“a bituminous product for pavement construction and a method of preparation thereof”
Patent Information
- Application Number
- IN202511001147
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2025-01-06
- Publication Date
- 2026-08-10
- Estimated Expiration
- 2045-01-06
AI Technical Summary
The use of higher dosages of waste low-density polyethylene (LDPE) in bitumen modification for pavement construction is hindered by phase separation and reduced fatigue performance at intermediate temperatures, making it unsuitable for national highways and expressways.
A wet process is employed to chemically blend viscosity graded bitumen with waste LDPE, using maleic anhydride as a compatibilizer and elemental sulfur as a cross-linker, to create a stable and homogeneous bituminous product suitable for paving applications.
The resulting bituminous product exhibits improved mechanical properties, including increased resilient modulus, enhanced rutting resistance, and extended fatigue life, making it suitable for high-traffic and harsh environmental conditions.
Abstract
Description
FIELD OF THE INVENTIONThe present invention relates to the field of plastic waste recycling. Moreparticularly, the present invention relates to a stable, resilient and sustainablebituminous product for pavement construction and a method of preparationthereof. Further, the present invention provides an environment friendlymethod of preparation that converts non-recyclable plastic waste into a valuableresource.BACKGROUND OF THE INVENTIONBitumen is a primary binder in bituminous pavements that is typically obtainedas a residue from the fractional distillation of petroleum crude oil. Bituminouspavements are preferred worldwide due to their superior ride quality, ease ofconstruction and low maintenance costs. However, increased traffic loads andharsh environmental conditions have led to the degradation of thesepavements, prompting research into new methods for improving the structuraland functional performance of bituminous pavements. For modification ofbitumen, polymers are among the most popular modifiers. Commonly usedmodifiers are styrene butadiene (SBS), ethylene vinyl acetate (EVA) and crumbrubber. Adding these modifiers can effectively improve the mechanicalproperties of bitumen. However, the cost of these virgin modifiers is very high,thus, researchers are exploring other alternatives to these modifiers. Use ofwaste polymers seems a viable option for the bitumen modification. Amongstthe waste polymers, plastics are in the most significant quantity. These plasticwastes are generated in huge quantities, and primarily single-use plastics areresponsible for plastic pollution in India. The use of waste plastic in bituminousmixtures reduces the consumption of virgin polymers thereby leading to overallcost savings. Previous studies have explored the modification of bitumen withwaste plastics such as polyethylene terephthalate (PET), polypropylene (PP),polyethylene (PE), high-density polyethylene (HDPE), and low-densitypolyethylene (LDPE) at lower dosages. However, higher dosages of LDPEhave been avoided due to concerns about phase separation in the modifiedbitumen and reduction in fatigue performance at intermediate temperatures.Plastic production and its use is increasing worldwide, surpassing recyclingefforts that further highlights the urgent need for effective waste managementstrategies. Global plastic waste generation have increased multifolds and nearlytwo-thirds of plastic waste comes from plastics with lifecycle of under five years.Among the unrecycled fraction, over 70% comprises polyethylene (PE),primarily low-density polyethylene (LDPE), that is primarily used as packagingmaterial and holds minimal value in further supply chains after recycling.Traditional disposal methods like landfilling and incineration are foundineffective due to limited land availability, pollution and high costs. Recentresearch suggests plastic recycling offers a sustainable alternative. Low-densitypolyethylene (LDPE) is a thermoplastic produced through the polymerizationof ethylene. Its lower density, compared to other types of polyethylene, resultsfrom its branched molecular structure. LDPE is primarily used as packagingmaterial such as plastic grocery bags, trash bags, bubble wraps and other typesof disposable bags, in agriculture, greenhouse films, mulch films and irrigationpipes. In healthcare industry, LDPE is often used as medical tubing, disposablegloves, packaging for syringes, medicines and other equipments.However, one of the concerns with LDPE is its environmental impact,particularly when it comes to plastic waste management. LDPE is non-biodegradable, meaning it doesn't break down naturally in the environment.The manufacturing of LDPE depends on fossil fuel-based resources, which arelimited. The extraction and processing of these materials can result inenvironmental consequences, such as greenhouse gas emissions and ecosystemdisruption. Certain chemicals used in the production of LDPE, includingadditives and stabilizers, have raised health concerns. When LDPE is burned itforms dioxins, a highly toxic group of chemicals that build up in a food chain,can cause cancer and harms the immune and reproductive systems. Dumpingof LDPE in landfills poses long term problem from leaching of toxic additivesleading to contamination of ground water and land around landfilling site.JP10088001A discloses about a method of manufacturing an asphalt mixtureused for pavement. The asphalt mixture in the cited document is formed bymixing an aggregate, a filler, asphalt, and a plastic material having a particlesize similar to that of the aggregate, the plastic material being thermoplastic.The method is comprising the steps of heating the aggregate at or above a heatdistortion temperature of the plastic material to a temperature within a rangethat does not cause thermal degradation of the mixture after mixing. Here, thedry process has been adopted for the addition of plastic in the bituminousmixture. The dry process for incorporating waste plastics in road constructionis well-established in India, with over 13,000 kilometres of low-volume roads.However, despite its usage in rural road projects, it was observed that dryprocess faces significant quality control challenges, making it unsuitable fornational highways and expressways.You Lingyun et al., in Journal of traffic and transformation engineering,2022; 9(5):742-764; doi: https: / / doi.org / 10.1016 / j.jtte.2022.07.002, is areview article that discloses about recent developments and the feasibility ofusing plastic wastes as modifiers or additives to asphalt binders or asphaltmixtures in dry and wet processes, focusing on different materials from wastestreams, how to produce such modified materials, and the characteristics ofplastic waste modified asphalt, thus contributing to the sustainablemanagement of resources and production of useful paving materials. However,the cited document predominantly discusses the utilization of waste LDPE atvery low levels as well as reportsissues with phase separation when using higherproportions of LDPE. Further, the cited document is primarily focussed onmethods where the recycled polyethylene and phase separation is occurringbetween the plastics and bitumen at low concentrations that renders themodified bitumen unsuitable for practical paving applications.Qabur Ali et al., in Canadian journal of Civil Engineering, 51:489-507(2024); doi: 10.11 / cjce-2023-0306, discloses about exploring the low-temperature performance of MPP-modified asphalt binders and mixtures usingwet method. The cited document explores the use of multilayered waste plasticas a modifier for bitumen, specifically analysing its impact on the low-temperature performance of asphalt binders and pavements. However, the citeddocument falls short in assessing the stability of the plastic-modified bitumenand it directly incorporates the modified bitumen into bituminous mixtureswithout evaluating the stability of the blend beforehand. This omission leavesa gap in understanding the stability of modified bitumen when stored underhigh temperature conditions.In view of the existing state of the art, recycling LDPE is not economicallyviable, traditional disposal methods are ineffective and burning LDPE releasescarcinogenic dioxins. The recycling of LDPE is currently low due to inefficientwaste segregation, outdated infrastructure, dominance of the informal sector,low collection rates, economic unviability, degradation of quality withrecycling, lack of public awareness and inconsistent regulatory enforcement.Moreover, the bituminous pavements that are preferred worldwide due to theirsuperior ride quality, ease of construction and low maintenance costs sufferfrom some drawbacks. These drawbacks are because of increased traffic loadsand harsh environmental conditions that led to the degradation of thesepavements.Therefore, there is a need of development of a cost-effective and sustainablemethod that addresses the technical challenges associated with using higherdosages of waste LDPE for bitumen modification for improving the structuraland functional performance of bituminous pavements.OBJECT OF THE INVENTIONThe main object of the present invention is to provide a bituminous product forpavement construction and a method of preparation thereof.Another object of the present invention is to provide a resilient and sustainablebituminous product for pavement construction by incorporating waste LDPEthat offers both environmental and economic benefits.Yet another object of the present invention is to provide a method for improvingthe compatibility of waste LDPE with bitumen and making the compositionsuitable for paving applications.Yet another object of the present invention is to provide an approach that alignswith global efforts to reduce carbon emissions, potentially cutting emissions inthe asphalt industry.Still another object of the present invention is to provide a method formodification of bitumen with waste polymers that can enhance pavementstiffness, elasticity and resistance to temperature variations as well as solves theproblem of waste management.SUMMARY OF THE INVENTIONThe present invention relates to a wet process for the preparation of wasteplastic incorporated bituminous product. The waste low density polyethyleneand a viscosity graded (VG30) bitumen were blended together to prepare abituminous product for paving purposes, i.e., road construction. The wetprocess of chemically blending bitumen and waste low density poly ethyleneleads to a homogenous and storage stable blend for making bituminous mixes.In an embodiment, the present invention provides a bituminous product forpavement construction comprising of a base binder, a compatibilizer, a cross-linker and a plastic waste. Here, said base binder is viscosity graded bitumen ina range of 93.35 to 98.15%; said compatibilizer is maleic anhydride (MAH) ina range of 0.8-1.5%; said cross-linker is elemental sulfur (S) in a range of 0.05-0.15%; and said plastic waste is low density polyethylene (LDPE) and saidplastic waste is incorporated into said base binder with 1-5% by weight of saidbase binder to obtain said bituminous product for pavement construction.In another embodiment, the present invention provides a method ofpreparation of a bituminous product for pavement construction comprising thesteps of (a) taking pipes of a waste plastic and cutting into flakes of size 5-10mm followed by washing with running water and drying at room temperatureto drain excess water to obtain a dried flake; (b) melting said dried flakeobtained in step (a) at a temperature range of 180-200°C by a single-screwextruder to obtain a plastic pellet; (c) grafting said plastic pellet obtained in step(b) with a compatibilizer in a defined ratio to obtain a grafted plastic pellet; (d)subjecting 5.9 gm of said grafted plastic pellet obtained in step (c) to blendingwith 100 gm of a base binder in a high-shear mixer at a definite speed and apredefined temperature to obtain a melted mixture; (e) increasing the mixingspeed after obtaining a melted mixture of step (d) ranging from 2500-3000 rpmfor a time period of 120-180 minutes to obtain a homogenous mixture; and (f)dispersing 0.13 gm of a cross-linker to the homogenous mixture of step (e) andcontinuing blending for 30 minutes to obtain a bituminous product forpavement construction.The present invention relates to incorporation of waste LDPE in bitumenthrough a wet process approach that effectively overcomes the issue of thephase separation of plastic and bitumen, resulting in a stable, homogeneousblend of waste LDPE and bitumen.The above objects and advantages of the present invention will becomeapparent from the hereinafter set forth brief description of the drawings,detailed description of the invention, and claims appended herewith.BRIEF DESCRIPTION OF THE DRAWINGSAn understanding of the bituminous product for pavement construction andthe method of preparation thereof, of the present invention may be obtained byreference to the following drawings:Figure 1 is a pictorial representation of low density polyethylene (LDPE)pellets, according to an embodiment of the present invention.Figure 2 is a graphical representation of comparison of indirect tensile strengthand tensile strength ratio (TSR) of bituminous mixes tested with otherbituminous mixes prepared with commonly known compositions of bitumen,according to the present invention.Figure 3 is a graphical representation of comparison of resilient modulus (MR)of bituminous mixes at 25°C and 35°C with other bituminous mixes preparedwith commonly known bitumen, according to the present invention.Figure 4 is a graphical representation of comparison of rut depth after 20,000passes of Hamburg wheel tracker with steel wheels at 60°C with otherbituminous mixes prepared with commonly known bitumen, according to thepresent invention.Figure 5 is a graphical representation of number of loading cycles required toinduce a crack in the sample under repeated loading of 350 kPa stress level withother bituminous mixes prepared with commonly known bitumen, accordingto the present invention.DETAILED DESCRIPTION OF THE INVENTIONThe present invention will now be described hereinafter with reference to theaccompanying drawings in which a preferred embodiment of the invention isshown. This invention may, however, be embodied in many different formsand should not be construed as being limited to the embodiment set forthherein. Rather, the embodiment is provided so that this disclosure will bethorough, and will fully convey the scope of the invention to those skilled in theart.The present invention now will be described hereinafter with reference to thedetailed description, in which some, but not all embodiments of the inventionare indicated. Indeed, the invention may be embodied in many different formsand shouldnot be construed as limited to the embodiments set forth herein;rather, these embodiments are provided so that this disclosure will satisfyapplicable legal requirements. Like numbers refer to like elements throughout.The present invention is described fully herein with non-limiting embodimentsand exemplary experimentation.The present invention relates to a wet process for the preparation of wasteplastic bituminous product. The waste low density polyethylene and a viscositygraded (VG30) bitumen were blended together to a bituminous product forpaving purposes, i.e., road construction. The wet process of chemicallyblending bitumen and waste low density poly ethylene leads to a homogenousand storage stable blend for making bituminous mixes.In a preferred embodiment, the present invention provides a bituminousproduct for pavement construction comprising of a base binder, acompatibilizer, a cross-linker and a plastic waste.Here, said base binder is viscosity graded bitumen in a range of 93.35 to 98.15%;said compatibilizer is maleic anhydride (MAH) in a range of 0.8-1.5%; saidcross-linker is elemental sulfur (S) in a range of 0.05-0.15%; and said plasticwaste is low density polyethylene (LDPE) and said plastic waste is incorporatedinto said base binder with 1-5% by weight of said base binder to obtain saidbituminous product for pavement construction.Additionally, said viscosity graded (VG) bitumen is VG 30. The bituminousproduct exhibits resilient modulus (MR) in a range of 5740 to 8611 at atemperature of 25°C and 4487 to 6512 MPa at a temperature of 35°C; exhibitsrutting resistance with a rut depth of 1.28 to 1.95 mm after 20,000 passes ofHamburg wheel tracker; exhibits fatigue life in a range of 70,000 to 1,10,000cycles to failure by cracking under repeated loading of 350 kPa stress level; andexhibits tensile strength of 1.75 to 2.16 kPa and tensile strength ratio in a rangeof 0.9 to 0.95.In another preferred embodiment, the present invention provides a method ofpreparation of a bituminous product for pavement construction comprising thesteps of (a) taking pipes of a waste plastic and cutting into flakes of size 5-10mm followed by washing with running water and drying at room temperatureto drain excess water to obtain a dried flake; (b) melting said dried flakeobtained in step (a) at a temperature range of 180-200°C by a single-screwextruder to obtain a plastic pellet; (c) grafting said plastic pellet obtained in step(b) with a compatibilizer in a defined ratio to obtain a grafted plastic pellet; (d)subjecting 5.9 gm of said grafted plastic pellet obtained in step (c) to blendingwith 100 gm of a base binder in a high-shear mixer at a definite speed and apredefined temperature to obtain a melted mixture; (e) increasing the mixingspeed after obtaining a melted mixture of step (d) ranging from 2500-3000 rpmfor a time period of 120-180 minutes to obtain a homogenous mixture; and (f)dispersing 0.13 gm of a cross-linker to the homogenous mixture of step (e) andcontinuing blending for 30 minutes to obtain a bituminous product forpavement construction.Here, said waste plastic in step (a) is LDPE; said compatibilizer in step (b) ismaleic anhydride (MAH); said defined ratio in step (c) is a weight ratio of 9:50of MAH and LDPE; said base binder in step (d) is viscosity graded bitumen i.e.VG30; said definite speed and said predefined temperature in step (d) is of 1000to 1500 rpm and 170-180°C; said cross-linker in step (f) is elemental sulfur; andsaid method employs a single use waste plastic content of 1-5% by weight ofsaid base binder to obtain said bituminous product for pavement constructionthat exhibits an optimum bitumen content (OBC) of 4.97.Referring to Figure 1, a pictorial representation of low density polyethylene(LDPE) pellets, is depicted.EXAMPLE 1For Experimentation detailsWet and dry methodThe two different methods of adding plastics to bituminous pavements widelyemployed are wet and dry method. In the dry process, waste plastic isintroduced either as a partial substitute for aggregates or mixed with the hotaggregates, followed by the addition of bitumen into the mixture. The aggregatereplacement approach is particularly suitable for rigid plastics with high meltingpoints, such as polystyrene (PS) and polyethylene terephthalate (PET) thatserve as either fillers or replacements for a portion of fine aggregates.Conversely, plastics characterized by lower melting points, such aspolyethylene (PE), are employed in the dry process. In the dry process, lowmelting temperature plastic melts, when mixed with hot aggregates, and formsa thin film enveloping the aggregates. The dry method is referred to as theaggregate modification, mixture modification, or bitumen replacementapproach.In contrast, the wet process involves the waste plastics being mixed withbitumen. The mixing of bitumen and plastics are done at high shear rate andhigh temperature. Preference is given to the utilization of plastics in pelletized,shredded or powdered forms, allowing for a high shear rate to achieve ahomogeneous and well-dispersed amalgamation of plastics within the bitumenmatrix. As per NCHRP project 9-66 and NAPA IS:142, the wet process issuitable for plastics having low melting temperatures. The dry process is widelyimplemented; however, the dry process usually presents quality controlchallenges that have limited the acceptance among researchers and industryprofessionals. On the other hand, the wet process provides more stringentquality control by directly modifying the bitumen with plastics. The maintechnical issue associated with the wet process is phase separation due to thelow compatibility between LDPE and bitumen, which is measured by storagestability tests (as per Indian Standard IS 15462-2019).BitumenBitumen is the primary binder in bituminous pavements that is typicallyobtained as a residue from the fractional distillation of petroleum crude oil.Usually, viscosity-graded bitumen (VG30 and VG40) is predominantlyemployed, with higher VG numbers representing higher viscosity and stiffness.For modification of bitumen, polymers are among the most popular modifiers.The incorporation of waste plastics into bitumen had shown to improveperformance parameters, including stability, strength, rutting resistance andlow-temperature cracking in bituminous pavements. Furthermore, employingwaste plastic in bituminous mixtures reduces the consumption of virginpolymers, leading to overall cost savings. In the dry process, plastic is mixedwith aggregates at high temperatures, then bitumen and fillers are mixed toproduce a waste-plastic bituminous mixture. Unlike wet process, the dryprocess does not involve any chemical modification or blending of thecomponents, focusing instead on physical integration to achieve desiredpavement properties. The present invention addresses the technical challengesassociated with higher dosages of waste LDPE (greater than 3%) for bitumenmodification by developing a method for improving the compatibility of wasteLDPE with bitumen, making the composition suitable for paving applications.The present invention utilizes the waste discarded LDPE in bituminouspavements by wet process.Waste LDPEThe waste LDPE was procured from the local recycler, first washed and driedthen converted in the form of pellets, as shown in Figure 1. Since, LDPEpossesses low compatibility with bitumen, the LDPE was made chemicallycompatible with bitumen so that a homogenous and storage stable blend wasformed when mixed with bitumen.Optimization of plastic contentA fixed amount of VG 30 bitumen was heated in a preheated draft oven at170°C for 1 hour in a closed container. After heating, the bitumen was slowlystirred over an electric heater, maintaining a constant temperature of 170°C toeliminate any temperature gradient across the depth of the container. Once thebitumen reached a temperature of 170°C, grafted LDPE plastic was added andmixed slowly at 500-1000 rpm until the LDPE melted into the bitumen, asverified by visual observation. After ensuring that the plastic had melted, themixing rate was increased to 2500-3000 rpm to achieve a homogeneousdispersion of plastic within the bitumen matrix, maintaining the temperaturebetween 170-180°C. The process continued for an additional 3 hours or until ahomogeneous blend was achieved. Subsequently, sulphur was added, and themixing was continued at a temperature range of 150-160°C for another 30minutes at a slow mixing speed of 500-1000 rpm to mix the sulphur and toreduce air bubbles. The modified bitumen samples were then cooled to roomtemperature and stored in closed containers for further testing. The optimumdosage of plastics and mixing time were determined through a trial-and-errormethod. The mixing temperature was 170-180°C. The optimum dosage ofgrafted LDPE was chosen based on storage stability test values according to theprocedure described as per IS 15460 2019. The results of storage stability testare depicted in Table 1. According to Indian standards, the modified bitumenis considered suitable for paving applications only if the storage stability valuesare below 3°C.To modify the bitumen, an initial plastic content of 1% by weight of the bitumenwas taken. After modification, the bitumen was cooled to room temperature. Ifthe modified bitumen exhibited a smooth surface texture, the modified bitumenwas then subjected to a storage stability test in accordance with IS 15462 - 2019.If the bitumen passed the test, the plastic content was increased by 1%, and theprocess was repeated. Mixing time was optimized by achieving a consistentHigh-Performance Grade (PG) over three consecutive 15-minute intervals. Ifthe consistency was not achieved, mixing was continued until the criterion wasmet.The combination of 5% LDPE, 0.9% MAH, and 0.13% sulphur yielded astorage-stable bituminous product. The modified bitumen was then subjectedto rheological testing, and bituminous mixes were prepared from the modifiedbitumen. Subsequently, mechanical performance tests were performed on theprepared mixes.Table 1: Optimization of plastic content based on storage stability testMethod of preparationThe present invention provides where waste LDPE was employed for safelymodifying the bitumen to prepare plastic modified bitumen that was furtherutilized in road construction process. Initially, the waste LDPE pipes were cutinto small flakes of 5-10 mm in size that were then washed with running waterand dried at room temperature (35 to 45°C) to drain excess water. The driedflakes were melted at a temperature of 180°C to 200°C by a single-screwextruder to form pellets. The process also removed other plastics, such as PET,HDPE and PP, from the waste stream. Table 2 highlights the properties of thepelletized plastic taken for preparation of bituminous product.Table 2: Properties of the waste plastic (LDPE) taken for the preparation ofthe bituminous productFurther, the LDPE pellets were grafted. The grafting was done with maleicanhydride (MAH) in a range 0f 0.8-1.5%. Preferably, the LDPE pellets weregrafted with MAH in a weight ratio of 9:50 (MAH: LDPE) that is 5 gm LDPEand 0.9 gm of MAH. Then, 5.9 gm of the grafted LDPE pellets were blendedwith base bitumen (VG30 bitumen) in varying amounts ranging from 1% to 5%by weight of the base bitumen. However, after optimization, the waste LDPEcontent was fixed at 5% by weight of the base bitumen and for grafted LDPE,the content was 5.9% by weight of the base bitumen. The blending was carriedout with the help of a high-shear mixer at a speed of 1,000 to 3,000 rpm and atemperature between 170°C and 180°C. Initially, the mixing speed was keptbetween 1000-1500 rpm, once the LDPE melted, the mixing speed wasincreased to 2500-3000 rpm for 120-180 minutes in order to homogeneouslydisperse the waste LDPE. Once the LDPE was fully melted and dispersed, theelemental sulfur (98% purity) in a range of 0.05-0.15%. Preferably, theelemental sulfur was added at a weight ratio of 13:500 relative to the non-grafted LDPE pellets and the blending was continued for another 30 minutes.The weight proportions of waste LDPE, MAH and sulphur was 5 gm, 0.9 gmand 0.13 gm were taken for every 100 g of the base bitumen. The obtainedbituminous product have viscosity graded bitumen in a range of 93.35 to98.15%.The bituminous product was subjected to a storage stability test in accordancewith the IS15462:2019 standard. The blend remained stable with LDPE contentup to 5%. Following storage stability test, the bituminous product (containing5% LDPE by weight of the base bitumen) was evaluated for the physicalproperties and rheological performance and compared with the base bitumen(VG30). Additionally, bituminous mixes were prepared by taking 5% LDPE-incorporated bituminous product. The stiffness, moisture resistance, ruttingand fatigue performance of the mixes were assessed by the standard testmethods. The performance of the bituminous mixes made with the LDPE-incorporated bituminous product was compared against the mixes preparedwith commonly employed bitumen such as VG30, VG40, CRMB60 andPMB40 for paving in India and were suited for traffic conditions ranging frommoderate to high traffic loading.EXAMPLE 2Properties of the bituminous product (LDPE-incorporated bitumen)Table 3 summarizes the index properties of both the base bitumen (VG30) andthe bituminous product (represented as LDPE in Tables 3-6). Rheologicalperformance was assessed through a dynamic shear rheometer (DSR).Resistance to high-temperature permanent deformation was measured throughthe multiple stress creep and recovery (MSCR) test, while resistance tointermediate-temperature fatigue damage was evaluated with the help of thelinear amplitude sweep (LAS) test.Table 3: Properties of the base bitumen and the bituminous productThe permanent deformation behavior of bitumen was assessed by the MultipleStress Creep and Recovery (MSCR) test at a temperature of 40, 50, 60 and70°C, following AASHTO T350. The chosen temperatures represented thehighest expected in-service conditions and to ensure that the material was testedin the non-linear domain. The MSCR test was conducted on short-term agedsamples that were aged by the rolling thin film oven (RTFO) according toASTM D 2872 standards.In contrast, the Linear Amplitude Sweep (LAS) test was employed to evaluatethe fatigue performance of long-term aged bitumen samples. Aging wasperformed in a pressure aging vessel (PAV) according to ASTM D 6521. TheLAS test was conducted at temperature of 5, 15 and 25°C, following AASHTOT391, since fatigue was a common failure mode at such temperatures. Thefatigue life (Nf), corresponding to 35% damage, was calculated throughviscoelastic continuum damage (VECD) models.Table 4: MSCR test results of the base bitumen and the bituminous productTables 4 and 5 present the MSCR and LAS test results. It was observed that themodified bitumen demonstrated higher resistance to permanent deformation,regardless of the test temperature, as indicated by the reduced Jnr values.Additionally, the elasticity of the bitumen increased after incorporation withLDPE, as reflected in the increased recovery values. Furthermore, the fatiguelife of the bitumen significantly improved with the addition of plastics, at everytest temperature. Therefore, it can be concluded that plastic-incorporatedbituminous product exhibits improved rheological performance andviscoelastic response.Table 5: Rheological fatigue life calculated from LAS test for the basebitumen and the bituminous productThe bituminous mixes were prepared with the plastic-incorporated bitumenand VG30 bitumen, to evaluate the mechanical performance. Along with theplastic modified bitumen, the bituminous mixes were also prepared with othercommon bitumen, i.e., VG40, CRMB60 and PMB40. The prepared bitumen'sare primarily preferred for surface course paving applications. Bituminousconcrete grade 1 (BC-1) mix was prepared, adhering to the guidelines outlinedby the Ministry of Road Transport and Highways (MoRTH). The sameaggregate gradation was adopted for all the bituminous mixes prepared bytaking different binders. For each mix, the calculated optimum binder content(OBC) is shown in Table 5. Bituminous mixes with different bitumen wererepresented with the following names mentioned in Table 6.Table 6: OBC of asphalt mixesThe OBC of mix prepared with waste LDPE incorporated bitumen was 5.94,7.13, 8.84 and 9.62% lower than mixes prepared with VG30, VG40, PMB40and CRMB60 bitumen, as given in Table 5. The reduction in OBC valuesresulted in direct cost saving during the construction of pavements.Performance of the bituminous product (or bituminous mixes)Various performance parameters of bituminous mixes such as stiffness,resistance to moisture damage, rutting, fatigue and tensile strength wereevaluated. LDPE-incorporated mixes showed higher stiffness that resulted inimproved pavement lifespan. Additionally, the prepared mixes showedimproved resistance to rutting and fatigue, further increasing pavementserviceability. Improved tensile strength and moisture resistance offered highertensile strength and resistance to moisture-induced damage. The experimentaltest results are provided in form of ITS, TSR test results. Additionally, therutting performance test results are provided, i.e., Hamburg wheel tracker testresults, fatigue performance in form of ITFT test results and stiffnessmeasurement in terms of MR test results.Stiffness was measured by the resilient modulus test at 25°C and 35°C. Ruttingand fatigue resistance were assessed through the Hamburg Wheel Tracker Test(HWTT) at a temperature of 60°C and the Indirect Tensile Fatigue Test at atemperature of 25°C. The tensile strength was evaluated by the Indirect TensileStrength (ITS) test, while resistance to moisture damage was evaluated throughthe Tensile Strength Ratio (TSR). Higher values for the parameters indicatedsuperior performance. LDPE-incorporated bituminous mixtures showed72.25%, 51.65%, 49%, and 40% higher tensile strength and 8.12%, 7.33%,2.03%, and 4.60% improved resistance to moisture damage compared to VG30,VG40, PMB and CRMB mixes, as shown in Figure 2. Additionally, LDPEmixes offered improved stiffness than VG30 (131% and 137.1%), VG40 (47%and 73%), PMB (48% and 180.50%) and CRMB (18.42% and 23.56%) at thetemperature of 25°C and 35°C, as shown in Figure 3. The improvement instiffness contributed to a longer pavement life and reduced maintenance,thereby lowered carbon emissions from frequent repairs and pavementconstruction. Furthermore, incorporation of LDPE reused 1,044 kg of wasteLDPE single-use plastics for every kilometer of a 50 mm-thick surface courseand for each 3.5 m wide lane.Bituminous mixes made with waste LDPE-incorporated bituminous productalso exhibited higher resistance to rutting at a temperature of 60°C and fatiguedamage at a temperature of 25°C. In the HWTT (in accordance to AASHTOT324), after 20,000 passes at 60°C, the rut depth observed was the lowest forLDPE-incorporated mixtures, as shown in Figure 4. The rut depth was 87.5%,72.6%, 60.17%, and 45.16% lower than VG30, VG40, CRMB, and PMB mixes.Fatigue performance was evaluated by the Indirect Tensile Fatigue Test (ITFT)in accordance with British Standard (BS EN 12697-24). A cyclic load of 350kPa was applied for a total of 100,000 cycles, with the number of cycles tofailure recorded as the fatigue life. Figure 5 shows the results of ITFT, a higherfatigue life indicated higher resistance to fatigue damage. The observedimprovement in fatigue life was 1,300%, 600%, 133% and 40% compared toVG30, VG40, CRMB and PMB.The present invention presents a significant advancement by providing anefficient method to repurpose one of the most abundant types of plastic waste-typically low-density polyethylene (LDPE) and having very limited recyclingpotential. Traditionally, the plastic waste (LDPE) poses a major environmentalchallenges in recycling and management. However, through the innovativeprocess of the present invention, the plastic waste was safely incorporated intobituminous pavement materials without the risk of releasing harmful dioxins orother toxic emissions during production. A key benefit of the method of thepresent invention is the ability to improve the mechanical properties ofbituminous mixes. By incorporating processed plastic waste, the resultingpavement material exhibited higher strength, durability and resistance todeformation, leading to long-lasting roads that perform better under varyingtraffic and environmental conditions. The present invention addresses twocritical global challenges. Firstly, the present invention offers an environmentfriendly solution to plastic waste management by converting non-recyclablewaste plastic into a valuable resource for infrastructure development. Secondly,meets the growing demand for sustainable yet resilient road constructionmaterials, reducing reliance on traditional raw materials while enhancing thelongevity and quality of road infrastructure. The dual impact of the process ofthe present invention not only reduced environmental pollution but alsocontributed to the development of more sustainable and durable road systems.Bitumen was incorporated with waste low density polyethylene (LDPE) andthe obtained bituminous product showed significant improvement inrheological performance in both high and intermediate temperature domain.Employing the plastic incorporated bitumen for preparation of bituminousmixes showed reduction in optimum bitumen demand up to 6% compared tothe base bitumen. The optimum bitumen content for mixes prepared withplastic-incorporated bitumen reduced by 9% and 10% as compared to mixescontaining elastomeric polymer and crumb rubber modified bitumen. Higheramount of waste low density polyethylene was taken with compatibilizer andcross linker for the preparation of composition for road pavement.Therefore, the present invention provides a bituminous product for pavementconstruction that was prepared by incorporating waste plastic (LDPE) into abase bitumen to exhibit higher stiffness, lower susceptibility to moisturedamage and higher resistance to high temperature rutting and intermediatetemperature fatigue damage.Many modifications and other embodiments of the invention set forth hereinwill readily occur to one skilled in the art to which the invention pertain havingthe benefit of the teachings presented in the foregoing descriptions and theassociated drawings. Therefore, it is to be understood that the invention is notto be limited to the specific embodiments disclosed and that modifications andother embodiments are intended to be included within the scope of theappended claims. Although specific terms are employed herein, they are usedin a generic and descriptive sense only and not for purposes of limitation.
Claims
1. A bituminous product for pavement construction comprising of: a base binder; a compatibilizer; a cross-linker; and a plastic waste; wherein, said base binder is viscosity graded bitumen in a range of 93.35 to 98.15%; said compatibilizer is maleic anhydride (MAH) in a range of 0.8-1.5%; said cross-linker is elemental sulfur (S) in a range of 0.05-0.15%; and said plastic waste is low density polyethylene (LDPE) and said plastic waste is incorporated into said base binder with 1-5% by weight of said base binder to obtain said bituminous product for pavement construction.
2. The bituminous product as claimed in claim 1, wherein said viscosity graded (VG) bitumen is VG 30.
3. The bituminous product as claimed in claim 1, wherein said bituminous product exhibits resilient modulus (MR) in a range of 5740 to 8611 at a temperature of 25°C and 4487 to 6512 MPa at a temperature of 35°C.
4. The bituminous product as claimed in claim 1, wherein said bituminous product exhibits rutting resistance with a rut depth of 1.28 to 1.95 mm after 20,000 passes of Hamburg wheel tracker.
5. The bituminous product as claimed in claim 1, wherein said bituminous product exhibits fatigue life in a range of 70,000 to 1,10,000 cycles to failure by cracking under repeated loading of 350 kPa stress level.
6. The bituminous product as claimed in claim 1, wherein said bituminous product exhibits tensile strength of 1.75 to 2.16 kPa and tensile strength ratio in a range of 0.9 to 0.95.
7. A method of preparation of a bituminous product for pavement construction comprising the steps of: (a) taking pipes of a waste plastic and cutting into flakes of size 5-10 mm followed by washing with running water and drying at room temperature to drain excess water to obtain a dried flake; (b) melting said dried flake obtained in step (a) at a temperature range of 180-200°C by a single-screw extruder to obtain a plastic pellet; (c) grafting said plastic pellet obtained in step (b) with a compatibilizer in a defined ratio to obtain a grafted plastic pellet; (d) subjecting 5.9 gm of said grafted plastic pellet obtained in step (c) to blending with 100 gm of a base binder in a high-shear mixer at a definite speed and a predefined temperature to obtain a melted mixture; (e) increasing the mixing speed after obtaining a melted mixture of step (d) ranging from 2500-3000 rpm for a time period of 120-180 minutes to obtain a homogenous mixture; and (f) dispersing 0.13 gm of a cross-linker to the homogenous mixture of step (e) and continuing blending for 30 minutes to obtain a bituminous product for pavement construction; wherein, said waste plastic in step (a) is LDPE; said compatibilizer in step (b) is maleic anhydride (MAH); said defined ratio in step (c) is a weight ratio of 9:50 of MAH and LDPE; said base binder in step (d) is viscosity graded bitumen, VG30; said definite speed and said predefined temperature in step (d) is of 1000 to 1500 rpm and 170-180°C; said cross-linker in step (f) is elemental sulfur; and said method employs a single use waste plastic content of 1-5% by weight of said base binder to obtain said bituminous product for pavement construction that exhibits an optimum bitumen content (OBC) of 4.97.