AI Technical Summary
Current synthetic wet strength resins used in paper production are costly, environmentally harmful, and pose health risks due to the use of carcinogenic and toxic chemicals, while also having limitations in storage life and pH control requirements.
A bio-based process utilizing epsilon poly-l-lysine (EPL) in combination with oxidized cellulose fibers to enhance the wet tensile strength of paper products, eliminating the need for synthetic additives and providing a safer, more environmentally friendly solution.
The process significantly improves both wet and dry tensile strengths of paper, achieving high wet over dry tensile ratios without the use of synthetic additives, making it suitable for applications such as tea bags, facial tissues, and filter papers.
Abstract
Description
FIELD OF THE INVENTIONThe invention belongs to the technical field of paper packaging additives, and particularly relates to a process to enhance a wet strength of papers with bio-based wet strength additive for making papers. BACKGROUND OF THE INVENTIONWet strength is a very important property for many grades of paper that are exposed to water during use. Paper not treated for wet strength typically has 3-7% of its original dry strength available when tested while wet. It is also possible to further subdivide wet strength papers based on the permanence of their strength when wet. Paper which has not been treated typically loses its strength within seconds of being soaked in water, while with some wet strength chemicals the rate of wet strength loss during soaking is slowed. Such papers are said to possess temporary wet strength. Other chemicals provide a longer lasting effect and are said to impart permanent wet strength, even though the wet strength is not fully permanent.Because of the need for paper products that retain some of their strength when soaked in water, chemical wet strength resins have been developed which produce paper products typically retaining 20-40% of their dry strength. In the paper industry, papers having wet tensile strengths of more than 15% of the original dry tensile strength are considered to be wet strength papers. In order to achieve wet strength, wet strength resins have been developed which are, in general, chemically reactive, water-soluble polymers that are added at the wet end of the paper machine. They are typically quite expensive and are prone to a host of problems. The first resins to become popular in use for improving wet strength were the aminoplast resins, urea-formaldehyde and melamine-formaldehyde. These resins are thermosetting and require heat and low pH to properly cure. They had adverse effects on brightness and absorbency, and the low pH was corrosive to the equipment. They have fallen out of common use because of environmental problems associated with their formaldehyde content / release. More recently, epoxidized polyamide resins (PAE) and glyoxalated polyacrylamide (GPAM) resins have been developed and have found generally good acceptance in the paper industry. They can be used in neutral or alkaline conditions and, while the epoxidized polyamide resins produce a permanent wet strength, the glyoxalated polyacrylamide resins provide only temporary wet strength, although some increase in dry strength is also achieved. Despite the significant advances that these resins represent, there are still a great many problems associated with their usage including high cost, limited storage life, expensive addition systems, pH control on the paper machine, curing time, and sensitivity to other chemicals. In addition, the epoxidized polyamide resins have environmental concerns because of the absorbable organic halogen (AOX) emissions, while the glyoxalated polyacrylamide resins are not suitable for all uses because of the temporary nature of their wet strength development.The synthetic additives used in wet strength papers, however, are not easily bio-degradable, toxic, and have negative health implications when consumed directly and / or indirectly, thereby shifting the focus towards Bio based additives. PAE is the most commonly used wet strength additive in paper application. But, the precursors of PAE, epichlorohydrin is carcinogenic in nature and releases harmful chemicals like adsorbable organic halides (AOX), making the environment harmful when working with it. Hence there exist a need to focus on developing an environmentally friendly and food safe material for use as a wet strength additive in papermaking. Lately, several natural additives have been explored to provide wet strength properties to paper. These additives include modified starch, chitosan, wheat gluten and galactomannan. Permanent wet strength is achieved by crosslinking hydroxyl groups of cellulose with other functional groups. Chitosan was able to impart permanent wet strength in cellulose fibers because it was able to form amide linkage with cellulose fibers. However, it was less effective when compared to synthetic additives. Epsilon poly-l-lysine (EPL) is a naturally occurring bacterial cationic polymer with amine groups, which can react with aldehydes forming irreversible imine bonds by Schiff base reaction. Crosslinking aldehydes with amine groups results in forming permanent imine group called azomethine. Dialdehyde groups can be incorporated into cellulose fibers by oxidizing cellulose with periodate, which modifies the C2 and C3 hydroxyl groups forming dialdehyde cellulose (DAC). EPL offers a promising substitute for traditional synthetic wet strength additives being used in making papers for various application and help in achieving the SDGs.The invention is about a process employing a wet strength additive that is bio-based and more compatible to a wide variety of ecological considerations while still accomplishing the task of providing suitable wet strength in the finished product.OBJECT OF THE INVENTIONThe objective of the present invention is to provide a bio-based solution to the challenge of enhancing the wet strength of paper products, thereby replacing harmful synthetic additives. Specifically, the invention aims to provide a paper that meets the high wet strength requirements while avoiding carcinogenic, toxic, and environmentally harmful substances.SUMMARY OF THE INVENTIONThe invention is about a process to enhance a wet strength of papers that can be used as packaging material for various application. The cellulose fiber can be modified to provide the wet strength function of a product without the addition of any synthetic chemically reactive polymer. In accordance with this invention, the modification of cellulose fibers with polylysine results in significant improvements to the wet tensile strength and the dry tensile strength exhibited by paper sheets made with the treated fibers of this invention. The wet tensile strength: dry tensile strength ratio (sometimes referred to as the "wet over dry" ratio) can be increased without the addition of any other traditional wet strength agents.The invention provides a process for enhancing the wet tensile strength of paper products by utilizing bio-based epsilon polylysine in combination with oxidized cellulose fibers. Cellulose fibers are first oxidized using sodium periodate to form dialdehyde cellulose, which is then treated with epsilon polylysine and cationic starch to form modified cellulose fibers. The resulting paper exhibits significantly improved wet and dry tensile strength, making it suitable for paper based applications such as tea bags, facial tissues, and filter papers.BRIEF DESCRIPTION OF THE DRAWINGSFIG. 1 Schematic diagram of grafting EPL on cellulose and preparing EoWet paperFIG. 2 FTIR spectra of Neat, DAC and DAC+EPL papersFIG. 3 Reaction Mechanism: EPL gets cross-linked with cellulose fibersDETAILED DESCRIPTION OF THE INVENTIONThe wet tensile strength of the papers is enhanced for different applications such as tea bags, filter papers, facial tissues, etc. The cellulose fibers are oxidized using sodium periodate to form dialdehyde cellulose. The epsilon polylysine solution and cationic starch solution are prepared and Ioaded onto the dialdehyde cellulose to modify the fibers. The modified cellulose fibers are utilized to prepare handsheets of 30 g / m2. The dry and wet tensile strength of the handsheets increased with the reaction time of dialdehyde cellulose and epsilon polylysine. This indicates the use of the process for designing paper, replacing the synthetic additives to impart wet strength to the paper.The invention provides a bio-based wet strength additive as an alternative replacing the usage of synthetic additives. Paper products such as tissues, tea bags, filter papers, etc., frequently come in contact with water; hence, wet strength of the material used for manufacturing plays a major role. However, the major problems to be addressed for the paper are: large amount of water absorption by paper due to its hydrophilic nature, use of synthetic additives in the existing solution, use of formaldehyde-based additives which can be carcinogenic, use of toxic and corrosive raw materials for synthesis of additives, lack of bio-based additives for making high wet-strength paper and a need for a simple processing technique to enhance the wet strength.Formaldehyde and epichlorohydrine-based synthetic additives are most commonly used to increase the wet strength of the paper. However, they involve chemicals that are harmful to the environment. The formaldehyde is carcinogenic in nature and releases volatile organic compounds into the atmosphere. The utilization of such material for packaging food where food comes in direct contact with packaging material paper, for instance, in tea bags or food wrapping paper, could affect human health and issues of migration of packaging substance and micro plastic inhibition exist in the foods. Many industries are interested in including bio-based wet strength additives in papermaking, providing a safe solution for the high-wet strength papers. This invention aims to develop a high wet strength paper using bio-based epsilon polylysine as a wet strength additive. The paper thus produced can also be utilized for food contact applications due to the absence of carcinogenic and health-affecting compounds.Sodium periodate is utilized to partially oxidize cellulose fibers into dialdehyde cellulose. Epsilon polylysine is a bio-based material that reduces the resistance to interaction with water by crosslinking with dialdehyde cellulose fibers. Moreover, the utilization of epsilon polylysine as a crosslinking agent of dialdehyde cellulose fibers can increase the wet strength of the paper along with reducing the reliability of carcinogenic and corrosive material being used in paper-making, especially that comes in contact with food such as tea bags, food wrapping paper, tissue paper, etc. The invention relates to a process of making cellulose fibers with increased wet strength that involves oxidation of cellulose fibers and grafting of oxidised cellulose fibers with polylysine. With regard to the oxidation reaction, there are a great many ways in which the chain units in cellulose can be oxidized. However, most oxidants are unspecific in their mode of attack. Suitable oxidants for purposes of this invention include, without limitation, sodium metaperiodate, sodium paraperiodate, periodic acid, sodium hypochlorite, hydrogen peroxide, ozone, potassium dichromate, potassium permanganate, and sodium chlorite. Periodate ions react with the cellulose without destroying its fibrous nature and result primarily in the oxidative scission of 1, 2 - diols to primarily produce dialdehyde oxycellulose under proper conditions. For this reason, the preferred oxidizing agents are the periodates, such as sodium metaperiodate (NaIO4). The utilization of epsilon polylysine as a crosslinking agent of dialdehyde cellulose fibers can increase the wet strength of the paper along with reducing the reliability of carcinogenic and corrosive material being used in paper-making, especially that comes in contact with food. The pH of the oxidation reaction can preferably be from about 3 to about 4.6. At higher pH, the sodium metaperiodate is converted to insoluble paraperiodate.When using sodium metaperiodate as the oxidation agent, the upper concentration of sodium metaperiodate is limited by its solubility in water, which is 14.44 grams per 100 milliliters at 25° C. The maximum concentration of sodium metaperiodate which can therefore be achieved is about 0.67M. On the other hand, at concentrations below about 0.005M the rate of reaction is too slow for the process to be economically feasible. Preferred concentrations are from about 0.01M to about 0.2M. At higher concentrations, although the reaction will proceed faster toward the desired degree of substitution, the shorter treatment time is likely to result in non-uniformity of the substitution.The preparation method of a dialdehyde cellulose cross-linked with epsilon polylysine is characterized in that epsilon polylysine is grafted on the dialdehyde cellulose fibers.Softwood bales were first disintegrated for 20 minutes (60,000 revolutions) in a disintegrator. The resulting pulp was then refined in a PFI mill at a consistency of 10 wt. / vol.% (30g oven-dried pulp in 300 ml of water) until a freeness (°SR) of 40 was achieved. To modify the cellulose fibers, sodium periodate (NaIO4) was added at varying amounts of 0.1, 0.25, and 0.5 moles per mole of anhydride group in the cellulose fibers and the reaction was carried out for 30, 15, and 5 minutes respectively at a controlled pH of 3, adjusted with acetic acid, and conducted in a dark environment to prevent oxidation of NaIO4. The reaction was then stopped by adding ethylene glycol, after which the dialdehyde cellulose (DAC) was washed and the pH was adjusted to 9 by adding sodium hydroxide (NaOH). For each mole of DAC, 2 moles of epsilon poly-l-lysine (EPL) were dissolved in water to prepare an EPL solution, and the pH of this solution was also adjusted to 9 with NaOH. Simultaneously, a cationic starch (CS) solution was prepared by mixing 1 wt.% of CS with dry fiber mass in water, and the pH of this solution was adjusted to 9 using NaOH. The EPL and CS solutions were combined and added to the modified cellulose fibers. Handsheets with a grammage of 30 GSM were then prepared, pressed at 4 kgf / cm², and dried in an oven at 105°C overnight. The resulting EPL-grafted handsheets were used to produce high wet strength papers.The oxidation / lysine crosslinking of cellulose results in significant improvements in the wet and dry tensile strength and provides high wet over dry tensile ratios for the cellulose pulp so treated. The wet and dry tensile strengths of cellulose pulp can be optionally further enhanced by refining the cellulose pulp prior to the oxidation / lysine cross-linking. Such refining also increases the wet over dry tensile ratio significantly. When used as a pre-treatment, refining serves to bring about external and internal fibrillation of the fibers. This increases the surface area of the fibers and also increases accessibility of the fibrils and cellulose chains to oxidation / crosslinking. These factors contribute to the observed increase in wet strengths which can be extremely useful in the manufacture of a wide variety of paper products such as tissue and towelling, board, tea bags, paper bags, wet wipes, and tissue wraps in personal care products and the like.In the main embodiment of the invention the invention is about increasing the wet strength of the paper by using bio based additives such as epsilon polylysine. In an embodiment of the invention, the cellulose was oxidized using periodate to produce dialdehyde cellulose. In further embodiment, the dialdehyde cellulose is treated with a polylysine solution and cationic starch to produce modified cellulose fibers. In the next embodiment, the polylysine treated dialdehyde cellulose are used to produce paper with enhanced wet tensile strength. In the other embodiment, the process leads to a partial modification of cellulose into dialdehyde cellulose by reacting with sodium metaperiodate for a limited time period at a controlled acidic pH. In further embodiment, the action of metaperiodate with cellulose is halted by adding ethylene glycol. In still further embodiment, the treatment of cellulose fibers with sodium metaperiodate is carried out in dark conditions to prevent the oxidation of sodium metaperiodate. In the next embodiment, epsilon polylysine coupled with cationic starch is grafted on the surface of partially modified dialdehyde cellulose at an alkaline pH of approximately 9.In the continued embodiment it leads to the formation of imine bonds between the amine groups of polylysine and aldehyde groups of dialdehyde cellulose. In the next embodiment, the percentage wet strength of the paper after crosslinking is 10-45%, as required by the wet strength papers. The tear strength index of the paper produced is in the range of 7 .5 to 9.5 mNm2 / g. EXAMPLESoftwood bales were disintegrated for 20 minutes (60,000 revolutions) in a disintegrator. Then the pulp was refined in a PFI mill at a pulp consistency of 10 wt. / vol.% (30g oven-dried pulp in 300 ml water) until the °SR of 40 is reached. For every mole of anhydride group in cellulose fibers, 0.1, 0.25 and 0.5 moles of NaIO4 are added and the reaction was allowed to carryout for 30, 15 and 5 minutes at a controlled pH of 3 obtained by adding acetic acid. The whole reaction was carried out in a dark environment to prevent oxidation of NaIO4. The reaction was halted by adding ethylene glycol and the obtained DAC was washed followed by adjusting pH to 9 by adding NaOH. For every mole of DAC, 2 moles of EPL were dissolved in water to prepare an EPL solution and the pH of this solution was adjusted to 9 by adding NaOH. Simultaneously, cationic starch solution was prepared by loading 1 wt.% of CS on dry fiber mass in water and the pH of this solutions was also corrected to 9 using NaOH. The CS and EPL solution were mixed and loaded into the modified fibers followed by preparing handsheets of 30 GSM. The prepared handsheets were pressed at 4kgf / cm2 and then dried in an oven at 105°C overnight. This process is illustrated in FIG. 1. The wet tensile strength of the resulting paper is found to be in the range of 10–45%, meeting the requirements for wet strength papers. The tear strength index of the paper is between 7.5 and 9.5 mNm² / g, further demonstrating its suitability for high-performance applications.Example Bleached softwood pulp containing 20 weight percent hardwood pulp was used as the cellulose pulp. 100 grams of the pulp was oxidized by slurrying the pulp with 2000 milliliters of 0.05M sodium metaperiodate solution at ambient temperature for 1 to 6 hours. At the end of the oxidation reaction, the pulp was washed with distilled water to free it from unreacted reagents and by-products. For this washing step, water having a pH of 8 or greater should be avoided because dialdehyde oxycellulose degrades at alkaline pH. The significant product of the oxidation step was dialdehyde oxycellulose.Fourier-Transform Infrared Spectroscopy (FTIR)The attenuated total reflection Fourier-transform infrared spectroscopy was conducted on the prepared handsheets to determine the chemical composition using a Perkin Elmer, C91158 spectrophotometer. The spectra were taken with 4 cm-1 resolution and 4000- 500 cm-1 wavelengths for every sample. All the spectra were baseline corrected and then normalized.The addition of NaIO4 to cellulose results in oxidizing the anhydride groups in cellulose fibers forming a C=O linkage as observed at 1740 cm-1. This indicates the modification of cellulose into DAC. Further addition of EPL resulted in collapsing the carbonyl group (C=O), which can be directly correlated to the absence of peak at 1740 cm-1 for the EPL grafted fibers (DAC+EPL). Further, the broadening of peak at 1610 cm-1 indicates the formation of imine bonds between the amide groups of EPL and aldehydes of DAC, which are responsible for the enhanced wet strength of the paper. FTIR spectra of Neat, DAC and DAC+EPL papers are presented in FIG. 2.Based on the visible modification in functional groups of papers, the possible mechanism of reaction between cellulose, NaIO4 and EPL is presented in FIG. 3. The cellulose fibers containing primary and secondary hydroxyl groups react with NaIO4 and are converted to dialdehyde cellulose. Further addition of EPL at an adjusted pH of 9 resulted in breakage of carbonyl groups and formation of imine bonds.Grammage, thickness and porosity of prepared handsheetsThe grammage of the prepared handsheets is maintained close to 30 g / m2 and the thickness of the handsheets along with mechanical properties is presented in Table 1. The dry and wet-tensile strength of the prepared handsheets were tested using a horizontal tensile tester (Frank PTI, Germany) following ISO 1924-2:2008 and IS-1060:2014. The dry-strength testing was performed on 15 mm wide strips, and the clamping length was set at 100 mm. Likewise, wet strength testing was done by dipping a 15 mm wide strip in distilled water for 1 minute, and the extra water was removed by manually rolling the strip placed in between the bloating papers. This wet sheet was then tested for tensile strength. Further % Wet strength was calculated using Eq 1. All the tests were carried out in triplicates% Wet Strength = (Wet Strength (N.m.g^(-1))) / (Dry Strength (N.m.g^(-1))) ×100 Eq 1The dry and wet tensile strength of the neat paper without any modification is found to be 1149.473 N / m and 54.87 N / m respectively. For the paper to be considered to possess good wet strength, the % wet strength in terms of dry strength should be greater than or equal to 15%. For neat paper, the % wet strength is 4.77%, which is below 15% indicating poor wet strength. When the EPL is added to the modified cellulose fibers, whose modification time with NaIO4 is 5 minutes, the wet strength increased from 54.87 N / m for neat papers to 251.53 N / m, 356.72 N / m, and 433.93 N / m for 10, 25 and 50% modification. The % wet strength also increased from 4.77% to 14.16%, 26.56 % and 32.79% respectively. It was clearly evident that the 5 minutes modification of cellulose fibers at all stages is more effective in enhancing the tensile strength of the handsheets. Moreover, the modification of cellulose fibers with NaIO4 and EPL enhanced the dry tensile strength from 1149.47 N / m to 1345.33 N / m at 50% modification, with maximum tensile strength at 10% modification with 1771.38 N / m. On the contrary, this modification reduced the tear strength of the handsheets, but the reduction is insignificant. The tear strength of prepared sheets was tested using a tear tester. The handsheets were cut into samples of size 50 mm × 60 mm and four of such samples were stacked for single measurement. The testing was done in triplicates. The mechanical properties of neat and 10%, 25%, and 50% modified paper containing EPL (DAC+EPL) for 5 min reaction time are tabulated Table 1.Table 1: Mechanical properties of neat and 10%, 25%, and 50% modified paper containing EPL (DAC+EPL) for 5 min reaction timeWhen the reaction time of NaIO4 was increased from 5 minutes to 15 and 30 minutes (Table 2 and Table 3 respectively), the dry strength of the handsheets continue to reduce. This is due to the prolonged interaction of periodate with cellulose fibers, which gradually degrades the cellulose fibers and reduce the individual size of fibers. This reduction directly affects the dry and wet strength of the handsheets produced thereof. This increase in reaction time also has negative implications in making significant loss in tear strength of the handsheets.Table 2: Mechanical properties of neat and 10%, 25%, and 50% modified paper containing EPL (DAC+EPL), respectively, for 15 min reaction timeTable 3: Mechanical properties of neat and 10%, 25%, and 50% modified paper containing EPL (DAC+EPL), respectively, for 30 min reaction timeThis indicates that the 5-minute modification of cellulose fibers with NaIO4 is best suited as there exist no loss in dry tensile strength of the fibers. The handsheet prepared for wet strength paper application was tested for porosity and was further compared with commercial tea bags. The porosity of neat handsheets without any modification in terms of time taken to transmit 300 ml of compressed air is 4.91 s. The porosity of handsheets obtained by 5-minute modification of fibers at 10%, 25% and 50% is 1.52 s, 1.45 s and 1.39 s respectively, which is similar to that of commercial tea bags at 1.51 s. The partial modification by converting 10%, 25% and 50% of cellulose fibers is more effective in enhancing the wet tensile strength of the handsheets and thus can be used to make wet strength papers such as tea bags, tissue paper, filter paper, and facial tissues. Table :The addition of periodate was successful in oxidizing the cellulose fibers into dialdehyde cellulose. The FTIR revealed that after addition of periodate, the carbonyl groups increased. The addition of EPL to this dialdehyde cellulose resulted in breaking those carbonyl groups and formation of imine bonds which was also confirmed through FTIR spectra. The dry and wet tensile strength of the handsheets increased with 5 minutes of reaction time between periodate and cellulose. This addition of EPL did not show any significant effect on tear index of the handsheets. Also, the handsheets possess similar porosity as that of commercial tea bags. However, with increasing the reaction time of periodate and cellulose fibers, the cellulose fibers degrade thereby reducing the strength of the handsheets. Therefore, this EPL grafted modified cellulose fibers can be utilized to produce handsheets where the wet strength of the paper is dominant such as filter papers, tea bags tissue papers, facial tissues, currency notes, paper bags and household paper.
Claims
1. A process for enhancing the wet tensile strength of paper by grafting Epsilon poly-l-lysine (EPL) on cellulose fibers comprising: a. oxidizing cellulose fibers by adding 0.1-0.5 moles of sodium periodate solution to the cellulose fibers at a controlled pH of 3 in dark condition, b. halting the reaction by adding ethylene glycol to obtain dialdehyde cellulose (DAC) c. washing the obtained DAC and adjusting the pH to 9 with sodium hydroxide d. preparing aqueous solution of Epsilon poly-l-lysine (EPL) maintaining pH at 9 e. preparing the cationic starch solution pH being maintained at 9 f. mixing the cationic starch solution and EPL solution and loading into the DAC fibers and g. preparing handsheets from the modified cellulose fibers2. The process for enhancing the wet tensile strength of paper as claimed in claim 1 wherein for every mole of DAC, 2 moles of EPL are dissolved in water.
3. The process for enhancing the wet tensile strength of paper as claimed in claim 1 wherein the cationic starch solution is loaded in an amount of 1wt% of cationic starch on dry fiber mass.
4. The process for enhancing the wet tensile strength of paper as claimed in claim 1 wherein the handsheets prepared are of 30 GSM.
5. The process for enhancing the wet tensile strength of paper as claimed in claim 1 wherein the handsheets prepared are pressed at 4Kgf / cm2 and dried at 105C overnight.
6. A paper produced by the process as claimed in claim 1 wherein the wet tensile strength of the paper is in the range of 10–45%.
7. A paper produced by the process as claimed in claim 1 wherein the tear strength index of the paper is between 7.5 and 9.5 mNm² / g.