Welding torch, shielding attachment for the same and method of surface-treatment of a welding region

IN595142BActive Publication Date: 2026-07-13NAT INST OF TECH KURUKSHETRA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202411067509
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2024-09-06
Publication Date
2026-07-13
Estimated Expiration
2044-09-06

AI Technical Summary

Technical Problem

Conventional nitriding methods for surface-treating welding regions are costly and time-consuming, requiring expensive infrastructure and prolonged processes in a vacuum furnace, which limits their practicality and efficiency.

Method used

A welding torch with a ceramic nozzle and shielding attachment that uses a dual gas-stream system, where a first gas-stream flows through the nozzle and a second gas-stream shields and ionizes the first gas-stream to create a near-plasma environment for nitriding, allowing for localized nitride formation without the need for a separate furnace, using nitrogen or argon gases and nitride former pastes like Aluminum or Chromium powder.

Benefits of technology

This method enables efficient and cost-effective nitriding of welding regions, achieving significant hardness improvements without the need for extensive furnace-based processes, as demonstrated by increased hardness values in AISI 1030 steel samples treated with the described technique.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to a welding torch (100) for surface-treatment of a welding region (W) and a shielding attachment (200) for the welding torch (100) for surface-treatment of the welding region (W). The welding torch (100) has a body (150). A nozzle (110) is attached to the body (150), such that a first gas-stream (S1) flows through the nozzle (110). A shielding attachment (120) is adapted to on the nozzle (110). A channel (130) is defined between an inner surface (175) of the shielding attachment (120) and the nozzle (110). The channel (130) is adapted to guide a second gas-stream (S2) on the welding region (W), such that the second gas-stream (S2) shields the first gas-stream (S1). The welding torch (100) disclosed herein provides surface-treatment on the welding region (W) when welding is being conducted on the welding region (W). Therefore, present invention is cost effective.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELD OF THE PRESENT INVENTIONThe present invention relates to a welding torch for surface-treatment, such as nitriding, of a welding region and a shielding attachment for the welding torch for nitriding the welding region. Additionally, the present invention relates to a method for surface-treating or nitriding the welding region by the welding torch.BACKGROUND OF THE PRESENT INVENTIONWelding torch deployed in Gas Tungsten Arc Welding method or GTAW method generally includes an electrode holder which holds a Tungsten electrode. A ceramic nozzle is removably fixed to the electrode holder, such that the Tungsten electrode is covered by the ceramic nozzle. The Tungsten electrode is adjusted along a longitudinal length of the Tungsten electrode as and when the Tungsten electrode becomes shortened or spent due to use overtime during the GTAW method. A shielding gas-stream of nitrogen gas, argon gas or any inert gas flows through the ceramic nozzle and creates a gas shield in the welding region.A surface-treatment method such as nitriding is used for improving wear resistance, surface properties and hardness of a surface proximal to the welding region. Some of the known welding techniques provide surface-treatment to the surface proximal to the welding region, for example hard facing. In such welding techniques, the welding torches which are used are unable to provide nitriding to the surface.The nitriding method is even more essential as it ensures that the surface is sufficiently hardened, so that it acquires wear resistance. Therefore, a thermo-chemical heat-treatment method is generally implemented in the prior art for nitriding the surface proximal to the welding region. Some factors which enable proper nitriding include a time for which the nitriding method is introduced over the surface, a temperature at which the nitriding method is conducted and effectiveness of an environment containing nitrogen as a shielding environment during application of the nitriding method, play significant role in nitride formation in on the surface close to the welding region. Nitriding methods are categorised as soft nitriding and hard nitriding. Temperature maintained during the soft nitriding method, and time required for completing the same are comparatively low in soft nitriding. Conversely, maintaining higher temperature along with prolonged time for completing the nitriding are required in the hard nitriding method. Additionally, an alternate method of nitriding which is in use in the prior art is plasma nitriding, which is also referred to as ion nitriding. During plasma nitriding of the surface proximal to the welding region, ionised nitrogen gas is introduced on the surface to form nitrides. Here, a reactivity of nitrogen gas in ionised state is key factor for forming nitrides in on the surface and is based on chemical composition of the surface. The conventional nitriding methods for surface-treating is quite expensive and time consuming. Additionally, surface-treating or nitriding the surface proximal to the welding region requires it to be placed in furnace having vacuum. Further, replacement of air with nitrogen, ammonia, carbon dioxide and hydrogen along with raising and maintaining temperature up to 1200°C for almost 96 hours is required in the furnace, which is time consuming and requires heavy furnace infrastructure. Hence, known nitriding methods for surface-treating the surface is costly and time consuming.Therefore, in view of the above-mentioned problems, it is advantageous / desirable to provide a product and a method that can overcome the above-mentioned problems and limitations.SUMMARY OF THE PRSENT INVENTIONThis summary is provided to introduce a selection of concepts, in a simplified format, that are further described in the detailed description of the invention. This summary is neither intended to identify key or essential inventive concepts of the invention nor is it intended for determining the scope of the invention.To further clarify the advantages and features of the present invention, a more particular description of the invention will be rendered by reference to specific embodiments thereof, which is illustrated in the appended drawing. It is appreciated that these drawings depict only typical embodiments of the invention and are therefore not to be considered limiting its scope. The invention will be described and explained with additional specificity and detail with the accompanying drawings.As per an embodiment of the present invention, a welding torch for surface-treatment of a welding region has been provided. The welding torch includes a body, a nozzle attached to the body. A first gas-stream flows through the nozzle in the welding region. A shielding attachment is adapted to be disposed on the nozzle, such that the shielding attachment includes a channel defined between an inner surface of the shielding attachment and the nozzle. The channel is adapted to guide a second gas-stream on the welding region. The second gas-stream shields the first gas-stream.As per another embodiment of the present invention, the nozzle is a ceramic nozzle.As per yet another embodiment of the present invention, the body includes a first gas inlet adapted to guide the first gas-stream within the nozzle.As per still another embodiment of the present invention, the shielding attachment includes a casing, such that a second gas inlet is disposed on the casing. The second gas inlet is adapted to guide the second gas-stream within the channel.As per an embodiment of the present invention, the first gas-stream flows at a first gas-stream flow rate in a range of 5 liter per minute and 8 liter per minute, and the second gas-stream flows at a second gas-stream flow rate in a range of 9 liter per minute and 12 liter per minute. As per yet another embodiment of the present invention, the second gas-stream flow rate is greater than the first gas-stream flow rate.As per still another embodiment of the present invention, the first gas-stream includes a nitrogen gas-stream, and the second gas-stream includes any one of a nitrogen gas-stream, an argon gas-stream, or a combination thereof.As per an embodiment of the present invention, a divergence ring is adapted on an open end of the nozzle. The divergence ring diverts the second gas-stream flowing out of the channel in the welding region to restrict the second gas-stream to mix with the first gas-stream.As per another embodiment of the present invention, the shielding attachment has a diffuser defined in the channel. The diffuser has a plurality of orifices adapted to equally disperse the second gas-stream on the welding region.As per an exemplary embodiment of the present invention, a shielding attachment for a welding torch for surface-treatment of a welding region has been provided. The shielding attachment includes a casing adapted to be attached to a nozzle of the welding torch, and a channel defined between an inner surface of the casing and the nozzle. The channel is adapted to guide a second gas-stream on the welding region. The second gas-stream shields a first gas-stream flowing through the nozzle.As per another exemplary embodiment of the present invention, a method for surface-treating a welding region by a welding torch has been provided. The said method includes the steps of, attaching a nozzle to a body, supplying a first gas-stream through a first gas inlet adapted on the body, such that the first gas-stream is flowing in the welding region through the nozzle, adapting a shielding attachment for disposing on the nozzle, supplying a second gas-stream through a second gas inlet adapted on a casing, such that the second gas-stream is flowing in the welding region through a channel defined between an inner surface of the shielding attachment and the nozzle, such that the second gas-stream is shielding the first gas-stream, further including the first gas-stream is surface-treating the welding region.As per an embodiment of the present invention, the step of surface-treating the welding region by the first gas-stream includes a step of nitriding the welding region.As per another embodiment of the present invention, the step of supplying the first gas-stream includes a step of the first gas-stream flowing at a first gas-stream flow rate in a range of 5 liter per minute and 8 liter per minute, and the step of supplying the second gas-stream includes a step of the second gas-stream flowing at a second gas-stream flow rate in a range of 9 liter per minute and 12 liter per minute.As per yet another embodiment of the present invention, the step of supplying the first gas-stream, simultaneously with the step of supplying the second gas-stream, includes an intermediate step of maintaining the second gas-stream flow rate greater than first gas-stream flow rate for decomposing and ionizing of the first gas-stream.As per still another embodiment of the present invention, the step of supplying the first gas-stream includes a step of supplying nitrogen gas-stream, and the step of supplying the second gas-stream includes a step of supplying any one of a nitrogen gas-stream, an argon gas-stream, or a combination thereof.As per another embodiment of the present invention, the step of nitriding the welding region is including a step of shielding the first gas-stream by the second gas-stream for decomposing nitrogen gas from the first gas-stream in the welding region, thereby forming nitrides in the welding region, such that the step of forming nitrides in the welding region includes a step of applying a strong nitride former paste on the welding region for enabling nitriding on the welding region, such that the step of applying the strong nitride former paste comprises a step of applying a thin layer of Aluminum powder, or Chromium powder or a combination paste thereof along with sodium silicate or potassium silicate as a binder. As per yet another embodiment of the present invention, an additional step of adapting a divergence ring on an open end of the nozzle for diverting the second gas-stream flowing out of the channel in the welding region is provided, for restricting the second gas-stream mixing with the first gas-stream.BRIEF DESCRIPTION OF THE ACCOMPANY DRAWINGSThe foregoing and other features of embodiments will become more apparent from the following detailed description of embodiments when read in conjunction with the accompanying drawings. In the drawings, like reference numerals refer to like elements.The accompanying Fig. 1 illustrates a sectional front view of the welding torch as per an embodiment of the present invention.The accompanying Fig. 2 illustrates a top view of a shielding attachment as per an embodiment of the present invention.The accompanying Fig. 3 illustrates a front view of the shielding attachment as per an embodiment of the present invention.Fig. 4 illustrates a flowchart depicting a method for surface-treating a welding region by a welding torch as per an embodiment of the present invention.Further, skilled artisans will appreciate that elements in the drawings are illustrated for simplicity and may not have necessarily been drawn to scale. For example, the flow charts illustrate the method in terms of the most prominent steps involved to help to improve understanding of aspects of the disclosure. Furthermore, in terms of the construction of the device, one or more components of the device may have been represented in the drawings by conventional symbols, and the drawings may show only those specific details that are pertinent to understanding the embodiments of the disclosure so as not to obscure the drawings with details that will be readily apparent to those of ordinary skill in the art having the benefit of the description herein.DETAILED DESCRIPTION OF THE PRESENT INVENTIONFor the purpose of promoting an understanding of the principles of the present disclosure, reference will now be made to the various embodiments and specific language will be used to describe the same. It will nevertheless be understood that no limitation of the scope of the present disclosure is thereby intended, such alterations and further modifications in the illustrated system, and such further applications of the principles of the present disclosure as illustrated therein being contemplated as would normally occur to one skilled in the art to which the present disclosure relates.It will be understood by those skilled in the art that the foregoing general description and the following detailed description are explanatory of the present disclosure and are not intended to be restrictive thereof. Whether or not a certain feature or element was limited to being used only once, it may still be referred to as "one or more features" or "one or more elements" or "at least one feature" or "at least one element." Furthermore, the use of the terms "one or more" or "at least one" feature or element does not preclude there being none of that feature or element, unless otherwise specified by limiting language including, but not limited to, "there needs to be one or more…" or "one or more elements is required."Reference is made herein to some "embodiments." It should be understood that an embodiment is an example of a possible implementation of any features and / or elements of the present disclosure. Some embodiments have been described for the purpose of explaining one or more of the potential ways in which the specific features and / or elements of the proposed disclosure fulfil the requirements of uniqueness, utility, and non-obviousness.Use of the phrases and / or terms including, but not limited to, "a first embodiment," "a further embodiment," "an alternate embodiment," "one embodiment," "an embodiment," "multiple embodiments," "some embodiments," "other embodiments," "further embodiment", "furthermore embodiment", "additional embodiment" or other variants thereof do not necessarily refer to the same embodiments. Unless otherwise specified, one or more particular features and / or elements described in connection with one or more embodiments may be found in one embodiment, or may be found in more than one embodiment, or may be found in all embodiments, or may be found in no embodiments. Although one or more features and / or elements may be described herein in the context of only a single embodiment, or in the context of more than one embodiment, or in the context of all embodiments, the features and / or elements may instead be provided separately or in any appropriate combination or not at all. Conversely, any features and / or elements described in the context of separate embodiments may alternatively be realized as existing together in the context of a single embodiment.Any particular and all details set forth herein are used in the context of some embodiments and therefore should not necessarily be taken as limiting factors to the proposed disclosure. The terms "comprises", "comprising", or any other variations thereof, are intended to cover a non-exclusive inclusion, such that a process or method that comprises a list of steps does not include only those steps but may include other steps not expressly listed or inherent to such process or method. Similarly, one or more devices or sub-systems or elements or structures or components proceeded by "comprises... a" does not, without more constraints, preclude the existence of other devices or other sub-systems or other elements or other structures or other components or additional devices or additional sub-systems or additional elements or additional structures or additional components.Embodiments of the present disclosure will be described below in detail with reference to the accompanying drawings.Referring to the accompanying Figs. 1-3, a welding torch 100 for surface-treatment of a welding region W, is disclosed. In a preferred embodiment of the present invention, surface-treatment of the welding region W includes nitriding the welding region W or a surface proximal to the welding region W. As per an exemplary embodiment of the present invention, the welding torch 100 for surface-treatment of a welding region W includes a body 150. The body 150 is a hollow structure, such that an electrode holder 155 is adapted to be disposed to hold an electrode E through the body 150. A nozzle 110 is attached to the body 150. A first gas-stream S1 flows through the nozzle 110 in the welding region W. A shielding attachment 120 is adapted to be disposed on the nozzle 110. The shielding attachment 120 includes a channel 130 that is defined between an inner surface 175 of the shielding attachment 120 and the nozzle 110. The channel 130 is adapted to guide a second gas-stream S2 on the welding region W, such that the second gas-stream S2 is shielding the first gas-stream S1. The nozzle 110 is a ceramic nozzle 110 in a preferred embodiment of the present invention.The body 150 has a first gas inlet 140 which is adapted to guide the first gas-stream S1 within the nozzle 110. The shielding attachment 120 has a casing 170, such that a second gas inlet 160 is disposed on the casing 170. The second gas inlet 160 is adapted to guide the second gas-stream S2 within the channel 130.In an exemplary embodiment of the present invention, the first gas-stream S1 flows at a first gas-stream flow rate in a range between 5 liter per minute and 8 liter per minute. Likewise, the second gas-stream S2 flows at a second gas-stream flow rate in a range between 9 liter per minute and 12 liter per minute. Therefore, the second gas-stream flow rate is greater than the first gas-stream flow rate. In additional embodiments of the present invention, the first gas-stream S1 includes a nitrogen gas-stream S1. Likewise, the second gas-stream S2 includes either a nitrogen gas-stream S2, an argon gas-stream S2 or a combination thereof.It is noteworthy that variation in flow rates of the first gas-stream S1 and the second gas-stream S2 ensures constriction of the first gas-stream S1 by the second gas-stream S2. That way, the first gas-stream S1, which is usually the nitrogen gas-stream S1, is forced to remain constrained and focused on the welding region W. Therefore, nitrogen is constrained on the welding region W in a near-plasma environment, which ensures ionization and decomposition of the nitrogen to form nascent nitrogen molecules for formation of nitrides. The formation of nitrides effectively help in nitriding the welding region W. In a preferred embodiment of the present invention, a divergence ring 180 is adapted on an open end of the nozzle 110. Here, the divergence ring 180 diverts the second gas-stream S2 flowing out of the channel 130 in the welding region W. Therefore, owing to presence of the divergence ring 180, the second gas-stream S2 is restricted from mixing with the first gas-stream S1.The shielding attachment 120 has a diffuser 190 defined in the channel 130. The diffuser 190 has a plurality of orifices 200 which are adapted to equally disperse the second gas-stream S2 on the welding region W. Referring to the accompanying Figs. 1-3, the shielding attachment 120 for the welding torch 100 for surface-treatment of the welding region W is disclosed herein. The shielding attachment 110 includes the casing 170 which is adapted to be attached to the nozzle 110 of the welding torch 100. The channel 130 is defined between the inner surface 175 of the casing 170 and the nozzle 110. The channel 130 is adapted to guide the second gas-stream S2 on the welding region W. The second gas-stream S2 shields the first gas-stream S1 flowing through the nozzle 110.Referring to the accompanying Fig. 4 which illustrates a flowchart depicting a method 400 for surface-treating the welding region by the welding torch 100 as per an embodiment of the present invention. In an embodiment of the present invention, the method 400 may be implemented by the welding torch 100 as explained with respect to accompanying Figs. 1-3. Referring to the accompanying Figs. 1-4, a method 400 for surface-treating a welding region W by the welding torch 100 is disclosed herein. The method 400 at the step 402 includes attaching the nozzle 110 to the body 150. The method 400 at the step 404 includes supplying the first gas-stream S1 through the first gas inlet 140 adapted on the body 150. The first gas-stream S1 is flowing in the welding region W through the nozzle 110. The method 400 at the step 406 adapting the shielding attachment 120 for disposing on the nozzle 110. Finally, the method 400 at the step 408 supplying the second gas-stream S2 through the second gas inlet 160 adapted on the casing 170. The second gas-stream S2 is flowing in the welding region W through the channel 130 defined between the inner surface 175 of the shielding attachment 120 and the nozzle 110. Furthermore, the step 408 includes the second gas-stream S2 to be shielding the first gas-stream S1, such that the first gas-stream S1 is surface-treating the welding region W. Additionally, the step of surface-treating the welding region W by the first gas-stream S1 includes a step of nitriding the welding region W. The step 404 of supplying the first gas-stream S1 includes a step of the first gas-stream S1 flowing at a first gas-stream flow rate in a range of 5 liter per minute and 8 liter per minute, and the step 408 of supplying the second gas-stream S2 includes a step of the second gas-stream S2 flowing at a second gas-stream flow rate in a range of 9 liter per minute and 12 liter per minute. The step 404 of supplying the first gas-stream S1, simultaneously with the step 408 of supplying the second gas-stream S2, includes an intermediate step of maintaining the second gas-stream flow rate greater than first gas-stream flow rate. The step 404 of supplying the first gas-stream S1 includes a step 404 of supplying the nitrogen gas-stream S1, and the step 308 of supplying the second gas-stream S2 includes a step 308 of supplying any one of the nitrogen gas-stream S2, the argon gas-stream S2 or the combination of the same. The step of nitriding the welding region W is having a step of shielding the first gas-stream S1 by the second gas-stream S2 for decomposing nitrogen gas from the first gas-stream S1 in the welding region W, thereby forming nitrides in the welding region W. Here, the step of forming nitrides in the welding region W includes a step of applying a strong nitride former paste in the welding region W for enabling nitriding on the welding region W. The step of applying the strong nitride former paste comprises a step of applying an Aluminum paste, or a Chromium paste, or a combination paste thereof. An additional step of adapting a divergence ring 180 on the open end of the nozzle 110 for diverting the second gas-stream S2 flowing out of the channel 130 in the welding region W, is disclosed herein. The step of adapting a divergence ring 180 helps in restricting the second gas-stream S2 from mixing with the first gas-stream S1.The welding torch 100 and the shielding attachment 200 disclosed herein is capable of providing surface-treatment on the welding region W when a welding arc is struck during use of the GTAW method. Therefore, surface-treatment in the form of nitriding on the welding region W is possible when welding is conducted on the welding region W. Therefore, the invention as disclosed herein does not require that the welding region W to be subjected to surface-treatment in a separate furnace having vacuum and supplemented with ammonia, carbon dioxide, nitrogen, and hydrogen, and hence the present invention saves time and is cost effective.EXAMPLESAISI 1030 steel having an average hardness of 182 HV is used. The experiments have been performed for validation of hardness achieved by with the AISI 1030 steel after being surface-treated by the welding torch along with the shielding attachment attached thereon, in following three cases.1. Nitriding without Nitride formers - The nitride formers are not employed in this case and allowed to form FeN (iron nitride) only. The average hardness on a top surface of the AISI 1030 steel is observed as 251 HV with maximum value of 315 HV.2. Nitriding with Chromium powder as Nitride former - Chromium powder with potassium silicate as the binder is employed with known mass of chromium powder. The average hardness on the top surface of the AISI 1030 steel is observed as 390 HV with maximum value of 463 HV.3. Nitriding with Aluminium powder as Nitride former - Pure aluminium powder with potassium silicate as the binder is employed with known mass of aluminium powder. The average hardness on the top surface of the AISI 1030 steel is observed as 308 HV with maximum value of 378 HV.From the above, it is seen that the average hardness on the top surface of the AISI 1030 steel is highest during nitriding of the AISI 1030 steel with the present invention disclosed herein, when the presently disclosed invention is used along with chromium powder and aluminium powder as nitride formers in the welding region W.

Claims

1. A welding torch (100) for surface-treatment of a welding region (W), the welding torch (100) comprising: a body (150); a nozzle (110) attached to the body (150), wherein a first gas-stream (S1) flows through the nozzle (110) in the welding region (W); a shielding attachment (120) adapted to be disposed on the nozzle (110), the shielding attachment (120) comprising: a channel (130) defined between an inner surface (175) of the shielding attachment (120) and the nozzle (110), wherein the channel (130) is adapted to guide a second gas-stream (S2) on the welding region (W), wherein the second gas-stream (S2) shields the first gas-stream (S1).

2. The welding torch as claimed in claim 1, wherein the body (150) comprises a first gas inlet (140) adapted to guide the first gas-stream (S1) within the nozzle (110), wherein the nozzle (110) is a ceramic nozzle (110).

3. The welding torch as claimed in claim 1, wherein the shielding attachment (120) comprises a casing (170), wherein a second gas inlet (160) is disposed on the casing (170), wherein the second gas inlet (160) is adapted to guide the second gas-stream (S2) within the channel (130), further wherein the second gas-stream flow rate is greater than the first gas-stream flow rate, wherein the first gas- stream (S1) flows at a first gas-stream flow rate in a range of 5 liter per minute and 8 liter per minute, and the second gas-stream (S2) flows at a second gas-stream flow rate in a range of 9 liter per minute and 12 liter per minute, wherein the first gas-stream (S1) includes a nitrogen gas-stream (S1), and the second gas-stream (S2) includes any one of a nitrogen gas-stream (S2), an argon gas-stream (S2) or a combination thereof.

4. The welding torch as claimed in claim 1, comprises a divergence ring (180) adapted on an open end of the nozzle (110), wherein the divergence ring (180) diverts the second gas-stream (S2) flowing out of the channel (130) in the welding region (W) to restrict the second gas-stream (S2) to mix with the first gas-stream (S1).

5. The welding torch as claimed in claim 1, wherein the shielding attachment (120) has a diffuser (190) defined in the channel (130), wherein the diffuser (190) has a plurality of orifices (200) adapted to equally disperse the second gas-stream (S2) on the welding region (W).

6. A shielding attachment (120) for a welding torch (100) for surface-treatment of a welding region (W), the shielding attachment (110) comprising: a casing (170) adapted to be attached to a nozzle (110) of the welding torch (100); and a channel (130) defined between an inner surface (175) of the casing (170) and the nozzle (110), wherein the channel (130) is adapted to guide a second gas-stream (S2) on the welding region (W), wherein the second gas-stream (S2) shields a first gas-stream (S1) flowing through the nozzle (110).

7. A method (400) for surface-treating a welding region (W) by a welding torch (100), the method comprising steps of: attaching (402) a nozzle (110) to a body (150); supplying (404) a first gas-stream (S1) through a first gas inlet (140) adapted on the body (150), wherein the first gas-stream (S1) is flowing in the welding region (W) through the nozzle (110); adapting (406) a shielding attachment (120) for disposing on the nozzle (110); supplying (408) a second gas-stream (S2) through a second gas inlet (160) adapted on a casing (170), wherein the second gas-stream (S2) is flowing in the welding region (W) through a channel (130) defined between an inner surface (175) of the shielding attachment (120) and the nozzle (110), wherein the second gas-stream (S2) is shielding the first gas-stream (S1), further wherein the first gas-stream (S1) is surfacetreating the welding region (W).

8. The method as claimed in claim 7, wherein the step of supplying the first gas-stream (S1), simultaneously with the step of supplying the second gas-stream (S2), includes an intermediate step of maintaining the second gas-stream flow rate greater than first gas-stream flow rate for decomposing and ionizing the first gas-stream (S1) on the welding region (W), wherein the step of supplying the first gas-stream (S1) includes a step of supplying a nitrogen gas-stream (S1), and the step of supplying the second gas-stream (S2) includes a step of supplying any one of a nitrogen gas-stream (S2), an argon gas-stream (S2) or a combination thereof, further wherein the step of supplying the first gas-stream (S1) includes a step of supplying the first gas-stream (S1) flowing at a first gas-stream flow rate in a range of 5 liter per minute and 8 liter per minute, and the step of supplying the second gas-stream (S2) includes a step of supplying the second gas-stream (S2) flowing at a second gas-stream flow rate in a range of 9 liter per minute and 12 liter per minute.

9. The method as claimed in claim 7, wherein the step of surfacetreating the welding region (W) by the first gas-stream (S1) includes a step of nitriding the welding region (W), wherein the step of nitriding the welding region (W) is comprising a step of shielding the first gas-stream (S1) by the second gas-stream (S2) for decomposing nitrogen gas from the first gas-stream (S1) in the welding region (W), thereby forming nitrides in the welding region (W), wherein the step of forming nitrides in the welding region (W) includes a step of applying a strong nitride former paste in the welding region (W) for enabling nitriding on the welding region (W), wherein the step of applying the strong nitride former paste comprises a step of applying a thin layer of Aluminum powder, or Chromium powder or a combination powder thereof along with sodium silicate or potassium silicate as a binder.

10. The method as claimed in claim 7, comprises an additional step of adapting a divergence ring (180) on an open end of the nozzle (110) for diverting the second gas-stream (S2) flowing out of the channel (130) in the welding region (W), thereby restricting the second gas-stream (S2) mixing with the first gas-stream (S1).