and AlGaAsSb. It should be noted that when selecting any binary, ternary, or quaternary semiconductor material for the above single-layer or multi-layer structure, it is advisable to achieve lattice matching between the semiconductor material of each layer of the specific structure and the selected semiconductor substrate (which may be made of InP, GaAs, or GaSb). Those skilled in the art can select suitable semiconductor materials for each layer that are lattice-matched with the semiconductor substrate and determine the required doping type and doping concentration level, as described above.

[0164] In some cases, the bottom structure includes at least 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24 or more pairs of n-type doped and undoped (or lightly doped) semiconductor layers, which are at least in contact before electrochemical etching.

[0165] Those skilled in the art are familiar with methods for fabricating such bottom structures, such as existing epitaxial or homoepitaxial methods, such as metal-organic chemical vapor deposition (MOCVD), molecular beam epitaxy (MBE) or liquid phase epitaxy (LPE), and using known reactants, dopants and precursors to form the doped and undoped (or lightly doped) semiconductor layers.

[0166] As shown in FIG4, the bottom structure can be placed under electrochemical (EC) etching conditions, wherein the present n-type doped semiconductor layers are selectively porosized and multiple pores are formed within the n-type doped semiconductor layers. These pores are surrounded and adjacent to undoped or low-n-type doped semiconductor layers (pages 21 / 31, CN 121532916 A), which remain pore-free or substantially pore-free under electrochemical conditions (where "substantially pore-free" means the porosity of the doped layer (or low-doped layer) is less than 25%, 20%, 15%, 10%, 5%, 4%, 3%, 2%, or 1%). In some other cases, the pores are horizontally aligned (i.e., parallel) with the planar direction of the n-type doped semiconductor layers.

[0167] In certain cases, the bottom structure is composed of a single type of doped and undoped (or low-doped) semiconductor. For example, the bottom structure may be composed of a full indium phosphide layer, a full gallium arsenide layer, or a full gallium antimonide layer, which are doped alternately as described above. However, a hybrid structure of different material types may also be used.

[0168] If the doping concentration of an N-type doped semiconductor layer is sufficiently high, it can be selectively treated by the electrochemical etching process described below to achieve selective porosimetry of the doped semiconductor layer, or selective electropolishing (i.e., removal) of specific regions therein. Undoped or poorly doped semiconductor layers are generally not subject to electrochemical etching. The specific conditions for controlling the degree of porosimetry or achieving electropolishing will be further described below. Porosimetry and electropolishing do not require complete removal of the N-type doped semiconductor layer; only a portion or region of it needs to be porosimetric or electropolished in a particular electrochemical process. The structures formed by porosimetry or electropolishing during electrochemical etching include (air) pores or channels, which can be formed in the horizontal direction—this is due to the selective lateral etching acting on one or more sidewalls of the bottom structure.

[0169] Electrochemical etching requires that the N-type doped semiconductor layer be doped with an N-type dopant. Therefore, existing N-type doped semiconductor layers are formed during deposition / formation processes. Typical dopants include, but are not limited to, N-type germanium (Ge) and silicon (Si) dopant. Such dopant sources can include silane (SiH4), germanane (GeH4), and isobutylgermanane (IBGe), etc. For n-type doped layers, the n-type doping concentration can remain uniform throughout the layer or form a concentration gradient (i.e., a layer with a gradient doping concentration along the layer axis, such as the width direction). A doping concentration of at least about 1 × 10¹⁹ cm⁻³ or higher is considered high concentration; or in the range of about 0.1 × 10¹⁹ cm⁻³ to 10 × 10²⁰ cm⁻³. In some cases, high doping concentration levels can be about 1 × 10¹⁹ cm⁻³, 2 × 10¹⁹ cm⁻³, 3 × 10¹⁹ cm⁻³, 4 × 10¹⁹ cm⁻³, 5 × 10¹⁹ cm⁻³, 6 × 10¹⁹ cm⁻³, 7 × 10¹⁹ cm⁻³, 8 × 10¹⁹ cm⁻³, 9 × 10¹⁹ cm⁻³, or 10 × 10¹⁹ cm⁻³. Doping concentrations of 1×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 2×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 3×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 44×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 5×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 6×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 7×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 8×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, 9×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³, and 10×10¹⁸ cm⁻³ to 1×10²⁰ cm⁻³ are considered medium doping concentrations. In some cases, the medium doping concentration range...The range is from 1×10¹⁹ cm⁻³ to less than 1×10²⁰ cm⁻³, or approximately 0.5×10¹⁹ cm⁻³ to less than 1×10²⁰ cm⁻³. In some cases, medium doping concentration levels may be approximately 1×10¹⁸ cm⁻³, 2×10¹⁸ cm⁻³, 3×10¹⁸ cm⁻³, 4×10¹⁸ cm⁻³, 5×10¹⁸ cm⁻³, 6×10¹⁸ cm⁻³, 7×10¹⁸ cm⁻³, 8×10¹⁸ cm⁻³, 9×10¹⁸ cm⁻³, or 10×10¹⁸ cm⁻³. Medium to high concentrations of n-type doping are affected by the electrochemical etching process and result in controlled porosimetry and / or electropolishing of the doped layer, depending on the operating conditions in the electrochemical etching process.

[0170] As described above, the bottom structure includes undoped semiconductor layers that are unaffected (not porosimetric or etched) when the bottom structure is electrochemically etched. However, in some cases, the bottom structure may include a low-doped or very low-doped semiconductor layer, the doping concentration of which is considered low, specifically below about 20 × 10¹⁷ cm⁻³ or between about 0.5 × 10¹⁷ cm⁻³ and 10 × 10¹⁷ cm⁻³. In some cases, a medium doping concentration level may be about 1 × 10¹⁷ cm⁻³, 2 × 10¹⁷ cm⁻³, 3 × 10¹⁷ cm⁻³, 4 × 10¹⁷ cm⁻³, 5 × 10¹⁷ cm⁻³, 6 × 10¹⁷ cm⁻³, 7 × 10¹⁷ cm⁻³, 8 × 10¹⁷ cm⁻³, 9 × 10¹⁷ cm⁻³, or 10 × 10¹⁷ cm⁻³.

[0171] Prior to electrochemical etching, the thickness of any single n-type doped or undoped layer (low-doped layer) may independently be between about 50 and 500 nm (including the subranges or individual thickness values ​​disclosed therein). In some cases, the total thickness of the bottom structure before or after electrochemical etching may range from about 600 nm to about 8,000 nm or from 600 nm to about 6,000 nm, and include its sub-ranges. The dimensions and / or shape of each layer or semiconductor substrate may be any suitable form / size required for the application. In some cases, for the bottom structure, the n-type doped semiconductor layers present in the alternating layers have the same or substantially the same thickness; and / or the undoped (or low-doped) semiconductor layers present in the alternating layers have the same or substantially the same thickness. "Substantially the same" as used herein means that the thickness of each particular layer differs from the thickness of all other similar layers by less than about 5%, 4%, 3%, 2%, 1% or less. The n-type doped layers and the undoped (or low-doped) layers may have the same or different thicknesses.

[0172] After electrochemical etching, the undoped or low-doped semiconductor layers in the bottom structure are generally unaffected (i.e., pore-free).porosification or substantially non-porosification, wherein "substantially non-porosification" refers to a porosity lower than 25%, 20%, 15%, 10%, 10%, 5%, 4%, 3%, 2% or 1%). In some embodiments, unintended porosification may occur in an undoped (or lightly doped) semiconductor layer, that is, even a lightly n-type doped semiconductor layer may form pores during electrochemical etching.

[0173] After being subjected to electrochemical etching, the n-type doped semiconductor layer in the bottom structure exhibits porosification characteristics compared to that before etching. When at least one region in the layer has a porosity ranging from about 10% to 90% or higher, the degree of porosification can be significantly increased. In some cases, the porosity can reach at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80% or 90% or above. Introducing a low-refractive-index substance (such as air) into the layer (or a part thereof) through porosification can reduce the refractive index, compared with the bulk semiconductor layer before porosification.

[0174] For an n-type doped semiconductor layer, by changing the type and concentration of the electrolyte, the n-type doping concentration of the layer and the applied bias voltage, electrochemical etching can produce different degrees of porosity and pore morphology (see details below).

[0175] Electrochemical etching can be used to selectively form lateral or horizontal pores in the hydrophobized n-type doped semiconductor layer of the bottom structure. These pores are selectively formed from the side surfaces of the multilayer structure. Without limitation, the lateral or horizontal pores formed during electrochemical etching can have any suitable length. The porosified semiconductor layer (or a region therein) included in the multilayer structure is preferably nano-scale, but can be further defined as micro-, meso-, or macro-pores or any combination of the above structures. The porosified layer or region can be further subdivided into micropores (d<2nm), mesopores (2nm<d<50nm) or macropores (d>50nm), where d is the average pore diameter. The pore morphology in the layer or region can be classified as circular, semicircular, elliptical or a combination thereof. The average size (i.e., length) of the pores can be between about 5 to 100 nm, 5 to 75 nm, 5 to 50 nm, or 5 to 25 nm. In some cases, the average pore diameter can reach about 5, 10, 20, 30, 40, 50, 60, 70, 80, 90, 100 nm or larger. In some cases, depending on the original doping concentration, the etchant used, and the applied voltage during electrochemical porosification, the average size of the pores can vary from less than about 20 nm to more than 50 nm. The spacing between adjacent pores (which can also be regarded as an indicator of pore wall thickness) can be distributed in the following intervals: about 1 to 50 nm, 5 to 50 nm, 5 to 40 nm, 5 to 30 nm, 5 to 25 nm, 5 to 20 nm, 5 to 15 nm, or 5 to 10 nm.

[0176] In a given bottom structure, all or part of the doped semiconductor layer can form a porous structure during electrochemical etching. In some cases, electrochemical etching starts from the sidewall, and the degree of porosification of the layer reaches at least the longest plane of the doped layer10%, 20%, 30%, 40%, 50%, 60%, 80%, or 90% of the size. In other cases involving electropolishing, the degree of electropolishing of a single layer is at least 10%, 20%, 30%, 40%, 50%, 60%, 80%, or 90% of the longest planar dimension of the doped layer. During electrochemical etching, porosity within each doped layer may occur uniformly or non-uniformly. During electrochemical etching, electropolishing may occur uniformly or non-uniformly within each doped layer.

[0177] As described above, in some cases, n-type doped semiconductor layers are removed (completely removed) by electropolishing, resulting in almost no or no material remaining between undoped (or lightly doped) layers—that is, where the original doped semiconductor material was located. The size of the voids formed by electropolishing depends on the thickness of the doped semiconductor layer and the amount of material removed by electropolishing. In some cases, electropolishing can form lateral or horizontal (air) pores or channels between undoped layers where the doped material has been removed.

[0178] a. Optical properties of the bottom structure: By selectively introducing a low-refractive-index material (such as air) into specific regions of the bottom structure or layers A of the specification (pages 23 / 31, CN 121532916 A), the refractive index of these regions can be reduced to be lower than that of the host semiconductor material constituting the structure. Therefore, the refractive index of the porous regions in the bottom structure can be selectively adjusted.

[0179] For example, before electrochemical etching, the refractive index of each layer of the bottom structure composed of InP is approximately 3.2. Electrochemical etching can selectively porosilicate or fully electropolish the n-type doped InP layers, thereby reducing the refractive index to below 3.2. In some cases, the refractive index of the porous InP layer is approximately 1.5 to 2.7. When the InP layer is removed by electropolishing, the refractive index is approximately 1. Therefore, the refractive index contrast (Δn) between InP layers after electrochemical etching can reach approximately 0.1 to 2. In some cases, the refractive index contrast (Δn) reaches at least 1.1, 1.2, 1.3, 1.4, or 1.5. In other cases, the refractive index contrast (Δn) is at least 1.5.

[0180] Prior to electrochemical etching, the refractive index of each layer in the bottom structure composed of gallium arsenide is approximately 3.95. Electrochemical etching selectively porosilicates or fully electropolishes the doped indium phosphide layers, thereby reducing the refractive index below 3.95. In some cases, the refractive index of the porosilicated GaAs layers is approximately 1.5 to 3.4. When the GaAs layers are removed by electropolishing, the refractive index is approximately 1. Therefore, the refractive index contrast (Δn) between the GaAs layers after electrochemical etching may be in the range of approximately 0.1 to 2.5. In some cases, the refractive index contrast (Δn) is at least 1.1, 1.2, 1.3, 1.4, or 1.5. In other cases, the refractive index contrast (Δn) is at least 1.5.

[0181] Before electrochemical etching, the refractive index of each layer in the bottom structure composed of GaSb is approximately 3.85. Electrochemical etching can selectively porosilicate or fully electropolish the doped InP layer, thereby reducing the refractive index to below 3.85. In some cases, the refractive index of the porosilicated GaAs layer is approximately 1.2 to 3.4. When the GaAs layer is removed by electropolishing, the refractive index is approximately 1. Therefore, the refractive index contrast (Δn) between the GaAs layers after electrochemical etching may be in the range of approximately 0.1 to approximately 2. In some cases, the refractive index contrast (Δn) reaches at least 1.1, 1.2, 1.3, 1.4, or 1.5. In other cases, the refractive index contrast (Δn) reaches at least 1.5.

[0182] The bottom structure can be used as a reflector with a reflectivity of at least approximately 99%, 99.1%, 99.2%, 99.3%, 99.4%, 99.5%, 99.6%, 99.7%, 99.8%, or 99.9%.

[0183] b. Method of Electrochemical (EC) Etching of the Bottom Structure As described above, the method of forming alternating doped and undoped (or lightly doped) semiconductor layers is described in the prior art. However, the method of forming the bottom structure may include the following non-limiting example steps: (a) forming a first undoped or lightly doped semiconductor layer over a semiconductor substrate; (b) depositing a second n-type doped semiconductor layer on the first layer; (c) depositing a third undoped or lightly doped semiconductor layer over the second layer; (d) optionally repeating steps (b) and (c) to form additional alternating n-type doped and undoped or lightly doped semiconductor layers.

[0184] The formed bottom structure can be used to fabricate other structures, as shown in Figures 2, 4, and 10. In such processes, it can be electrochemically (EC) etched, as shown in Figures 4 and 10.

[0185] Electrochemical (EC) etching of the n-type doped semiconductor layer can be performed in an electrolyte and under an applied bias voltage to selectively porosilicate or electropolish at least a portion of the n-type doped semiconductor. The porosilicate and / or electropolishing phenomena occurring during the electrochemical (EC) etching process can be controlled by adjusting the electrolyte concentration, doping concentration, and applied bias voltage (described below). The applied bias voltage is typically a positive voltage, ranging from approximately 0.1 to 10 V, 1.0 to 5 V, or 1.0 to 2.5 V. In some cases, depending on the initial doping concentration and the type of etchant used, the applied bias voltage range can be less than about 1 V to at least about 10 V or higher. When using a lower relative doping concentration, porosity can be selectively minimized—for example, in a non-limiting example, a doping concentration of 5 × 10¹⁸ cm⁻³ in a sample results in a lower porosity than a doping concentration of 2 × 10¹⁹ cm⁻³ under the same etching conditions. In all relative concentration differences, the following can be expected: (Instructions for Use, Page 24 / 31, 36, CN 121532916 A)This phenomenon indicates that, when other electrochemical etching parameters are constant, higher doping concentrations produce a more significant porosity effect compared to lower relative concentrations. In some cases, depending on the choice of electrolyte concentration, doping concentration, and applied bias voltage, electrochemical etching conditions can selectively and controllably produce only porosity (introducing approximately 30% to 90% or higher porosity) or achieve complete electropolishing (i.e., complete or near-complete removal of doped material, with removal rates greater than 95%, 96%, 97%, 98%, or 99%). The direction of the electric field during electrochemical etching can be used to control the etching direction, thereby modulating the porosity orientation etched into the n-type doped semiconductor layer. For example, the electroetching direction can be determined as a function of the electric field direction. This process preferably produces a lateral etching direction. The lateral etching rate can be set to approximately 0.1 μm / min, 0.2 μm / min, 0.3 μm / min, 0.4 μm / min, 0.5 μm / min, 0.6 μm / min, 0.7 μm / min, 0.8 μm / min, 0.9 μm / min, 1 μm / min, 2 μm / min, 3 μm / min, 4 μm / min, 5 μm / min, 6 μm / min, 7 μm / min, 8 μm / min, 9 μm / min, 10 μm / min, 20 μm / min, 30 μm / min, 40 μm / min, or 50 μm / min.

[0186] Electrochemical etching can be performed under the applied bias voltage for a time range of approximately 1 minute to 24 hours, 1 minute to 12 hours, 1 minute to 6 hours, 1 minute to 4 hours, 1 minute to 2 hours, 1 minute to 1 hour, or 1 minute to 30 minutes. In some cases, electrochemical etching needs to be performed at the applied bias voltage for at least approximately 5 minutes, 10 minutes, 15 minutes, 20 minutes, 25 minutes, 30 minutes, 35 minutes, 40 minutes, 45 minutes, 50 minutes, 55 minutes, 60 minutes, 2 hours, 3 hours, 4 hours, 5 hours, 6 hours, 10 hours, 15 hours, 20 hours, 24 hours, or longer. Electrochemical etching can be performed at room temperature or within a temperature range of approximately 10°C to 50°C at the applied bias voltage. The etching can be performed at room temperature or optionally in an inert atmosphere (such as nitrogen or argon).

[0187] Electrochemical etching can be performed in highly conductive electrolytes (salts or acids) of various types and concentrations. Exemplary highly conductive electrolytes include, but are not limited to: halide ions (fluoride, chloride, bromide, iodide), hydrochloric acid (HCl), sulfuric acid (H₂SO₄), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)₂, Ca(OH)₂, Sr(OH)₂, NH₄OH, NaCl, NaF, nitric acid (HNO₃), organic acids and their salts (such as oxalic acid and citric acid), and mixtures thereof. The electrolyte concentration range in highly conductive electrolyte solutions (typically aqueous solutions) is approximately 0.0.1 to 10 mol / L. In some other cases, the concentration of the electrolyte in a highly conductive electrolyte solution (typically an aqueous solution) can be defined as the volume percentage of the electrolyte to the solvent (e.g., water), ranging from about 0.1% to 30% (volume percentage). In other cases, the concentration of the electrolyte in a highly conductive electrolyte solution (typically an aqueous solution) can be defined as the percentage (weight / volume) of the electrolyte relative to the solvent (e.g., water) in which it is dissolved, ranging from about 0.1% to 30% (weight). The above-mentioned electrolytes typically do not etch semiconductor materials such as InP, GaAs, or GaSb at room temperature, but can etch such semiconductors when electrochemical anodic conditions are applied.

[0188] It is believed that the electrochemical etching described herein begins with the exposure of sidewall edges, for example, preferentially forming horizontal pores in the lateral direction. Lateral etching leads to porosification, causing pores (typically nanopores) to form horizontally or predominantly horizontally within the doped layer. The bottom structure has a vertical axis from the bottommost layer to the top layer, on which alternating doped and undoped (or lightly doped) planar structures exist. When electrochemical etching is initiated, the porosification process of the n-type doped layer will occur perpendicular or primarily perpendicular to the vertical axis. "Primarily perpendicular" as used herein refers to an average deviation of the pore direction from the vertical axis perpendicular / horizontal plane of approximately 20, 15, 10, or 5 degrees. In other words, porosification occurs horizontally or primarily horizontally, parallel or nearly parallel to the plane of the doped layer. For the bottom structure, after electrochemical etching, vertically aligned pores may be minimal or nonexistent. Pores do not need to be aligned with the vertical axis of the bottom structure. In some cases, vertically aligned pores will not form in the doped layer; only horizontal pores will form during electrochemical etching. In some cases, undoped (or poorly doped) InP, GaAs, or GaSb materials will also form nm pores in the

[111] crystallographic direction, which are inclined at a 45-degree angle to the vertical

[001] plane and the horizontal direction. In other cases, macroscopic-level nm pores may form in n-type doped semiconductors and diffuse laterally during porosification; while microscopic-level nm pore formation may occur along specific crystallographic directions (e.g., at an angle of +45° or -45° relative to the surface of the doped layer).

[0189] Electrochemical etching typically involves two steps: oxide formation and removal (Quill, N. et al., 2013, ECS transactions, 58(8), 25-38). Studies suggest that the presence of free holes at the semiconductor / electrolyte interface is crucial for the oxidation process, and the formed oxides can be readily dissolved in various electrolytes. Free holes are provided by the electric field-assisted tunneling effect, and their quantity depends primarily on the anode bias and doping concentration. In some cases, electrochemical etching conditions can lead to low anode density.Electrochemical etching is not possible at extreme bias and / or low doping concentration (low doping as described above), while electropolishing (i.e., complete etching) is observed at high bias and / or high n-type doping concentration. Porosity occurs at medium bias and / or doping concentration.

[0190] V. Application of Structures and Optoelectronic Devices The various structures and optoelectronic devices described herein (such as light-emitting structures with DBR mirrors and VCSELs) can be applied in the fields of electronics, photonics, and optoelectronics. Typical applications include, but are not limited to: low-power on-chip laser sources for optoelectronic integrated circuits; eye-friendly optical sensing systems based on VCSELs and VCSEL arrays; low-cost optical links for transmission over 1km based on single-mode fiber; free-space (last kilometer or indoor personal network) optical communication for 6G mobile networks and optical wireless networks; Internet of Things; low-cost optical detection and ranging systems; and biomedical sensing and diagnostic equipment and systems.

[0191] Of particular note is that the vertical-cavity surface-emitting laser (VCSEL) can achieve long-wavelength emission (i.e., emitting red, near-infrared, or infrared light in the 900 to 3,000 nm band, covering sub-bands and specific wavelengths within this range). In specific cases, the VCSEL can emit specific wavelengths or bands, such as approximately 650 nm, approximately 850 nm to approximately 940 nm, approximately 1,300 nm to approximately 1,600 nm, or approximately 2,000 nm to approximately 2,400 nm. In some cases, the VCSEL can emit in the red light band of the spectrum. Vertical-cavity surface-emitting lasers (VCSELs) have important application value in fields such as information processing, micro-displays, micro-projection, laser headlights, high-resolution printing, biophotonics, spectral detection, and atomic clocks.

[0192] Compared to the more commonly used edge-emitting laser diodes (EELDs), the various VCSELs described herein offer significant advantages in optical and electrical performance, such as: superior beam quality, compact form factor, low power consumption operation, cost-effective wafer-level testing, higher manufacturing yield, and lower manufacturing cost.

[0193] The invention can be further understood by referring to the following non-limiting examples.

[0194] Example 1: nm Multi-Porous Vertical-Cavity Surface-Emitting Laser (VCSEL) with Buried Tunnel Junction (BTJ) Materials and Methods: As shown in FIG1, a semiconductor structure 100 with a buried tunnel junction (BTJ) is fabricated starting from the epitaxial growth structure 10 shown in FIG2 (top row, far left). All layers are grown in a planar continuous manner. From bottom to top, structure 10 comprises six parts: (1) a stack 110 consisting of 12 pairs of alternating layers, wherein an n+ type indium phosphide (InP) layer (dark band, doping concentration: 5 × 10¹⁸ cm⁻³) and an n- type InP layer (light band, lightly doped, doping concentration: < 5 × 10¹⁸ cm⁻³) are interposed, wherein the n+ type InP can be passed through...Electrochemical etching forms a nm porous (NP) type InP layer with a low refractive index (lower than the refractive index of the layer before porosification); (2) a thick n-type InP layer 120 (light gray, doping concentration: 5 × 10¹⁷ cm⁻³), with a thickness of at least about 200 nm, constituting the bulk volume of the structure; (3) a light-emitting structure 130 composed of InAlGaAs, providing an active region with a target emission wavelength of 1,550 nm; (4) a p-type InP layer 140 (doping concentration: 5 × 10¹⁷ cm⁻³); (5) a p++ type InGaAs layer 150 (doping concentration > 1 × 10¹⁹ cm⁻³); and (6) an n++ type InGaAs layer 160 (black, doping concentration > 1 × 10¹⁹ cm⁻³). Structure 10 is grown by metal-organic chemical vapor deposition (MOCVD).

[0195] As shown in FIG1, the semiconductor structure 100 includes, from bottom to top: (1) a stack 110 consisting of 12 pairs of alternating layers, wherein n+ type indium phosphide (InP) layers and n- type InP layers are alternately arranged; (2) a thick n-type InP layer 120 with a thickness of at least about 200 nm; (3) a light-emitting structure 130 composed of InAlGaAs, providing an active region with a target emission wavelength of 1,550 nm; (4) a p-type InP layer 140; (5) a buried tunnel junction consisting of a p-type InGaAs layer 150 and an n++ type InGaAs layer 160; wherein (6) a current diffusion layer 170 encloses the tunnel junction; and optionally (7) the surface of the current diffusion layer has a non-planar structure, forming a stepped feature (180) and producing an optical confinement effect.

[0196] Starting with structure 10, Figure 2 shows a non-limiting process diagram for forming the BTJ structure. This process involves patterning a mask material on the top surface of structure 10 (middle of the top row in Figure 2). Subsequently, a wet etching process using a mixture of citric acid and hydrogen peroxide is performed to remove portions of the outer layers 150 and 160 of the mask region (far right of the top row in Figure 2). After mask removal (far left of the bottom row in Figure 2), an n-type indium phosphide layer (layer 170 in Figure 1) is regrown, burying the patterned tunnel junction beneath it (far right of the bottom row in Figure 2). The final result is a tunnel junction consisting of layer 150 (p++ type InGaAs) and layer 160 (n++ type InGaAs) as shown in Figure 1. This junction is confined to a small area and surrounded by an n-type InP layer (layer 170 in Figure 1). The BTJ structure is considered to have the following characteristics: 1) Current is mainly injected through the BTJ region (which can also be called the aperture region); in optoelectronic devices, only the carrier injection region can emit light and provide laser gain. Therefore, localized current injection is considered to achieve gain guidance to achieve optical localization; 2) After the regeneration of the layer 170, this process results in the top surface of the semiconductor structure 100 not being flattened.In other words, the surface above the BTJ or hole region is higher than the rest of the peripheral surface of layer 170, which can be regarded as a step feature 180 present in the structure, which provides an optical confinement effect for the optoelectronic device fabricated using structure 100.

[0197] As shown in FIG3, a light-emitting structure 200 including a distributed Bragg reflector (DBR) mirror is fabricated based on the aforementioned semiconductor structure 100. FIG3 shows the fabrication process flow for providing DBR for the light-emitting structure. Starting from semiconductor structure 100 (top left of FIG4), a mesa structure is formed by an etching process, which can be wet etching (dilute HCl followed by citric acid and H2O2) or dry etching (top center of FIG4), wherein the bottom of the mesa structure is located at layer 120. A SiO2 layer (30) is deposited by plasma-enhanced chemical vapor deposition (PECVD) and patterned so that the layer covers most of the top surface except for the left side (top right of top row of FIG4). In other words, SiO230 covers the entire mesa structure, except for the top edge of the sidewall surface. The SiO230 layer serves two purposes: 1) as a dry etching mask for subsequent process steps; and 2) to protect the mesa structure from subsequent electrochemical (EC) etching. Deep dry etching (8 sccm CH4, 4 sccm H2, 10 sccm Cl2, HF power 100W, ICP power 1,200W) is then performed, using SiO230 as a mask to form trenches that extend to the bottom of the stacked structure 110 (far left in Figure 4). This structure (anode) and platinum (Pt) wire / plate (cathode) are then immersed in an electrolyte for electrochemical (EC) etching (center in Figure 4). By applying a positive voltage, the electrochemical etching begins from the sidewall of the trench. The porosilicated region (dark region) expands laterally, eventually covering the entire BTJ or hole region above. It is worth noting that porosification is limited to the n+ type InP layer of the stacked structure 110, while the lightly doped InP layer remains intact (unporosified). The selectivity between the porosified and non-porosified regions is achieved through the difference in doping concentration. Porosification causes the n+ type InP layer to be filled with air, and its refractive index is lower than that of the lightly doped InP layer. This alternating structure of high-refractive-index and low-refractive-index layers forms a mirror in the DBR structure for fabricating vertical-cavity surface-emitting lasers (VCSELs).

[0198] After selective porosification of the stacked structure, another PECVD SiO2 layer (40) was deposited on the surface of the porosified sample (far right in the row of Figure 4). The purpose of this 40th layer is to cover and protect the entrance of the porosified stacked structure—the nanopore (NP) type InP. However, since PECVD SiO2 is known to induce leakage current (especially through the mesa sidewalls) (Jpn.J.Appl.Phys.38),1195(1999)), therefore, a buffered oxide etchant was used to remove the SiO2 layers 30 and 40 on the mesa structure (leftmost of the bottom row in Figure 4), and an Al2O3 layer (50) was deposited on it by atomic layer deposition (middle of the bottom row in Figure 4). Finally, the Al2O3 (50) layer was partially removed to expose the top of the mesa structure and at least a portion of the top surface of the 120th layer (rightmost of the bottom row in Figure 4), thereby forming a light-emitting structure including a distributed total reflection mirror.

[0199] Figure 3 shows in detail the light-emitting structure 200 including a DBR mirror. From bottom to top, the light-emitting structure 200 consists of the following parts: (1) a bottom structure 210, consisting of 12 pairs of alternating n+ type InP layers and n- type InP layers, wherein the n+ type InP layers are selectively porosized (as shown in the dark band) by electrochemical etching (as shown in the manual, page 27 / 31, CN 121532916 A); (2) a thick n-type InP layer 220 with a thickness of at least about 200 nm; (3) a tapered structure from bottom to top including: an InAlGaAs layer 230, a p-type InAlAs layer 240; a bipolar transistor composed of a p-type InAlAs layer 250 and an n-type InP layer 260; and a top n-type InP current diffusion layer 270. The top surface of the bipolar transistor is composed of a p-type InAlAs layer 250 and an n-type InP layer 260. A mesa structure consisting of a p++ type InAlAs layer 240, a p++ type InAlAs layer 250, and an n++ type InP layer 260; the top is an n-type InP current diffusion layer 270, the surface of which has a stepped feature 280. The additional layers shown in Figure 3 include an Al2O3 layer (295) and a SiO2 layer (290), which are present due to the manufacturing process but are not necessary for the light-emitting device or the dual-layer reflector (DBR) function included therein.

[0200] As shown in Figure 5, the light-emitting structure 200 including the dual-layer reflector mirror is used to form a vertical cavity surface-emitting laser 300. The light-emitting structure 200 including the dual-layer thin-film reflector (DBR) constitutes the bottom DBR reflector of the vertical cavity surface-emitting laser (VCSEL), while a top dielectric DBR reflector 310 and a metal electrode 320 are placed on top of the mesa structure, as shown in Figure 5. Figure 6 illustrates the fabrication process of VCSEL300, specifically including the formation of a top DBR 310 and metal contacts 320 on the light-emitting structure 200. The top DBR reflector is fabricated using a lift-off process: first, a dielectric DBR layer formed by sputtering is uniformly deposited on the surface, then patterned with photoresist, and finally the DBR layer in the photoresist area is lifted off using a solvent. Therefore, the top DBR is only retained in the original photoresist hole area. The top DBR reflector can also be achieved by overall sputtering deposition followed by patterned dry etching to remove the DBR layer outside the target area. The metal contacts 320 are formed by a metal stack lift-off process using electro-optical evaporation deposition.

[0201] Characteristic Analysis and Discussion of the Light-Emitting Structure with Buried Tunnel Junction (BTJ) and Vertical-Cavity Surface-Emitting Laser (VCSEL): To verify the current aperture effect of the BTJ structure, the current-voltage (I-V) characteristics of the light-emitting structure with a DBR mirror containing a BTJ (10 μm in diameter) and a control light-emitting structure without a BTJ were compared. Measurements were performed on both devices before the top dielectric DBR deposition. The device without a BTJ was used to simulate the structure outside the aperture region. Figure 7 summarizes the I-V curves of the two devices, showing that the current value of the device with a BTJ (solid line) at 2V is 5 times that of the device without a BTJ (dashed line). This indicates that the current is mainly confined to the BTJ or aperture region in the light-emitting structure 200 with the DBR mirror. Notably, the current of the device without a BTJ is much higher than the reported value in the literature (Journal of Applied Physics, Vol. 39, 2000), which may be due to the penetration effect of the p-type InP layer. When a large forward bias voltage (>1.5V) is applied, the pn junction between layers 140 and 170 is in a reverse bias state, and the p-type InP layer (layer 120) is completely depleted. Electrons from the n-type InP layer (layer 120) are swept across the p-type InP layer, resulting in high current in the BTJ-less device.

[0202] On the probe station, multiple VCSEL300 devices (at least 10, up to 10,000 to millions, depending on the wafer size) were fabricated and tested at the wafer level. All tests were performed in continuous wave (CW) mode. The current source used for characterization was a Keithley 2400, and the optical power was measured using a photodiode (Thorlab S122C) placed directly above the device under test. The photodiode was calibrated using an independent commercial 1,550nm EEL light source and compared with the factory calibration values, and the data were found to be consistent. Figure 8a shows the relationship between the optical output power of the 6μm diameter aperture device and the injection current or current density (L-I or L-J). The clearly measured laser threshold current density is 2.37kA / cm². Figure 8b shows the single-laser mode emission spectrum (wavelength approximately 1,553nm) acquired using a Thorlab OSA 203, which operates above the laser threshold. When the current density exceeds the threshold, the linewidth reaches 63pm. The side-mode rejection ratio (SMSR) exceeds 30dB. The output power is several orders of magnitude lower than the short-wave infrared values ​​reported in the literature. In addition to the large leakage current outside the aperture region, the fabricated VCSEL300 device also has the following problems: 1) The reflectivity of the top dielectric mirror is too high (approximately 99.9%), which is speculated to have a negative impact on cavity light extraction; 2) An oxide layer may form at the interface between layers 260 and 270, hindering effective current injection and potentially leading to increased device resistance and internal heating.

[0203] In summary, the fabricated VCSEL300 device uses a bottom DBR reflector based on NP-type InP, and its BTJ structure achieves current constraint. Single-mode VCSEL operation at approximately 1,553 nm wavelength was achieved at room temperature, with a threshold current density of 2.37 kA / cm² and a narrow linewidth of 63 pm observed in continuous wave operation.

[0204] Example 2: nm Multi-Porous Vertical-Cavity Surface Emitting Laser (VCSEL) with Hole Region Formed by Ion Implantation Materials and Methods: Unlike the BJT structure used in Example 1, the second VCSEL structure employs a light-emitting structure including a bottom double-sided reflector (DBR) reflector based on nanoporous (NP) InP and a hole region.

[0205] As shown in Figure 9, a light-emitting structure including a distributed Bragg reflector (DBR) reflector was fabricated based on an epitaxial growth structure 400. All layers were grown in a planar continuous manner. From bottom to top, structure 400 comprises seven parts: (1) a stack 410 consisting of 12 pairs of alternating layers, namely an n+ type InP layer (dark band, doping concentration: 5×10¹⁸ cm⁻³) and an n- type InP layer (light band, low doping, doping concentration: <5×10¹⁸ cm⁻³), wherein the n+ type InP layer can be electrochemically etched to form an NP type InP with a low refractive index (its refractive index is lower than that of the layer before porosification); (2) a thick n-type InP layer 420 (light gray, doping concentration: 5×10¹⁷ cm⁻³), with a thickness of at least about 200 nm; (3) a light-emitting structure 430 of InAlGaAs, constituting an active region with a target emission wavelength of 1,550 nm; (4) a p-type InAlAs layer 440 (doping concentration: 1×10¹⁸ cm⁻³); (5) a p++ type InAlAs layer 450 (doping concentration > (6) n++ type InP layer 460 (black, doping concentration > 1 × 10¹⁸ cm⁻³); and (7) top n type InP layer 470 (light gray, doping concentration: 2 × 10¹⁸ cm⁻³). Structure 400 is grown by metal-organic chemical vapor deposition (MOCVD).

[0206] Figure 10 shows a non-limiting NP InP vertical cavity surface-emitting laser (VCSEL) fabrication process, starting with epitaxial structure 400 (leftmost of the top row of Figure 10), in which a SiO2 (510) layer is deposited on the top surface of structure 400 and patterned by photoresist (520) to define the location of the hole region (middle of the top row of Figure 10). Ion implantation (H+; 530) is then performed to destroy / reduce the conductivity of the outer layer 440 of the hole region. Ion implantation uses 38-45 kEV energy and the implantation dose is6.4 × 10¹³ cm⁻³. In other words, ion implantation will not occur in the regions covered by layers 510 and 520. Typical implantation depths can reach 430 layers. For example, Figure 11 shows the distribution of doping-induced defects based on the Stop and Range of Ions in the Material (SRIM) simulation, where the boundaries of each layer are marked with black dashed lines. It can be seen that the top n-type InP layer (layer 470) is damaged to some extent during ion implantation. According to the literature ("Ion Implantation Techniques for Isolation of Group III-V Semiconductors", Materials Science Reports Vol. 4 (1990)), InAlAs requires a higher annealing temperature than InP to recover conductivity. Based on this difference, the conductivity of the top n-type InP layer can be selectively recovered by annealing while maintaining the resistance characteristics of InAlAs layer 440.

[0207] A self-aligned process is employed, in which the patterned mask formed by layers 510 and 520 simultaneously acts as a mask. A portion of layer 470 is removed by dry etching, leaving the patterned mask coverage area higher than the remaining surface of layer 470. This structure can be considered as having a stepped feature 540, providing an optical confinement effect for optoelectronic devices. The ion implantation region 535 is also illustrated (see the leftmost part of the second row of Figure 10). During dry etching, the area outside the aperture region is etched by approximately 20 nm, thereby forming a refractive index guide for the optical mode and helping to lower the threshold. After removing the mask material, a PECVD SiO2 layer 550 is deposited on a portion of the surface, and the structure is annealed at 350°C for 20 minutes (center of the second row of Figure 10). Annealing is believed to restore the conductivity of layer 470 damaged by ion implantation. Subsequently, a mesa structure 560 is formed by a wet etching process: first, wet chemical etching is performed with a diluted hydrochloric acid solution, followed by treatment with a citric acid + hydrogen peroxide solution, extending the bottom of the step to layer 420 (the rightmost part of the second row of Figure 10). A PECVD SiO2 layer (570) was then deposited and patterned, covering most of the surface except for the leftmost region. This layer served as a mask for subsequent dry etching and also protected the mesa structure from erosion during electrochemical etching (leftmost region, third row, Fig. 10). In other words, the SiO2 570 deposition covered the entire mesa structure, except for the top sidewall edge region. Deep dry etching was performed using SiO2 570 as a mask to form trenches reaching the bottom of the periodic layers (stack 410) (middle of the third row, Fig. 10). The structure (anode) and platinum (Pt) wire / plate (cathode) were then immersed in an electrolyte for electrochemical (EC) etching (rightmost region, third row, Fig. 10). Electrochemical etching was initiated from the sidewalls of the trench by applying a positive bias to the structure. The porous region (dark region) expanded laterally, eventually covering the entire hole region above. It is worth noting that porosity is limited to the n+ type InP layer of stack 410, while the lightly doped InP layer is preserved.The structure remains intact (unporosized). The selectivity between porosized and non-porosized regions is achieved through differences in doping concentration. Porosity results in the n+ type InP layer being filled with air, with a refractive index lower than that of the lightly doped InP layer. The alternating high-refractive-index and low-refractive-index layers form a mirror in the DBR structure, which is used to fabricate a vertical-cavity surface-emitting laser (VCSEL). Subsequently, a 600 nm PECVD SiO2 layer (580) is deposited to form a uniform and intact capping layer on the exposed sidewalls (Figure 10 continued, bottom row, left). The SiO2 layer 580 has a dual function: 1) as a mesa sidewall passivation layer; 2) as an electrochemical etching sidewall protection layer to prevent solvents in subsequent wet chemical steps from penetrating into the nanoporous InP structure in the stack 410. Finally, by forming openings in the SiO2 layer 580 on the top and sides of the mesa structure, a light-emitting structure 600 including a DBR mirror is constructed. These openings are used to place metal contacts and deposit the top dielectric DBR, as shown on the bottom right of Figure 10 continued.

[0208] Figure 12 shows in detail the light-emitting structure 600 including the DBR mirror. From bottom to top, the light-emitting structure 600 consists of the following parts: (1) a bottom structure 610 consisting of 12 pairs of alternating n+ type InP layers and n- type InP layers, wherein the n+ type InP layers are selectively porosized by electrochemical etching (as shown by the dark band); (2) a thick n-type InP layer 620 with a thickness of at least about 200 nm; (3) a tapered structure from bottom to top including: an InAlGaAs layer 630 providing an active region for the target emission wavelength of 1,550 nm; a p-type InAlAs layer 640; a p++ type InAlAs layer 650; an n++ type InP layer 660; and an n-type InP current diffusion layer 670 on top, wherein the top surface of the current diffusion layer 670 includes a stepped feature 680. The mesa structure includes a hole region composed of p-type InAlAs, p++-type InAlAs, n++-type InP, and n-type InP portions, partially shown as regions 645, 655, and 665 below the step feature 680. The p-type InAlAs, p++-type InAlAs, n++-type InP, and n-type InP layers outside the hole region are ion-implanted to reduce conductivity, and then annealed to restore the conductivity of the n-type InP current diffusion layer covering at least the hole region. The additional layer shown in Figure 12 includes a SiO2 layer (690), which is present due to the manufacturing process but is not essential to the function of the light-emitting structure or the included DBR reflector.

[0209] As shown in Figure 13, a vertical-cavity surface-emitting laser (VCSEL) 700 is formed using a light-emitting structure 600 including a double-layer reflector mirror. The light-emitting structure 600 includes a double-layer thin-film reflector, forming the bottom reflector of the VCSEL; as shown in Figure 13, the top of the mesa structure is equipped with a top dielectric double-layer thin-film reflector 710 and a metal electrode 720. Figure 14 shows the VCSEL 300.The fabrication process specifically includes forming a top double-layer thin-film reflector 710 and a metal electrode 720 on the light-emitting structure 600. The top DBR reflector is fabricated by a lift-off method: first, a dielectric DBR layer formed by sputtering is uniformly deposited on the surface, then DBR is deposited in the photoresist pattern area, and finally the DBR on the photoresist is lifted off using a solvent. Therefore, the top DBR is only retained in the previous PR opening area. The top DBR reflector can also be fabricated by patterned dry etching after overall sputtering deposition to remove the DBR layer outside the target area. The metal contact 720 is formed by lift-off of the metal stack deposited by electric beam evaporation.

[0210] Analysis and discussion of the light-emitting structure and vertical cavity surface-emitting laser characteristics in the ion implantation-formed aperture region: To verify the effect of current confinement achieved by the ion implantation method, two sets of light-emitting structures were fabricated: one set has a current aperture region with a diameter of 10 μm, and the other set does not have this region. Both sets of structures use NP-type InP substrate double-reflective thin-film mirrors with a porous region. Figure 15 shows the forward I-V curves of these two devices. The results show that at 2V, the current value of the device with a current aperture region (such as the light-emitting structure 600 with a DBR mirror) is nearly three orders of magnitude higher than that of the device without an aperture region, confirming that the current is successfully confined within the aperture region.

[0211] Two vertical cavity surface-emitting lasers (VCSELs) with different structures were designed with emission wavelengths of 1,380nm and 1,550nm, respectively, but both were fabricated using the same process shown in Figure 10. The fully fabricated VCSEL devices were tested at the wafer level on a probe station. All tests were performed in continuous wave (CW) mode. The current source used for characterization was a Keithley 2400, and the optical power was measured by a photodiode (Thorlab S122C) placed directly above the device.

[0212] Figure 16a shows the current-voltage-power curves of the 1,380nm vertical cavity surface-emitting laser (VCSEL) device with a 7μm aperture. Its threshold current is 0.5 mA, equivalent to a current density of 1.3 kA / cm2, and the extracted slope efficiency is approximately 0.23 W / A. The power conversion efficiency of the device reaches a peak of 10.4% at an injection current of 2.5 mA. The laser spectrum was acquired using a Thorlab OSA 203 acquisition unit, as shown in Figure 16b. The experiment observed that in single-mode operation, the side-mode rejection ratio (SMSR) was close to 30 dB. When the injection current increased from 0.5 mA (threshold) to 8 mA (close to the thermal inversion point), the laser wavelength redshifted due to device heating.

[0213] Similarly, a 1,550 nm wavelength was also achieved using another InP VCSEL structure that scales all dimensions according to the wavelength ratio.The VCSEL achieved room-temperature continuous-wave operation. Figures 17a and 17b show the L-I-V curves and laser spectrum of the 7 μm aperture device, respectively. The threshold current was 0.67 mA, equivalent to a current density of 1.7 kA / cm², and the extracted slope efficiency was approximately 0.15 W / A. The 1,550 nm VCSEL exhibited a significantly higher threshold current density and a lower slope efficiency (compared to the 1,380 nm device). This was likely due to the unoptimized process of the top dielectric DBR (a-Si:H / SiO2) mirror during the deposition of the 1,550 nm device, which was subsequently corrected in the subsequent processes of the 1,380 nm device. Nevertheless, the device still achieved single-mode operation with a side-mode rejection ratio (SMSR) exceeding 30 dB.

[0214] Conclusion: Examples 1 and 2 above demonstrate the concept of constructing a light-emitting structure containing an NP-type InP dual-sided reflector (DBR) using two different current-limited forming processes, thereby realizing an operational demonstration of a continuous-wave vertical-cavity surface-emitting laser (CW VCSEL). These exemplary VCSELs achieve room-temperature continuous-wave operation in the short-wave infrared (SWIR) band with a threshold current density of approximately 1 kA / cm², output power in the milliwatt range, and a power conversion efficiency (PCE) of 10%.

[0215] Unless otherwise defined, all technical terms used herein have the meaning generally accepted by one of ordinary skill in the art to which this invention pertains. All references and materials cited herein are explicitly incorporated by reference.

[0216] Those skilled in the art will recognize, or can be determined by conventional experimentation, that numerous equivalent embodiments of the present invention exist. Such equivalent embodiments are to be covered by the following claims. Instruction Manual Page 31 / 31, 43 CN 121532916 A, Figure 1A, Figure 1B, Figure 1C; Instruction Manual Drawings 1 / 15, Page 44 CN 121532916 A, Figure 1D, Figure 1E, Figure 1F; Instruction Manual Drawings 2 / 15, Page 45 CN 121532916 A, Figure 2; Instruction Manual Drawings 3 / 15, Page 46 CN 121532916 A, Figure 3; Instruction Manual Drawings 4 / 15, Page 47 CN 121532916 A, Figure 4; Instruction Manual Drawings 5 / 15, Page 48 CN 121532916 A, Figure 5, Figure 6; Instruction Manual Drawings 6 / 15, Page 49 CN 121532916 A, Figure 7, Figure 8A; Instruction Manual Drawings 7 / 15, Page 50 CN 121532916 A, Figure 8B, Figure 9; Instruction Manual Drawings 8 / 15, Page 51 CN 121532916 A, Figure 10; Instruction Manual Drawings 9 / 15 Page 52 CN 121532916 A Figure 10 (continued) (Explanation)Figures 10 / 15, page 53, CN 121532916 A, Figures 11 and 12; Figures 11 / 15, page 54, CN 121532916 A, Figures 13 and 14; Figures 12 / 15, page 55, CN 121532916 A, Figures 15 and 16A; Figures 13 / 15, page 56, CN 121532916 A, Figures 16B and 17A; Figures 14 / 15, page 57, CN 121532916 A, Figure 17B; Figures 15 / 15, page 58, CN 121532916 A. Abstract: The present invention describes various semiconductor structures containing buried tunnel junctions or aperture regions. Further disclosed are methods for preparing and using such semiconductor structures which can be used, for example, in optoelectronic devices, such as vertical cavity surface emitting lasers (VCSELs), which can emit at long wavelengths.

Claims

1. A semiconductor structure including a buried tunnel junction (BTJ), said semiconductor structure comprising: The bottom structure comprises alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; The n-type doped first semiconductor layer is located at the top of the bottom structure; A light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the n-type doped first semiconductor layer; The p-type doped first semiconductor layer is located on top of the light-emitting structure; as well as A buried tunnel junction (BTJ) exists on the p-type doped first semiconductor layer. The embedded tunnel structure includes: p-type doped second semiconductor layer, the p-type doped second semiconductor layer having a density greater than about 1 × 10⁻⁶ 18 cm -3 p-type doping level; An n-type doped second semiconductor layer is located on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having a density greater than approximately 1 × 10⁻⁶. 18 cm -3 n-type doping level; Wherein at least the n-type doped second semiconductor layer has a surface area smaller than the surface area of ​​the p-type doped first semiconductor layer; Optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; An n-type doped current diffusion layer is provided, wherein the n-type doped current diffusion layer encapsulates at least a portion of the n-type doped second semiconductor layer, and optionally also encapsulates at least a portion of the p-type doped second semiconductor layer; The current diffusion layer, excluding the portion thereof having the n-type doped second semiconductor layer, contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and The surface of the current diffusion layer may optionally include a region above the embedded tunnel junction, the region being raised and forming a stepped feature to provide an optical confinement effect.

2. The semiconductor structure of claim 1, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide.

3. The semiconductor structure according to any one of claims 1-2, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness.

4. The semiconductor structure according to any one of claims 1 to 3, wherein the alternating layers of the bottom structure comprise a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, and gallium antimonide; and wherein the alternating layers are lattice-matched with the semiconductor substrate.

5. The semiconductor structure according to any one of claims 1 to 4, wherein, The alternating layers of the bottom structure comprise ternary semiconductor materials that match the lattice of the semiconductor substrate.

6. The semiconductor structure according to any one of claims 1 to 4, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material that matches the lattice of the semiconductor substrate.

7. The semiconductor structure according to any one of claims 1 to 6, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer comprise one or more semiconductor materials that are lattice-matched with the semiconductor substrate.

8. The semiconductor structure of claim 7, wherein the one or more semiconductor materials are lattice-matched with an indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the semiconductor material is lattice-matched with a gallium arsenide semiconductor substrate and is selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the semiconductor material is lattice-matched with a gallium antimonide semiconductor substrate and is selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb.

9. The semiconductor structure according to any one of claims 1 to 6, wherein the light-emitting structure, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer each comprise one or more semiconductor materials that are lattice mismatched with the semiconductor substrate.

10. The semiconductor structure of claim 9, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb.

11. A method for manufacturing a semiconductor structure including a buried tunnel junction (BTJ), the method comprising the steps of: (i) A bottom structure is formed on a semiconductor substrate, the bottom structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers; (ii) Deposit an n-type doped first semiconductor layer on top of the bottom structure; (iii) Depositing or forming a light-emitting structure including multiple quantum wells (MQWs) on top of the first semiconductor layer; (iv) Deposit a p-type doped first semiconductor layer on top of the light-emitting structure; (v) A p-type doped second semiconductor layer is deposited on top of the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a density greater than approximately 1 × 10⁻⁶. 18 cm -3 p-type doping concentration; (vi) Deposit an n-type doped second semiconductor layer on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having a density greater than approximately 1 × 10⁻⁶. 18 cm -3 n-type doping concentration; (vii) A mask material is formed or patterned over the top surface region of the n-type doped second semiconductor layer; (viii) At least the n-type doped second semiconductor layer is removed by etching, and optionally the p-type doped second semiconductor layer thereon other than the surface portion having the mask material is removed; (ix) Remove the mask material; as well as (x) Deposit an n-type doped current diffusion layer, wherein the n-type doped current diffusion layer at least covers a portion of the n-type doped second semiconductor layer, and optionally covers a portion of the p-type doped second semiconductor layer, wherein the current diffusion layer outside the surface portion contacts the p-type doped second semiconductor layer or the p-type doped first semiconductor layer.

12. The method of claim 11, wherein any structure or layer can be independently formed or deposited by metal-organic vapor deposition (MOCVD), molecular beam epitaxy (MBE), or liquid phase epitaxy (LPE).

13. The method of any one of claims 11-12, wherein the mask material is selected from the group consisting of dielectric materials and / or photoresists, such as silicon dioxide, silicon nitride, and aluminum oxide.

14. The method of any one of claims 11-13, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide.

15. The method of any one of claims 11-14, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness.

16. The method of any one of claims 11 to 15, wherein the alternating layers of the bottom structure comprise a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, or gallium antimonide; and the alternating layers are lattice-matched with the semiconductor substrate.

17. The method of any one of claims 11 to 15, wherein the alternating layers of the bottom structure comprise a ternary semiconductor material that matches the lattice of the semiconductor substrate.

18. The method of any one of claims 11 to 15, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material that matches the lattice of the semiconductor substrate.

19. The method of any one of claims 11 to 18, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer comprise one or more semiconductor materials that are lattice-matched with the semiconductor substrate.

20. The method of claim 19, wherein the one or more semiconductor materials are lattice-matched with an indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the semiconductor material is lattice-matched with a gallium arsenide semiconductor substrate and is selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the semiconductor material is lattice-matched with a gallium antimonide semiconductor substrate and is selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb.

21. The method of any one of claims 11-18, wherein the light-emitting structure, the p-type doped second semiconductor layer, and the n-type doped second semiconductor layer each comprise one or more semiconductor materials that are lattice mismatched with the semiconductor substrate.

22. The method of claim 21, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb.

23. A light-emitting structure comprising an embedded tunnel junction (BTJ), the light-emitting structure comprising: A bottom reflector structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on the semiconductor substrate; The n-type doped layer is a porous structure and includes multiple pores; and the undoped or low-doped semiconductor layer is a non-porous or substantially non-porous structure. An n-type doped first semiconductor layer disposed on top of the bottom structure; A light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the semiconductor layer; The p-type doped first semiconductor layer is located on top of the light-emitting structure; as well as A buried tunnel junction (BTJ) existing on a portion of the p-type doped first semiconductor layer. The embedded tunnel junction defines a borehole region and includes: p-type doped second semiconductor layer, wherein the p-type doped second semiconductor layer has a concentration greater than about 1 × 10⁻⁶. 18 cm -3 p-type doping; The n-type doped second semiconductor layer has a concentration greater than about 1 × 10⁻⁶. 18 cm -3 The n-type doping is located on top of the p-type doped second semiconductor layer; Wherein at least the n-type doped second semiconductor layer has a surface area smaller than the surface area of ​​the p-type doped first semiconductor layer; Optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; An n-type doped current diffusion layer is provided, wherein the n-type doped current diffusion layer encapsulates at least a portion of the n-type doped second semiconductor layer, and optionally encapsulates at least a portion of the p-type doped second semiconductor layer; The current diffusion layer, excluding the portion thereof having the n-type doped second semiconductor layer, contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and The surface of the current diffusion layer may optionally include a region above the embedded tunnel junction, the region being raised and forming a stepped feature, thereby producing an optical confinement effect.

24. The light-emitting structure of claim 23, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide.

25. The light-emitting structure according to any one of claims 23-24, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness.

26. The light-emitting structure according to any one of claims 23-25, wherein the alternating layers of the bottom structure comprise a binary semiconductor material selected from the group consisting of indium phosphide, gallium arsenide, or gallium antimonide; and the alternating layers are lattice-matched with the semiconductor substrate.

27. The light-emitting structure according to any one of claims 23-25, wherein the alternating layers of the bottom structure comprise a ternary semiconductor material that matches the lattice of the semiconductor substrate.

28. The light-emitting structure of any one of claims 23 to 25, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material lattice-matched to the semiconductor substrate.

29. The light-emitting structure according to any one of claims 23-28, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer comprise one or more semiconductor materials that are lattice-matched with the semiconductor substrate.

30. The light-emitting structure of claim 29, wherein the one or more semiconductor materials are lattice-matched with an indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the semiconductor material is lattice-matched with a gallium arsenide semiconductor substrate and is selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the semiconductor material is lattice-matched with a gallium antimonide semiconductor substrate and is selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb.

31. The light-emitting structure according to any one of claims 23-28, wherein the light-emitting structure, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer each comprise one or more semiconductor materials that are lattice mismatched with the semiconductor substrate.

32. The light-emitting structure of claim 31, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb.

33. The light-emitting structure according to any one of claims 23-32, wherein the porosity is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80% or 90%.

34. The light-emitting structure according to any one of claims 23-33, wherein there is a refractive index contrast (Δn) between the alternating layers, which ranges from about 0.1 to 2 or from about 0.1 to 2.

5.

35. A method for forming a light-emitting structure, comprising the following steps: (i') Setting up or forming a structure including an embedded tunnel junction (BTJ), said structure comprising: The bottom structure comprises alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; The n-type doped first semiconductor layer is located at the top of the bottom structure; A light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the n-type doped first semiconductor layer; The p-type doped first semiconductor layer located on top of the light-emitting structure; and A buried tunnel junction (BTJ) exists on the p-type doped first semiconductor layer. The embedded tunnel structure includes: p-type doped second semiconductor layer, the p-type doped second semiconductor layer having a density greater than about 1 × 10⁻⁶ 18 cm -3 p-type doping concentration; An n-type doped second semiconductor layer is located on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having a density greater than approximately 1 × 10⁻⁶. 18 cm -3 n-type doping concentration; Wherein at least the surface area of ​​the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer; Optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; and An n-type doped current diffusion layer is provided, wherein the n-type doped current diffusion layer encapsulates at least a portion of the n-type doped second semiconductor layer, and optionally encapsulates at least a portion of the p-type doped second semiconductor layer; The current diffusion layer, excluding the portion thereof having the n-type doped second semiconductor layer, contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and The surface of the current diffusion layer may optionally include a region above the embedded tunnel junction, the region being raised and forming a stepped feature to produce an optical confinement effect; (ii') A mesa structure is formed by etching the current diffusion layer, the light-emitting structure, the p-type doped first semiconductor layer, and optionally a portion of the p-type doped second semiconductor layer; (iii') A silicon dioxide layer is deposited over the mesa structure, wherein at least a portion of the n-type doped first semiconductor layer is not covered by the silicon dioxide layer; (iv') Etch the portion not covered by the silicon dioxide layer to form a trench thereby exposing the sidewalls of the alternating layers of the bottom structure; (v') Selectively porosilicate the n-type doped semiconductor layer in the alternating layers of the bottom structure, wherein a plurality of pores are formed, and wherein the undoped or low-doped semiconductor layer is kept pore-free or substantially pore-free. (vi') Deposit one or more materials to cover the trench, the sidewalls, and the sidewalls of the platform structure; (vii') Selectively remove the one or more materials to expose at least a portion of the top of the mesa structure, and optionally expose a portion of the n-type doped first semiconductor covered by the one or more materials; and (viii') Metal contacts are formed on a portion of the top of the mesa structure and optionally on a portion of the n-type doped first semiconductor.

36. The method of claim 35, wherein the porosity formed in step (v') is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80%, or 90%.

37. The method of any one of claims 35-36, wherein step (v') is performed by electrochemical etching in an electrolyte solution and under an applied bias voltage.

38. The method of claim 37, wherein the electrolyte solution comprises halide ions, hydrochloric acid (HCl), sulfuric acid (H2SO4), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)2, Ca(OH)2, Sr(OH)2, NH4OH, NaCl, NaF, nitric acid (HNO3), organic acids and their salts (such as oxalic acid and citric acid), and mixtures thereof.

39. The method of any one of claims 35-38, wherein the one or more materials are selected from the group consisting of silicon dioxide, alumina, silicon nitride, and spin-coated glass; and / or the one or more materials are organic materials selected from the group consisting of benzocyclobutene (BCB), polyimide, and photoresist; and combinations thereof.

40. The method of any one of claims 35-39, wherein the metal contact formed in step (viii') comprises a metal selected from Ti, Pt, Au, Ge, Ni, Pd, In and combinations thereof.

41. An optoelectronic device, comprising: The light-emitting structure according to any one of claims 23-34; Top-distributed Bragg reflectors; as well as Metal contacts.

42. The optoelectronic device of claim 41, wherein the top distributed Bragg reflector comprises alternating layers of any of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof.

43. The optoelectronic device according to any one of claims 41-42, wherein the metal contact comprises one or more metals selected from the group consisting of Ti, Pt, Au, Ge, Ni, Pd, In and combinations thereof.

44. The optoelectronic device according to any one of claims 41-43, wherein the optoelectronic device is a vertical cavity surface-emitting laser (VCSEL).

45. The optoelectronic device of claim 44, wherein the vertical cavity surface-emitting laser operates in continuous wave mode at room temperature (about 25°C).

46. ​​The optoelectronic device of claim 44, wherein the vertical cavity surface-emitting laser operates at a temperature below about 0°C, above about 25°C, or above about 85°C.

47. The optoelectronic device of claim 44, wherein the vertical cavity surface-emitting laser operates in pulsed mode.

48. The optoelectronic device of claim 44, wherein the vertical cavity surface-emitting laser emits in the infrared wavelength region.

49. The optoelectronic device of claim 44, wherein the power conversion efficiency of the vertical cavity surface-emitting laser is at least about 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 7.5% or 10%.

50. A method for manufacturing an optoelectronic device, comprising the following steps: (i”) Setting or forming a light-emitting structure, the light-emitting structure comprising: A bottom reflector structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; wherein the n-type doped layers are porous and include multiple pores; and wherein the undoped or lightly doped semiconductor layers are non-porous or substantially non-porous. The n-type doped first semiconductor layer is located at the top of the bottom structure; A light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the semiconductor layer; The p-type doped first semiconductor layer located on top of the light-emitting structure; and A buried tunnel junction (BTJ) existing on a portion of the p-type doped first semiconductor layer. The embedded tunnel junction defines a borehole region and includes: p-type doped second semiconductor layer, wherein the p-type doped second semiconductor layer has a concentration greater than about 1 × 10⁻⁶. 18 cm -3 p-type doping; The n-type doped second semiconductor layer has a concentration greater than about 1 × 10⁻⁶. 18 cm -3 The n-type doping is located on top of the p-type doped second semiconductor layer; Wherein at least the surface area of ​​the n-type doped second semiconductor layer is smaller than the surface area of ​​the p-type doped first semiconductor layer; Optionally, the p-type doped second semiconductor layer and the n-type doped second semiconductor layer have equal or substantially equal areas on the p-type doped first semiconductor layer; An n-type doped current diffusion layer is provided, wherein the n-type doped current diffusion layer encapsulates at least a portion of the n-type doped second semiconductor layer, and optionally also encapsulates at least a portion of the p-type doped second semiconductor layer; The current diffusion layer, excluding the portion having the n-type doped second semiconductor layer thereon, covers and contacts the p-type doped second semiconductor or the p-type doped first semiconductor; and The surface of the current diffusion layer may optionally include a region above the embedded tunnel junction, the region being raised and forming a stepped feature to produce an optical confinement effect; (ii”) A top distributed Bragg reflector is disposed or formed on the light-emitting structure; and (iii) Metal contacts are provided or formed on the optoelectronic device.

51. The method of claim 50, wherein the top distributed Bragg reflector in step (ii”) comprises alternating layers of any of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof.

52. The method according to any one of claims 50-51, wherein the metal contact in step (iii”) comprises one or more metals selected from the group consisting of Ti, Pt, Au, Ge, Ni, Pd, In and combinations thereof.

53. The method of any one of claims 50 to 52, wherein the optoelectronic device is a vertical cavity surface-emitting laser (VCSEL).

54. A light-emitting structure, comprising: A bottom reflector structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; wherein the n-type doped semiconductor layers are porous and include multiple pores; and wherein the undoped or lightly doped semiconductor layers are non-porous or substantially non-porous. The n-type doped first semiconductor layer is located at the top of the bottom structure; A light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the semiconductor layer; The p-type doped first semiconductor layer is located on top of the light-emitting structure; A p-type doped second semiconductor layer is located on top of the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a concentration greater than about 1 × 10⁻⁶. 18 cm -3 p-type doping; An n-type doped second semiconductor layer is located on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having a concentration greater than about 1 × 10⁻⁶. 18 cm -3 n-type doping; An n-type doped current diffusion layer located on top of the n-type doped second semiconductor layer; There exists a hole region, wherein the conductivity of the p-type doped first semiconductor layer within the hole region is greater than the conductivity of the p-type doped first semiconductor layer outside the hole region; Wherein, the resistivity of the p-type doped first semiconductor layer, the optional p-type doped second semiconductor layer, and the optional n-type doped semiconductor layer outside the hole region is higher than that inside the hole region; The current diffusion layer is conductive both inside and outside the hole; and The current diffusion layer may optionally include a region on the top surface above the aperture region, the region being raised and forming a stepped feature to provide an optical confinement effect.

55. The light-emitting structure of claim 54, wherein the semiconductor substrate is composed of indium phosphide, gallium arsenide, or gallium antimonide.

56. The light-emitting structure according to any one of claims 54-55, wherein the n-type doped semiconductor layers in the bottom structure each have the same thickness; and / or the undoped or lightly doped semiconductor layers in the bottom structure each have the same thickness.

57. The light-emitting structure of claim 54, wherein the alternating layers of the bottom structure comprise a binary semiconductor material lattice-matched to the semiconductor substrate.

58. The light-emitting structure of claim 54, wherein the alternating layers of the bottom structure comprise a ternary semiconductor material lattice-matched to the semiconductor substrate.

59. The light-emitting structure of claim 54, wherein the alternating layers of the bottom structure comprise a quaternary semiconductor material lattice-matched to the semiconductor substrate.

60. The light-emitting structure according to any one of claims 54 to 59, wherein the n-type doped first semiconductor, the light-emitting structure, the p-type doped first semiconductor, the p-type doped second semiconductor, the n-type doped second semiconductor, and the current diffusion layer each independently comprise one or more materials lattice-matched with the semiconductor substrate.

61. The light-emitting structure of claim 60, wherein the one or more materials are lattice-matched with an indium phosphide semiconductor substrate and are selected from the group consisting of InP, InAlAs, InAlGaAs, InGaAsP, InGaAs, and AlGaAsSb; or the one or more semiconductor materials are lattice-matched with a gallium arsenide semiconductor substrate and are selected from the group consisting of GaAs, AlGaAs, AlAs, InAlP, and InGaP; or the one or more semiconductor materials are lattice-matched with a gallium arsenide semiconductor substrate and are selected from the group consisting of GaSb, AlAsSb, and AlGaAsSb.

62. The light-emitting structure as described in claims 54-59, wherein the light-emitting structure, the p-type doped second semiconductor, and the n-type doped second semiconductor each independently comprise one or more materials that are lattice mismatched with the indium phosphide semiconductor substrate.

63. The light-emitting structure of claim 62, wherein the one or more semiconductor materials are lattice mismatched with the indium phosphide semiconductor substrate and are selected from the group consisting of InAlGaAs, InGaAsP, InGaAs, InAs, and InGaAsSb; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InGaAs, AlGaAs, and In(Al)GaP; or the one or more semiconductor materials are lattice mismatched with the gallium arsenide semiconductor substrate and are selected from the group consisting of InAl(As)Sb, AlAsSb, and AlGaAsSb.

64. The light-emitting structure according to any one of claims 54-63, wherein the conductivity of the p-type doped first semiconductor layer outside the aperture region, and optionally the p-type doped second semiconductor layer and optionally the n-type doped second semiconductor layer is about 1-4 orders of magnitude lower than that of the aperture region.

65. The light-emitting structure according to any one of claims 54-64, wherein the porosity is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80% or 90%.

66. The light-emitting structure according to any one of claims 54-65, wherein the refractive index contrast (Δn) between the alternating layers in the bottom reflector structure is about 0.1 to 2 or 0.1 to 2.

5.

67. A method for forming a light-emitting structure, comprising the following steps: (a) Setting up or forming a structure that includes the following: A bottom structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; The n-type doped first semiconductor layer is located at the top of the bottom structure; A light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the first semiconductor layer; The p-type doped first semiconductor layer is located on top of the light-emitting structure; p-type doped second semiconductor layer, wherein the p-type doped second semiconductor layer has a concentration greater than about 1 × 10⁻⁶. 18 cm -3 The p-type doping is located on top of the p-type doped first semiconductor layer; The n-type doped second semiconductor layer has a concentration greater than about 1 × 10⁻⁶. 18 cm -3 The n-type doping is located on top of the p-type doped second semiconductor layer; as well as An n-type doped current diffusion layer located on top of the n-type doped second semiconductor layer; (b) Place a mask material above the top surface region of the current diffusion layer of the structure; (c) Perform ion implantation to reduce the conductivity of at least the p-type doped first semiconductor layer not covered by the mask material; (d) Etching a portion of the current diffusion layer, wherein the etching does not remove the current diffusion layer beneath the mask material; (e) Remove the mask material; (f) Deposit a first layer of silicon dioxide over a portion of the current diffusion layer to cover the area where at least the mask material is present; (g) Annealing the structure to improve the conductivity of the top layer of the current diffusion layer; (h) A mesa structure is formed by etching the current diffusion layer, the n-type doped second semiconductor, the p-type doped second semiconductor, the p-type doped first semiconductor, and the portion of the light-emitting structure not covered by the first silicon dioxide; (i) depositing a second layer of silicon dioxide over the mesa structure, wherein at least a portion of the n-type doped first semiconductor is not covered by the second layer of silicon dioxide; (j) etching the structure not covered by the second layer of silicon dioxide to form trenches that expose the sidewalls of the alternating layers of the bottom structure; (k) Selectively porosilicate the n-type doped semiconductor layer in the alternating layers of the bottom structure, wherein the formed pores include air, and wherein the undoped or low-doped semiconductor layer remains in a pore-free or substantially pore-free state. (l) Deposit one or more materials to cover the trench, the sidewalls of the trench, and the sidewalls of the platform structure; (m) Selectively remove the one or more materials to expose at least a portion of the top of the mesa structure and optionally expose portions of the semiconductor layer covered by the one or more materials; as well as (n) Metal contacts are formed on a portion of the top of the mesa structure and optionally on a portion of the semiconductor layer.

68. The method of claim 67, wherein the mask material is selected from the group consisting of insulating materials composed of silicon dioxide, aluminum oxide and silicon nitride; or an organic material (such as photoresist); or a metal (such as nickel); or a combination thereof.

69. The method of any one of claims 67-68, wherein the porosity formed in step (k) is at least about 10%, 20%, 30%, 40%, 50%, 60%, 70%, 80% or 90%.

70. The method of any one of claims 67-69, wherein step (k) is performed by electrochemical etching in an electrolyte solution and under an applied bias voltage.

71. The method of claim 70, wherein the electrolyte solution comprises halide ions, hydrochloric acid (HCl), sulfuric acid (H2SO4), hydrofluoric acid (HF), KOH, NaOH, Ba(OH)2, Ca(OH)2, Sr(OH)2, NH4OH, NaCl, NaF, nitric acid (HNO3), organic acids and their salts (such as oxalic acid and citric acid), and mixtures thereof.

72. The method of any one of claims 67-71, wherein the one or more materials are selected from the group consisting of silicon dioxide, aluminum oxide and silicon nitride; and / or the one or more materials are organic materials selected from the group consisting of benzocyclobutene (BCB), polyimide and photoresist; and combinations thereof.

73. The method of any one of claims 67-72, wherein the metal contact comprises a metal selected from Ti, Pt, Au, Ge, Ni, Pd, In, and combinations thereof.

74. An optoelectronic device, comprising: The light-emitting structure according to any one of claims 54-66; Top-distributed Bragg reflectors; as well as Metal contacts.

75. The optoelectronic device of claim 74, wherein the top distributed Bragg reflector comprises alternating layers consisting of any one of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof.

76. The optoelectronic device according to any one of claims 74-75, wherein the metal contact comprises a metal selected from Ti, Pt, Au, Ge, Ni, Pd, In and combinations thereof.

77. The optoelectronic device according to any one of claims 74-76, wherein the optoelectronic device is a vertical cavity surface-emitting laser (VCSEL).

78. The optoelectronic device of claim 77, wherein the vertical cavity surface-emitting laser operates in continuous wave mode at room temperature (about 25°C).

79. The optoelectronic device of claim 77, wherein the vertical cavity surface-emitting laser operates at a temperature below about 0°C, above about 25°C, or above about 85°C.

80. The optoelectronic device of claim 77, wherein the vertical cavity surface-emitting laser operates in pulsed mode.

81. The optoelectronic device of claim 77, wherein the vertical cavity surface-emitting laser emits in the infrared and / or red wavelength region.

82. The optoelectronic device of claim 77, wherein the power conversion efficiency of the vertical cavity surface-emitting laser is at least about 0%, 0.1%, 0.5%, 1%, 2%, 3%, 4%, 5%, 7.5%, or 10%.

83. A method for manufacturing an optoelectronic device, comprising the following steps: (a') Setting or forming a light-emitting structure, including: A bottom reflector structure comprising alternating n-type doped layers and undoped or lightly doped semiconductor layers on a semiconductor substrate; wherein the n-type doped semiconductor layers are porous and include multiple pores; and the undoped or lightly doped semiconductor layers are non-porous or substantially non-porous. The n-type doped first semiconductor layer is located at the top of the bottom structure; A light-emitting structure, the light-emitting structure comprising multiple quantum wells (MQWs) located on top of the semiconductor layer; The p-type doped first semiconductor layer is located on top of the light-emitting structure; A p-type doped second semiconductor layer is located on top of the p-type doped first semiconductor layer, the p-type doped second semiconductor layer having a concentration greater than about 1 × 10⁻⁶. 18 cm -3 p-type doping; An n-type doped second semiconductor layer is located on top of the p-type doped second semiconductor layer, the n-type doped second semiconductor layer having a concentration greater than about 1 × 10⁻⁶. 18 cm -3 n-type doping; An n-type doped current diffusion layer located on top of the n-type doped second semiconductor layer; There exists a hole region, wherein the conductivity of the p-type doped first semiconductor layer within the hole region is greater than the conductivity of the p-type doped first semiconductor layer outside the hole region; The p-type doped first semiconductor layer, the optional p-type doped second semiconductor layer, and the optional n-type doped second semiconductor layer have higher resistivity outside the hole region than inside the hole region. The current diffusion layer is conductive both inside and outside the aperture region; and The current diffusion layer may optionally include a region on the top surface above the aperture region, the region being raised and forming a stepped feature to provide an optical confinement effect; (b') To provide or form a top distributed Bragg reflector on the light-emitting structure; and (c') A metal contact is provided or formed on the optoelectronic device.

84. The method of claim 83, wherein the top distributed Bragg reflector in step (b') comprises alternating layers of any of the following: a-Si / SiO2, TiO2 / SiO2, Ta2O5 / SiO2, Nb2O5 / SiO2, ZnSe / SiO2, a-Si / Al2O3, a-Si / MgF, ZnS / MgF, a-Si / CaF2, or combinations thereof.

85. The method of any one of claims 83-84, wherein the metal contact in step (c') comprises one or more metals selected from the group consisting of Ti, Pt, Au, Ge, Ni, Pd, In and combinations thereof.

86. The method of any one of claims 83-85, wherein the optoelectronic device is a vertical-cavity surface-emitting laser (VCSEL).