Battery for achieving high cycle life and zinc utilization in secondary zinc anodes using electrocoagulants

IN598998BActive Publication Date: 2026-08-13RES FOUND THE CITY UNIV OF NEW YORK
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202217044501
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-01-23
Filing Date
2022-08-03
Publication Date
2026-08-13
Estimated Expiration
2041-01-22

AI Technical Summary

Technical Problem

Zinc anode batteries face issues with irreversible characteristics, such as shape-change and dendrite formation, leading to short circuits and limited cycle life, which restrict their use in high-energy applications due to the high energy density of zinc being compromised by the irreversible nature of zinc oxide and zincate ion migration.

Method used

Incorporating electrocoagulants like aluminum, iron, titanium, or calcium, along with their hydroxides or oxides, into the battery design to coagulate zincate ions and prevent migration, thereby enhancing cycle life and zinc utilization by maintaining zinc reaction products near the anode.

Benefits of technology

The use of electrocoagulants significantly increases zinc utilization to 15-40% and cycle life to 200-1000 cycles, making zinc anode batteries more suitable for high-depth discharge and long-term applications.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A battery comprises a housing, an electrolyte disposed in the housing, a cathode disposed in the housing, an anode disposed in the housing and comprising an anode material comprising: zinc or zinc oxide, an electrocoagulant material selected from the group consisting of: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, a salt thereof, an oxide thereof, and a combination thereof, and a binder.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND

[0003] Zinc anode batteries like alkaline manganese dioxide (MnQ2)-zinc, nickel (Ni)-zing, silver (Ag)-zinc and zinc-air batteries have very high energy densities that could be veryuseful for a number of applications like grid-storage, cell phones and electric vehicles.However, the use of zinc has been relegated to primary batteries due to the irreversiblecharacteristics of a zinc (Zn) anode, where the anode has the tendency to dissolve and relocateto different regions of the electrode to create a phenomenon called shape-change, formirreversible oxides like zinc oxide at the end of discharge, and form dendritic structures thatpuncture the separator to create a short circuit.

[0004] The high energy density of the alkaline cell stems from the high capacity of itsactive materials and the high overall cell potential caused due to the electrochemical activityof zinc at a lower potential. Zinc has a theoretical capacity of 820 mAh / g, which originates[rom its two electron (2e-) reaction. Zinc undergoes the 2e- reaction through a dissolution-precipitation process to form zinc oxide (ZnO) as the discharged product. In a rechargeablesystem, typically the zinc oxide should undergo the dissolution-precipitation process reversiblyto form charged zinc, however, the electrical resistivity of zinc oxide impedes this process.The dissolved zinc in alkaline solution is called zincate [Zn(OH)42-], which has a tendency toform immediately when zinc is in contact with alkaline electrolyte. Due to the high density ofzinc, the zincate ions never deposit at the same region of the electrode and this tends to causethe shape-change phenomenon. Also, in MnO2-Zn batteries the zincate ions interfere in theMnO2 reactions and poison the cathode to form irreversible hetaerolite (ZnMn2O4). Tomitigate some of these problems, researchers have resorted to cycling the Zn anodes to lessthan 8% of the theoretical capacity to increase the cycle life of the cell. However, reducing thetheoretical capacity also limits the overall energy density of the cell and thus, reducing its usein many applications.

[0005] Many researchers have tried in the past to solve some of the aforementionedproblems. For example, U.S. Pat. No. 5,863,676 used an anode containing calcium zincate,which is a mixture of calcium hydroxide and zinc oxide to create an insoluble structure.Calcium zincate 1s supposed to trap the dissolved zincate ions and prevent it from migratingtowards the bulk electrolyte, therefore preventing shape-change and dendrite formation. Thebest cycle life reported in this reference is ~170 cycles. However, the content of zinc in theelectrodes is low, which reduces the energy density of the cell. Many calcium zincate patentsexist of which some of them relate to calcium zincate synthesis procedure. Other researchershave tried to use a number of additives containing Bi, In, etc. to reduce corrosion and gassingin Zn anode alkaline batteries, however, none have tried to improve the cycle life. Maintaininga cycle life (e.g, >150 cycles) and a Zn utilization or depth of discharge (DOD, DOD orutilization = Zn anode capacity delivered / Zn theoretical capacity * 100) of >10% is an endeavorwhich has not been achieved success(ully.SUMMARY

[0006] In some embodiments, a battery comprises a housing, an electrolyte disposed inthe housing, a cathode disposed in the housing, an anode disposed in the housing andcomprising an anode material comprising: zinc or zinc oxide, an electrocoagulant materialselected from the group consisting of: aluminum, iron, titanium, calcium, zirconium, ahydroxide thereof, a salt thereof, an oxide thereof, or a combination thereof, and a binder.

[0007] In some embodiments, a battery comprises a housing, an electrolyte disposed inthe housing, wherein the electrolyte comprises an elecirocoagulant material selected (rom thegroup consisting of: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, a saltthereof, an oxide thereol, and a combination thereof, a cathode disposed in the housing, ananode disposed in the housing and comprising an anode material comprising: zinc or zincoxide, and a binder.

[0008] In some embodiments, a method of operating a battery comprises discharging abattery, recharging the battery, coagulating one or more reaction products of the zinc or zincoxide with the electrocoagulant material, and retaining the one or more reaction products ofthe zinc or zinc oxide at or near the anode during the discharging, recharging, or both using theelectrocoagulant material. The battery comprises a housing, an electrolyte disposed in thehousing, a cathode disposed in the housing, an anode disposed in the housing and comprisingan anode material comprising: zinc or zinc oxide, an electrocoagulant material selected fromthe group consisting of: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, asalt thereof, an oxide thereof, and a combination thereof, and a binder.

[0009] These and other features will be more clearly understood from the followingdetailed description taken in conjunction with the accompanying claims.BRIEF DESCRIPTION OF THE DRAWINGS

[0010] For a more complete understanding of the present disclosure and the advantagesthereof, reference is now made to the following brief description, taken in connection with theaccompanying drawings and detailed description, wherein like reference numerals representlike parts.

[0011] Figures 1A-1D show examples different battery designs and configurations.

[0012] Figure 2 shows the cycle life and Zn utilization of electrodes containing aluminumhydroxide [AI(OH)3] compared to a baseline electrode as described with respect to Example 1.

[0013] Figures 3A, 3B, and 3C show the potential and current-time curves of the electrodecontaining the AI(OH)s as an electrocoagulant additive versus the baseline electrode asdescribed with respect to Example 1.

[0014] Figures 4A, 4B, and 4C show the beneficial effects of adding a conductive agentlike copper (Cu) powder to the electrode containing AI(OH); as described with respect toExample 2.DETAILED DESCRIPTION

[0015] In this disclosure, the terms "negative electrode and "anode" are both used tomean "negative electrode." Likewise, the terms "positive electrode" and "cathode" are bothused to mean "positive electrode." Reference to an "electrode" alone can refer to the anode,cathode, or both. Relerence to the term "primary battery" (e.g., "primary battery," "primaryelectrochemical cell," or "primary cell"), refers to a cell or battery that after a single dischargeis disposed of and replaced. Reference to the term "secondary battery" (e.g., "secondarybattery," "secondary electrochemical cell," or "secondary cell"), refers to a cell or battery thatcan be recharged one or more times and reused.

[0016] The present disclosure is with regards to the development of a Zn-anoderechargeable electrode. This electrode can be used in various rechargeable batteries that use aZn-anode. Applications for such a battery could be in grid-scale energy storage, tractionbatteries, aerospace applications, telecommunications, uninterruptible power supply (UPS),medical applications, etc. to name a few.

[0017] As described herein, the battery can comprise an electrocoagulant.Electrocoagulants, which can also be referred to as simply coagulants herein, can be used insome instances in an electrocoagulation process to treat water and wastewater to removepollutants, pesticides, oil, etc. In an electrocoagulation wastewater process, sacrificialelectrodes are used where an electric current passing through the electrodes dissolves theelectrodes to generate metal ions or coagulating agents that coagulate the pollutants in water.Example of electrocoagulants can include, but are not limited to, aluminum, iron, manganese(e.g. MnO2 and Mn;0y4), titanium (e.g. TiO2), calcium, and / or zirconium as well as theelectrolysis products of such elements such as oxides. hydroxides, salts, and the like. Thedissolved coagulants generate a number of aqueous complex ions that increase the coagulationefficiency. For example, aluminum (Al) in water can produce various compounds such asAI(OH)2+, Al2(OH)24+, Al6(OH)153+*, Al13(OH)345+, Al(H2O)63+, Al(H2O)5OH2+ andAl(H2O)4OH+.

[0018] In an alkaline battery system, the zincate ions can be viewed as dissolved impuritiesthat poison the cathode, and the loss of the zinc in the zincate ions from the localized vicinityof the anodes results in loss of capacity of the Zn anodes. In some instances, aluminum hasbeen used as a corrosion inhibiting agent in Zn anode batteries. For example, aluminum sulfateand aluminum potassium sulfate additives can be used to reduce the hydrogen gassing rates inthe cell that resulted from Zn corrosion. However, aluminum or its other compound derivativeshave not been used as electrocoagulants or coagulants to localize the zincate ions near thevicinity of the electrode and prevent zinc migration. Also, the presence of aluminum with zincoxide can increase the conductivity of the oxide. and thus, increase the reversibility of zincoxide lo zinc in its charged state.

[0019] In this disclosure, the addition of electrocoagulants or compound derivative(s) ofcoagulants like aluminum hydroxide [Al(OH);] are provided that increase the Zn utilization to15-40% and increase the cycle life to 200-1000 cvcles.

[0020] A rechargeable Zn anode alkaline battery is also described. The battery includes acathode material and an anode material with zinc or zinc oxide, a coagulant and a binder. Insome embodiments, coagulants can comprise aluminum or compounds, derivatives, and / orsalts of aluminum, or iron or compounds and / or derivatives of iron, or compounds containingaluminum and / or iron. In some of the embodiments, a conductive additive like copper orcompounds, derivatives, oxides, and / or salts of copper could be added to reduce the chargetransfer resistance of the electrode. An advantage that may be realized in the practice of somedisclosed embodiments of the battery is that a Zn anode battery is rendered rechargeable forlonger cycle life and at high depths of discharge.

[0021] Some embodiments of the cell or battery design where this rechargeable anodecould be used is shown in Figures 1A-1D. A prismatic and cylindrical battery design is shown,but it is not limited to these battery form factors. The battery comprises a cathode, an anode,electrolyte, and optionally, a separator. The designs shown are just a guide and are not limitedto the designs shown in Figures 1A-1D.

[0022] Referring to Figures 1A-1C, a cell or battery 10 can have a housing 7, a cathode12, which can include a cathode current collector 1 and a cathode material 2, and an anode 13.In some embodiments, the anode 13 can comprise an anode current collector 4, and an anodematerial 5. It is noted that the scale of the components in Figures 1A-1C may not be exact asthe features are illustrates to clearly show the anode 13 and the cathode 12 with the separator9. Figures 1A-1B show a prismatic battery arrangement having a single anode 13 and cathode12. The prismatic configuration can have a number of form factors such as a verticalconfiguration as shown in Figure 1A or a horizontal configuration as shown in Figure 1B. Inanother embodiment, the battery can be a cylindrical battery having the electrodes arrangedconcentrically as shown in Figure 1C or in a rolled configuration as shown in Figure 1D inwhich the anode 13 and cathode 12 are layered and then rolled to form ajelly roll configuration.The cathode current collector 1 and cathode material 2 are collectively called either the cathode12 or the positive electrode 12, as shown in Figure 1A. Similarly, the anode material 5 withthe optional anode current collector 4 can be collectively called either the anode 13 or thenegative electrode 13. An electrolyte can be in contact with the cathode 12 and the anode 13within the housing 7.

[0023] In some embodiments, the battery 10 can comprise one or more cathodes 12 andone or more anodes 13, which can be present in any configuration or form factor. When aplurality of anodes 13 and / or a plurality of cathodes 12 are present, the electrodes can beconfigured in a layered configuration such that the electrodes alternate (e.g., anode, cathode,anode, etc.). Any number of anodes 13 and / or cathodes 12 can be present to provide a desiredcapacity and / or output voltage. In the jellyroll configuration (e.g., as shown in Figure 1D), thebattery 10 may only have one cathode 12 and one anode 13 in a rolled configuration such thata cross section of the battery 10 includes a lavered configuration of alternating electrodes,though a plurality of cathodes 12 and anodes 13 can be used in a layered configuration androlled to form the rolled configuration with alternating layers.

[0024] In an embodiment, housing 7 comprises a molded box or container that is generallynon-reactive with respect to the electrolyte solutions in the battery 10. In an embodiment, thehousing 7 comprises a polymer (e.g., a polypropylene molded box, an acrylic poly mer moldedbox, etc.), a coated metal, or the like.

[0025] The cathode 12 can comprise a mixture of components including anelectrochemically active material. Additional components such as a binder, a conductivematerial, and / or one or more additional components can also be optionally included that canserve to improve the lifespan, rechargeability, and electrochemical properties of the cathode12. The cathode used can comprise manganese dioxide for Zn / MnO:2 battery or air withmanganese dioxide as the catalyst for the bifunctional electrocatalytic reactions in a Zn / airbattery. In some aspects, the cathode used can comprise nickel oxyhydroxide (NIOOH), silver(Ag), copper (Cu), bromine (Br), or combinations thereol.

[0026] In some embodiments, the cathode material 2 can be based on one or manypolymorphs of MnO-, including electrolytic (EMD), α-MnQ2, β-MnO2, γ-MnO2, δ-MnO2, ε-MnO2, λ-MnOz2, and / or chemically modified manganese dioxide. Other forms of MnO:z canalso be present such as hydrated MnO2, pyrolusite, bimessite, ramsdellite, hollandite,romanechite, todorkite, lithiophorite, chalcophanite, sodium or potassium rich bimessite,cryptomelane, buserite, manganese oxyvhydroxide (MnOOH), α-MnOOH, γ-MnOOH, β-MnOOH, manganese hydroxide [Mn(OH)2], partially or fully protonated manganese dioxide,Mn304, M205, bixbyite, MnO, lithiated manganese dioxide (LiMn204, Li2MnO3), CuMn2O4,aluminum manganese oxide, zinc manganese dioxide, bismuth manganese oxide, copperintercalated bimessite, copper intercalated bismuth birnessite, tin doped manganese oxide,magnesium manganese oxide, or any combination thereof. In general, the cycled form ofmanganese dioxide in the cathode can have a layered configuration, which in someembodiment can comprise δ-MnQz that is interchangeably referred to as birnessite. If non-birnessite polymorphic forms of manganese dioxide are used, these can be converted tobirnessite in-situ by one or more conditioning cycles as described in more details below. Forexample, a [ull or partial discharge to the end of the MnO2 second electron stage (e.g., betweenabout 20% to about 100% of the 2nd electron capacity of the cathode) may be performed andsubsequently recharging back to its Mn4+ slate, resulting in bimessile-phase manganesedioxide.

[0027] In some embodiments, the cathode composition is 1-90 wt.% manganese dioxide,0-30 wt.% bismuth or bismuth-based compounds, 0-50 wt.% copper or copper-basedcompounds, 1-90 wt.% conductive additive, and 0-10 wt.% binder.

[0028] In some embodiments, a binder can be used with the cathode material 2. In someembodiments, the binder comprises water-soluble cellulose-based hydrogels, which can beused as thickeners and strong binders, and have been cross-linked with good mechanicalstrength and with conductive polymers. The binder may also be a cellulose film sold ascellophane. The binders can be made by physically cross-linking the water-soluble cellulose-based hydrogels with a polymer through repeated cooling and thawing cycles. In someembodiments, the binder can comprise a 0-10 wt.% methyl cellulose (MC) and / orcarboxymethyl cellulose (CMC) solution cross-linked with 0-10 wt.% polyvinyl alcohol (PV A)on an equal volume basis. The binder, compared to the (raditionally-usedpolytetrafluoroethylene (PTFE), shows superior performance. PTFE is a very resistivematerial, but its use in the industry has been widespread due to its good rollable properties.This, however, does not rule out using PTFE as a binder. Mixtures of PTFE with the aqueousbinder and some conductive carbon can be used to create rollable binders. Using the aqueous-based binder can help in achieving a significant fraction of the two-electron capacity withminimal capacity loss over many cvcles. In some embodiments, the binder can be water-based,have superior water retention capabilities, adhesion properties, and help to maintain theconductivity relative to an identical cathode using a PTFE binder instead. Examples of suitablewater-based hydrogels can include, but are not limited to, methyl cellulose (MC),carboxymethyl cellulose (CMC), hydroypropyl cellulose (HPH), hydroypropylmethylcellulose (HPMC), hydroxethylmethyl cellulose (HEMC), carboxymethylhydroxyethylcellulose, hydroxyethyl cellulose (HEC), and combinations thereof. Examples of crosslinkingpolymers include polyvinyl alcohol, polyvinylacelate, polyaniline, polyvinylpyrrolidone,polyvinylidene fluoride, polypyrrole, and combinations thereof. In some embodiments, a 0-10wi. % solution of water-cased cellulose hydrogen can be cross linked with a 0-10 wt.% solutionof crosslinking polymers by, for example, repeated freeze / thaw cycles, radiation treatment,and / or chemical agents (e.g. epichlorohydrin). The aqueous binder may be mixed with 0-5%wt.% PTFE to improve manufacturability. The binder can be present in a concentration ofbetween about 0-10 wt.%.

[0029] The cathode material 2 can also comprise additional elements. The additionalelements can be included in the cathode material including a bismuth compound and / orcopper / copper compounds, which together allow improved galvanostatic battery cycling of thecathode. When present as birnessite, the copper and / or bismuth can be incorporated into thelayered nanostructure of the birnessite. The resulting birnessite cathode material can exhibitimproved cvceling and long term performance with the copper and bismuth incorporated intothe crystal and nanostructure of the birnessite.

[0030] The bismuth or bismuth-based compounds are used to access greater capacity (20-100% of 617 mAh / g) from the manganese dioxide 2" electron capacity. They are used inbatteries where manganese dioxide is usually the layered-phase bimnessite. It is also used inbatteries where the manganese dioxide can be any polymorph and discharging it completely to617 mAh / g and charging it back results in the formation of birnessite. In batteries, whereaccessing 0-100% of 310 mAh / g of the manganese dioxide capacity (e.g., accessing the 1stelectron capacity with a material such as EMD), bismuth or bismuth-based compounds may ormay not be used.

[0031] The bismuth compound can be incorporated into the cathode 12 as an inorganic ororganic salt of bismuth (oxidation states 5, 4, 3, 2, or 1), as a bismuth oxide, or as bismuthmetal (i.e. elemental bismuth). Examples of bismuth compounds include bismuth oxide,bismuth chloride, bismuth bromide, bismuth fluoride, bismuth iodide, bismuth sulfate, bismuthnitrate, bismuth trichloride, bismuth citrate, bismuth telluride, bismuth selenide, bismuthsubsalicylate, bismuth neodecanoate, bismuth carbonate, bismuth subgallate, bismuthstrontium calcium copper oxide, bismuth acetate, bismuth trifluoromethanesulfonate, bismuthnitrate oxide, bismuth gallate hydrate, bismuth phosphate, bismuth cobalt zinc oxide, bismuthsulphite agar, bismuth oxychloride, bismuth aluminate hydrate, bismuth tungsten oxide,bismuth lead strontium calcium copper oxide, bismuth antimonide, bismuth antimony telluride,bismuth oxide viltia stabilized, bismuth-lead alloy, ammonium bismuth citrate, 2-naptholbismuth salt, duchloritri(o-tolyl) bismuth, dichlordiphenyl(p-tolyl)bismuth, ortriphenylbismuth.

[0032] The copper or copper-based compounds are used to access greater capacity (20-100% of 617 mAh / g) from the manganese dioxide 2nd electron capacity. They are used inbatteries where manganese dioxide is usually the layered-phase birnessite. It is also used inbatteries where the manganese dioxide can be any poly morph and discharging it completely to617 mAh / g and charging it back results in the formation of birnessite. Itis desirable to be usedin batteries accessing 20-100% of 617 mAh / g for thousands of cycles as Cu helps in therechargeability and reducing the charge transfer resistance. In batteries, where accessing 0-100% of 310 mAh / g of the manganese dioxide capacity (e.g., accessing the 1% electron capacitywith a material such as EMD), copper or copper-based compounds may or may not be used.The effect of copper is to alter the oxidation and reduction voltages of bismuth. This results ina cathode with full reversibility during galvanostatic cycling, as compared to a bismuth-modified MnO:2 which cannot withstand galvanostatic cycling as well.

[0033] The copper compound can be incorporated into the cathode 12 as an organic orinorganic salt of copper (oxidation states 1, 2, 3, or 4), as a copper oxide, or as copper metal(i.e., elemental copper). The copper compound can be present in a concentration between about1-70 wt.% of the weight of the cathode material 2. In some embodiments, the coppercompound is present in a concentration between about 5-50 wt.% of the weight of the cathodematerial 2. In other embodiments, the copper compound is present in a concentration betweenabout 10-50 wt.% of the weight o[ the cathode material 2. In yet other embodiments, the coppercompound is present in a concentration between about 5-20 wt. % of the weight of the cathodematerial 2. Examples of copper compounds include copper and copper salts such as copperaluminum oxide, copper (I) oxide, copper (I) oxide and / or copper salts in a +1, +2, +3, or +4oxidation state including, but not limited to, copper nitrate, copper sullate, copper chloride, elc.

[0034] The addition of a conductive additive allows higher loadings of MnO: to be usedthal increase gravimetric and volumetric energy density. The conductive additive can bepresent in a concentration between about 1-30 wt.%. Example of a conductive additive includeconductive carbon including single walled carbon nanotubes, multiwalled carbon nanotubes,graphene, carbon blacks of various surface areas, and others that have specifically very highsurface area and conductivity. Higher loadings of the MnO: in the mixed material electrodeare, in some embodiments, desirable to increase the energy density. Other examples ofconductive carbon include TIMREX Primary Synthetic Graphite (all types), TIMREX NaturalFlake Graphite (all types), TIMREX MB, MK, MX, KC, B, LB Grades(examples, KS15,KS44, KC44, MB15, MB25, MK15, MK25, MK44, MX15, MX25, BNB90, LB family)TIMREX Dispersions; ENASCO 150G, 210G, 250G, 260G, 350G, 150P, 250P; SUPER P ,SUPER P Li, carbon black (examples include Ketjenblack EC-300J, Ketjenblack EC-600JD,Ketjenblack EC-600JD powder), acetylene black, carbon nanotubes (single or multi-walled),graphene, graphyne, graphene oxide, Zenyatta graphite and combinations thereof.

[0035] In some embodiments, the conductive additive can have a particle size range fromabout 1 to about 50 microns, or between about 2 and about 30 microns, or between about 5 andabout 15 microns. The total conductive additive mass percentage in the cathode material 2 canrange from about 5% to about 99% or between about 10% to about 80%. In someembodiments, the electroactive component in the cathode material 2 can be between 1 and 99wt. % of the weight of the cathode material 2, and the conductive additive can be between 1 and99 wt.%.

[0036] In some embodiments, the cathode material 2 can also comprise a conductivecomponent. The addition of a conductive component such as metal additives to the cathodematerial 2 may be accomplished by addition of one or more metal powders such as nickelpowder to the cathode material 2. The conductive metal component can be present in aconcentration of between about 0-30 wt.% in the cathode material 2. The conductive metalcomponent may be, for example, nickel, copper, silver, gold, tin, cobalt, antimony, brass,bronze, aluminum, calcium, iron, or platinum. In one embodiment, the conductive metalcomponent is a powder. In some embodiments, the conductive component can be added as anoxide and / or salt. For example, the conductive component can be cobalt oxide, cobalthydroxide, lead oxide, lead hydroxide, or a combination thereol. In some embodiments, asecond conductive metal component is added to act as a supportive conductive backbone forthe first and second electron reactions to take place. The second electron reaction has adissolution-precipitation reaction where Mn3+ ions become soluble in the electrolyte andprecipitate out on the materials such as graphite resulting in an electrochemical reaction andthe formation of manganese hydroxide [Mn(OH)2] which is non-conductive. This ultimatelyresults in a capacity fade in subsequent cycles. Suitable conductive components that can helpto reduce the solubility of the manganese ions include transition metals like Ni, Co, Fe, Ti andmetals like Ag, Au, Al, Ca. Oxides and salts of such metals are also suitable. Transition metalslike Co can also help in reducing the solubility of Mn* ions. Such conductive metalcomponents may be incorporated into the electrode by chemical means or by physical means(e.g. ball milling, mortar / pestle, spex mixture). An example of such an electrode comprises 5-95% bimessite, 35-95% conductive carbon, 0-50% conductive component (e.g., a conductivemetal), and 1-10% binder.

[0037] The cathode material 2 can be formed on a cathode current collector 1, which canbe formed [rom a conductive material that serves as an electrical connection between thecathode material and an external electrical connection or connections. In some embodiments,the cathode current collector 1 can be made from, for example, carbon, lead, nickel, steel (e.g.,stainless steel, etc.), nickel-coated steel, nickel plated copper, tin-coated steel, copper platednickel, silver coated copper, copper, magnesium, aluminum, tin, iron, platinum, silver, gold,titanium, bismuth, titanium, half nickel and half copper, or any combination thereof. In someembodiments, the current collector 1 can comprise a carbon felt or conductive polymer mesh.The cathode current collector 1 may be formed into a mesh (e.g., an expanded mesh, wovenmesh, etc.), perforated metal, foam, foil, felt, fibrous architecture, porous block architecture,perforated foil, wire screen, a wrapped assembly, or any combination thereof. In someembodiments, the current collector can be formed into or form a part of a pocket assembly,where the pocket can hold the cathode material 2 within the cathode current collector 1. A tab(e.g., a portion of the cathode current collector 1 extending outside of the cathode material 2 asshown at the top of the cathode 12 in Figure 1A) can be coupled to the current collector toprovide an electrical connection between an external source and the current collector.

[0038] When the anode comprises zinc, the anode 13 can comprise zinc in the form of Znmetal (100 wt. %), zinc oxide, and / or Zn powder of various morphologies (sphere, fiber, wire,tube, sheet, etc.) and sizes. An anode containing Zn powder as the active material can comprise1-99 wt.% Zn powder, 0-99 wt.% zinc oxide (Zn0) and the remaining wt.% as binder. In someembodiment, the Zn may be present in the anode material 5 in an amount of (rom about 50wt.% to about 90 wt.%, alternatively from about 60 wt.% to about 80 wt.%, or alternatively[rom about 65 w1.% to about 75 wt.%, based on the total weight of the anode material. In someembodiments conductive additives, gas inhibitor(s), and / or complexing additives like lithium,copper (Cu), indium, iron, cadmium, bismuth, aluminum, calcium, oxides thereof, hvdroxidesthereof, or any combination thereof can be added in 1-20 wt.%.

[0039] In some embodiments, the anode material 5 can comprise zine oxide (ZnO), whichmay be present in an amount of from about 5 wt.% to about 20 wt.%, alternatively from about5 wt.% to about 15 wt. %, or alternatively from about 5 wt.% to about 10 wt.%, based on thetotal weight of anode material. As will be appreciated by one of skill in the art, and with thehelp of this disclosure, the purpose of the ZnO in the anode mixture is to provide a source ofZn during the recharging steps, and the zinc present can be converted between zinc and zincoxide during charging and discharging phases.

[0040] In some embodiments, an electrically conductive material may be optionallypresent in the anode material 5 in an amount of from about 5 wt.% to about 20 wt.%,alternatively [rom about 5 wi.% to about 15 w1.%, alternatively [rom about 5 wt1.% to about 10wt.%, or in some aspects between 0% and 10 wt.% based on the total weight of the anodematerial 5. As will be appreciated by one of skill in the art, and with the help of this disclosure,the electrically conductive material can be used in the anode mixture as a conducting agent,e.g.. to enhance the overall electric conductivity of the anode mixture. Non-limiting examplesof electrically conductive material suitable for use can include any of the conductive carbonsdescribed herein such as carbon, graphite, graphite powder, graphite powder flakes, graphitepowder spheroids, carbon black, activated carbon, conductive carbon, amorphous carbon,glassy carbon, and the like, or combinations thereof. The conductive carbons can be used aloneor with the metallic coating or layer. The conductive material can also comprise any of theconductive carbon materials described with respect to the cathode material including, but notlimited to, acetylene black, single walled carbon nanotubes, multi-walled carbon nanotubes,graphene, graphyne, or any combinations thereof (e.g., with or without the metallic coating(s)).

[0041] In some aspects, a conductive metal additive can be included in the anode. Theuse of the conductive metal additive 1s another possibility of increasing conductivity of theelectrode and reducing charge transfer resistance. The conductive metal additive can be presentin a concentration of 0-10 wt.%. The conductive metal additive may be, for example, nickel,copper, silver, gold, brass, bronze, cobalt, nickel-cobalt, nickel-copper, bismuth, bismuth oxideand tin. The conductive metal additive can be plated using electroless plating solution, wherea reducing agent reduces the conductive metal ions in the solution onto the anode mix or Zn orderivatives of Zn. The electroless plating method does not require anv power source or anodeto plate the conductive metal ions. The conductive metal additive can also be added as powdersin their metallic state, as salts or salt-derivatives, and / or as oxides. A combination of two ormore metallic additives can also be used.

[0042] The anode material 5 may also comprise an optional binder. Generally, a binderfunctions to hold the electroactive material particles together and in contact with the currentcollector. The binder can be present in a concentration of 0-10 wt.%. The binders maycomprise water-soluble cellulose-based hydrogels like methyl cellulose (MC), carboxymethylcellulose (CMC), hvdroypropyl cellulose (HPH), hydrovpropylmethyl cellulose (HPMC),hydroxethylmethyl cellulose (HEMC), carboxymethylhydroxyethyl cellulose andhydroxyethyl cellulose (HEC), which were used as thickeners and strong binders, and havebeen cross-linked with good mechanical strength and with conductive polymers like polyvinylalcohol, polyvinylacetate, polyaniline, polyvinylpyrrolidone, polyvinylidene fluoride andpolypvrrole. The binder may also be a cellulose film sold as cellophane. The binder may alsobe PTFE, which is a very resistive material, but its use in the industry has been widespread dueto its good rollable properties. In some embodiments, the binder may be present in anodematerial in an amount of from about 2 wt.% to about 10 wt.%, alternatively from about 2 wt.%to about 7 wt.%, or alternatively from about 4 wt.% to about 6 wt.%, based on the total weightof the anode material 5.

[0043] In some embodiments, the anode material 5 can be used by itself without a separateanode current collector 4, though a tab or other electrical connection can still be provided tothe anode material 5. In this embodiment, the anode material may have the form or architectureof a foil, a mesh, a perforated layer, a foam, a felt, or a powder. For example, the anode cancomprise a metal foil electrode, a mesh electrode, or a perforated metal foil electrode. In someembodiments, the anode 13 can comprise an optional anode current collector 4. The anodecurrent collector 4 can be used with an anode 13, including any of those described with respectto the cathode 12. For example, the anode current collector may be a conductive material, forexample, nickel, nickel-coated steel, tin-coated steel, silver coated copper, copper plated nickel,nickel plated copper, copper or similar material, and the anode current collector may be formedinto an expanded mesh, perforated mesh, foil or a wrapped assembly.

[0044] The rechargeable Zn-anode capable of accessing high DOD from 0-50%comprising of zinc or a derivative of zinc-based compound, coagulant additive, conductiveadditive and binder. The anode comprises of 1-30 wt.% coagulant additive, 0-10 wt.% binder,0-10 wt.% conductive additive and the balance zinc or derivatives of zinc-based compound.

[0045] The coagulant additives can be in the form of substrates, powder additives to theelectrode, and / or as additive to the electrolyte, where it can be activated through anelectrochemical process by passage of a current. Example of electrocoagulants can include,but are not limited to, aluminum, iron, manganese (e.g. MnQO2 and Mn304), titanium (e.g. TiO2),calcium, and / or zirconium as well as the electrolysis products of such elements such as oxides,hydroxides, salts, and the like. The dissolved coagulants generate a number of aqueouscomplex ions that increase the coagulation efficiency. For example, aluminum (Al) in watercan produce various compounds such as Al(OH)2+, Al2(OH)24+, Al6(OH)153+, Al13(OH)345+,Al(H2O)63+, Al(H2O)5OH2+ and Al(H2O)4OH+.

[0046] In some aspects, the coagulant can comprise, but is not limited to, aluminum,aluminum hydroxide, aluminum oxide, aluminum oxinate, aluminum monostearate, aluminumhydroxide hydrate, aluminum silicate, bismuth aluminate hydrate, aluminum titanate,strontium aluminate, lithium aluminate, strontium lanthanum aluminate, sodium aluminate andyttrium aluminum oxide, iron, iron hydroxide, iron hydroxide hydrate, iron oxide, manganeseiron oxide, copper iron oxide, zinc iron oxide, nickel zinc iron oxide, copper zinc iron oxide,barium ferrite, alloys of aluminum and iron, or any combination thereof. In some embodiments,the coagulant can comprise, but is not limited to titanium, calcium, zirconium, hydroxidesthereof, oxides thereof, oxinates thereof, hydrates thereof, and any combination thereof. Forexample, the coagulant can comprise titanium oxide (TiO2), zirconium oxide, calcium oxide,calcium hydroxide, titanium hydroxide, zirconium hydroxide, calcium titanate, orcombinations thereof. The coagulant additive can be present in a concentration of 1-30 wt.%by weight of the anode.

[0047] The cathode and anode materials can be adhered to the current collector by pressingat, for example, a pressure between 1,000 psi and 20,000 psi (between 6.9x10 and 1.4x10%Pascals). The cathode and anode materials may be adhered to the current collector as a paste.A tab of each current collector extends outside of the device and covers less than 0.2% of theelectrode area.

[0048] In some embodiments, a separator 9 can be disposed between the anode 13 and thecathode 12 when the electrodes are constructed into the cell or battery 10. While shown asbeing disposed between the anode 13 and the cathode 12 in Figure 1A, the separator 9 can beused to wrap one or more of the anode 13 and / or the cathode 12, or alternatively one or moreanodes 13 and / or cathodes 12 when multiple anodes 13 and cathodes 12 are present.

[0049] The separator 9 may comprise one or more layers. For example, when the separatoris used, between 1 10 5 layers of the separator can be applied between adjacent electrodes. Theseparator can be formed from a suitable material such as nylon, polyester, polyethylene,polypropylene, poly(letralluoroethylene) (PTFE), poly(vinyl chloride) (PVC), polyvinylalcohol, cellulose, or any combination thereof. Suitable layers and separator forms can include,but are not limited to, a polvmeric separator layer such as a sintered polymer film membrane,polyolefin membrane, a polyolefin nonwoven membrane, a cellulose membrane, a cellophane,a battery-grade cellophane, a hydrophilically modified polyolefin membrane, and the like, orcombinations thereof. As used herein, the phrase "hydrophilically modified" refers to amaterial whose contact angle with water is less than 45°. In another embodiment, the contactangle with water is less than 30°. In yet another embodiment, the contact angle with water isless than 20°. The polyolefin may be modified by, for example, the addition of TRITON X-100 or oxygen plasma treaiment. In some embodiments, the separator 9 can comprise aCELGARD brand microporous separator. In an embodiment, the separator 9 can comprisea FS 2192 SG membrane, which is a polyolefin nonwoven membrane commercially availablefrom Freudenberg, Germany. In some embodiments, the separator can comprise a lithiumsuper ionic conductor (LISICON), sodium super ionic conductions (NASICON), NAFION,a bipolar membrane, water electrolysis membrane, a composite of polyvinyl alcohol andgraphene oxide, polyvinyl alcohol, crosslinked polyvinyl alcohol, or a combination thereof.

[0050] An electrolyte (e.g. an alkaline hydroxide, such as NaOH, KOH, LiOH, or mixturesthereof) can be contained within the free spaces of the electrodes 12, 13, the separator 9, andthe housing 7. The electrolvte may have a concentration of between 5% and 50% w / w. Theelectrolyte can be in the form of a liquid and / or gel. For example, the battery 10 can comprisean electrolyte that can be gelled to form a semi-solid polymerized electrolyte. In someembodiments, the electrolyte can be an alkaline electrolyte. The alkaline electrolyte can be ahydroxide such as potassium hydroxide, sodium hydroxide, lithium hydroxide, ammoniumhydroxide, cesium hvdroxide, or any combination thereof. The resulting electrolyte can havea pH greater than 7, for example between 7 and 15.1. In some embodiments, the pH of theelectrolyte can be greater than or equal to 10 and less than or equal to about 15.13.

[0051] In addition to a hydroxide, the electrolyte can comprise additional components. Insome embodiments, the alkaline electrolyte can have zinc oxide, potassium carbonate,potassium iodide, and / or potassium fluoride as additives. When zinc compounds are presentin the electrolyte, the electrolyte can comprise zinc sulfate, zinc chloride, zinc acetate, zinccarbonate, zinc chlorate, zinc fluoride, zinc formate, zinc nitrate, zinc oxalate, zinc sulfite, zinctartrate, zinc cyanide, zinc oxide, sodium hydroxide, potassium hydroxide, lithium hydroxide,potassium chloride, sodium chloride, potassium (luoride, lithium nitrate, lithium chloride,lithium bromide, lithium bicarbonate, lithium acetate, lithium sulfate, lithium permanganate,lithium nitrate, lithium nitrite, lithium perchlorate, lithium oxalate, lithium {luoride, lithiumcarbonate, lithium bromate, acrylic acid, N.N'-Methvlenebisacrylamide, potassium persulfate,ammonium persulfate, sodium persulfate, or a combination thereof.

[0052] In some embodiments, the electrolyte can be an aqueous solution having an acidicor neutral pH. When the electrolyte is acid, the electrolyte can comprise an acid such as amineral acid (e.g., hydrochloric acid, nitric acid, sulfuric acid, etc.). In some embodiments, theelectrolyte solution can comprise a solution comprising potassium permanganate, sodiumpermanganate, lithium permanganate, calcium permanganate, manganese sulfate, manganesechloride, manganese nitrate, manganese perchlorate, manganese acetate, manganesebis(trilluoromethanesul fonate), manganese trillate, manganese carbonate, manganese oxalate,manganese fluorosilicate, manganese ferrocyanide, manganese bromide, magnesium sulfate,zinc sulfate, zinc triflate, zinc acetate, zinc nitrate, bismuth chloride, bismuth nitrate, nitricacid, sulfuric acid, hydrochloric acid, sodium sulfate, potassium sulfate, sodium hydroxide,potassium hydroxide, titanium sulfate, titanium chloride, lithium nitrate, lithium chloride,lithium bromide, lithium bicarbonate, lithium acetate, lithium sulfate, lithium nitrate, lithiumnitrite, lithium hydroxide, lithium perchlorate, lithium oxalate, lithium fluoride, lithiumcarbonate, lithium sulfate, lithium bromate, or any combination thereof. In some embodiments,the electrolyte can be an acidic or neutral solution, and the pH of the electrolyte can be between0 and 7.

[0053] In some embodiments, the electrolyte can comprise a gassing inhibitor that cancoat on metallic anodes surface and reduce or prevent gas formation. In an embodiment,gassing inhibitors can be used that are mixed in with the electrolyte. Suitable gassing inhibitorscan include. but are not limited to, indium hydroxide, indium, indium oxide, bismuth oxide,bismuth, carboxymethyl cellulose, polyethylene glycol, zinc oxide, cetyltrimethylammoniumbromide, polytetrafluoroethylene, and combinations thereof.

[0054] As noted herein, the coagulants can also be included in the electrolyte rather thanin the anode, and / or the coagulants can be in both the electrolyte and the anode.

[0055] In use, a battery or cell having the coagulants and electrodes as described hereincan be constructed and used as a cell. During cycling of the cell, the coagulants can be formedby the passage of electrical current through the cell. The coagulants can then serve to retainthe zinc reaction products within the proper location within the cell and help to prevent the zincreaction products (e.g.. zincate ions) from migrating in the cell. For example, the coagulantscan help to reduce or prevent the zinc reaction products from migrating to the cathode and / orreallocating within the anode.EXAMPLES

[0056] The embodiments having been generally described, the following examples aregiven as particular embodiments of the disclosure and to demonstrate the practice andadvantages thereof. It is understood that the examples are given bv way of illustration and arenot intended to limit the specification or the claims in any manner.EXAMPLE 1

[0057] The benefit of adding AI(OH)3 as an electrocoagulant to the Zn-anode is shown inFigure 2. In example 1, an electrode is made containing 72.7 wt.% ZnO, 3.6 wt.% Teflon and23.7 wt.% AlI(OH)3. To test the beneficial effect of adding AI(OH)3, a baseline electrode wasmade without containing the electrocoagulant additive and keeping the same binder weightcomposition i.e, 3.6 wt.% Teflon and 96.4 wt.% ZnO. The anodes were paired with Ni(OH):2electrodes in a prismatic cell with vertically aligned electrodes (see Figure 1) containing25wt.% KOH. The baseline electrode was cycled at 1C at ~21% utilization of the Zn theoreticalcapacity (820mAh / g), which it was able to deliver the without capacity [ade for ~200 cyclesand then with constant fade till 450 cycles at which the electrode failed. In comparison, theelectrode containing Al(OH): cycled at the similar conditions was able to deliver the completecapacity till ~320 cycles and then ~17-19% till 1000 cvcles. The slight fade could have beendue to loss of active material from the electrode as a result of Zn dissolution in the electrolyte,which is easy to occur in a design containing vertically aligned electrodes as shown in Figure1A.

[0058] A way to circumvent this issue would be to horizontally align the electrodes asshown in Figure 1B to prohibit the dissolved Zn ions moving away from the electrode surface.An example of this method is shown in Figure 2, where the AI(OH)3 containing electrode,when cycled at similar conditions, is able to deliver the capacity without fade till 600 cycles.The AI(OH)s containing electrode was also cycled at higher Zn utilizations of ~30% and ~50%,where we see that the capacity retention was better than the baseline electrode and any datareported in literature. Typical composition of the electrodes containing AI(OH)s were 72.7wt.% ZnO, 3.6 wt.% Teflon and 23.7 wt.% AI(OH);. The baseline electrodes had acomposition of 96.4 wt.% ZnO and 3.6 wt.% Teflon. The electrodes containing Al(OH); werecycled at different Zn utilizations and compared to the baseline electrode cvcled at ~21% ofthe Zn theoretical capacity of 820mAh / g. The electrode containing the electrocoagulantadditive achieved higher cycle life and better Zn utilizations compared to the baseline.

[0059] Figures 3A, 3B, 3C, and 3D show the potential and current-time characteristics ofthe baseline electrode and the electrode containing Al(OH); cycled at 21% utilization at cycles20, 100, 300 and 500, respectively. Cycles 20, 100, 300 and 500 are shown in Figures 3A, 3B,3C, and 3D, respectively. Figure 3A shows thal at the 20% cycle the potential and curreni-limecharacteristics of both the electrodes are very similar, where they are able to obtain and deliverthe capacity at constant current. In Figure 3B at the 100" cycle we start seeing differencesbetween the electrodes. The baseline electrode hits the voltage limit during charge and entersinto constant voltage mode (~2 hours) to get its capacity. Zinc plates on the anode during thecharging step and, at long constant voltage (CV) times the zinc deposition on the anode isaffected, which leads to an undesirable mossy structure that leads to the ultimate failure of theanode. In comparison we see that the electrode containing AI(OH); obtains almost all of itscapacity on constant current. In Figures 3C and 3D, we see that at the 300% and 500" cycle thebaseline electrodes enter into longer constant voltage times during the charging step. At the500" cycle, almost all of the capacity of the baseline electrode is obtained on constant voltage,which is not a desirable characteristic of any electrode. Longer constant voltage times are alsoindicative of increasing electrode resistance due to the formation of resistive ZnO duringdischarge. These are not seen in the electrodes containing AI(OH)s. The role of AI(OH)s is tocoagulate with the dissolved zinc ions and prevent it from diffusing away from the vicinity ofthe electrode. Also, shorter CV times could be indicative of the presence of Al ions in reducingthe electrode resistance compared to the baseline electrode.EXAMPLE 2

[0060] Figures 4A, 4B, and 4C contain an example of an electrode containing anelectrocoagulant and a conductive metal additive that maintains the high capacity utilizationand energy efficiency of the electrode. Cycle life and potential-time curves are shown inFigures 4A, 4B, and 4C, respectively, to show the effects of Cu. The electrode containing Cuhas a composition of 72.7 wt.% ZnO, 10 wt.% Cu metal powder, 3.6 wt.% Teflon and 13.7wt.% AI(OH);. The baseline electrodes had a composition of 96.4 wt.% ZnO and 3.6 wt.%Teflon. An electrode containing 72.7 wt. % ZnO, 10 wt.% Cu metal powder, 3.6 wt.% Teflonand 13.7 wt.% Al(OH); was made and cycled at 21% utilization at 1C. This electrode wascompared to the electrode containing AI(OH)s and the baseline electrode cycled at the similarconditions. Figure 4A shows that the electrode containing Cu as the conductive metal additivemaintains the capacity utilization near 21% for over 750 cycles. Figures 4B and 4C show thatthe vollage efficiency of the electrode containing Cu is improved al the 300 and 500% cycle,which means that the cell is cycling at a higher energy efficiency. A combination ofelecirocoagulant and metal conductive additives improve the cycling performance of the Znanodes.

[0061] Having described various batteries, systems, and methods, specific aspects caninclude, but are not limited to:

[0062] In a first aspect, a battery comprises: a housing; an electrolyte disposed in thehousing; a cathode disposed in the housing; an anode disposed in the housing and comprisingan anode material comprising: aluminum, iron, titanium, calcium, zirconium, a hydroxidethereof, a salt thereof, an oxide thereof, or a combination thereof; and a binder.

[0063] A second aspect can include the battery of the first aspect, wherein theelectrocoagulant material comprises aluminum, an oxide thereof, a hydroxide thereol, or a saltthereof.

[0064] A third aspect can include the battery of the first aspect, wherein theelectrocoagulant material comprises iron, an oxide thereof, a hydroxide thereof, or a saltthereol.

[0065] A fourth aspect can include the battery of any one of the first to third aspects,wherein the anode further comprises a conductive metal additive, and wherein the conductivemetal additive is copper, a copper salt, nickel, or a nickel salt.

[0066] A fifth aspect can include the battery of the first aspect, wherein the anode furthercomprises an electrocoagulant additive selected from the group consisting of aluminum, analuminum salt; iron, an iron salt, and combinations thereof.

[0067] A sixth aspect can include the battery of the first aspect, wherein theelectrocoagulant additive is aluminum, aluminum hydroxide, aluminum oxide, aluminumoxinate, aluminum monostearate, aluminum hydroxide hydrate, aluminum silicate, bismuthaluminate hydrate, aluminum titanate, strontium aluminate, lithium aluminate, strontiumlanthanum aluminate, sodium aluminate and vttrium aluminum oxide, iron, iron hydroxide,iron hydroxide hydrate, iron oxide, manganese iron oxide, copper iron oxide, zinc iron oxide,nickel zinc iron oxide, copper zinc iron oxide, barium ferrite, an alloy of aluminum and iron,titanium, titanium hydroxide, titanium hydroxide hydrate, titanium oxide, calcium, calciumhydroxide, calcium hydroxide hydrate, calcium oxide, zirconium, zirconium hydroxide,zirconium hydroxide hydrate, zirconium oxide, or a combination thereof.

[0068] A seventh aspect can include the battery of any one of the first to sixth aspects,[urther comprising a conductive metal additive, wherein the conductive metal additive isnickel, copper, silver, gold, brass, bronze, cobalt, nickel-cobalt, nickel-copper, bismuth,bismuth oxide, tin, or a combination thereof.

[0069] An eighth aspect can include the battery of any one of the first to seventh aspects,wherein the binder comprises a polytetrafluoroethyvlene, a cellulose-based hydrogel, or acombination thereof.

[0070] A ninth aspect can include the battery of the eighth aspect, wherein the binder is acellulose-based hydrogel selected from the group consisting of methyl cellulose (MC),carboxymethyl cellulose (CMC), hydroxypropyl cellulose (HPC), hydroxypropylmethylcellulose (HPMC), hvdroxyehtylmethyl cellulose (HEMC), carboxymethylhyvdroxyethylcellulose and hydroxyethyl cellulose (HEC).

[0071] A tenth aspect can include the battery of the eighth aspect, wherein the binder is acellulose-based hydrogel crosslinked with a copolymer selected from the group consisting ofpolyvinyl alcohol, polyvinylacetate, polyaniline, polyvinyvlpyrrolidone, polyvinylidenefluoride, and polypyrrole.

[0072] An eleventh aspect can include the battery of any one of the [irst to tenth aspects,wherein the anode comprises 1-30wt.% of the electrocoagulant material, greater than Owt.%and less than or equal to 10wt.% of a conductive metal additive, and greater than Owt.% andless than or equal to 10wt.% of the binder, and a remainder of the anode as zinc (Zn) or zincoxide (ZnO).

[0073] A twelfth aspect can include the battery of the eleventh aspect, wherein the zinc(Zn) or zinc oxide (ZnO) comprises a gassing inhibitor.

[0074] A thirteenth aspect can include the battery of the twelfth aspect, wherein thegassing inhibitor is bismuth or indium compounds in a concentration greater than 0 ppm andless than 1 wt.%.

[0075] A fourteenth aspect can include the battery of any one of the first to thirteenthaspects, wherein the anode has a porosity between 5-95%.

[0076] A fifteenth aspect can include the battery of any one of the first to fourteenthaspects, wherein the cathode is selected from the group consisting of manganese dioxide(MnO2), copper intercalated birmessite, birnessite, vanadium oxide, alpha-manganese dioxide,nickel oxyhydroxide (NIOOH), nickel hydroxide (Ni(OH)2) silver (Ag), copper (Cu), bromine(Br), and air.

[0077] A sixteenth aspect can include the battery of any one of the first to fifteenth aspects,[urther comprising a current collector [or the cathode or the anode, the current collector selectedfrom the group consisting of a copper mesh, a copper foil, a nickel mesh, a nickel foil, a copperplated nickel mesh or foil, and a nickel-plated copper mesh or foil.

[0078] A seventeenth aspect can include the battery of any one of the first to sixteenthaspects, wherein the anode is formed by pressing electrode material on to a current collector at1000 - 20000 psi.

[0079] An eighteenth aspect can include the battery of any one of the first to seventeenthaspects, wherein the electrolyte comprises an alkaline hydroxide selected from the groupconsisting of sodium hydroxide, potassium hydroxide, cesium hydroxide, rubidium hydroxide,lithium hydroxide, or a combination thereof.

[0080] A nineteenth aspect can include the battery of any one of the first to eighteenthaspects, [urther comprising a polymeric separator between the anode and the cathode.

[0081] In a twentieth aspect, a battery comprises: a housing; an electrolyte disposed in thehousing, wherein the electrolyle comprises an electrocoagulant material selected [rom thegroup consisting of: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, a saltthereof, an oxide thereof, and a combination thereof a cathode disposed in the housing; ananode disposed in the housing and comprising an anode material comprising: zinc or zincoxide; and a binder.

[0082] A twenty first aspect can include the battery of the twentieth aspect, wherein theelectrocoagulant material comprises aluminum, an oxide thereof, a hydroxide thereof, or a saltthereof.

[0083] A twenty second aspect can include the battery of the twentieth aspect, wherein theelectrocoagulant material comprises iron, an oxide thereof, a hydroxide thereof, or a saltthereof.

[0084] In a twenty third aspect, a method of operating a battery comprises: discharging abattery, the battery comprising: a housing; an electrolyte disposed in the housing; a cathodedisposed in the housing; an anode disposed in the housing and comprising an anode materialcomprising: zinc or zinc oxide; an electrocoagulant material selected from the group consistingof: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, a salt thereof, an oxidethereof, and a combination thereof; and a binder; recharging the battery; coagulating one ormore reaction products of the zinc or zinc oxide with the electrocoagulant material; andretaining the one or more reaction products of the zinc or zinc oxide at or near the anode duringthe discharging, recharging, or both using the electrocoagulant material.

[0085] A twenty fourth aspect can include the method of the twenty third aspect, whereinthe electrocoagulant material comprises aluminum, an oxide thereof, a hydroxide thereol; or asalt thereof.

[0086] A twenty fifth aspect can include the method of the twenty third aspect, whereinthe electrocoagulant material comprises iron, an oxide thereof, a hydroxide thereof, or a saltthereof.

[0087] A twenty sixth aspect can include the method of any one of the twenty third totwenty fifth aspects, wherein the anode further comprises a conductive additive, and whereinthe conductive metal additive is copper, a copper salt, nickel, or a nickel salt.

[0088] Embodiments are discussed herein with reference to the Figures. However, thoseskilled in the art will readily appreciate that the detailed description given herein with respectto these figures is for explanatory purposes as the systems and methods extend beyond theselimited embodiments. For example, it should be appreciated that those skilled in the art will,in light of the teachings of the present description, recognize a multiplicity of alternate andsuitable approaches, depending upon the needs of the particular application, to implement thefunctionality of any given detail described herein, beyond the particular implementationchoices in the following embodiments described and shown. That is, there are numerousmodifications and variations that are too numerous to be listed but that all fit within the scopeof the present description. Also, singular words should be read as plural and vice versa andmasculine as feminine and vice versa, where appropriate, and alternative embodiments do notnecessarily imply that the two are mutually exclusive.

[0089] It is to be further understood that the present description is not limited to theparticular methodology, compounds, materials, manufacturing techniques, uses, andapplications, described herein, as these may vary. It is also to be understood that theterminology used herein is used for the purpose of describing particular embodiments only,and is not intended to limit the scope of the present systems and methods. It must be noted thatas used herein and in the appended claims (in this application, or any derived applicationsthereof), the singular forms "a," "an," and "the" include the plural reference unless the contextclearly dictates otherwise. Thus, for example, a reference to "an element" is a reference to oneor more elements and includes equivalents thereof known to those skilled in the art. Allconjunctions used are to be understood in the most inclusive sense possible. Thus, the word"or" should be understood as having the definition of a logical "or" rather than that of a logical"exclusive or" unless the context clearly necessitates otherwise. Structures described hereinare to be understood also to refer to functional equivalents of such structures. Language thatmay be construed to express approximation should be so understood unless the context clearlydictates otherwise.

[0090] Unless defined otherwise, all technical and scientific terms used herein have thesame meanings as commonly understood by one of ordinary skill in the art to which thisdescription belongs. Preferred methods, techniques, devices, and materials are described,although any methods, techniques, devices, or materials similar or equivalent to those describedherein may be used in the practice or testing of the present systems and methods. Structuresdescribed herein are to be understood also to refer to functional equivalents of such structures.The present systems and methods will now be described in detail with reference toembodiments thereof as illustrated in the accompanying drawings.

[0091] From reading the present disclosure, other variations and modifications will beapparent to persons skilled in the art. Such variations and modifications may involve equivalentand other features which are already known in the art, and which may be used instead of or inaddition to [eatures already described herein.

[0092] Although Claims may be formulated in this Application or of any furtherApplication derived therefrom, to particular combinations of features, it should be understoodthat the scope of the disclosure also includes any novel feature or any novel combination offeatures disclosed herein either explicitly or implicitly or any generalization thereof, whetheror not it relates to the same systems or methods as presently claimed in any Claim and whetheror not it mitigates any or all of the same technical problems as do the present systems andmethods.

[0093] Features which are described in the context of separate embodiments may also beprovided in combination in a single embodiment. Conversely, various features which are, forbrevity, described in the context of a single embodiment, may also be provided separately orin any suitable sub-combination. The Applicants hereby give notice that new claims may beformulated to such features and / or combinations of such features during the prosecution of thepresent Application or of any further Application derived therefrom.

Claims

1. A battery comprising: a housing; an electrolyte disposed in the housing; a cathode disposed in the housing; an anode disposed in the housing and comprising an anode material comprising: zing or zinc oxide; an electrocoagulant material selected from the group consisting of: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, a salt thereof, an oxide thereof, or a combination thereof: and a binder.

2. The battery of claim 1, wherein the electrocoagulant material comprises aluminum, an oxide thereof, a hydroxide thereof, or a salt thereof.

3. The battery of claim 1, wherein the electrocoagulant material comprises iron, an oxide thereof, a hydroxide thereof, or a salt thereof.

4. The battery of claim 1, wherein the anode further comprises a conductive metal additive, and wherein the conductive metal additive is copper, a copper salt, nickel, or anickel salt.

5. The battery of claim 1, wherein the electrocoagulant additive is aluminum, aluminum hydroxide, aluminum oxide, aluminum oxinate, aluminum monostearate, aluminum hydroxide hydrate, aluminum silicate, bismuth aluminate hydrate, aluminum titanate, strontium aluminate, lithium aluminate, strontium lanthanum aluminate, sodium aluminate and yttrium aluminum oxide, iron, iron hydroxide, iron hydroxide hydrate, iron oxide, manganese iron oxide, copper iron oxide, zinc iron oxide, nickel zinc iron oxide, copper zinc iron oxide, barium ferrite, an alloy of aluminum and iron, titanium, titanium hydroxide, titanium hydroxide hydrate, titanium oxide, calcium, calcium hydroxide, calcium hydroxide hydrate, calcium oxide, zirconium, zirconium hydroxide, zirconium hydroxide hydrate, zirconium oxide, or a combination thereof.

6. The battery of claim 1, further comprising a conductive metal additive, wherein the conductive metal additive is nickel, copper, silver, gold, brass, bronze, cobalt, nickel- cobalt, nickel-copper, bismuth, bismuth oxide, tin, or a combination thereof.

7. The battery of claim 1, wherein the binder comprises a polytetrafluoroethylene, a cellulose-based hydrogel, or a combination thereof.

8. The battery of claim 7, wherein the binder is a cellulose-based hydrogel selected from the group consisting of methyl cellulose (MC). carboxymethyl cellulose (CMC), hydroxypropyl cellulose (HPC), hydroxypropylmethyl cellulose (HPMCQ), hydroxyehtylmethyl cellulose (HEMC), carboxymethylhydroxyethyl cellulose and hydroxyethyl cellulose (HEC).

9. The battery of claim 7, wherein the binder is a cellulose-based hydrogel crosslinked with a copolymer selected from the group consisting of polyvinyl alcohol, polyvinylacetate, polyaniline, polyvinylpyrrolidone, polyvinylidene fluoride, and polypyrrole.

10. The battery of claim 1, wherein the anode comprises 1-30 wt.% of the electrocoagulant material, greater than 0 wt.% and less than or equal to 10 wt. % of a conductive metal additive, and greater than 0 w1.% and less than or equal to 10 w1.% of the binder, and a remainder of the anode as zinc (Zn) or zinc oxide (ZnO).

11. The battery of claim 10, wherein the zinc (Zn) or zinc oxide (ZnO) comprises a gassing inhibitor.

12. The battery of claim 11, wherein the gassing inhibitor is bismuth or indium compounds in a concentration greater than 0 ppm and less than 1 wt.%.

13. The battery of claim 1, wherein the anode has a porosity between 5-95%.

14. The battery of claim 1, wherein the cathode is selected from the group consisting of manganese dioxide (MnQz), copper intercalated birnessite, birnessite, vanadium oxide, alpha-manganese dioxide, nickel oxyhydroxide (NiOOH), nickel hydroxide (Ni{(OH)z2) silver (Ag), copper (Cu), bromine (Br), and air.

15. The battery of claim 1, [urther comprising a current collector [or the cathode or the anode, the current collector selected from the group consisting of a copper mesh, a copper [oil, a nickel mesh, a nickel (oil, a copper plated nickel mesh or (oil, and a nickel-plated copper mesh or foil.

16. The battery of claim 1, wherein the electrolyte comprises an alkaline hydroxide selected from the group consisting of sodium hydroxide, potassium hydroxide, cesium hydroxide, rubidium hydroxide, lithium hydroxide or a combination thereof.

17. The battery of claim 1, further comprising a polymeric separator between the anode and the cathode.

18. A battery comprising: ahousing; an electrolyte disposed in the housing, wherein the electrolyte comprises an electrocoagulant material selected from the group consisting of: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, a salt thereof, an oxide thereof, and a combination thereof, a cathode disposed in the housing; an anode disposed in the housing and comprising an anode material comprising: zinc or zinc oxide; and a binder.

19. The battery of claim 18, wherein the electrocoagulant material comprises aluminum, an oxide thereof, a hydroxide thereof, or a salt thereof.

20. The battery of claim 18, wherein the electrocoagulant material comprises iron, an oxide thereof, a hydroxide thereof, or a salt thereof.

21. A method of operating a battery, the method comprising: discharging a baltlery, the ballery comprising: a housing; an electrolyte disposed in the housing; a cathode disposed in the housing; an anode disposed in the housing and comprising an anode material comprising: zinc or zinc oxide; an electrocoagulant material selected from the group consisting of: aluminum, iron, titanium, calcium, zirconium, a hydroxide thereof, a salt thereof, an oxide thereof, and a combination thereof ; and a binder; recharging the battery; coagulating one or more reaction products of the zinc or zinc oxide with the electrocoagulant material; and retaining the one or more reaction products of the zinc or zinc oxide at or near the anode during the discharging, recharging, or both using the electrocoagulant material.

22. The method of claim 21, wherein the electrocoagulant material comprises aluminum, an oxide thereof, a hydroxide thereof, or a salt thereof.

23. The method of claim 21, wherein the electrocoagulant material comprises iron, an oxide thereof, a hydroxide thereof, or a salt thereof.

24. The method of claim 21, wherein the anode [urther comprises a conductive additive, and wherein the conductive metal additive is copper, a copper salt, nickel, or a nickel salt.