Method for preparing a catalyst comprising an active nickel phase distributed in a shell
Patent Information
- Application Number
- IN202247067585
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-05-29
- Filing Date
- 2022-11-24
- Publication Date
- 2026-07-30
- Estimated Expiration
- 2041-05-18
Abstract
Description
Technical fieldThe present invention relates to a process for preparing a supported metal catalyst based onnickel intended particularly for the hydrogenation of unsaturated hydrocarbons, and moreparticularly for the selective hydrogenation of polyunsaturated compounds or thehydrogenation of aromatics.Prior artMonounsaturated organic compounds, such as, for example, ethylene and propylene, are atthe root of the manufacture of polymers, of plastics and of other chemicals having added value.These compounds are obtained from natural gas, from naphtha or from gas oil which havebeen treated by steam cracking or catalytic cracking processes. These processes are carriedout at high temperature and produce, in addition to the desired monounsaturated compounds,polyunsaturated organic compounds, such as acetylene, propadiene and methylacetylene (orpropyne), 1,2-butadiene and 1,3-butadiene, vinylacetylene and ethylacetylene, and otherpolyunsaturated compounds, the boiling point of which corresponds to the C5+ gasolinefraction (gasolines containing hydrocarbon compounds having 5 or more carbon atoms), inparticular styrene or indene compounds. These polyunsaturated compounds are highlyreactive and result in side reactions in the polymerization units. It is thus necessary to removethem before making economic use of these fractions. Selective hydrogenation is the maintreatment developed to specifically remove undesirable polyunsaturated compounds fromthese hydrocarbon feedstocks. It enables the conversion of polyunsaturated compounds to thecorresponding alkenes or aromatics while avoiding the complete saturation thereof and thusthe formation of the corresponding alkanes or naphthenes.Selective hydrogenation catalysts are generally based on metals from Group VIII of thePeriodic Table, preferably palladium or nickel. The metal is provided in the form of metalparticles deposited on a support. The metal content, the size of the metal particles and thedistribution of the active phase in the support are among the criteria which have an influenceon the activity and the selectivity of the catalysts.The macroscopic distribution of the metal particles in the support constitutes an importantcriterion, mainly in the context of rapid and consecutive reactions such as selectivehydrogenations. It is generally desirable for these elements to be located in a crust at theperiphery of the support in order to avoid problems of intragranular material transfer which mayresult in activity defects and a loss of selectivity. Such catalysts are also referred to as"eggshell" catalysts.Such catalysts are widely known in the case of selective hydrogenation catalysts based onpalladium. Indeed, owing to the low palladium content (generally less than 1% by weight (1wt%) of palladium relative to the catalyst) and suitable preparation processes, a thin crust ofpalladium at the periphery of the support grains can be obtained (FR2922784,US2010 / 217052).It is often proposed to replace palladium with nickel, a metal which is less active than palladium,and which it is therefore necessary to have in a larger amount in the catalyst. Thus, nickelbasedcatalysts generally have a metal content of between 5% and 50% by weight of nickelrelative to the catalyst. In these catalysts, the nickel is generally distributed homogeneouslywithin the support. One possible way of improving these catalysts in terms of activity andselectivity is to control the distribution of nickel within the support by depositing the nickel in amore concentrated manner on a crust, at the periphery of the support. Such catalysts areknown from the prior art.Document US 4 519 951 describes an "eggshell" catalyst with nickel on a porous supporthaving a pore volume of at least 0.2 ml / g for the pores having a size of less than 11.7 nm anda pore volume of at least 0.1 ml / g for the pores having a size of greater than 11.7 nm. Morethan 50% by weight of the nickel is found in a crust, the thickness of which is equal to 0.15times the radius of the support. This catalyst is used for the hydrogenation of fats.Document CN101890351 describes a supported nickel catalyst in which more than 90% byweight of the nickel is found in a 700 μm-thick crust. The catalyst is prepared using anammoniacal solution to dissolve the nickel salt. These catalysts are used in a selectivehydrogenation application.Document US 2012 / 0065442 describes a supported nickel catalyst with the nickel distributedboth on a crust with a thickness of 3% to 15% of the diameter and at the core, the nickelconcentration ratio between the crust and the core being between 3.0: 1 and 1.3: 1. The nickelactive phase is deposited by spray coating of an ammoniacal solution of a nickel salt on thesupport.French patent application filed under no. 19 / 08.719 by the applicant describes a process forpreparing a nickel-based catalyst on an alumina support obtained according to a very specificmethod, the nickel being distributed both on a crust at the periphery of the support, and at thecore of the support, the thickness of said crust being between 2% and 15% of the diameter ofthe catalyst. The process for preparing such a catalyst requires firstly the use of a specificalumina support that has undergone a hydrothermal treatment in the presence of an acidsolution, and secondly the implementation of a step of hydrothermal treatment after adding aspecific organic additive to the catalyst precursor.Subjects of the inventionThe present invention thus relates to a new process for preparing a catalyst which makes itpossible to obtain a catalyst comprising performance qualities at least as good, or even better,in terms of activity and selectivity within the context of the selective hydrogenation reactions ofpolyunsaturated compounds or hydrogenation reactions of aromatics, while using a lowereffective amount of nickel phase (i.e. an amount of nickel located ultimately in the crust at theperiphery of the support allowing the selective hydrogenation reactions or hydrogenationreactions of aromatics to be carried out) than the amount typically used in the prior art, owingin particular to a better distribution of the active nickel phase in the support, making the lattermore accessible to the reagents.One subject of the present invention is a process for preparing a catalyst comprising an activephase based on nickel and an alumina support, said catalyst comprising between 1% and 50%by weight of elemental nickel relative to the total weight of the catalyst, the nickel beingdistributed both over a crust at the periphery of the support, and at the core of the support, thethickness of said crust being between 2% and 15% of the diameter of the catalyst, the size ofthe nickel particles in the catalyst, measured in oxide form, being between 7 nm and 25 nm,which process comprises the following steps:a) said support is impregnated with a volume V1 of a butanol solution of between 0.2 and 0.8times the total pore volume TPV of said support in order to obtain an impregnated support;b) the impregnated support obtained at the end of step a) is left to mature for 0.5 hour to 40hours;c) the matured impregnated support obtained at the end of step b) is impregnated with asolution comprising at least one precursor of the nickel active phase in order to obtain acatalyst precursor;d) the catalyst precursor obtained at the end of step c) is dried at a temperature below 250°C.Preferably, in step c), the volume V2 of the solution comprising at least one precursor of thenickel active phase impregnated on the matured impregnated support obtained at the end ofstep b) is such that V2 = TPV - V1.Surprisingly, the applicant has discovered that carrying out a particular step of impregnating abutanol solution on a porous alumina support, regardless of its origin, followed by a maturationstep before the step of adding the precursor of the active nickel phase to said maturedimpregnated support, and this without carrying out an intermediate drying step between theimpregnation of the butanol and the impregnation of the precursor of the active nickel phase,makes it possible to obtain a catalyst in which at least one portion of the nickel is distributedover a crust at the periphery of the support, the other portion of the nickel being distributed inthe core of the catalyst. Without wishing to be bound by any theory, the presence of butanollimits the migration of the active nickel phase to the core of the support. This is because onlya portion of the porosity is occupied by the butanol. The maturation step allows the butanolsolution to migrate to the core of the support and to liberate a "ring of free pores" at theperiphery of the support accessible by the nickel during the step of impregnation of theprecursor of the active phase. In addition, since the butanol and water are poorly miscible, thebutanol layer constitutes a barrier that limits the diffusion of nickel to the core of the support.Preferably, step b) is carried out at a temperature below or equal to 60°C.Preferably, in step a), a solution of n-butanol is used.Preferably, step d) is carried out for a time of between 0.5 hour and 12 hours.Preferably, the process further comprises a step e) in which the catalyst obtained at the endof step d) is calcined at a temperature of between 250°C and 600°C.Preferably, step e) is carried out for 0.5 hour to 24 hours.Preferably, in step a), said volume V1 of said butanol solution is between 0.25 and 0.75 timesthe total pore volume TPV of said support.Preferably, the precursor of the nickel active phase is nickel nitrate, nickel chloride, nickelacetate or nickel hydroxycarbonate.Preferably, the catalyst comprises a specific surface area of between 10 m2 / g and 350 m2 / g.Another subject according to the invention relates to a catalyst that can be obtained via thepreparation process according to the invention.Another subject according to the invention relates to a process for the selective hydrogenationof polyunsaturated compounds containing at least 2 carbon atoms per molecule, contained ina hydrocarbon feedstock having a final boiling point below or equal to 300°C, which processis carried out at a temperature of between 0°C and 300°C, at a pressure of between 0.1 MPaand 10 MPa, at a hydrogen / (polyunsaturated compounds to be hydrogenated) mole ratio ofbetween 0.1 and 10 and at an hourly space velocity of between 0.1 h-1 and 200 h-1 when theprocess is carried out in the liquid phase, or at a hydrogen / (polyunsaturated compounds to behydrogenated) mole ratio of between 0.5 and 1000 and at an hourly space velocity of between100 h-1 and 40 000 h-1 when the process is carried out in the gas phase, in the presence of acatalyst according to the invention or obtained according to the preparation process accordingto the invention.Another subject according to the invention relates to a process for the hydrogenation of at leastone aromatic or polyaromatic compound contained in a hydrocarbon feedstock having a finalboiling point below or equal to 650°C, said process being carried out in the gas phase or in theliquid phase, at a temperature of between 30°C and 350°C, at a pressure of between 0.1 and20 MPa, at a hydrogen / (aromatic compounds to be hydrogenated) mole ratio of between 0.1and 10 and at an hourly space velocity of between 0.05 h-1 and 50 h-1, in the presence of acatalyst according to the invention or obtained according to the preparation process accordingto the invention.Description of the figureFigure 1 is a diagram showing the distribution of nickel in the catalyst. The x-axis correspondsto the thickness of the catalyst, measured from the edge of the catalyst (in μm). The y-axiscorresponds to the nickel density (in grams of Ni / mm3). The nickel is distributed both on a crustat the periphery of the support, of thickness ep1, and in the core of the support. The nickeldensity on the crust dcrust is greater than the nickel density in the core of the support dcore. Thetransition interval between the core and the crust of the catalyst has a thickness denoted ep2-ep1.Detailed description of the invention1. DefinitionsIn the text hereinbelow, the groups of chemical elements are given according to the CASclassification (CRC Handbook of Chemistry and Physics, published by CRC Press, editor-inchiefD.R. Lide, 81st edition, 2000-2001). For example, group VIII according to the CASclassification corresponds to the metals of columns 8, 9 and 10 according to the new IUPACclassification.In the present description, according to the IUPAC convention, "micropores" are understoodto mean the pores having a diameter of less than 2 nm, i.e. 0.002 μm; "mesopores" areunderstood to mean the pores having a diameter of greater than 2 nm, i.e. 0.002 μm, and lessthan 50 nm, i.e. 0.05 μm, and "macropores" are understood to mean the pores having adiameter of greater than 50 nm, i.e. 0.05 μm.In order to analyze the distribution of the metallic phase on the support, a crust thickness ismeasured by Castaing microprobe (or electron microprobe microanalysis). The device used isa CAMECA XS100, equipped with four monochromator crystals allowing the simultaneousanalysis of four elements. The Castaing microprobe analysis technique consists of thedetection of X-rays emitted by a solid after excitation of its elements by a high-energy electronbeam. For the purposes of this characterization, the catalyst grains are coated in blocks ofepoxy resin. These blocks are polished until the cross section through the diameter of thebeads or extrudates is reached, and then metallized by depositing carbon in a metalevaporator. The electron probe is scanned along the diameter of five beads or extrudates toobtain the mean distribution profile of the constituent elements of the solids. This method, wellknown to those skilled in the art, is defined in the publication by L. Sorbier et al. "Measurementof palladium crust thickness on catalyst by EPMA" Materials Science and Engineering 32(2012). It makes it possible to establish the distribution profile of a given element, here nickel,within the grain. Furthermore, the Ni concentration is defined for each measurement andtherefore for each analysis step. The density of Ni within the grain is therefore defined as theconcentration of Ni per mm3.The total pore volume is measured by mercury porosimetry according to the standard ASTMD4284-92 with a wetting angle of 140°, for example using an Autopore III model device fromthe brand Micromeritics.The BET specific surface area is measured by nitrogen physisorption according to the standardASTM D3663-03, a method described in the work by Rouquerol F., Rouquerol J. and SinghK., "Adsorption by Powders & Porous Solids: Principles, Methodology and Applications",Academic Press, 1999).The median mesopore diameter is also defined as being the diameter such that all the pores,among the combined pores constituting the mesopore volume, with a size of less than thisdiameter constitute 50% of the total mesopore volume determined by mercury porosimetryintrusion.The term "size of the nickel particles" is understood to mean the diameter of the nickelcrystallites in oxide form. The diameter of the nickel crystallites in oxide form is determined byX-ray diffraction, from the width of the diffraction line located at the angle 2θ = 43° (that is tosay, along the crystallographic direction
[200] ) using the Scherrer relationship. This method,used in X-ray diffraction on polycrystalline samples or powders, which links the full width athalf maximum of the diffraction peaks to the size of the particles, is described in detail in thereference: Appl. Cryst. (1978), 11, 102-113, "Scherrer after sixty years: A survey and somenew results in the determination of crystallite size", J. I. Langford and A. J. C. Wilson.The content of nickel is measured by X-ray fluorescence.2. Process for preparing the catalystOne subject of the present invention is a process for preparing a catalyst comprising an activephase based on nickel and an alumina support, said catalyst comprising between 1% and 50%by weight of elemental nickel relative to the total weight of the catalyst, the nickel beingdistributed both over a crust at the periphery of the support, and at the core of the support, thethickness of said crust being between 2% and 15% of the diameter of the catalyst, the size ofthe nickel particles in the catalyst, measured in oxide form, being between 7 nm and 25 nm,which process comprises the following steps:a) said support is impregnated with a volume V1 of a butanol solution of between 0.2 and 0.8times the total pore volume TPV of said support in order to obtain an impregnated support;b) the impregnated support obtained at the end of step a) is left to mature for 0.5 to 40 hours;c) the matured impregnated support obtained at the end of step b) is impregnated with asolution comprising at least one precursor of the nickel active phase in order to obtain acatalyst precursor;d) the catalyst precursor obtained at the end of step c) is dried at a temperature below 250°C.The order of steps a) to d) is not interchangeable. However, it is possible to add additionalsteps before using the catalyst at the end of step d).The steps of said preparation process are described in detail below.Step a)According to step a) of the process, the alumina support is impregnated with a volume V1 of abutanol solution of between 0.2 and 0.8 times the total pore volume (also referred to here asTPV) of said support to be impregnated , preferably between 0.25 and 0.75.Butanol is understood to mean the organic compounds comprising an alcohol functioncorresponding to the empirical chemical formula C4H10O. Butanol is thus understood to meanthe family of the following organic compounds: butan-1-ol (or n-butanol), butan-2-ol,isobutanol, and tert-butanol. Preferably, step a) is carried out in the presence of butan-1-ol.Step b)After step a), the impregnated support is matured in the wet state for 0.5 hour to 40 hours,preferably for 1 hour to 30 hours. The maturation step b) is preferably carried out at atemperature below or equal to 60°C, and more preferentially at ambient temperature. This stepenables the migration of the butanol solution to the core of the support.Step c)During step c) of the process, the matured impregnated porous alumina support obtained atthe end of step b) is impregnated with a solution comprising at least one precursor of the nickelactive phase in order to obtain a catalyst precursor. The impregnation step is carried outaccording to methods that are well known to those skilled in the art.Preferably, the volume V2 of the solution comprising at least one precursor of the nickel activephase impregnated on the matured impregnated support obtained at the end of step b) is suchthat V2 = TPV - V1.The pH of said solution comprising at least one precursor of the impregnated nickel activephase can be modified by the optional addition of an acid or a base.Preferably, said nickel precursor is introduced in aqueous solution, for example in nitrate,carbonate, acetate, chloride or oxalate form, in the form of complexes formed by a polyacid oran acid alcohol and its salts, in the form of complexes formed with acetylacetonates or in theform of any other inorganic derivative soluble in aqueous solution, which is brought into contactwith said support. Preferably, use is advantageously made, as nickel precursor, of nickelnitrate, nickel chloride, nickel acetate or nickel hydroxycarbonate. Very preferably, the nickelprecursor is nickel nitrate.The concentration of nickel in solution is adjusted depending on the pore volume of the supportstill available so as to obtain, for the supported catalyst, a nickel content of between 1% and50% by weight of nickel element relative to the total weight of the catalyst, more preferentiallybetween 2% and 40% by weight and even more preferentially between 3% and 35% by weightand even more preferentially 5% and 25% by weight.Step d)The drying step d) is advantageously carried out at a temperature below 250°C, preferablybetween 15°C and 180°C, more preferentially between 30°C and 160°C, even morepreferentially between 50°C and 150°C, and even more preferentially between 70°C and140°C, for a period of typically between 0.5 hour and 12 hours, and even more preferably fora period of 0.5 hour to 5 hours. Longer periods of time are not ruled out but do not necessarilyprovide any improvement.The drying step can be carried out by any technique known to those skilled in the art. It isadvantageously carried out under an inert atmosphere or under an oxygen-containingatmosphere or under a mixture of inert gas and oxygen. It is advantageously performed atatmospheric pressure or at reduced pressure. Preferably, this step is carried out atatmospheric pressure and in the presence of air or nitrogen.At the end of step d), the total or partial presence, or the absence, of the butanol solution inthe catalyst has no effect on the activity and / or the selectivity of the catalyst in the context ofthe selective hydrogenation of polyunsaturated compounds or the hydrogenation of aromaticcompounds.Step e) (optional)The calcining step e) can be carried out at a temperature of between 250°C and 600°C,preferably between 350°C and 550°C, for a period typically of between 0.5 hour and 24 hours,preferably for a period of 0.5 hour to 12 hours, and even more preferably for a period of 0.5hour to 10 hours, preferably under an inert atmosphere or under an oxygen-containingatmosphere. Longer periods of time are not ruled out but do not necessarily provide anyimprovement.At the end of step e), the total or partial presence, or the absence, of the butanol solution inthe catalyst has no effect on the activity and / or the selectivity of the catalyst in the context ofthe selective hydrogenation of polyunsaturated compounds or the hydrogenation of aromaticcompounds.Step f) (optional)Prior to the use of the catalyst in the catalytic reactor and the implementation of ahydrogenation process, advantageously at least one reducing treatment step f) is carried outin the presence of a reducing gas after steps d) or e) so as to obtain a catalyst comprisingnickel at least partially in the metallic form.This treatment makes it possible to activate said catalyst and to form metal particles, inparticular of nickel in the zero-valent state. Said reducing treatment may be carried out in situor ex situ, that is to say after or before the charging of the catalyst to the hydrogenation reactor.The reducing gas is preferably hydrogen. The hydrogen may be used pure or as a mixture (forexample a hydrogen / nitrogen, or hydrogen / argon or hydrogen / methane mixture). In the casewhere the hydrogen is used as a mixture, any proportion may be envisaged.Said reducing treatment is carried out at a temperature of between 120°C and 500°C,preferably between 150°C and 450°C. When the catalyst does not undergo any passivation,or undergoes reducing treatment prior to passivation, the reducing treatment is carried out ata temperature of between 180°C and 500°C, preferably between 200°C and 450°C, and evenmore preferentially between 350°C and 450°C. When the catalyst has previously undergonepassivation, the reducing treatment is generally carried out at a temperature of between 120°Cand 350°C, preferably between 150°C and 350°C.The duration of the reducing treatment is generally between 2 hours and 40 hours, preferablybetween 3 hours and 30 hours. The rise in temperature up to the desired reduction temperatureis generally slow, for example set between 0.1°C / min and 10°C / min, preferably between0.3°C / min and 7°C / min.The hydrogen flow rate, expressed in l / hour / gram of catalyst, is between 0.01 and 100l / hour / gram of catalyst, preferably between 0.05 and 10 l / hour / gram of catalyst and morepreferably still between 0.1 and 5 l / hour / gram of catalyst.3. CatalystThe preparation process according to the invention makes it possible to obtain a catalystcomprising an active phase based on nickel and an alumina support, said catalyst comprisingbetween 1% and 50% by weight of elemental nickel relative to the total weight of the catalyst,the nickel being distributed both over a crust at the periphery of the support, and at the core ofthe support, the thickness of said crust (also called ep1) being between 2% and 15% of thediameter of the catalyst, and the size of the nickel particles, measured in oxide form, in thecatalyst is between 7 nm and 25 nm.Preferably, the nickel is distributed both on a crust at the periphery of the support, and in thecore of the support, the thickness of said crust ep1 being between 2% and 15% of the diameterof the catalyst, preferably between 2.5% and 12% of the diameter of the catalyst, even morepreferably between 3% and 10% of the diameter of the catalyst and even more preferablybetween 3% and 7.5% of the diameter of the catalyst.Preferably, the nickel density ratio between the crust and the core (also referred to here asdcrust / dcore) is strictly greater than 3, preferably greater than 3.5 and preferably between 3.8and 15.Preferably, said crust comprises more than 25% by weight of nickel element relative to thetotal weight of nickel element contained in the catalyst, preferably more than 40% by weight,more preferentially between 45% and 90% by weight, and even more preferentially between60% and 90% by weight.Advantageously, the transition interval between the core and the crust of the catalyst (alsoreferred to here as the core / crust transition interval, or ep2-ep1 according to the notations infigure 1), linked to the variation in the nickel density measured over the thickness of the catalystfrom the edge of the catalyst to the center of the catalyst, is very abrupt. Preferably, thecore / crust transition interval is between 0.05% and 3% of the diameter of the catalyst,preferably between 0.5% and 2.5% of the diameter of the catalyst.The nickel content in said catalyst is advantageously between 1% and 50% by weight relativeto the total weight of the catalyst, more preferentially between 2% and 40% by weight and evenmore preferentially between 3% and 35% by weight and even more preferentially 5% and 25%by weight relative to the total weight of the catalyst. The values "% by weight" are based onthe elemental form of the nickel.The catalyst can be described as a "semi eggshell" catalyst in which the concentration of nickelis higher at the periphery of the support than in the core of the support, said concentration ofnickel in the core of the support being non-zero.The specific surface area of the catalyst is generally between 10 m2 / g and 350 m2 / g, preferablybetween 25 m2 / g and 300 m2 / g, more preferably between 40 m2 / g and 250 m2 / g.The total pore volume of the catalyst is generally between 0.1 ml / g and 1 ml / g, preferablybetween 0.2 ml / g and 0.8 ml / g, and particularly preferably between 0.3 ml / g and 0.7 ml / g.The size of the nickel particles, measured in oxide form, in the catalyst is between 7 nm and25 nm, preferably between 8 nm and 23 nm.Preferably, the active p hase of the catalyst does not comprise a metal from group VIB. Inparticular, it does not comprise molybdenum or tungsten.Said catalyst (and the support used for the preparation of the catalyst) is in the form of grainsadvantageously having a diameter of between 0.5 mm and 10 mm. The grains may have anyform known to those skilled in the art, for example the form of beads (preferably having adiameter of between 1 mm and 8 mm), of extrudates, of tablets or of hollow cylinders.Preferably, the catalyst (and the support used for the preparation of the catalyst) are in theform of extrudates with a diameter of between 0.5 mm and 10 mm, preferably between 0.8 mmand 3.2 mm and very preferably between 1.0 mm and 2.5 mm and with a length of between0.5 and 20 mm. The "diameter" of the extrudates is intended to mean the diameter of the circlecircumscribed in the cross section of these extrudates. The catalyst can advantageously bepresented in the form of cylindrical, multilobate, trilobate or quadrilobate extrudates. Preferablyits shape is trilobate or quadrilobate. The shape of the lobes can be adjusted according to allthe known methods of the prior art.4. SupportThe characteristics of the alumina, mentioned in this section, correspond to the characteristicsof the alumina before carrying out step a) of the preparation process according to the invention.The support is an alumina, that is to say that the support comprises at least 95%, preferablyat least 98% and particularly preferably at least 99% by weight of alumina, relative to the weightof the support. The alumina generally exhibits a crystallographic structure of the δ-, γ- or θ-alumina type, alone or as a mixture.The alumina support may comprise impurities such as oxides of metals from groups IIA, IIIB,IVB, IIB, IIIA and IVA according to the CAS classification, preferably silica, titanium dioxide,zirconium dioxide, zinc oxide, magnesium oxide and calcium oxide, or else alkali metals,preferably lithium, sodium or potassium, and / or alkaline earth metals, preferably magnesium,calcium, strontium or barium, or else sulfur.The specific surface area of the alumina is generally between 10 m2 / g and 400 m2 / g, preferablybetween 30 m2 / g and 350 m2 / g, more preferably between 50 m2 / g and 300 m2 / g.The total pore volume of the alumina is generally between 0.1 ml / g and 1.2 ml / g, preferablybetween 0.3 ml / g and 0.9 ml / g, and very preferably between 0.5 ml / g and 0.9 ml / g.5. Selective hydrogenation processAnother subject of the present invention is a process for the selective hydrogenation ofpolyunsaturated compounds containing at least 2 carbon atoms per molecule, such as diolefinsand / or acetylenics and / or alkenylaromatics, also known as styrenics, contained in ahydrocarbon feedstock having a final boiling point below or equal to 300°C, said process beingcarried out at a temperature of between 0°C and 300°C, at a pressure of between 0.1 MPaand 10 MPa, at a hydrogen / (polyunsaturated compounds to be hydrogenated) mole ratio ofbetween 0.1 and 10 and at an hourly space velocity of between 0.1 h-1 and 200 h-1 when theprocess is carried out in the liquid phase, or at a hydrogen / (polyunsaturated compounds to behydrogenated) mole ratio of between 0.5 and 1000 and at an hourly space velocity of between100 h-1and 40 000 h-1 when the process is carried out in the gas phase, in the presence of acatalyst obtained by the preparation process as described above in the description.Monounsaturated organic compounds, such as, for example, ethylene and propylene, are atthe root of the manufacture of polymers, of plastics and of other chemicals having added value.These compounds are obtained from natural gas, from naphtha or from gas oil which havebeen treated by steam cracking or catalytic cracking processes. These processes are carriedout at high temperature and produce, in addition to the desired monounsaturated compounds,polyunsaturated organic compounds, such as acetylene, propadiene and methylacetylene (orpropyne), 1,2-butadiene and 1,3-butadiene, vinylacetylene and ethylacetylene, and otherpolyunsaturated compounds, the boiling point of which corresponds to the C5+ fraction(hydrocarbon compounds having at least 5 carbon atoms), in particular diolefinic or styrene orindene compounds. These polyunsaturated compounds are highly reactive and result in sidereactions in the polymerization units. It is thus necessary to remove them before makingeconomic use of these fractions.Selective hydrogenation is the main treatment developed to specifically remove undesirablepolyunsaturated compounds from these hydrocarbon feedstocks. It enables the conversion ofpolyunsaturated compounds to the corresponding alkenes or aromatics while avoiding thecomplete saturation thereof and thus the formation of the corresponding alkanes ornaphthenes. In the case of steam cracking gasolines used as feedstock, the selectivehydrogenation also makes it possible to selectively hydrogenate the alkenylaromatics to givearomatics while avoiding the hydrogenation of the aromatic rings.The hydrocarbon feedstock treated in the selective hydrogenation process has a final boilingpoint of below or equal to 300°C and contains at least 2 carbon atoms per molecule andcomprises at least one polyunsaturated compound. The term "polyunsaturated compounds" isintended to mean compounds comprising at least one acetylenic function and / or at least onediene function and / or at least one alkenylaromatic function.More particularly, the feedstock is chosen from the group consisting of a steam cracking C2fraction, a steam cracking C2-C3 fraction, a steam cracking C3 fraction, a steam cracking C4fraction, a steam cracking C5 fraction and a steam cracking gasoline, also known as pyrolysisgasoline or C5+ fraction.The steam cracking C2 fraction, advantageously used for the implementation of the selectivehydrogenation process according to the invention, exhibits, for example, the followingcomposition: between 40% and 95% by weight of ethylene and of the order of 0.1% to 5% byweight of acetylene, the remainder being essentially ethane and methane. In some steamcracking C2 fractions, between 0.1% and 1% by weight of C3 compounds may also be present.The steam cracking C3 fraction, advantageously used for the implementation of the selectivehydrogenation process according to the invention, exhibits, for example, the following meancomposition: of the order of 90% by weight of propylene and of the order of 1% to 8% by weightof propadiene and of methylacetylene, the remainder being essentially propane. In some C3fractions, between 0.1% and 2% by weight of C2 compounds and of C4 compounds may alsobe present.A C2-C3 fraction can also advantageously be used for the implementation of the selectivehydrogenation process according to the invention. It exhibits, for example, the followingcomposition: of the order of 0.1% to 5% by weight of acetylene, of the order of 0.1% to 3% byweight of propadiene and of methylacetylene, of the order of 30% by weight of ethylene andof the order of 5% by weight of propylene, the remainder being essentially methane, ethaneand propane. This feedstock may also contain between 0.1% and 2% by weight of C4compounds.The steam cracking C4 fraction, advantageously used for the implementation of the selectivehydrogenation process according to the invention, exhibits, for example, the following meancomposition by weight: 1% by weight of butane, 46.5% by weight of butene, 51% by weight ofbutadiene, 1.3% by weight of vinylacetylene and 0.2% by weight of butyne. In some C4fractions, between 0.1% and 2% by weight of C3 compounds and of C5 compounds may alsobe present.The steam cracking C5 fraction, advantageously used for the implementation of the selectivehydrogenation process according to the invention, exhibits, for example, the followingcomposition: 21% by weight of pentanes, 45% by weight of pentenes and 34% by weight ofpentadienes.The s team cracking gasoline or pyrolysis gasoline, advantageously used for theimplementation of the selective hydrogenation process according to the invention, correspondsto a hydrocarbon fraction, the boiling point of which is generally between 0°C and 300°C,preferably between 10°C and 250°C. The polyunsaturated hydrocarbons to be hydrogenatedpresent in said steam cracking gasoline are in particular diolefin compounds (butadiene,isoprene, cyclopentadiene, and the like), styrene compounds (styrene, α-methylstyrene, andthe like) and indene compounds (indene, and the like). The steam cracking gasoline generallycomprises the C5-C12 fraction with traces of C3, C4, C13, C14 and C15 (for example between0.1% and 3% by weight for each of these fractions). For example, a feedstock formed ofpyrolysis gasoline generally has a composition as follows: 5% to 30% by weight of saturatedcompounds (paraffins and naphthenes), 40% to 80% by weight of aromatic compounds, 5%to 20% by weight of mono-olefins, 5% to 40% by weight of diolefins and 1% to 20% by weightof alkenylaromatic compounds, the combined compounds forming 100%. It also contains from0 to 1000 ppm by weight of sulfur, preferably from 0 to 500 ppm by weight of sulfur.Preferably, the polyunsaturated hydrocarbon feedstock treated in accordance with theselective hydrogenation process according to the invention is a steam cracking C2 fraction ora steam cracking C2-C3 fraction or a steam cracking gasoline.The selective hydrogenation process according to the invention is targeted at removing saidpolyunsaturated hydrocarbons present in said feedstock to be hydrogenated withouthydrogenating the monounsaturated hydrocarbons. For example, when said feedstock is a C2fraction, the selective hydrogenation process is targeted at selectively hydrogenatingacetylene. When said feedstock is a C3 fraction, the selective hydrogenation process istargeted at selectively hydrogenating propadiene and methylacetylene. In the case of a C4fraction, the aim is to remove butadiene, vinylacetylene (VAC) and butyne; in the case of a C5fraction, the aim is to remove the pentadienes. When said feedstock is a steam crackinggasoline, the selective hydrogenation process is targeted at selectively hydrogenating saidpolyunsaturated hydrocarbons present in said feedstock to be treated so that the diolefincompounds are partially hydrogenated to give mono-olefins and so that the styrene and indenecompounds are partially hydrogenated to give corresponding aromatic compounds whileavoiding the hydrogenation of the aromatic rings.The technological implementation of the selective hydrogenation process is, for example,carried out by injection, as upflow or downflow, of the polyunsaturated hydrocarbon feedstockand of the hydrogen into at least one fixed bed reactor. Said reactor can be of isothermal typeor of adiabatic type. An adiabatic reactor is preferred. The polyunsaturated hydrocarbonfeedstock can advantageously be diluted by one or more reinjection(s) of the effluent, resultingfrom said reactor where the selective hydrogenation reaction takes place, at various points ofthe reactor, located between the inlet and the outlet of the reactor, in order to limit thetemperature gradient in the reactor. The technological implementation of the selectivehydrogenation process according to the invention can also advantageously be carried out bythe implantation of at least said supported catalyst in a reactive distillation column or inreactors-exchangers or in a slurry-type reactor. The stream of hydrogen can be introduced atthe same time as the feedstock to be hydrogenated and / or at one or more different points ofthe reactor.The selective hydrogenation of the steam cracking C2, C2-C3, C3, C4, C5 and C5+ fractionscan be carried out in the gas phase or in the liquid phase, preferably in the liquid phase for theC3, C4, C5 and C5+ fractions and in the gas phase for the C2 and C2-C3 fractions. A liquidphasereaction makes it possible to lower the energy cost and to increase the cycle period ofthe catalyst.In general, the selective hydrogenation of a hydrocarbon feedstock containing polyunsaturatedcompounds containing at least 2 carbon atoms per molecule and having a final boiling pointbelow or equal to 300°C is carried out at a temperature of between 0°C and 300°C, at apressure of between 0.1 MPa and 10 MPa, at a hydrogen / (polyunsaturated compounds to behydrogenated) mole ratio of between 0.1 and 10 and at an hourly space velocity (defined asthe ratio of the volume flow rate of feedstock to the volume of catalyst) of between 0.1 h-1 and200 h-1 for a process carried out in the liquid phase, or at a hydrogen / (polyunsaturatedcompounds to be hydrogenated) mole ratio of between 0.5 and 1000 and at an hourly spacevelocity of between 100 h-1 and 40 000 h-1 for a process carried out in the gas phase.In one embodiment according to the invention, when a selective hydrogenation process iscarried out wherein the feedstock is a steam cracking gasoline comprising polyunsaturatedcompounds, the (hydrogen) / (polyunsaturated compounds to be hydrogenated) mole ratio isgenerally between 0.5 and 10, preferably between 0.7 and 5.0 and more preferably stillbetween 1.0 and 2.0, the temperature is between 0°C and 200°C, preferably between 20°Cand 200°C and more preferably still between 30°C and 180°C, the hourly space velocity (HSV)is generally between 0.5 h-1 and 100 h-1, preferably between 1 h-1 and 50 h-1, and the pressureis generally between 0.3 and 8.0 MPa, preferably between 1.0 MPa and 7.0 MPa and morepreferably still between 1.5 MPa and 4.0 MPa.More preferentially, a selective hydrogenation process is carried out wherein the feedstock isa steam cracking gasoline comprising polyunsaturated compounds, thehydrogen / (poly unsaturated compounds to be hydrogenated) mole ratio is between 0.7 and 5.0,the temperature is between 20°C and 200°C, the hourly space velocity (HSV) is generallybetween 1 h-1 and 50 h-1 and the pressure is between 1.0 MPa and 7.0 MPa.More preferentially still, a selective hydrogenation process is carried out wherein the feedstockis a steam cracking gasoline comprising polyunsaturated compounds, thehydrogen / (polyunsaturated compounds to be hydrogenated) mole ratio is between 1.0 and 2.0,the temperature is between 30°C and 180°C, the hourly space velocity (HSV) is generallybetween 1 h-1 and 50 h-1 and the pressure is between 1.5 MPa and 4.0 MPa.The hydrogen flow rate is adjusted in order to have available a sufficient amount thereof totheoretically hydrogenate all of the polyunsaturated compounds and to maintain an excess ofhydrogen at the reactor outlet.In another embodiment according to the invention, when a selective hydrogenation process iscarried out wherein the feedstock is a steam cracking C2 fraction and / or a steam cracking C2-C3 fraction comprising polyunsaturated compounds, the (hydrogen) / (polyunsaturatedcompounds to be hydrogenated) mole ratio is generally between 0.5 and 1000, preferablybetween 0.7 and 800, the temperature is between 0°C and 300°C, preferably between 15°Cand 280°C, the hourly space velocity (HSV) is generally between 100 h-1 and 40 000 h-1,preferably between 500 h-1 and 30 000 h-1, and the pressure is generally between 0.1 MPaand 6.0 MPa, preferably between 0.2 MPa and 5.0 MPa.6. Process for the hydrogenation of aromaticsAnother subject of the present invention is a process for the hydrogenation of at least onearomatic or polyaromatic compound contained in a hydrocarbon feedstock having a finalboiling point below or equal to 650°C, generally between 20°C and 650°C, and preferablybetween 20°C and 450°C. Said hydrocarbon feedstock containing at least one aromatic orpolyaromatic compound can be chosen from the following petroleum or petrochemicalfractions: the reformate from catalytic reforming, kerosene, light gas oil, heavy gas oil, crackingdistillates, such as FCC recycle oil, coking unit gas oil or hydrocracking distillates.The content of aromatic or polyaromatic compounds contained in the hydrocarbon feedstocktreated in the hydrogenation process according to the invention is generally between 0.1% and80% by weight, preferably between 1% and 50% by weight and particularly preferably between2% and 35% by weight, the percentage being based on the total weight of the hydrocarbonfeedstock. The aromatic compounds present in said hydrocarbon feedstock are, for example,benzene or alkylaromatics, such as toluene, ethylbenzene, o-xylene, m-xylene or p-xylene, oralso aromatics having several aromatic rings (polyaromatics), such as naphthalene.The sulfur or chlorine content of the feedstock is generally less than 5000 ppm by weight ofsulfur or chlorine, preferably less than 100 ppm by weight and particularly preferably less than10 ppm by weight.The technological implementation of the process for the hydrogenation of aromatic orpolyaromatic compounds is, for example, carried out by injection, as upflow or downflow, ofthe hydrocarbon feedstock and of the hydrogen into at least one fixed bed reactor. Said reactorcan be of isothermal type or of adiabatic type. An adiabatic reactor is preferred. Thehydrocarbon feedstock can advantageously be diluted by one or more reinjection(s) of theeffluent, resulting from said reactor where the reaction for the hydrogenation of the aromaticstakes place, at various points of the reactor, located between the inlet and the outlet of thereactor, in order to limit the temperature gradient in the reactor. The technologicalimplementation of the process for the hydrogenation of the aromatics according to theinvention may also advantageously be carried out by the implantation of at least said supportedcatalyst in a reactive distillation column or in reactors-exchangers or in a slurry-type reactor.The stream of hydrogen can be introduced at the same time as the feedstock to behydrogenated and / or at one or more different points of the reactor.The hydrogenation of the aromatic or polyaromatic compounds can be carried out in the gasphase or in the liquid phase, preferably in the liquid phase. Generally, the hydrogenation of thearomatic or polyaromatic compounds is carried out at a temperature of between 30°C and350°C, preferably between 50°C and 325°C, at a pressure of between 0.1 MPa and 20 MPa,preferably between 0.5 MPa and 10 MPa, at a hydrogen / (aromatic compounds to behydrogenated) mole ratio of between 0.1 and 10 and at an hourly space velocity of between0.05 h-1 and 50 h-1, preferably between 0.1 h-1 and 10 h-1, of a hydrocarbon feedstockcontaining aromatic or polyaromatic compounds and having a final boiling point below or equalto 650°C, generally between 20°C and 650°C, and preferably between 20°C and 450°C.The hydrogen flow rate is adjusted in order to have available a sufficient amount thereof totheoretically hydrogenate all of the aromatic compounds and to maintain an excess ofhydrogen at the reactor outlet.The conversion of the aromatic or polyaromatic compounds is generally greater than 20 mol%,preferably greater than 40 mol%, more preferably greater than 80 mol% and particularlypreferably greater than 90 mol% of the aromatic or polyaromatic compounds contained in thehydrocarbon feedstock. The conversion is calculated by dividing the difference between thetotal moles of the aromatic or polyaromatic compounds in the hydrocarbon feedstock and inthe product by the total moles of the aromatic or polyaromatic compounds in the hydrocarbonfeedstock.According to a specific alternative form of the process according to the invention, a processfor the hydrogenation of the benzene of a hydrocarbon feedstock, such as the reformateresulting from a catalytic reforming unit, is carried out. The benzene content in saidhydrocarbon feedstock is generally between 0.1% and 40% by weight, preferably between0.5% and 35% by weight and particularly preferably between 2% and 30% by weight, thepercentage by weight being based on the total weight of the hydrocarbon feedstock.The sulfur or chlorine content of the feedstock is generally less than 10 ppm by weight of sulfuror chlorine respectively and preferably less than 2 ppm by weight.The hydrogenation of the benzene contained in the hydrocarbon feedstock can be carried outin the gas phase or in the liquid phase, preferably in the liquid phase. When it is carried out inthe liquid phase, a solvent can be present, such as cyclohexane, heptane or octane. Generally,the hydrogenation of the benzene is carried out at a temperature of between 30°C and 250°C,preferably between 50°C and 200°C and more preferably between 80°C and 180°C, at apressure of between 0.1 MPa and 10 MPa, preferably between 0.5 and 4 MPa, at ahydrogen / (benzene) mole ratio of between 0.1 and 10 and at an hourly space velocity ofbetween 0.05 h-1 and 50 h-1, preferably between 0.5 h-1 and 10 h-1.The conversion of the benzene is generally greater than 50 mol%, preferably greater than 80mol%, more preferably greater than 90 mol% and particularly preferably greater than 98 mol%.The invention is illustrated via the examples below which are in no way limiting.ExamplesFor all the catalysts mentioned in the examples below, the support is an alumina A having aspecific surface area of 80 m² / g, a total pore volume TPV of 0.7 ml / g and a median mesoporediameter of 12 nm.Example 1: Preparation of an aqueous solution of Ni precursorThe aqueous solution of Ni precursors (solution S) used for the preparation of catalysts A to Gis prepared by dissolving 43.5 grams (g) of nickel nitrate (NiNO3, supplier Strem Chemicals)in a volume of 13 ml of distilled water. The solution S, the Ni concentration of which is 350 gof Ni per liter of solution, is obtained.Example 2: Preparation of a catalyst A according to the invention [10 wt% of Ni - ButOH 25%TPV, in pre-impregnation]10 g of alumina A are impregnated with 2.4 ml of n-butanol added dropwise. The impregnatedsupport is then left to mature for 30 min at 60°C. Next, 7.1 ml of solution S prepared in example1 is impregnated dropwise on the impregnated support. The catalyst precursor thus obtainedis subsequently dried in an oven at 120°C for 12 hours and then calcined under a stream ofdry air of 1 l / h / g of catalyst at 450°C for 2 hours.Catalyst A containing 10% by weight of the nickel element relative to the total weight of thecatalyst is obtained.The characteristics of catalyst A thus obtained are given in table 1 below.Example 3: Preparation of a catalyst B according to the invention [5 wt% of Ni- ButOH 25%TPV in pre-impregnation]10 g of alumina A are impregnated with 2.4 ml of n-butanol added dropwise. The impregnatedsupport is then left to mature for 30 min at 60°C. Next, 3.55 ml of solution S prepared inexample 1 diluted with water in order to make it up to 7.1 ml is impregnated dropwise on theimpregnated support. The catalyst precursor thus obtained is subsequently dried in an oven at120°C for 12 hours and then calcined under a stream of dry air of 1 l / h / g of catalyst at 450°Cfor 2 hours.Catalyst B containing 5% by weight of the nickel element relative to the total weight of thecatalyst is obtained.The characteristics of catalyst B thus obtained are given in table 1 below.Example 4: Preparation of a catalyst C according to the invention [10 wt% of Ni - ButOH 75%TPV in pre-impregnation]10 g of alumina A are impregnated with 7.2 ml of n-butanol added dropwise. The impregnatedsupport is then left to mature for 30 min at 60°C. Next, 2.4 ml of solution S prepared in example1 is impregnated dropwise on the impregnated support. The catalyst precursor thus obtainedis subsequently dried in an oven for 12 hours at 120°C and then calcined under a stream ofdry air of 1 l / h / g of catalyst at 450°C for 2 hours.Catalyst C containing 10% by weight of the nickel element relative to the total weight of thecatalyst is obtained.The characteristics of catalyst C thus obtained are given in table 1 below.Example 5: Preparation of a catalyst D not in accordance with the invention [conventionalimpregnation 10% Ni]The solution S prepared in example 1 is dry impregnated, by adding it dropwise, on 10 g ofalumina. The catalyst precursor thus obtained is subsequently dried in an oven for 12 hours at120°C and then calcined under a stream of dry air of 1 l / h / g of catalyst at 450°C for 2 hours.Catalyst D containing 10% by weight of the nickel element relative to the total weight of thecatalyst is obtained.The characteristics of catalyst D thus obtained are given in table 1 below.Example 6: Preparation of a catalyst E not in accordance with the invention [10 wt% of Ni -ButOH 25% TPV in post-impregnation]7.1 ml of solution S prepared in example 1 is dry impregnated, by adding it dropwise, on 10 gof alumina. The 10 g of the catalyst precursor prepared are impregnated with 2.4 ml of nbutanoladded dropwise. The solid is then left to mature for 30 min at 60°C.The solid thus obtained is subsequently dried in an oven for 12 hours at 120°C and thencalcined under a stream of dry air of 1 l / h / g of catalyst at 450°C for 2 hours.Catalyst E containing 10% by weight of the nickel element relative to the total weight of thecatalyst is obtained.The characteristics of catalyst E thus obtained are given in table 1 below.Example 7: Preparation of a catalyst F not in accordance with the invention [10 wt% of Ni -Toluene 25% TPV in pre-impregnation]10 g of alumina A are impregnated with 2.4 ml of toluene added dropwise. The impregnatedsupport is then left to mature for 30 min at 60°C. Next, 7.1 ml of solution S prepared in example1 is impregnated dropwise on the impregnated support. The catalyst precursor thus obtainedis subsequently dried in an oven at 120°C for 12 hours and then calcined under a stream ofdry air of 1 l / h / g of catalyst at 450°C for 2 hours.Catalyst F containing 10% by weight of the nickel element relative to the total weight of thecatalyst is obtained.The characteristics of catalyst F thus obtained are given in table 1 below.Example 8: Preparation of a catalyst G not in accordance with the invention [10 wt% of Ni - npropanol25% TPV in pre-impregnation]10 g of alumina A are impregnated with 2.4 ml of n-propanol added dropwise. The impregnatedsupport is then left to mature for 30 min at 60°C. Next, 7.1 ml of solution S prepared in example1 is impregnated dropwise on the impregnated support. The catalyst precursor thus obtainedis subsequently dried in an oven at 120°C for 12 hours and then calcined under a stream ofdry air of 1 l / h / g of catalyst at 450°C for 2 hours.Catalyst G containing 10% by weight of the nickel element relative to the total weight of thecatalyst is obtained.The characteristics of catalyst G thus obtained are given in table 1 below.CatalystSolvent (% byvolume relative tothe TPV of thesupport)Ni(wt%)Particlesize (nm)Crustthickness / graindiameter(%)dcrust / dcoreNi content incrust / total Ni(%)A (inaccordance)25% BuTOH inpre-impregnation10 14.5 6.8 6 68B (inaccordance)25% BuTOH inpre-impregnation5 7 3.8 12 71C (inaccordance)75% BuTOH inpre-impregnation10 14 4.7 13 75D(not inaccordance)- 10 12 <1% 1.5 7E(not inaccordance)25% BuTOH inpostimpregnation10 12Homogeneousdistribution- -F(not inaccordance)25% toluene inpre-impregnation10 11.5Homogeneousdistribution- -G(not inaccordance)25% n-propanolin preimpregnation10 11.5Homogeneousdistribution- -Table 1: Characteristics of catalysts A to GExample 9: Catalytic tests: performance in selective hydrogenation of a mixture containingstyrene and isoprene (AHYD1)Catalysts A to G described in the examples above are tested with regard to the reaction for theselective hydrogenation of a mixture containing styrene and isoprene.The composition of the feedstock to be selectively hydrogenated is as follows: 8 wt% styrene(supplier Sigma Aldrich, purity 99%), 8 wt% isoprene (supplier Sigma Aldrich, purity 99%)and 84 wt% n-heptane (solvent) (supplier VWR, purity > 99% Chromanorm HPLC). Thisfeedstock also contains a very low content of sulfur compounds: 10 ppm by weight of sulfurintroduced in pentanethiol form (supplier Fluka, purity > 97%) and 100 ppm by weight ofsulfur introduced in thiophene form (supplier Merck, purity 99%). This compositioncorresponds to the initial composition of the reaction mixture. This mixture of model moleculesis representative of a pyrolysis gasoline.The selective hydrogenation reaction is carried out in a 500 ml stainless steel autoclave whichis provided with a magnetically-driven mechanical stirrer and which is able to operate under amaximum pressure of 100 bar (10 MPa) and temperatures of between 5°C and 200°C.Prior to its introduction into the autoclave, an amount of 3 ml of catalyst is reduced ex situunder a hydrogen stream of 1 l / h / g of catalyst, at 400°C for 16 hours (temperature rise gradientof 1°C / min), then it is transferred into the autoclave, with air excluded. After addition of 214 mlof n-heptane (supplier VWR, purity > 99% Chromanorm HPLC), the autoclave is closed,purged, then pressurized under 35 bar (3.5 MPa) of hydrogen, and brought to the testtemperature equal to 30°C. At time t = 0, approximately 30 g of a mixture containing styrene,isoprene, n-heptane, pentanethiol and thiophene are introduced into the autoclave. Thereaction mixture then has the composition described above and stirring is started at 1600 rpm.The pressure is kept constant at 35 bar (3.5 MPa) in the autoclave using a storage cylinderlocated upstream of the reactor.The progress of the reaction is monitored by taking samples from the reaction medium atregular time intervals: the styrene is hydrogenated to give ethylbenzene, without hydrogenationof the aromatic ring, and the isoprene is hydrogenated to give methylbutenes. If the reactionis prolonged for longer than necessary, the methylbutenes are in their turn hydrogenated togive isopentane. The hydrogen consumption is also monitored over time by the decrease inpressure in a storage cylinder located upstream of the reactor. The catalytic activity isexpressed in moles of H2 consumed per minute and per gram of Ni.The catalytic activities measured (AHYD1) for catalysts A to G are given in table 2 below. Theyare related to the catalytic activity measured for catalyst D.Example 10: Catalytic tests: performance in hydrogenation of toluene (AHYD2)Catalysts A to G described in the above examples are also tested with regard to the reactionfor the hydrogenation of toluene.The selective hydrogenation reaction is carried out in the same autoclave as that described inexample 9.Prior to its introduction into the autoclave, an amount of 2 ml of catalyst is reduced ex situunder a hydrogen stream of 1 l / h / g of catalyst, at 400°C for 16 hours (temperature rise gradientof 1°C / min), then it is transferred into the autoclave, with air excluded. After addition of 216 mlof n-heptane (supplier VWR, purity > 99% Chromanorm HPLC), the autoclave is closed,purged, then pressurized under 35 bar (3.5 MPa) of hydrogen and brought to the testtemperature, equal to 80°C. At time t = 0, approximately 26 g of toluene (supplier SDS, purity> 99.8%) are introduced into the autoclave (the initial composition of the reaction mixture isthen 6 wt% toluene / 94 wt% n-heptane) and stirring is started at 1600 rpm. The pressure is keptconstant at 35 bar (3.5 MPa) in the autoclave using a storage cylinder located upstream of thereactor.The progress of the reaction is monitored by taking samples from the reaction medium atregular time intervals: the toluene is completely hydrogenated to give methylcyclohexane. Thehydrogen consumption is also monitored over time by the decrease in pressure in a storagecylinder located upstream of the reactor. The catalytic activity is expressed in moles of H2consumed per minute and per gram of Ni.The catalytic activities (AHYD2) measured for catalysts A to G are given in table 2 below. Theyare related to the catalytic activity measured for catalyst D.CatalystContent of Ni0(%)AHYD1 (%) AHYD2 (%)A (in accordance) 10 180 210B (in accordance) 5 130 150C (in accordance) 10 190 230D (not in accordance) 10 100 100E (not in accordance) 10 50 50F (not in accordance) 10 70 80G (not inaccordance)10 95 98Table 2: Comparison of the performances of catalysts A to G in terms of selectivehydrogenation of a mixture containing styrene and isoprene (AHYD1) and in terms ofhydrogenation of toluene (AHYD2)This clearly shows the improved performance of catalysts A, B and C according to theinvention, compared to catalysts D, E, F and G not in accordance with the invention. This isexplained by the distribution of the nickel in the crust on catalysts A, B and C, which gives thema markedly improved activity, in particular in rapid hydrogenation reactions.Catalyst D has lower activity due to the conventional impregnation carried out without preimpregnation of butanol. Catalyst E underwent a post-impregnation with butanol which doesnot allow a crust distribution of the nickel. Catalyst F is prepared with a step of pre-impregnationof toluene. Thus, although toluene is not very miscible with water, as in the case of butanol,the absence of -OH groups in the molecule does not enable it to have a strong interaction withthe -OH groups of the alumina support, which may explain the migration of toluene via thewater contained in the nickel nitrate solution during the nickel impregnation step. In the caseof propanol, the -OH groups appear to allow it to both go to the core of the support and tointeract with the support. On the other hand, as water and n-propanol are highly miscible,unlike the butanol / water pair, diffusion of the aqueous Ni nitrate solution to the core appearsto take place considering both the physicochemical characteristics of the final catalyst obtainedand the results of catalytic tests. Thus, for catalysts E, F and G, the nickel is distributedhomogeneously throughout the catalyst grain. Catalysts E and F therefore have a much loweractivity than catalyst A in terms of AHYD1 and AHYD2. Catalyst F is low due to the presence oftoluene which disrupts the impregnation of the nickel nitrate solution.
Claims
1. A process for preparing a catalyst comprising an active phase based on nickel and alumina support, said catalyst comprising between 1% and 50% by weight of elemental nickel relative to the total weight of the catalyst, the nickel being distributed both over a crust at the periphery of the support, and at the core of the support, the thickness of said crust being between 2% and 15% of the diameter of the catalyst, the size of the nickel particles in the catalyst, measured in oxide form, being between 7 nm and 25 nm, which process comprises the following steps: a) said support is impregnated with a volume V1 of a butanol solution of between 0.2 and 0.8 times the total pore volume TPV of said support in order to obtain an impregnated support; b) the impregnated support obtained at the end of step a) is left to mature for 0.5 hour to 40 hours; c) the matured impregnated support obtained at the end of step b) is impregnated with a solution comprising at least one precursor of the nickel active phase in order to obtain a catalyst precursor; d) the catalyst precursor obtained at the end of step c) is dried at a temperature below 250°C.
2. The process as claimed in claim 1, wherein, in step c), the volume V2 of the solution comprising at least one precursor of the nickel active phase impregnated on the matured impregnated support obtained at the end of step b) is such that V2 = TPV - V1.
3. The process as claimed in either of claims 1 and 2, wherein step b) is carried out at a temperature below or equal to 60°C.
4. The process as claimed in any one of claims 1 to 3, wherein, in step a), an n-butanol solution is used.
5. The process as claimed in any one of claims 1 to 4, characterized in that step d) is carried out for a time of between 0.5 hour and 12 hours.
6. The process as claimed in any one of claims 1 to 5, characterized in that it further comprises a step e) in which the catalyst obtained at the end of step d) is calcined at a temperature of between 250°C and 600°C.
7. The process as claimed in claim 6, wherein step e) is carried out for between 0.5 hour and 24 hours.
8. The process as claimed in any one of claims 1 or 7, wherein, in step a), said volume V1 of said butanol solution is between 0.25 and 0.75 times the total pore volume TPV of said support.
9. The process as claimed in any one of claims 1 to 8, wherein the precursor of the nickel active phase is nickel nitrate, nick el chloride, nickel acetate or nickel hydroxycarbonate.
10. The process as claimed in any one of claims 1 to 9, wherein the catalyst comprises a specific surface area of between 10 m2 / g and 350 m2 / g.
11. A catalyst which can be obtained via the process as claimed in any one of claims 1 to 10.
12. A process for the selective hydrogenation of polyunsaturated compounds containing at least 2 carbon atoms per molecule, contained in a hydrocarbon feedstock having a final boiling point below or equal to 300°C, said process being carried out at a temperature of between 0°C and 300°C, at a pressure of between 0.1 and 10 MPa, at a hydrogen / (polyunsaturated compounds to be hydrogenated) mole ratio of between 0.1 and 10 and at an hourly space velocity of between 0.1 and 200 h-1 when the process is carried out in the liquid phase, or at a hydrogen / (polyunsaturated compounds to be hydrogenated) mole ratio of between 0.5 and 1000 and at an hourly space velocity of between 100 and 40 000 h-1 when the process is carried out in the gas phase, in the presence of a catalyst as claimed in claim 11 or obtained according to the preparation process as claimed in any one of claims 1 to 10.
13. A process for the hydrogenation of at least one aromatic or polyaromatic compound contained in a hydrocarbon feedstock having a final boiling point below or equal to 650°C, said process being carried out in the gas phase or in the liquid phase, at a temperature of between 30°C and 350°C, at a pressure of between 0.1 MPa and 20 MPa, at a hydrogen / (aromatic compounds to be hydrogenated) mole ratio of between 0.1 and 10 and at an hourly space velocity of between 0.05 h-1 and 50 h-1, in the presence of a catalyst as claimed in claim 11 or obtained according to the preparation process as claimed in any one of claims 1 to 10.