A method for manufacturing kenaf fiber-reinforced concrete

IN597387BActive Publication Date: 2026-07-30SONA COLLEGE OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202341043034
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-06-27
Publication Date
2026-07-30
Estimated Expiration
2043-06-27
Patent Text Reader

Abstract

ABSTRACT The present invention relates to a method for manufacturing kenaf fiber-reinforced concrete, wherein the said kenaf fiber is treated with NaOH, HCl, and distilled water for enhanced characteristics. The invention describes that HCl treated 0.75 % of kenaf fiber when added to M20 grade concrete mixture exhibits high compressive strength with good water properties and reduces pollution in construction by absorbing CO2 from the air thereby making it environment friendly. Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

FIELD OF THE INVENTIONThe present invention relates to a method for manufacturing kenaf fiber-reinforcedconcrete. More specifically, the present invention relates to a method for manufacturing kenaffiber-reinforced concrete that absorbs CO2 from air making the said concrete environmentfriendlyBACKGROUND OF THE INVENTIONIt is time for the concrete industry to move towards sustainability and to minimize airpollution. It is estimated that approximately 1T of CO2 is released during the production of eachvolume of standard Portland cement, according to a database, endangering the environment. TheEuropean Commission (EC) in this regard has a proposal to limit CO2-based emissions by fourlevels below the EU's emissions by 2031. One way of achieving this is by incorporating naturalfibers into the concrete mix, particularly fibers from native-based plants, which may increaseconcrete's durability and strength properties (in particular, tensile strength) in addition to itssignificant mechanical strength. Green buildings are an emerging concept for sustainability. Withthe addition of short, discrete man-made or natural fibers, fiber-reinforced concrete (FRC),ensures the abundance of benefits in the list like improved shear capacity and ductility, delayedcrack propagation, high impact resistance, greater energy concentration, and changes in thefailure category of concrete.Kenaf fibers were at the top of the list of natural fibers used in practice because of theirincreased flexural and shear properties as well as ductility when used to make fiber-reinforcedconcrete. The plants that produce kenaf fiber grow in the hot, humid climates that are prevalentin places like Africa, India, and China. Studies show that kenaf-based particleboard performsbetter than traditional wood in terms of physical and mechanical qualities over a longer period.Additionally, it was discovered that the kenaf fiber's core particles could be coupled with fireretardant chemicals to create particle-based boards that generate less spark when a fire starts andrelease the heat instead. Besides, kenaf plant fiber is advantageous for the environment since itabsorbs carbon dioxide better than other plant fibers.The tensile behavior of short kenaf fibers mixed with maleated polyethylene (MAPE) andmaleated polypropylenes (MAPP) as coupling agents were studied. The fiber is immersed invarious sodium hydroxide (NaOH) concentrations for a day before being oven dried at 82°C. Theresults concluded that treated kenaf fibers perform better than untreated kenaf fibers.There are many literatures in the art describe the inclusion of kenaf fibers in concreteproduction because of its lower cost requirements, low density, and naturally biodegradablecharacteristics, however, the present invention provides an optimum percentage of pre-treatedkenaf fibers used for the manufacturing reinforced concrete with maximum compressive strengthand minimum water absorption properties that ultimately sequester maximum carbon dioxide toimprove the environment.SUMMARY OF THE INVENTIONThe present invention relates to a method for manufacturing kenaf fiber-reinforcedconcrete.In one embodiment, the present invention relates to a method for manufacturing fiber-reinforced concrete by adding chemically pre-treated kenaf fiber to the concrete.In another embodiment, the present invention relates to kenaf fiber treated with NaOH,HCl, and distilled water and added to a concrete mixture to produce kenaf fiber-reinforcedconcrete. The kenaf fiber in the mixture is added in the range of 0.75, 1 and 1.5 percent. Afterone week, two weeks, and 28 days of curing, the compressive strength, water and carbon dioxideabsorption properties of the produced kenaf fiber-reinforced concrete were studied.In yet another embodiment, the present invention relates to a method for manufacturingfiber-reinforced concrete by adding HCl treated 0.75 % of kenaf fiber to a M20 grade concretemixture. The said mixture exhibited high compressive strength with good water and carbondioxide absorption properties.BRIEF DESCRIPTION OF THE DRAWINGSFigure 1 depicts the pictorial representation of kenaf fiber before and after the cutting process.Figure 2 depicts the kenaf fiber before and after treatment.Figure 3 depicts the specimen preparation with kenaf fiber.Figure 4 depicts the compressive strength at different fiber percentages.Figure 5 depicts the compressive strength of the concrete specimen.Figure 6 depicts the Phenolphthalein spray done over the concrete cube.Figure 7 depicts the steps involved in the CO2 absorption test.Figure 8 depicts the SEM analysis of concrete specimen.Referring to the drawings, the embodiments of the present invention are further described. Thefigures are not necessarily drawn to scale, and in some instances the drawings have beenexaggerated or simplified for illustrative purposes only. One of ordinary skill in the art mayappreciate the many possible applications and variations of the present invention based on thefollowing examples of possible embodiments of the present invention.DETAILED DESCRIPTION OF THE INVENTIONThe present invention relates to a method for manufacturing kenaf fiber-reinforcedconcrete, wherein the said kenaf fiber is treated with NaOH, HCl, and distilled water forenhanced characteristics.In one embodiment, the present invention relates to a method for manufacturing fiberreinforced concrete by adding HCl treated 0.75 % of kenaf fiber to a M20 grade concretemixture. The said mixture exhibited high compressive strength with good water and carbondioxide absorption properties.Preparation of Test SpecimenThe kenaf fiber-infused concrete composite exhibits a uniform distribution of fracturefailure patterns and greater toughness, both of which contribute to structural stiffness. Byguaranteeing the linear connection between the stress and strain parameters, the first and mostimportant fracture resistance experiment was conducted. The testing specimen, which was madeof 5 kg of fiber and has a length of 2.5 m, was further reduced to 25 mm in length and 0.017 to0.021 mm in diameter using a real slicing machine. Figure 1 is to locate the appropriateness thatmakes mixing the concrete specimen easy, precutting is done to determine the needed size.When compared to other grades of cement, ordinary Portland concrete (OPC) 53 grade,which complies with IS 12269:1987, consistently has better strength. For this reason, it wasincluded as the primary component in the mix created for the study. Calcium, silica, alumina,and iron are the major chemical components that support OPC's strength. Ultra-modern concretewas used in the study since it achieves great strength and quick setting. Fundamental tests wereconducted on the concrete species, and the results were given with the specific gravity value of3.150, beginning and final setting time intervals of 170 and 240 minutes, and sulfateconcentrations of 2-3% and 0.01-0.02%, respectively.In the present invention, granite was used as a coarse type aggregate with a nominal sizeof 10 to 12 mm. The aggregate has been cleaned with clean water, dried, and scrubbed to get ridof any dust particles. Before being added to the concrete, coarse and fine aggregate will besieved to ensure that the particle size in the mix is homogeneous. The sand was used as a fineaggregate, and an ASTM-required sieve test was run to verify the particle size. To get theconcrete to a dry state under saturated surface dry conditions, fine aggregate is used as a filleringredient.In general, the ratio of cement weight to water concentration is quite important inforecasting the concrete's overall strength zone. Increased workability is aided by a higher water-to-cement ratio, but the concrete loses strength and durability. When water is added to cement, achemical complex is created that allows cement to be ground into powder. The necessaryquantity of strength and durability attributes will be added to the mixture in this hardeningcondition to make sure it is ready for the experiment. For the concrete, a value of 0.45 water -cement ratio was chosen as the ideal ratio.The kenaf fibers used in the current investigation must be pre-treated with water beforethe sequential procedure as mentioned in figure 2. The crucial step in ensuring that the kenaffiber utilized in the study has the best possible characteristics is pre-treatment. To achieve thegoal, kenaf fibers with a 0.017 to 0.021 mm in diameter were cut to the ideal length of 25 to 50mm. After being treated with NaOH, HCl, and distilled water the kenaf fiber characteristics wereevaluated. When treated with HCl, the kenaf fiber was soaked in distilled water for five minutesto achieve the correct pH which is 12-13 while accounting for the fiber's water absorption.A concrete mixture with the proportions 1:1.5:3 is intended to verify the M20 castinggrade. After adding water to the concrete mix, mixing was carried out in the dry condition. Theconcrete sample measured 150x150mm in size. The 30 concrete cube samples were created withfiber percentages of 0.75, 1 and 1.5 percent. After one week, two weeks, and 28 days of curing,the concrete specimen was tested. The mixing and molding procedures examined was depicted infigure 3 and the various mix proportions used for casting the specimen is mentioned in Table 1.Table 1: Mix proportionS.No. Material Amount (%)1 Cement 18.182 Coarse Aggregate 54.543 M-Sand 27.274 Kenaf Fiber 0.75,1 and 1.55 Water 8Test and ResultsLaboratory experiments were done on the prepared specimens, including the kenaf fibers,to accurately anticipate the reaction. The tests that were conducted included the water absorptiontest following the casting process, the compressive strength test, and the slump test in fresh stage.Concrete specimen's compressive strengths provide insight into all the properties neededto determine the strength of concrete which is mentioned in figure 4. The test will determine theconcrete-making process, including the mixing process's quality and efficiency. The type ofcement mix used, the quality of the materials used, the W / C ratio, and the right quality controlpractices utilized during the time are only a few of the factors that affect the quality and strength.Table 2 displays test results that show the specimen's compressive strength after 7, 14, and 28days.Table 2: Compressive strength with incorporation of fibersCompressive strength, (N / mm2) 7 Days 14 Days 28 Days0% 14.1 16.8 20.50.75% 28.2 32.11 41.81% 20.41 29.3 38.21.5% 18.34 26 37.12In general, compressive strength declines as the amount of kenaf fiber increases. Whencompared to other concrete specimens with increasing percentages of kenaf fiber, the above tablesuggests that the compressive strength of concrete with 0.75 % of kenaf fiber has the maximumcompressive strength.Compressive strength of pretreated fibers concrete specimens with 7, 14 and 28 daysstrength was depicted in Table 3. Of the various mixtures, the pretreated fibers treated with HClsolution had the highest strength, followed by pretreatment with boiling distilled water.According to reports, NaOH solution-treated fibers exhibit the least strength and are notrecommended for practical applications when it comes to the compressive strength criterion.Table 3: Compressive strengthCompressive strength, (N / mm2) 7 Days 14 Days 28 DaysHCl - 0.75% 9.57 15.15 24.5NaOH - 0.75% 4.30 8.61 17.22Boiled Distilled water - 0.75% 5.01 10.10 20.12Raw Kenaf - 0.75% 5.03 9.44 20.15When compared to other kenaf fiber-reinforced concrete specimens treated with NaOHand boiled distilled water, the above table suggests that the compressive strength of kenaf fiber-reinforced concrete treated with HCl has the maximum compressive strength of 24.5 N / mm2.The compressive strength of conventional concrete is 20.5 N / mm2.Once the compressive strength test was performed, crack pattern was studied from figureon various proportion of kenaf fiber incorporated in concrete samples. After the compressivestrength test, the fracture pattern on different percentages of kenaf fiber added to concretesamples was examined. The failure patterns of treated fibers were also examined, and the resultswere presented in table 4. In contrast to other combinations of fibers, which often show acombination of brittle and ductile failure, concrete specimens without fiber inclusion show brittlefailure.Table 4: Cracking mode and failure pattern of cubeTable 4According to IS 1124(1974), the kenaf fiber concrete water absorption test wasperformed at 7, 14, and 28 days to evaluate the concrete's durability for practical applications.Conventional concrete tested in the water absorption test performed better than the kenaf fiber-reinforced concrete, especially at mix amounts of 0.75%. The test results from table 5 shows thatkenaf fiber-reinforced concrete had greater water absorption rate than ordinary concrete for 0.75percent incorporation of fiber and the shows decreasing water absorption trend for 1-1.5percentage of fiber addition. The reaction of kenaf fiber with the concrete mix to lower itsporosity response, which is an important parameter for concrete strength, can be seen from thetendency, which was more evident on the days corresponding to values 14 and 28.Table 5: Water absorption at different fiber percentages without treatment of fibersWater Absorption (%) 7 days 14 days 28 days0 1.34 1.67 2.120.75 2.05 2.30 2.561 2.58 1.62 1.471.5 1.27 1.21 0.304According to the tale, concrete that contains 1.5 % of Kenaf Fiber absorbs less water thanregular concrete. As a consequence, when compared to other combinations, concrete with 1.5 %of kenaf fiber produces the best results in terms of water absorption properties without anypretreatment. After receiving pre-treatment with NaOH, HCl, and distilled water, 0.75% hasbeen fixed considering the high compressive strength value (41.8 N / mm2) to test the specimensince it exhibits higher strength characteristics from a compression strength point of view. Whentreated with HCl as opposed to other solutions, the reaction in terms of reduced water absorptionphenomena was intriguing to see. Pre-treatment before use in concrete applications is stronglyadvised since a reduction of 71 percent was found compared to the nominal mix percentage.According to test findings, HCl, boiled distilled water, and NaOH record the lowest percentagesof water absorption (Table 6).Table 6: Water absorption at 0.75 percentages (with treatment of fibers)Days Nominal Mix Kenaf NaOH HCl Raw Kenaf Boiled Distil Water7 2.05 1.03 0.57 1.50 0.9114 1.98 0.91 0.42 1.31 0.8228 1.72 0.75 0.38 1.11 0.67CO2 sequestration rate of concrete specimens with kenaf fiberAccording to past scientific research, carbon dioxide is the main cause of the greenhousegas effect, hence great efforts have been made to lower the amount of CO2 in the atmosphere. Itwas determined, after studying a variety of corrective actions, that carbon absorption by plantscan be one of the most effective ways to reduce greenhouse gas emissions. Out of several plantkinds, it was discovered that the kenaf plant can absorb 1.5 times the carbon dioxide in terms ofits weight, which is thought to be the primary determinant of the sequestration ability of kenaffibers. When compared to other plant categories and other C3 category plants that are present inthe atmosphere, the photosynthetic value of kenaf is 3-8 times greater. According to a databaseon biomass generated by different natural fibers, kenaf plants absorb 22 to 89 tons of CO2 perhectare per year, depending on the climatic conditions in the nation. Figure 6 shows that thecarbon footprints of the various natural fibers (flax, hemp, jute, and kenaf) are not noticeablydifferent in terms of the proportion of carbon gas absorbed. Jute and kenaf, , exhibit loweremissions during the growing and harvesting processes and are thus strongly recommended fromthe standpoint of their positive effects on the environment.In the current work, concrete test specimens made with kenaf fibers are subjected to aCO2 absorption test, which gives insight into the concrete test specimens' CO2 absorptionproperties. Spraying phenolphthalein solution on both sides of the concrete cube is the first stagein the CO2 absorption test. The carbonation procedure was started by performing aphenolphthalein test on the concrete samples. The dry weight of a concrete cube is measuredbefore the specimen is tested. A laboratory cylinder with a 60 PSI capacity is utilized, and thesample specimen was entered and locked before the experiment. A pressure gauge is used torelease a controlled amount of CO2 gas, and a timer is used to monitor the measurement after 30minutes of absorption. Cubes were removed after the gas injection and their increased weightwas evaluated to determine the rate of CO2 absorption. The gas flow rate is maintainedthroughout the operation in the range of 60 kg / cm2 to 1000 lb / in2. Pressure is released more oftenand necessary safety measures should be taken on-site because if the pressure is released morequickly, there may be a chance of a blast operation occurring within the cylinder from figure 7.CO2 sequestration rate of concrete specimens with kenaf fiber variation from 0 to 1.5percent was carried out. Testing was done on concrete specimens with kenaf fiber variationsranging from 0 to 1.5 percent. Out of several variants, 0.75 was selected as the ideal value. Fiberswere then pretreated with various solutions, and both outcomes were displayed in a pie chart.Comparing untreated fibers to solution-treated fibers, untreated fibers demonstrated good CO2absorption. In comparison to other variants, fibers in concrete included at a rate of 1.5 percentshow good absorption capability. As far as this type of fiber was concerned, a kenaf fiber mixwith 0.75 percent has demonstrated noteworthy performance, which points to the optimalutilization of 0.75 to 1.5 percent integration of kenaf fibers to produce superior absorption rates.Studies using a scanning electronic microscope (SEM) was revealed in figure 8. After 28 days ofcuring, the dispersion pattern shows the specimens' uniform and irregular responses as well astheir delamination reflection.

Claims

1. A method for manufacturing kenaf fiber-reinforced concrete, the said method comprises of: (i) pre-treating the kenaf fiber that is going to be used in the concrete mixture with HCl, (ii) soaking the HCl pre-treated kenaf fiber in distill water for five minutes to achieve the pH in the range of 12-13; (iii) preparing a M20 grade concrete mixture; (iv) adding the HCl pre-treated kenaf fiber soaked in distill water to the M20 grade concrete mixture; (v) curing the mixture obtained from step (iv) for 7, 14 and 28 days; characterized in that, on curing for 28 days, the HCl pre-treated kenaf fiber added to the concrete mixture in the range of 0.75%, exhibits high compressive strength of 24.5 N / mm2, least water absorption rate of 0.38% and reduces pollution in construction by absorbing CO2 from the air thereby making it environment friendly.

2. The method as claimed in claim 1, wherein the NaOH-treated kenaf fiber added to the concrete mixture in the range of 0.75% has the least compressive strength of 17.22 N / mm2 and high water absorption capacity of 0.75%.

3. The method as claimed in claim 1, wherein the boiled distilled water-treated kenaf fiber added to the concrete mixture in the range of 0.75% has a compressive strength of 20.12 N / mm2 20 and a water absorption capacity of 0.67%.

4. The method as claimed in claim 1, wherein the M20 grade concrete is a mixture of cement, coarse aggregate and fine aggregate proportions in the range of 1:1.5:3.