Zero rpm-synthesized tunable plasmonic hollow silver nanoshells in the first and second near-IR windows for enhanced solar-catalysis

IN597876BActive Publication Date: 2026-08-04CENTRAL UNIVERSITY OF BIHAR
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN201931047638
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2019-11-21
Publication Date
2026-08-04
Estimated Expiration
2039-11-21

AI Technical Summary

Technical Problem

Current methods for synthesizing hollow silver nanoshells struggle with achieving intense and tunable surface plasmon resonances in the second Near-IR window (NIR-II), lack quadrupole mode observation, require stirring, result in larger particle sizes, and are costly, while also underutilizing the NIR region for photocatalysis.

Method used

The synthesis of dimethylglyoxime (DMG)-capped hollow silver nanoshells at zero rpm stirring speed, optimizing reagent ratios and temperature, achieves narrow and tunable plasmon peaks in the NIR-II region with both quadrupole and symmetric dipole modes, and utilizes the NIR region for efficient photocatalytic dye degradation.

Benefits of technology

This approach results in high-quality, small-sized nanoshells with intense and tunable plasmon resonances in the NIR-II region, reducing energy costs, and enables efficient photocatalysis in the NIR region with subpicomolar catalyst concentrations, enhancing biomedical applications and solar photocatalytic efficiency.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

Hollow silver nanoshells (HAgNS) having surface plasmon resonances (SPR) in the first and second near-IR window (NIR-I: 650-950 nm; NIR-II:1000-1400 nm) have been synthesized for the first time. A new method based on nanoscale Kirkendall effect has been developed in which dimethylglyoxime (DMG) acts as capping agent as well as growth moderator. Folic Acid (FA) is further added to impart aqueous solubility and stabilization. It finally yields water-soluble, DMG-FA-capped HAgNS. The synthesis process was analyzed for wide range of stirring speeds from zero rpm to 1350 rpm and the synthesis at zero rpm was found to be the best as it yielded HAgNS having narrower SPR band (reduced FWHM) along with greater red-shift of the SPR peak upto 1150 nm in the NIR region. The invention establishes zero-rpm synthesis (no stirring, magnetic or otherwise) as a greener and cost-effective route to obtain ‘high quality’ HAgNS thereby bringing the energy expenditure to zero. HAgNS exhibits two prominent SPR peaks in the absorption spectra, one corresponding to the quadrupole mode (Q-SPR) and the other symmetric dipole mode (SD-SPR). By deftly controlling the aspect ratio (outer diameter / shell thickness), the dipolar resonances (SD-SPR) have been tuned in a wide NIR range spanning 780 nm to 1150 nm. For the hollow silver nanoshells, this is the maximum red-shift achieved till date in SPR peaks. The spectral range corresponding to 650-1400 nm represents the biologically transparent window which is further divided into two sub-windows: NIR-I ranging from 650-950 and NIR-II ranging from 1000-1400 nm. The latter, i.e, NIR-II window, is more suitable for theranostic applications as scattering becomes very low which means light can penetrate deeper and photothermal efficiency is enhanced. As the SD-SPR is tuned in the NIR II window, the Q-SPR of the HAgNS is concomitantly tuned from 450 to 560 nm in the visible region. Additionally, a less prominent peak is also observed at 330 nm in all these samples which are attributed to antisymmetric dipolar resonances (AD-SPR). Transmission electron microscopy (TEM) revealed that all HAgNS are single-crystal hollow spheres. HAgNSs with tunable plasmon peaks (?SD-SPR) at 780, 850, 920, 1010, and 1150 nm were synthesized (hence named as HAgNS-780, HAgNS-850, HAgNS-920, HAgNS-1010, and HAgNS-1150, respectively). The corresponding outer diameters were 53±3, 50±3, 54±3, 62±4, and 40±1 nm as determined by HR-TEM and the aspect ratios (Outer diameter / Shell thickness) were 3.31, 3.33, 3.48, 4.13, and 5.33, respectively. Besides, the HAgNSs were found to be good catalysts in sunlight, for the degradation of dyes, namely, Methyl Orange (MO) and Bromocresol Green (BCG). The solar photocatalytic efficiency of the hollow plasmonic nanoshells, HAgNS-780 and HAgNS-920 were found to be 3.6 and 3.2 times higher, respectively, as compared to solid silver nanospheres (SAgNS-400; ?SPR=400 nm). Additionally, HAgNS-920 vis-à-vis HAgNS-780 acted as a better catalyst for BCG within NIR window. Thus, the NIR window of the solar spectrum displayed greater efficiency with HAgNSs as plasmonic photocatalysts. The invention will open up new vistas in faster and effective remediation of dye-effluents emanating from the textile industry.
Need to check novelty before this filing date? Find Prior Art

Description

THE FIELD OF INVENTION The invention relates to plasmonic hollow silver nanoshells (referred to as HAgNS, for the sake of brevity), i.e, spherical silver nanocrystals with inner void space. In particular, it relates to HAgNS showing intense and tunable surface plasmon resonances (SPR) in the second Near-IR window (NIR-II), i.e, 1000-1400 nm.It also relates to novel energy-efficient and green methods to prepare such high-quality HAgNS at zero rpm, i.e, a synthesis devoid of any stirring. [Here, the properties that define the ‘high-quality’ of nanoshells are as following: (a) intense and narrow SPR bands (i.e, lower FWHM), (b) narrow size distribution, (c) versatile vis-to-NIR tunability of SPR peaks, (d) presence of quadrupole mode (Q-SPR) along with the symmetric dipole mode of SPR (SD-SPR) and (e) good crystallinity]It further relates to plasmon-enhanced photocatalytic degradation of industrial dyes in the sunlight. Thus, it provides a solar-catalytic process for the remediation of industrial dye wastes at subpicomolar concentrations of the HAgNS-catalysts. 4.2 EXISTING STATE-OF-ARTNoble metal nanostructures, particularly that of gold and silver, with hollow interiors are getting prominence in the realm of plasmonics due to their single, intense and highly tunable surface plasmon resonance (SPR) peaks ranging from visible to near-IR (NIR) spectral region.1–6 These plasmonic hollow nanoshells (HNSs) offer several advantages over solid nanospheres which have a limited plasmon tunability in the visible range only. Due to versatile near-IR plasmonic properties in the biologically transparent window (650–1400 nm), HNSs have become the most-sought-after plasmonic nanomaterials for biological applications such as imaging,12–15 and photo-thermal therapy.6,12,16,19 Halas and coworkers,3,12,18,20-22 pioneered the research field and demonstrated the synthesis of gold nanoshells (larger than 100 nm) supported on silica core. They showed that by changing the size of silica core and the thickness of the gold shell, surface plasmon resonance (SPR) could be continuously tuned from visible to NIR (650–1200 nm) region. For such silica-cored nanoshells, some cytotoxicity concerns were raised.6,23 New methodologies have been developed by the Wan24 and Zhang6,25,26 groups to produce gold nanoshells with a hollow interior that are more suitable for biological applications due to their smaller size and the absence of silica core. In this approach, cobalt nanoparticles (NPs) are first prepared, which act as sacrificial templates.24,26 Subsequent addition of gold salts results in a reduction of gold ions on the surface of cobalt nanoparticles and this galvanic replacement along with outward diffusion of cobalt ions leads to the formation of the hollow structure. Depending on the aspect ratio (outer diameter, d / wall thickness, t), the SPR peak of the hollow gold nanoshells was varied in the wide range spanning Vis-to-NIR (550–900 nm) and the nanoshells were further used for making biological sensors.26,27 By replacing magnetic stirring with mechanical / manual stirring / Argon bubbling, SPR was further red-shifted to 1320 nm in the NIR region.28 It should be noted here that the NIR spectral region is divided into two sub-windows: NIR-I spanning 650 to 950 nm, and NIR-II spanning 1000 to 1400 nm. In the NIR-II region, scattering becomes very low; consequently, sensitivity and spatial resolution are improved.33 Due to deeper tissue penetration in the NIR-II window, in-vivo detection of deep-seated tumors can be done in a non-invasive manner. In contrast to hollow gold nanoshells, there are only a few reports29,30 on the hollow silver nanoshells (HAgNS). Following the cobalt template approach, Chen et al.29 prepared hollow silver nanoshells exhibiting a broad plasmon band at 506 nm. Silver–gold bimetallic nanostructures with hollow interiors have been synthesized by Jin and Dong.31 In 2011, single-crystalline hollow silver nanoshells with plasmon band centered at 480 nm were synthesized using Ag2O NPs as a template.30 By developing a new ‘mild stabilizer, mild reductant’ approach and using the same template, Priyam and co-workers further extended the plasmon tunability in hollow silver nanoshells to 630 nm.8,32 Further, Kado et al. reported the synthesis of hollow silver nanoshells using silver thiocyanate as precursor instead of silver oxide.11 By doing so, they could achieve the plasmon tunability in HAgNS upto 800 nm in the NIR-I region. However, tuning the SPR peak of hollow silver nanocrystals in the NIR-II region is quite challenging11,32 and, to the best of our knowledge, no such report exists.Recent theoretical models have also predicted an additional quadrupole band (Q-SPR) along with symmetric and antisymmetric dipole SPR in HNSs.9-11 However, in all the previous reports on hollow nanospheres (<100 nm), it is the (Symmetric dipole SPR) SD-SPR mode which has been observed. There was one such attempt previously by Kado et al.,11 in which only one of the HAgNS samples showed a feeble Q-SPR peak in addition to a dominant SD-SPR peak. Furthermore, the size of such nanoshells were also larger than 100 nm. We also note that there is no method available till date to obtain hollow noble metal nanoshells with tunable Q-SPR peaks. Our method is the first one in which both Q-SPR as well as SD-SPR peaks have been tuned in a wide range and have comparable intensities. Besides bioimaging and photothermal therapy, photocatalysis is one of the major areas where these plasmonic nanomaterials have the potential to be utilized effectively.34,35 There are only a few reports32,40-42 found on the use of hollow plasmonic nanostructures in catalysis. So far UV-Visible region of the solar spectrum has been mostly utilized for photocatalysis by plasmonic nanomaterials.43,44 In order to make it cost-effective and applicable to industrial scale, it is imperative to harvest the sunlight in a more effective manner. As near infrared region is also a dominant part of solar spectrum (54.3%),45,46 this region also needs to be tapped for photocatalysis. However, the reports on photocatalysis by plasmonic and semiconductor nanomaterials in the NIR region is scarce.47-50 Thus, there is a need to explore the catalytic properties of NIR-plasmonic HAgNS in sunlight.References: 1. L. R. Hirsch, Ann. Biomed. Eng., 2006, 34, 15–22. 2. E. Hao, S. Li, R. C. Bailey, S. Zou, G. C. Schatz and J. T. Hupp, J. Phys. Chem. B, 2004, 108, 1224–1229. 3. N. Halas, Opt. Photonics News, 2002, 13, 26–30. 4. V. V. Kulish and P. M. Tomchuk, Surf. Sci., 2008, 602, 1045–1052. 5. S. Lal, N. K. Grady, J. Kundu, C. S. Levin, J. B. Lassiter and N. J. Halas, Chem. Soc. Rev., 2008, 37, 898–911. 6. J. Z. Zhang, J. Phys. Chem. Lett., 2010, 1, 686–695. 7. S. Kado, S. Yokomine and K. Kimura, RSC Adv., 2014, 4, 10830–10833.8. S. Pattanayak, A. Priyam and P. Paik, Dalt. Trans., 2013, 42, 10597.9. J. Yin, Y. Zang, B. Xu, S. Li, J. Kang, Y. Fang, Z. Wu and J. Li, Nanoscale, 2014, 6, 3934–3940.10. A. S. Kumbhar, M. K. Kinnan and G. Chumanov, J. Am. Chem. Soc., 2005, 127, 12444–12445.11. S. Kado, S. Yokomine and K. Kimura, Bull. Chem. Soc. Jpn., 2017, 90, 537–545.12. R. Bardhan, S. Lal, A. Joshi and N. J. Halas, Acc. Chem. Res., 2011, 44, 936–946. 13. S. Kawata, Y. Inouye and P. Verma, Nat. Photonics, 2009, 3, 388–394. 14. C. J. Murphy, Acc. Chem. Res., 2008, 41, 1721–1730. 15. A. Priyam, N. M. Idris and Y. Zhang, J. Mater. Chem., 2012, 22, 960–965. 16. J. C. Andrew and L. W. Jennifer, J. Am. Chem. Soc, 2012, 2, 37–54. 17. P. K. Jain, X. Huang, I. H. El-Sayed and M. A. El-Sayed, Acc. Chem. Res., 2008, 41, 1578–1586. 18. S. Lal, S. E. Clare and N. J. Halas, Acc. Chem. Res., 2008, 41, 1842–1851. 19. M. P. Melancon, M. Zhou and C. Li, Acc. Chem. Res., 2011, 44, 947–956. 20. S. J. Oldenburg, R. D. Averitt, S. L. Westcott and N. J. Halas, Chem. Phys. Lett., 1998, 288, 243–247. 21. S. J. Oldenburg, J. B. Jackson, S. L. Westcott and N. J. Halas, Appl. Phys. Lett., 1999, 75, 2897–2899. 22. J. B. Jackson and N. J. Halas, Proc. Natl. Acad. Sci. U. S. A., 2004, 101, 17930–17935. 23. M. P. Melancon, W. Lu, Z. Yang, R. Zhang, Z. Cheng, A. M. Elliot, J. Stafford, T. Olson, J. Z. Zhang and C. Li, Mol. Cancer Ther., 2008, 7, 1730–1739. 24. H.-P. Liang, L.-J. Wan, C.-L. Bai and L. Jiang, J. Phys. Chem. B, 2005, 109, 7795–7800. 25. A. M. Schwartzberg, T. Y. Oshiro, J. Z. Zhang, T. Huser and C. E. Talley, Anal. Chem., 2006, 78, 4732–4736. 26. A. M. Schwartzberg, T. Y. Olson, C. E. Talley and J. Z. Zhang, J. Phys. Chem. B, 2006, 110, 19935–19944. 27. S. Adams, D. Thai, X. Mascona, A. M. Schwartzberg, and J. Z. Zhang, Chem. Mater., 2014, 26, 6805–6810. 28. H. H. Xie, A. W. Wark, V. V. Tileli, K. Faulds, I. A. Larmour, Y.-C. Chen, A. W. Wark, V. V. Tileli, D. W. McComb, K. Faulds and D. Graham, Nanoscale, 2013, 5, 765–771. 29. M. Chen and L. Gao, Inorg. Chem., 2006, 45, 5145–5149. 30. A. Ben Moshe and G. Markovich, Chem. Mater., 2011, 23, 1239–1245. 31. Y. Jin and S. Dong, J. Phys. Chem. B, 2003, 107, 12902–12905. 32. B. K. Dadhich, B. Bhushan, A. Saha and A. Priyam, ACS Appl. Nano Mater., 2018, 1, 4294-430533. L. A. Lane, R. Xue and S. Nie, Curr. Opin. Chem. Biol., 2018, 45, 95–103.34. S. Linic, P. Christopher and D. B. Ingram, Nat. Mater., 2011, 10, 911–921.35. C. Wang, X. G. Nie, Y. Shi, Y. Zhou, J. J. Xu, X. H. Xia and H. Y. Chen, ACS Nano, 2017, 11, 5897–5905.36. B. S. Kim S, Thiessen PA, Bolton EE, Chen J, Fu G, Gindulyte A, Han L, He J, He S, Shoemaker BA, Wang J, Yu B, Zhang J, Methyl orange | C14H14N3NaO3S - PubChem.37. P. Magee, in Side Effects of Drugs Annual, 2011, vol. 33, pp. 479–490.38. A. Nezamzadeh-Ejhieh and N. Moazzeni, J. Ind. Eng. Chem., 2013, 19, 1433–1442.39. Y. H. Chiu, T. F. M. Chang, C. Y. Chen, M. Sone and Y. J. Hsu, Catalysts, 2019, 9, 1-32.40. S. Anandhakumar, M. Sasidharan, C. W. Tsao and A. M. Raichur, ACS Appl. Mater. Interfaces, 2014, 6, 3275–3281.41 M. A. Mahmoud, F. Saira and M. A. El-Sayed, Nano Lett., 2010, 10, 3764–3769.42. C. L. Lee, C. M. Tseng, R. B. Wu, C. C. Wu and S. C. Syu, Electrochim. Acta, 2009, 54, 5544–5547.43. U. Aslam, V. G. Rao, S. and S. Linic, Nat. Catalysis, 2018, 1, 656–665.44. R. Long, K. Mao, X. Ye, W. Yan, Y. Huang, J. Wang, Y. Fu, X. Wang, X. Wu, Y. Xie and Y. Xiong, J. Am. Chem. Soc., 2013, 135, 3200–3207.45. Kochevar I, Pathak MA, Parrish JA. Photophysics, photochemistry, and photobiology. New York: McGraw-Hill; 1999.46. S. Cho, M. J. Lee, M. S. Kim, S. Lee, Y. K. Kim, D. H. Lee, C. W. Lee, K. H. Cho and J. H. Chung, J. Dermatol. Sci., 2008, 50, 123–133.47. G. Wang, B. Huang, X. Ma, Z. Wang, X. Qin, X. Zhang, Y. Dai and M. H. Whangbo, Angew. Chemie - Int. Ed., 2013, 52, 4810–4813.48. H. Li, R. Liu, S. Lian, Y. Liu, H. Huang and Z. Kang, Nanoscale, 2013, 5, 3289.49. Q. Tian, W. Yao, W. Wu and C. Jiang, Nanoscale Horizons, 2019, 4, 10–25.50. J. Cui, Y. Li, L. Liu, L. Chen, J. Xu, J. Ma, G. Fang, E. Zhu, H. Wu, L. Zhao, L. Wang and Y. Huang, Nano Lett., 2015, 15, 6295–6301.4.3 DRAWBACKS IN EXISTING STATE-OF-ART & HOW THE DRAWBACKS HAVE BEEN OVERCOME BY OUR INVENTION:i. Limited tunability up to the first NIR window onlyTo the best of our knowledge, there is no report of ‘hollow silver nanoshells’ having plasmon resonances in the second NIR (NIR-II) window (650-950 nm). The maximum red-shifted SPR peak was observed at 800 nm by Kado et al.1, which lies in the first NIR window (NIR-I) only. For biomedical applications, it is desirable to have the SPR peaks in the NIR-II region (1000-1400 nm).The enhanced SPR tunability in the NIR-II region was achieved by utilizing dimethylglyoxime (DMG) as capping agent, which is the first report of its own kind. There is no precedent of DMG being employed as a capping agent in the synthesis of nanomaterials. Further, after analyzing various stirring speeds, zero rpm was found to be the best for obtaining spectrally narrow nanoshells with intense, and tunable plasmon peaks in the second NIR window. Other conditions such as reagent ratio and temperature were also optimized.ii. Absence of Quadrupole mode of surface plasmon resonances (Q-SPR) in nanoshellsIn most of the previous reports on hollow gold and silver nanoshells,2-5 a single SPR peak is observed which is tunable from visible to NIR-I spectral region depending on the aspect ratio. This peak is attributed to symmetric dipole resonance (SD-SPR). There is no observation of any other plasmonic modes. However, in the recent work by Kado et al.,1 one of the HAgNS samples showed a feeble SPR peak at a shorter wavelength (400 nm) in addition to a highly intense SPR peak at 800 nm. The less intense peak at 400 nm was attributed to quadrupole resonances (Q-SPR) in these hollow nanospheres. So, going by literature reports, the observance of quadrupole resonances in spherical nanoshells is a rare phenomenon.In contrast to the previous reports,1,4,5 all the HAgNS samples prepared by us, exhibit two prominent peaks and the Quadrupole peak is the most intense one. The quadrupole peaks (Q-SPR) are tunable in the range of 450-560 nm while the symmetric dipole resonances (SD-SPR) are tunable in the range of 780-1150 nm. The appearance of tunable Q-SPR in smaller sized (< 50 nm) has been possible due to the use of DMG as capping agent, choosing zero rpm as the stirring speed and optimizing the temperature and reagent ratio.iii. The necessity of stirring the reaction mixture during synthesis and energy expenditure incurred due to magnetic stirringIn all the previous works,1-6 stirring of the reaction mixture has been emphasized to achieve greater monodispersity of nanoparticles and better optical properties. The reaction mixtures were either vigorously stirred (Sun et al.6) or gently (Pattanayak et al.2) stirred to obtain hollow nanoshells. So, in all the prior syntheses, energy costs due to the use of magnetic stirrer was involved.In contrast, we have developed a zero-rpm method to obtain hollow nanoshells with good monodispersity and versatile SPR tunability upto the NIR-II region. To obtain ‘high-quality’ DMG-capped HAgNS, the synthesis process was analyzed for wide range of stirring speeds from zero to 1350 rpm. The synthesis at zero rpm was found to be the best as it yielded HAgNS having narrower SPR band (reduced FWHM) along with greater red-shift upto 1150 nm in the NIR-II region. iv. Size of NIR plasmonic silver nanoshells larger than 100 nmHollow silver nanoshells with SPR peak in the NIR region are difficult to prepare. There is only one research group (Kado et al.1) who have reported such hollow silver nanoshells with SPR peak around 800 nm in the NIR-I region. However, the sizes of such nanoshells are too big i.e, greater than 100 nm which is not suitable for biomedical applications.Alongwith attaining SPR tunability in the NIR-II region, the smaller sized HAgNS (in the range of 40 to 6o nm) were prepared by employing DMG as capping agent and carrying out the synthesis at zero rpm at an optimized temperature and reagent ratio. The outer diameters of the HAgNSs were 53±3, 50±3, 54±3, 62±4, and 40±1nm as determined by HR-TEM.v. Cost escalation due to the use of silver thiocyanate as a templateTo achieve plasmon tunability up to 800 nm in the NIR region, the aforementioned research group (Kado et al.1) replaced silver oxide with silver thiocyanate as a template which escalates the cost of synthesis and complicates the synthesis procedure. Silver oxide and silver thiocyanate templates are synthesized by the addition of silver nitrate with sodium hydroxide (NaOH) and Sodium thiocyanate (NaSCN) respectively. The synthesis of silver oxide vis-à-vis silver thiocyanate is cost-effective because sodium hydroxide (https: / / www.fishersci.com / shop / products / sodium-hydroxide-pellets-certified-acs-fisher-chemical-7 / S318500) is nearly 2.5 times less expensive than sodium thiocyanate (https: / / www.fishersci.com / shop / products / sodium-thiocyanate-crystalline-certified-acs-fisher-chemical / S441500).vi. NIR region was not utilized for plasmonic catalysis in sunlightSunlight consists of almost 6.8 % UV, 38.9 % Visible, and 54.3 % NIR light.8,9 Several efforts have been done to use the visible region for plasmon driven photocatalytic applications.10,11 On the other hand, due to limited tunability of SPR in NIR, the window has not been not explored much for plasmonic-catalysis by hollow nanocrystals. In some cases, NIR radiation has been utilized by using Plasmonic nanocrystals bound to some semiconductor nanocrystals. Even for such semiconductor-metal composite nanocrystals, there is no report available on the dependence of the solar photocatalytic efficiency on the tunable SPR wavelength in the NIR region.. Further, there is no example of NIR solar photocatalysis solely by plasmonic nanocrystals. The problem of plasmonic NIR-catalysis in sunlight has been addressed by the synthesis of tunable NIR-plasmonic DMG-capped HAgNSs in this work. They were then utilized for plasmonic catalysis of dye degradation in the sunlight. References:1. S. Kado, S. Yokomine and K. Kimura, Bull. Chem. Soc. Jpn., 2017, 90, 537–545.2. S. Pattanayak, A. Priyam and P. Paik, Dalton Trans., 2013, 42, 10597-10607.3. S. Adams, D. Thai, X. Mascona, A. M. Schwartzberg, and J. Z. Zhang, Chem. Mater., 2014, 26, 6805–6810.4. A. M. Schwartzberg, T. Y. Olson, C. E. Talley and J. Z. Zhang, J. Phys. Chem. B, 2006, 110, 19935–19944.5. A. Ben Moshe and G. Markovich, Chem. Mater., 2011, 23, 1239–1245.6. Y. G. Sun and Y. N. Xia, Science, 2002, 298, 2176–2179.7. B. K. Dadhich, B. Bhushan, A. Saha and A. Priyam, ACS Appl. Nano Mater., 2018, 1, 4294-43058. Kochevar I, Pathak MA, Parrish JA. Photophysics, photochemistry, and photobiology. New York: McGraw-Hill; 1999.9. S. Cho, M. J. Lee, M. S. Kim, S. Lee, Y. K. Kim, D. H. Lee, C. W. Lee, K. H. Cho and J. H. Chung, J. Dermatol. Sci., 2008, 50, 123–133.10. P. Christopher, H. Xin and S. Linic, Nat. Chem., 2011, 3, 467–472.11. M. Sun and H. Xu, Small, 2012, 8, 2777–2786.4.4 OBJECTIVES OF THE INVENTION:The objectives of the current research are the following:i. To develop an energy-efficient and green methodology for the synthesis of small-sized (<50 nm), near-IR plasmonic, hollow silver nanoshells.ii. To achieve enhanced tunability of plasmon peaks in the second NIR window (1000-1400 nm)iii. To enhance the intensity and tunability of quadrupole mode of surface plasmon resonances (Q-SPR) in hollow nanoshells.iv. To enhance the intensity and tunability of symmetric dipole mode of surface plasmon resonances (SD-SPR) in hollow nanoshells.iv. To minimize the energy cost by developing a methodology, ‘zero rpm synthesis’, devoid of any kind of stirring.v. To employ the plasmonic nanoshells as an efficient Vis-to-NIR-photocatalysts in the degradation of dyes, namely, Methyl orange and Bromocresol green in sunlight4.5 ADVANTAGES OVER OTHER KNOWN ALTERNATIVES INCLUDING IMPORTED ALTERNATIVES:Advantages over other known alternatives including imported alternatives are the following:i. Hollow, spherical silver nanoshells (HAgNS) shows enhanced plasmon tunability with two plasmon modes, Q-SPR & SD-SPR, encompassing the Vis-to-NIR region, 450-1150 nm, which the maximum tunability achieved in hollow silver nanostructures. No such hollow silver-nanoshell product exists in the world to date.The NIR-tunability of plasmons in hollow silver nanostructure has a clear advantage as the NIR-II region (1000-1400 nm) is more suitable for biomedical applications (Lane et al., Current opinion in chemical biology, 2018, 45, 95-103). This spectral region is also advantageous for photocatalytic work as a significant part of the sunlight comprises of IR radiations (Cui et al., Nano Lett., 2015, 15, 6295–6301).ii. The synthesis in this invention has been carried out at zero rpm (no stirring). Several stirring speeds ranging from zero to 1350 rpm were analyzed with respect to the plasmonic features and size distribution of nanoshells. The zero-rpm synthesis was found to be the best as it yielded hollow nanoshells having narrow size distribution and extended SPR tunability in the NIR-II region. It reduces any energy cost incurred due to the magnetic or mechanical stirring of solutions. This makes the process cost-effective and greener as well. All previous methods necessitate magnetic (or mechanical) stirring (Sun et al., Science, 2002, 298, 2176–2179).iii. The average sizes of different HAgNS samples synthesized by us lie in the range 40-62 nm, which is much smaller than that synthesized by other groups. This makes the HAgNS more suitable for biomedical applications as cell-internalization is facilitated. They are also capped by dimethlglyoxime (DMG) and folic acid (FA) molecules which further help in targeted delivery to cancer cells. Such hollow plasmonic silver systems with small size, NIR tunability, and DMG-FA capping did not exist before our work.iv. All the samples of DMG-capped HAgNSs synthesized here, consistently show two intense plasmon peaks. 1. Quadrupole-SPR (Q-SPR) and 2. Symmetric dipole-SPR. Amongst the two SPR peaks, the Q-SPR is the dominant one. No previous research group has shown dual SPR modes in hollow silver or gold nanostructures with such consistency. There is only one previous report (Kado et al. Bull. Chem. Soc. Jpn., 2017, 90, 537–545), in which one of the hollow silver samples prepared showed only a feeble Q-SPR.v. Solar-photocatalysis has been carried out in the NIR region and catalytic efficiency was found to increase with greater red-shift of the SPR peaks. No such result has been shown previously. Utilization of the NIR region of the solar spectrum represents a paradigm shift in photocatalysis as nearly 44% of solar radiation lies in the IR region.Existing methods mostly rely on using the UV-visible radiations (Aslam et al, Nat. Catalysis, 2018, 1, 656–665) and thus do not utilize the NIR part which is the other dominant component of solar radiation. In some cases, NIR radiation has been utilized by using Plasmonic nanocrystals bound to some semiconductor nanocrystals (Cui et al., Nano Lett., 2015, 15, 6295–6301). Even for such-semiconductor-metal composite nanocrystals, there is no report available on the effect on solar photocatalytic efficiency as the SPR absorption is tuned within NIR region. Further, there is no example of NIR solar photocatalysis solely by hollow plasmonic nanocrystals.vi. The HAgNS concentration required for photocatalysis lies in the subpicomolar (ng / L) regime while existing methods (Paul et al, J. Photochem. Photobiol. B, 2016, 154, 1-7.) necessitate catalyst concentration on the order of few mg / L. There is a clear factor of thousand by which the cost will be reduced simply considering this aspect only.Further, this weight advantage coupled with the use of the NIR part of the solar spectrum (point v) together reduces the costs incurred in the dye degradation significantly.4.6 BRIEF DISCUSSION OF THE DRAWINGS: Scheme 1. Schematic representation of the synthesis of DMG-FA-capped HAgNSs at a stirring rate of zero rpm.Scheme 1 shows a step-by-step illustration of a synthesis procedure for DMG-FA-capped HAgNSs. The synthesis is based on the nanoscale Kirkendall effect. In the first step, a colloidal solution of DMG-capped silver oxide nanoparticles (Ag2O NPs) was synthesized by the addition of sodium hydroxide (NaOH; 0.1 M, 500 µL) to the solution of silver nitrate (AgNO3; 10 mM, 150 µL) and dimethylglyoxime (DMG; 10 mM, 50 µL). In the second step, DMG-capped HAgNSs were synthesized by the reduction of Ag2O NPs, it is a double diffusion process where two reaction fronts move in the opposite direction. Silver ions diffuse outward and hydrazine hydrate (N2H4; 10 mM, 272 µL) diffuses inward. Oppositely mobile reaction fronts generate random vacuoles and these small voids coalesce to create a centralized cavity. In the third step, some of the capping DMG molecules are exchanged with folic acid for better solubility and stability in aqueous medium.Figure 1. UV-Visible-NIR electronic absorption spectra of different DMG-capped HAgNSs.Figure 1 shows the optical properties of the as-synthesized DMG-capped HAgNSs. Two prominent SPR peaks can be seen for each of the samples. The SPR was tuned from the blue end of visible to NIR- II region. The Q-SPR and SD-SPR of the HAgNS are tuned from 450 to 560 nm and 780 nm to 1150 nm by changing the molar ratio of reagents and temperature. All samples were synthesized at a stirring rate of zero rpm (i.e, without stirring). The synthesis temperature, silver ions to DMG molar ratio (Ag+: DMG) and silver ions to hydrazine hydrate (HH) molar ratio (Ag+: HH) were maintained as following: 2 °C, 1:1.33, 1:150 for HAgNS-780; 2 °C, 1:0.33, 1:80 for HAgNS-850; 2 °C, 1:0.33, 1:150 for HAgNS-920; 2 °C, 1:0.33, 1:100 for HAgNS-1000; and 25 °C, 1:0.33, 1:150 for HAgNS-1150 respectively. Figure 2. FTIR spectra of native dimethylglyoxime (DMG) and DMG-stabilized HAgNSs. Structure of DMG molecule (inset). Figure 2 shows the DMG capping on the surface of HAgNSs. The peaks at 3205, 1441, 1144, 979 and 716 cm-1 can be assigned to O-H, C=C, N-O, C-H (aliphatic), and C=N-O bond stretching vibration respectively.Figure 3. (a?e) TEM and (a'?e') HR-TEM images for HAgNS-780, HAgNS-850, HAgNS-920, HAgNS-1010, and HAgNS -1150, respectively. The scale for TEM and HR-TEM images are 20 and 10 nm, respectively. Figure 3 shows transmission electron micrographs (TEM) of the as-synthesized HAgNSs. Figure a, b, c, d, and e are bright-field TEM images. The high-resolution TEM of a single HAgNS is shown in figure a', b', c', d', and e'. The hollow nature and crystallinity are clearly visible. The outer diameters were 53±3, 50±3, 54±3, 62±4, and 40±1nm as determined by HR-TEM and the aspect ratios (Outer diameter / Shell thickness) were 3.31, 3.33, 3.48, 4.13, and 5.33, respectively.Figure 4. SPR peak position v / s aspect ratio of HAgNS. Figure 4 illustrates the dependence of SPR on the aspect ratio of DMG-capped HAgNS. The symmetric dipole mode (SD-SPR) gradually increases with the aspect ratio whereas antisymmetric dipole mode (AD-SPR) remains unaffected by the aspect ratio.Figure 5. UV-Vis extinction spectra for degradation of methyl orange (MO) and Bromocresol Green (BCG) in sunlight. Figure (a), (b), and (c) shows the solar-degradation of MO by HAgNP-400, HAgNS-780 and HAgNS-920 respectively. Figure (d) and (e) shows the solar-degradation of BCG by HAgNS-780 and HAgNS-920 respectively. Figure 5 is the evidence of the remediation of dyes MO and BCG by HAgNS under sunlight. First of all, 50 ml of stock solutions for each dye (10 ppm) were prepared. One set of 25 ml is used as controls while another set is mixed with 1.5 ml of as-synthesized HAgNSs. The ensuing reactions were monitored by the UV-Vis-NIR absorption spectrophotometer (Jasco V 770) at regular time intervals, following the decrease in MO and BCG absorption at 485 and 616 nm respectively. The photocatalytic process was found to follow first-order decay kinetics and accordingly, the quantitative estimations were made. The value of rate constant (k) were calculated to be 0.084, 0.268, 0.303 hrs-1 for MO degradation by HAgNS-400, HAgNS-780, and HAgNS-920. For BCG degradation, k were calculated to be 0.034 and 0.047 hrs-1 by HAgNS-780 and HAgNS-920. After 6 hours 84% and 24% degradation of MO and BCG were analysed. Here, we also note that a good catalytic efficiency has been achieved for HAgNSs, even without the aid of electron donor species, such as NaBH4 or semiconductor nanoparticles, which is in contrast to the earlier reports.1- 4References: 1. B. Paul , B. Bhuyan, D. D. Purkayastha and S. S. Dhar , J. Photochem. Photobiol . B Biol., 2016, 154, 1–7. 2. M. Meena Kumari, D. Philip, Spectrochim. Acta, Part A 2013, 111 , 154-160 . 3. H. Wu, P. Wang, H. He and Y. Jin, Nano Res., 2012, 5, 135–144. 4. P. Huo, Y. Yan, S. Li , H. Li , W. Huang, S. Chen and X. Zhang, Desalination, 2010, 263, 258–263.

Claims

We claim:

1. A material comprising of:i. Single crystalline, spherically hollow silver with interior void space.ii. Hollow nanospheres with average outer diameter tunable from 40±1 nm to 62±4 nm.iii. Hollow nanospheres with average inner void diameter tunable from 20±3 nm to 32±4 nm.iv. Tunable ‘surface plasmon resonances’ (SPR) in the first near-IR window (NIR-I, 650-950 nm) and second near-IR window (NIR-II, 1000-1400 nm).v. Two peaks corresponding to two SPR modes: both being intense and widely tunable: symmetric dipole (SD-SPR) peaks tunable from 780 to 1150nm and quadrupole (Q-SPR) peaks tunable from 450 nm to 560 nm, 2. A synthesis method for hollow silver nanoshells (HAgNSs), according to claim 1, comprising the steps of: i. Preparation of separate aqueous solution of silver salt, capping agent, base, and reducing agent. ii. Addition of silver salt (10 mM, 150 µl) and stabilizer (10 mM, 50 µl) in deionized water (2.5 ml).iii. Addition of a basic solution (0.1 M, 500 µl) to adjust the pH of the solution (2.7 ml) at11. iv. Addition of reducing agent solution (272 µl, 825 mM) in the solution (3.2 ml) in a single shot. v. Instant-addition of biomolecular capping agent to the synthesized HAgNSs.vi. Maintaining a constant stirring speed in the steps i to v.

3. The method of claim 2, the silver salts consists of AgNO3.

4. The method of claim 2, the capping agent consists of dimethylglyoxime (DMG).

5. The method of claim 2, the base consists of NaOH.

6. The method of claim 2, the reducing agent consists of hydrazine hydrate.

7. The method of claim 2, the biomolecular capping agent consists of folic acid.

8. The method of claim 2, the constant stirring speed is zero rpm.

9. Hollow silver nanoshells, according to claim 1 and 2, is employed as a solar-catalyst for the effective degradation of organic dyes, namely, Methyl Orange (MO) and Bromocresol Green (BCG).

10. The solar-catalysis experiment, according to claim 9, comprising the steps of:i. Preparation of a 50 ml stock solution of both dyes (MO & BCG, 10 ppm each). ii. Placing the 25 ml of each dye in sunlight and the remaining 25 ml of dye to be used as control. iii. Addition of sub-picomolar concentration of as-synthesized HAgNSs to both dyes.iv. Irradiation with sunlight for six hours.