Method for enhancing supercapacitor performance using nickel foam as active material source and current collector

IN603273BActive Publication Date: 2026-09-21INDIAN INSTITUTE OF TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202511010133
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Filing Date
2025-02-06
Publication Date
2026-09-21
Estimated Expiration
2045-02-06

AI Technical Summary

Technical Problem

The energy density of supercapacitors is limited by traditional electrode materials and inefficient ion diffusion, and the use of binders to attach active materials to current collectors increases internal resistance and reduces the active surface area.

Method used

A novel binder-free approach is used where nickel foam serves as both the current collector and active material, directly integrating nickel cobalt layered double hydroxide (NiCoLDH) to enhance electron and ion transport, eliminating the need for binders and optimizing the synthesis process.

Benefits of technology

This method improves capacitance, energy density, and power density of supercapacitors by maximizing ion-accessible surface area and reducing resistance, making them more efficient and cost-effective for energy storage applications.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention discloses an innovative and efficient method for fabricating high-performance, binder-free supercapacitor electrodes. The method utilizes a hydrothermal process with cobalt precursors, and Nickel Cobalt Layered Double Hydroxide (NiCoLDH) is grown in-situ on the Ni foam, eliminating the need for binders or external material deposition. This approach leverages the intrinsic properties of NiCoLDH, including its high theoretical capacitance, exceptional redox activity, and layered flexibility. The unique integration of Ni foam as the current collector and the source of nickel to synthesize NiCoLDH enhances electrochemical performance by optimizing interfacial contact, reducing resistance, and improving the ion transport. The resulting electrodes demonstrate remarkable capacitance, energy density, and power density, offering a scalable, cost-effective, and sustainable solution for advanced energy storage applications.
Need to check novelty before this filing date? Find Prior Art

Description

FIELD OF THE INVENTION:The present invention generally relates to the field of supercapacitor electrodes. Thepresent invention particularly relates to an innovative and efficient method forfabricating high-performance, binder-free supercapacitor electrodes, where nickel foam(Ni-foam) serves both as the structural current collector and as the active material.BACKGROUND OF THE INVENTION:Energy storage devices, particularly supercapacitors, have garnered substantial interestdue to their high power density, rapid charge-discharge capabilities, and long cycle life.These features make them suitable for a variety of applications, including portableelectronics, electric vehicles, and renewable energy systems. However, despite theirpromising performance, the energy density of supercapacitors remains limited by theelectrode materials and inefficient ion diffusion.Recent advances in energy storage have focused on improving electrode materials toovercome these limitations, with particular emphasis on enhancing both energy andpower densities. M. Aulice Scibioh et al. in document titled "Electrode materials forsupercapacitors" published in Materials for Supercapacitor Applications, 2020, 35-204,discusses that supercapacitors are also known as ultracapacitors or electrochemicalcapacitors, having other advantages compared to batteries. Performance comparisonreveals that supercapacitor devices exhibit significantly lower energy storage capabilitycompared to existing commercial batteries. The energy density of commercialsupercapacitor cells is limited to 10 Wh kg-1 whereas that of common lead acid batteriesreaches 35-40 Wh kg-1, while lithium-ion batteries exhibit values higher than100 Wh kg-1 . As supercapacitors are characterized by fast discharge rates and minimummaintenance requirements, these are in demand for frequency regulation applications,apart from their applications in the fields of power electronics, large scale transportsystems, energy storage at intermittent power generations, such as wind mills, solar, andtidal renewable technologies.NiCoLDH are considered highly promising for supercapacitor electrodes due to theirhigh theoretical capacitance, excellent redox activity, and 2D layered structure. The sameis discussed in Chen, X., Zhang, Z., Zhou, S., Wei, Y., Han, S., Jiang, J. (2024). In-situgrowth transformation and oxygen vacancy synergistic modulation of the electronicstructure of NiCo-LDH enables high-performance hybrid supercapacitors. AppliedEnergy, 371, 123670.The synergy between nickel and cobalt enhances electron transfer and electrochemicalperformance. The same is discussed in Zheng, X., Gu, Z., Hu, Q., Geng, B., Zhang, X.(2015). Ultrathin porous nickel-cobalt hydroxide nanosheets for high-performancesupercapacitor electrodes. RSC Advances, 5, 17007-17013.The unique 2D layered structure of NiCoLDH facilitates effective ion diffusion andcharge storage, making it ideal for energy storage applications. This structure allows foreasy ion penetration, which is crucial for achieving high performance in energy storagesystems, particularly under high-power discharge conditions. The same is discussed inWang, S., Jiang, W., Fei, L., Yang, X., Huang, Z., Deng, H., Zhang, X., Gu, H., Hu, Y.(2022). Unveiling the synergistic effect of cobalt ion in nickel-cobalt layered doublehydroxide for electrochemical energy storage: Experimental and computationalapproaches. Electrochimica Acta, 423, 140547.Traditionally, electrode fabrication requires binders to attach the active material to thecurrent collector, but this adds internal resistance and reduces the active surface areaavailable for ion diffusion. The need for binders significantly impacts the overallefficiency of supercapacitors, as it can limit ion access to the electrode material andhinder performance. The same is discussed in Zhang, N., Wang, M., Quan, Y., Li, X.,Hu, X., Yan, J., Wang, Y., Sun, M., Li, S. (2025). A review of binder-free electrodes foradvanced supercapacitors. Journal of Industrial and Engineering Chemistry, 141, 1-31.Accordingly, a binder-free approach is highly desirable, where the active material isdirectly integrated with the current collector, thereby maximizing electrochemicalperformance. Ni-Foam, with its three-dimensional porous structure and high surfacearea, serves not only as a current collector but can also be used as a precursor for nickelin the synthesis of NiCoLDH. By utilizing Ni foam both as the current collector and thenickel source, the electrode fabrication process is simplified, eliminating the need forbinders and external coatings. This integration not only improves interfacial contactbetween the active material and current collector but also enhances electron and iontransport. This results in a maximized ion-accessible surface area, ultimately improvingcapacitance, energy storage capacity, and the overall electrochemical performance of thesupercapacitor.OBJECTIVES OF THE INVENTION:The objective of the present invention is to provide a novel synthesis approach forhigh-performance supercapacitor electrodes, utilizing Ni-Foam not only as the currentcollector but also as the active material.Another objective of this invention is to significantly enhance electrochemical propertiesby directly growing NiCoLDH on Ni-Foam, thereby improving capacitance, energydensity, and power density, ensuring superior performance in energy storageapplications.Another objective of this invention is to streamline the electrode fabrication process byleveraging Ni-Foam as the direct source of nickel for NiCoLDH synthesis, eliminatingthe complexities of multi-step coating and deposition processes commonly used inconventional methods.SUMMARY OF THE INVENTION:The present invention addresses key challenges in the development of high-performancesupercapacitors by proposing a novel binder-free approach for synthesizing NiCoLDHdirectly on Ni-foam. This method eliminates the need for traditional binders, which oftencompromise energy storage capacity, surface area, and overall electrochemicalperformance. By utilizing Ni-Foam not only as the current collector but also as theprecursor for nickel in the synthesis of NiCoLDH, this research focuses on increasing thecapacitance and hence thereby increasing the energy and power density of the electrodematerial.The present invention compares two distinct synthesis methods: (1) NiCoLDHsynthesized directly onto Ni-Foam using it as both current collector and active materialfor nickel, and (2) a dual-salt approach where nickel and cobalt salts are used to formNiCoLDH with Ni-Foam acting only as the current collector. The resulting electrodesdemonstrate improved capacitance, energy density, and power density, highlighting theadvantages of directly using Ni foam as active material to synthesize NiCoLDH overtraditional methods.Specifically, the present invention discloses a method for fabricating high-performance,binder-free supercapacitor electrodes. Wherein, the method comprises preparation ofNi(OH)2 precursor from Ni-foam, followed by synthesis of nickel cobalt layered doublehydroxides (NiCoLDH) arrays from Ni(OH)2 precursor, Co(NO3)2.6H2O, and urea,wherein nickel cobalt layered double hydroxides (NiCoLDH) arrays act as asupercapacitor positive electrode. Then preparing an activated carbon (AC) material asnegative electrode, followed by preparing a supercapacitor device by hybridizing thenickel cobalt layered double hydroxides (NiCoLDH) arrays with Activated Carbon (AC).In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, the preparation of Ni(OH)2precursor comprises cutting Ni-foam into small Ni-foam pieces having a size in a rangeof 1x1 cm to 5x5 cm, followed by cleaning the small Ni-foam pieces with HCl solutionto get cleaned Ni-foam pieces, then washing the cleaned Ni-foam pieces with absoluteethanol for 10 to 20 minutes and deionized water for 10 to 20 minutes to obtain thewashed Ni-foam pieces. Placing the washed Ni-foam pieces in sealed glass vials for 20to 28 hours, immersing the washed Ni-foam pieces in a mixture of NaOH and(NH4)2S2O8 at room temperature for 10 to 20 hours, and rinsing the washed Ni-foampieces in distilled water, followed by vacuum-drying at 140 to 160°C for 5 to 7 hours toprepare the Ni(OH)2 precursor.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, synthesis of nickel cobaltlayered double hydroxides (NiCoLDH) Arrays comprises dissolving Co(NO3)2.6H2O indistilled water to obtain a first solution, followed by adding urea in the first solution andstirring the first solution at room temperature for 20 minutes to form a pink solution.Then immersing Ni(OH)2 precursor in the pink solution and subjecting Ni(OH)2precursor to hydrothermal treatment at 120 to 140°C for 12 to 18 hours, followed bycooling the pink solution at room temperature to obtain the nickel cobalt layered doublehydroxides (NiCoLDH) array samples, followed by washing the NiCoLDH arraysamples with deionized water. Finally, vacuum-drying the NiCoLDH array samplesovernight at 60 to 80°C and labelling the NiCoLDH array samples based on theconcentration of cobalt nitrate used.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, the Activated Carbon (AC)material is prepared from cotton material through a process comprising of washing thecotton material with a soap solution to remove impurities, followed by rinsing withdeionized water to obtain a washed cotton material. Then drying the washed cottonmaterial in a vacuum oven at 50 to 80°C for 12 to 24 hours to obtain a dry cottonmaterial, followed by placing the dry cotton material in a tube furnace and stabilizing thedry cotton material in air at 220 to 300°C for 1 to 2 hours. Then carbonizing the drycotton material at a temperature in a range of 800 to 1100°C at a rate of 5°C / min under anitrogen atmosphere for 1 to 2 hours to obtain a carbonized cotton (CC). Then soakingthe carbonized cotton (CC) in a solution of KOH and distilled water for 30 minutes,followed by heating at 5°C / min at a temperature in a range of 800 to 1000°C for 1 to 2hours to obtain the activated carbon (AC) material. Followed by washing the activatedcarbon (AC) material with 1M HCl to neutralize residual KOH, followed by rinsing theactivated carbon (AC) with deionized water, and drying at 60 to 80°C for 24 to 48 hoursin a vacuum oven.This binder-free approach improves the interfacial contact between the active materialand current collector, thereby reducing the resistance and enhancing overallelectrochemical performance. The innovation results in a more efficient, cost-effective,and scalable solution for high-performance supercapacitors, with applications in energystorage systems requiring rapid charge-discharge capabilities, and high energy and powerdensity.BRIEF DESCRIPTION OF THE DRAWINGS:The drawings provided here are intended solely for illustrative purposes, showcasingselected embodiments, and do not encompass all possible implementations. They are notmeant to restrict the scope of the present disclosure. Additional objectives andadvantages of this invention will become clearer from the following description, whichshould be reviewed in conjunction with the accompanying drawings.Figure 1 illustrates a schematic diagram for synthesis process of NiCoLDH nanoneedles.Figure 2 illustrates FESEM images of (a-c) NiCoLDH-7.5mM; (d-f) NiCoLDH-10mM;(g-i) NiCoLDH-12.5mM; (j-l) DS-NiCoLDH-10mM.Figure 3 illustrates (a) EDX elemental mapping images showing the distribution of Ni,Co, and O in NiCoLDH-10mM; (b-d) TEM images of NiCoLDH-10mM nanoneedlescaptured at different resolutions; (e-g) High-resolution transmission electron microscopy(HRTEM) images and (h) the corresponding selected area electron diffraction (SAED)patterns of NiCo-LDH-10mM.Figure 4 illustrates (a) XRD patterns of NiCoLDH synthesized at 7.5mM, 10mM, and12mM concentrations, as well as DS-NiCoLDH-10mM. (b) Raman spectra of NiCoLDH(7.5mM, 10mM, and 12mM) and DS-NiCoLDH-10mM samples (c) XPS survey spectra;High-Resolution Spectrum of (d) Ni 2p, (e) Co 2p, and (f) O 1s high-resolution ofNiCoLDH-10mM.Figure 5 illustrates (a) CV curves at 5 mV / s; (b) GCD curves at 1 mA cm-2; (c)Impedance curves of NiCoLDH at 7.5mM, 10mM, 12mM concentrations, andDS-NiCoLDH-10mM; (d) CV curves at different scan rates (2-200 mV s-1); (e) GCD curvesof NiCoLDH-10mM electrode at different current densities (1-10 mA cm-2); and (f)Comparison of areal capacitance of different electrodes.Figure 6 illustrates (a) CV curves at 50 mV / s; and (b) GCD curves at 1 mA cm-2 ofNiCo-LDH-10mM / / AC ASC under different voltage windows; (c) CV curves at differentscan rates (2-200 mV s-1); and (d) GCD curves at different current densities (1-10 mAcm-2) of NiCo-LDH-10mM / / AC ASC; (e) CV curves at different scan rates (2-200 mVs-1); and (f) GCD curves at different current densities (1-10 mA cm-2) of NiCo-LDH10mM / / Zn ASC.It will be understood by one skilled in the art, upon reviewing this disclosure, that theexamples presented in the figures are not necessarily to scale. Certain features orcomponents may have been exaggerated, reduced, or altered to better highlight keyaspects and facilitate a clearer understanding of the disclosed concepts and examples.Additionally, the use of shading, patterns, dashed lines, or similar elements in the figuresis not intended to represent any specific material or orientation unless explicitly indicatedin the context.DETAILED DESCRIPTION OF THE INVENTION:The following description outlines the preferred embodiment of the present invention. Itshould be understood that the invention is not confined to the specific embodimentsillustrated, as various modifications and alternatives may be included within the scope ofthe invention. Therefore, this description is intended to be illustrative rather thanrestrictive. Although the invention may be subject to various changes and alternativeconstructions, it is not the intent to limit it to the specific form presented. On thecontrary, the invention aims to encompass all modifications, alternative constructions,and equivalents that fall within the spirit and scope of the claims. In any embodimentdescribed herein, terms like "comprising," "comprises," and similar phrases (which areequivalent to "including," "having," or "characterized by") can be replaced with morerestrictive terms such as "consisting essentially of" or "consists of," depending on thecontext. Additionally, the singular forms "a," "an," and "the" are intended to encompassboth singular and plural meanings, unless otherwise explicitly stated.The present invention discloses a method for enhancing supercapacitor performanceusing nickel foam as an active material source and current collector. Specifically, thepresent invention discloses a method for the synthesis of NiCoLDH using Ni foam as thesource of nickel and the current collector. Additionally, the present invention discloses amethod for the synthesis of a variant of NiCoLDH (DS-NiCoLDH) from a dual salt (DS)of nickel and cobalt, which was also treated directly on Ni foam. This dual approach i.e.one using Ni foam as both the precursor and current collector, and the other employingnickel salt for NiCoLDH formation, provides a valuable comparison to evaluate theimpact of different synthesis methods on the electrochemical performance ofNiCoLDH-based supercapacitors. The comparison allows for a comprehensive understanding ofhow the choice of synthesis route influences factors such as ion accessibility, resistance,and overall energy storage capabilities.In the present invention, the binder-free, direct integration method of NiCoLDH on Nifoam presents a promising approach for developing high-energy-densitysupercapacitors. By eliminating binders and optimizing the synthesis method, thisinvention enhances electrochemical performance. The present approach offers significantpotential for advancing energy storage technology and contributes to the development ofmore efficient supercapacitors for next-generation energy storage devices.In an important embodiment, the present invention provides a method for enhancingsupercapacitor performance by preparing nickel cobalt layered double hydroxides,wherein the method comprises preparation of Ni(OH)2 precursor from Ni-foam andpreparation of nickel cobalt layered double hydroxides from group of materials selectedfrom Co(NO3)2.6H2O, urea, Ni(OH)2@Ni-foam.Specifically, the present invention discloses a method for fabricating high-performance,binder-free supercapacitor electrodes. Wherein, the method comprises preparation ofNi(OH)2 precursor from Ni-foam, followed by synthesis of nickel cobalt layered doublehydroxides (NiCoLDH) arrays from Ni(OH)2 precursor, Co(NO3)2.6H2O, and urea,wherein nickel cobalt layered double hydroxides (NiCoLDH) arrays act as asupercapacitor positive electrode. Then preparing an activated carbon (AC) material asnegative electrode, followed by preparing a supercapacitor device by hybridizing thenickel cobalt layered double hydroxides (NiCoLDH) arrays with Activated Carbon (AC).In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, the preparation of Ni(OH)2precursor comprises cutting Ni-foam into small Ni-foam pieces having a size in a rangeof 1x1 cm to 5x5 cm, followed by cleaning the small Ni-foam pieces with HCl solutionto get cleaned Ni-foam pieces, then washing the cleaned Ni-foam pieces with absoluteethanol for 10 to 20 minutes and deionized water for 10 to 20 minutes to obtain thewashed Ni-foam pieces. Placing the washed Ni-foam pieces in sealed glass vials for 20to 28 hours, immersing the washed Ni-foam pieces in a mixture of NaOH and(NH4)2S2O8 at room temperature for 10 to 20 hours, and rinsing the washed Ni-foampieces in distilled water, followed by vacuum-drying at 140 to 160°C for 5 to 7 hours toprepare the Ni(OH)2 precursor.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, cleaning of the smallNi-foam pieces is done by immersing the small Ni-foam pieces in an ultrasonic bath for 20to 40 minutes to remove the oxide layer, wherein the ultrasonic bath contains 3 M HClsolution.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, the mixture of NaOH and(NH4)2S2O8 comprises 3M NaOH and 1M (NH4)2S2O8 having a volume percentage ratioof 2:1.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, synthesis of nickel cobaltlayered double hydroxides (NiCoLDH) Arrays comprises dissolving Co(NO3)2.6H2O indistilled water to obtain a first solution, followed by adding urea in the first solution andstirring the first solution at room temperature for 20 minutes to form a pink solution.Then immersing Ni(OH)2 precursor in the pink solution and subjecting Ni(OH)2precursor to hydrothermal treatment at 120 to 140°C for 12 to 18 hours, followed bycooling the pink solution at room temperature to obtain the nickel cobalt layered doublehydroxides (NiCoLDH) array samples, followed by washing the NiCoLDH arraysamples with deionized water. Finally, vacuum-drying the NiCoLDH array samplesovernight at 60 to 80°C and labelling the NiCoLDH array samples based on theconcentration of cobalt nitrate used.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, Co(NO3)2.6H2O isdissolved in distilled water at concentrations of 7.5 mM, 10 mM, and 12.5 mM.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, urea and cobalt nitrate arein a weight percentage ratio of 2:1.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, the Activated Carbon (AC)material is prepared from cotton material through a process comprising of washing thecotton material with a soap solution to remove impurities, followed by rinsing withdeionized water to obtain a washed cotton material. Then drying the washed cottonmaterial in a vacuum oven at 50 to 80°C for 12 to 24 hours to obtain a dry cottonmaterial, followed by placing the dry cotton material in a tube furnace and stabilizing thedry cotton material in air at 220 to 300°C for 1 to 2 hours. Then carbonizing the drycotton material at a temperature in a range of 800 to 1100°C at a rate of 5°C / min under anitrogen atmosphere for 1 to 2 hours to obtain a carbonized cotton (CC). Then soakingthe carbonized cotton (CC) in a solution of KOH and distilled water for 30 minutes,followed by heating at 5°C / min at a temperature in a range of 800 to 1000°C for 1 to 2hours to obtain the activated carbon (AC) material. Followed by washing the activatedcarbon (AC) material with 1M HCl to neutralize residual KOH, followed by rinsing theactivated carbon (AC) with deionized water, and drying at 60 to 80°C for 24 to 48 hoursin a vacuum oven.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, the cotton material is awaste cotton material.In an embodiment, the present invention discloses a method for fabricatinghigh-performance, binder-free supercapacitor electrodes, wherein, the KOH and carbonizedcotton (CC) are in a ratio of 4:1.In a preferred embodiment the preparation of Ni(OH)2 precursor comprisescutting Ni-foam into 3x3 cm pieces, then cleaning the Ni-foam pieces by immersing in a3 M HCl solution using an ultrasonic bath for 20-40 minutes to remove the oxide layer.Washing the cleaned Ni-foam pieces with absolute ethanol and deionized water for 10-20 minutes, followed by keeping the obtained washed and cleaned Ni-foam pieces insealed glass vials for 20-28 hours. Immersing the washed and cleaned Ni-foam pieces ina mixture of 20 mL 3M NaOH and 10 mL 1M (NH4)2S2O8 at room temperature for 10-20 hours. Rinsing the obtained Ni-foam pieces with water, followed by vacuum drying at140-160°C for 5-7 hours to prepare the Ni(OH)2 precursor.In another preferred embodiment the preparation of nickel cobalt layered doublehydroxides comprises preparation of NiCoLDH and DS-NiCoLDH.In another preferred embodiment the NiCoLDH is prepared by a process comprisingsteps of dissolving Co(NO3)2.6H2O in distilled water at concentrations of 7.5 mM, 10mM, and 12.5 mM and adding Urea at twice the concentration of Co(NO3)2.6H2O,followed by stirring the obtained solution at room temperature for 20 minutes to form apink solution. Immerging the Ni(OH)2-coated Ni-foam in the pink solution andsubjecting to hydrothermal treatment at a temperature in a range of 120-140°C for 12-18hours, cooling the obtained samples at room temperature followed by washing theobtained samples thrice with deionized water. Followed by vacuum drying the obtainedsamples overnight at 60-80°C, and labelling the obtained samples NiCoLDH-7.5mM,NiCoLDH-10mM, and NiCoLDH-12.5mM, based on the concentration of cobalt nitrateused.In another preferred embodiment the DS-NiCoLDH is prepared by a process comprisingsteps of dissolving 10 mM Co(NO3)2.6H2O, 20 mM Ni(NO3)2.6H2O, and 20 mmol ureain 40 mL distilled water and stirred the obtained solution at room temperature for 15-25minutes to form a light pink solution. Immersing the Ni-foam in the obtained solutionwithin a Teflon-lined stainless-steel autoclave, sealing and heating at 110-150°C for 10-20 hours. Cooling the obtained samples at room temperature followed by washing theobtained samples thrice with deionized water, vacuum drying the obtained samplesovernight at 60-80°C, and labelling the obtained sample as DS-NiCoLDH-10mM.Chemicals: The chemicals used in this study were sourced from reputable suppliers:Ammonium Persulfate [(NH4)2S2O8], Hydrochloric Acid (HCl), and Sodium Hydroxide(NaOH) were procured from Merck; Cobalt Nitrate Hexahydrate [Co(NO3)2.6H2O], Zincacetate dihydrate [Zn(CH3COO)2.2H2O], and Nickel Nitrate Hexahydrate[Ni(NO3)2.6H2O] were obtained from Sigma-Aldrich; Ni-Foam and Zinc foil weresupplied by Nanoshel; Urea (CH4N2O) was purchased from CDH.Preparation of Ni(OH)2 Precursor: Ni-foam was cut into 3x3 cm pieces and cleanedby immersion in a 3 M HCl solution using an ultrasonic bath for 20-40 minutes toremove the oxide layer. Following this, the foam was washed with absolute ethanol anddeionized water for 10-20 minutes each. It was then left in sealed glass vials for 20-28hours. The cleaned foam was immersed in a mixture of 20 mL 3M NaOH and 10 mL 1M(NH4)2S2O8 at room temperature for 10-20 hours. Afterward, the foam was rinsed andvacuum-dried at 140-160°C for 5-7 hours to prepare the Ni(OH)2 precursor.Preparation of NiCoLDH Arrays: To make NiCoLDH solution, Co(NO3)2.6H2O wasdissolved in distilled water at concentrations of 7.5 mM, 10 mM, and 12.5 mM. Ureawas added at twice the concentration of cobalt nitrate. The solutions were stirred at roomtemperature for 20 minutes to form a pink solution. The Ni(OH)2-coated Ni-foam wasthen immersed in the solution and subjected to hydrothermal treatment at 120-140°C for12-18 hours. On natural cooling, the samples were washed thrice with deionized water,vacuum-dried overnight at 60-80°C, and labelled as NiCoLDH-7.5mM, NiCoLDH-10mM,and NiCoLDH-12.5mM, based on the concentration of cobalt nitrate used.Preparation of DS-NiCoLDH: To prepare DS-NiCoLDH, 10 mM Co(NO3)2.6H2O, 20mM Ni(NO3)2.6H2O, and 20 mmol urea were dissolved in 40 mL distilled water andstirred at room temperature for 15-25 minutes to form a light pink solution. The Ni-foamwas immersed in this solution within a Teflon-lined stainless-steel autoclave, sealed, andheated at 110-150°C for 10-20 hours. After cooling, the samples were washed thrice withdeionized water, vacuum-dried overnight at 60-80°C, and labelled as DS-NiCoLDH10mM.Preparation of Activated Carbon (AC) from Waste Cotton Textile: Cotton cloth waswashed with a soap solution to remove impurities and then rinsed with deionized water.After drying in a vacuum oven at 50 to 80°C for 12 to 24 hours, the cloth was placed in atube furnace. It was first stabilized in air at 220 to 300°C for 1 to 2 hours, thencarbonized at a temperature in a range of 800 to 1100°C at a rate of 5°C / min under anitrogen atmosphere for 1 to 2 hours. The resulting carbonized cotton (CC) was soakedin a 4:1 KOH-to-CC solution in distilled water for 30 minutes and then heated at5°C / min at a temperature in a range of 800 to 1000°C for 1 to 2 hours. The formedactivated carbon (AC) was washed with 1M HCl to neutralize residual KOH, followedby multiple rinses with deionized water, and dried at 60 to 80°C for 24 to 48 hours in avacuum oven.The entire synthesis process for NiCoLDH using Ni foam as the direct source of Ni isdepicted in Figure 1. Wherein, Figure 1 depicts schematic illustration for synthesisprocess of NiCoLDH nanoneedles.Material Characterization: Field emission scanning electron microscopy (FESEM),coupled with energy-dispersive X-ray spectroscopy (EDX), was employed forhigh-resolution imaging and elemental mapping of the samples. Transmission electronmicroscopy (TEM; JEOL JEM-1400) and high-resolution transmission electronmicroscopy (HRTEM; JEOL JEM-2100F / HR, operating at 200 kV) were utilized toanalyse the morphology and crystal structure of the materials. Powder X-ray diffraction(XRD; PAN Analytical X'Pert PRO, using Cu Kα radiation, λ = 1.54056 A) was used toinvestigate the crystallinity and phase composition. X-ray photoelectron spectroscopy(XPS; AXIS Supra with an Al Kα monochromatic X-ray source, 148.6 eV) wasemployed to determine the chemical composition and valence states of the elementswithin the sample. Raman spectroscopy (Horiba Jobin Yvon HR 785 nm near-infrared)was used to identify structural features and vibrational modes associated with thesynthesized material.Electrochemical Characterization: The electrochemical properties of NiCoLDH wereassessed using a BioLogic VMP3 electrochemical workstation through cyclicvoltammetry (CV), galvanostatic charge-discharge (GCD), and electrochemicalimpedance spectroscopy (EIS). In a three-electrode system, NiCoLDH, derived from Nifoam, was used as the working electrode, with a Hg / HgO reference electrode and a Ptfoil counter electrode, all in a 3M KOH aqueous electrolyte. For full-cell tests, inCR2032 coin cells, NiCoLDH-10mM was used as the positive electrode, with activatedcarbon (AC) serving as the negative electrode, and a 3M KOH electrolyte. In the hybridZn-ion system, NiCoLDH-10mM was used as the positive electrode, with zinc metal asthe negative electrode, and the electrolyte consisted of a 3M KOH and 10mM zincacetate aqueous solution.Results and Discussions:The morphological properties of the electrode materials were investigated using FESEM,as shown in Fig. 2. The NiCoLDH-7.5mM (Fig. 2a-c) displayed sparsely distributednanoneedles, suggesting that the lower cobalt (Co) concentration is insufficient forforming a uniform NiCoLDH layer. This irregular morphology could limit theelectrochemical performance by restricting ion access and active sites. In contrast, theNiCoLDH-10mM (Fig. 2d-f) demonstrated a more densely packed, well-organizednanoneedle structure, which enhances the surface area and ion accessibility, thusimproving electrochemical efficiency. However, the NiCoLDH-12.5mM (Fig. 2g-i)showed aggregated nanoneedles, likely due to accelerated nucleation resulting from thehigher Co concentration. This aggregation could hinder electrolyte accessibility and iondiffusion. The DS-NiCoLDH-10mM (Fig. 2j-l) exhibited a uniform distribution ofnanoneedles across the Ni foam, suggesting a more efficient structure for charge storageand transport.Energy Dispersive X-ray Spectroscopy (EDX) analysis of NiCoLDH-10mM confirmedthe presence of nickel (Ni), cobalt (Co), and oxygen (O), with a homogeneousdistribution of elements across the nanostructured surface, promoting efficient chargetransfer and ion accessibility-key features for high-performance supercapacitors (Fig.3a). Transmission Electron Microscopy (TEM) further revealed well-defined andelongated nanoneedles (Fig. 3b-d). High-Resolution Transmission Electron Microscopy(HRTEM) image (Fig. 3e) showed the nanoneedle structure at a lower magnification.Magnified images displayed clear lattice fringes with inter-lattice spacings of 0.26 nm,0.148 nm, and 0.20 nm, corresponding to the (012), (113), and (107) planes, respectively(Fig. 3f, 3g). The Selected Area Electron Diffraction (SAED) pattern (Fig. 3h)confirmed the ordered crystalline structure, validating the material's high crystallinity,with diffraction spots corresponding to the (0111) and (012) planes.The structural and compositional characteristics of the NiCoLDH samples were furtherexamined using X-ray diffraction (XRD), Raman spectroscopy, and X-ray photoelectronspectroscopy (XPS). The XRD analysis (Fig. 4a) of NiCoLDH samples at concentrationsof 7.5 mM, 10 mM, and 12.5 mM, as well as DS-NiCoLDH, revealed significant peakscorresponding to both metallic nickel and NiCoLDH phases. Peaks at 44.51°, 52.1° and76° were identified as the (111), (200) and (220) plane of the Ni foam substrate (JCPDSCard No. 40-0850). Characteristic NiCoLDH peaks at 19.1°, 34.5°, 39.5°, 59.6°, and63.5° were identified as the (060), (101), (015), (110), and (113) planes (JCPDS CardNo. 33-0429), confirming the successful formation and phase purity of NiCoLDH.Raman spectroscopy (Fig. 4b) was used to further analyse the NiCoLDH samples,revealing two significant peaks at 464 cm-1 and 527 cm-1. These peaks correspond to thevibrational modes of Ni-O and Co-O, respectively, which confirms the successfulsynthesis of NiCoLDH structure. This observation aligns with the X-ray diffraction(XRD) results, which show that the overall structural integrity of NiCoLDH ismaintained across different synthesis concentrations.X-ray photoelectron spectroscopy (XPS) analysis of NiCoLDH-10mM provides a deeperunderstanding of its elemental composition and bonding states, as shown in Fig. 4c. TheNi 2p spectrum shows peaks at 857.02 eV and 875.16 eV (Ni3+) and at 855.59 eV and873.33 eV (Ni2+), with satellite peaks at 861.61 eV and 879.89 eV, confirming thepresence of both nickel oxidation states (Fig. 4d). Similarly, the Co 2p spectrum revealspeaks at 781.07 eV and 796.72 eV (Co3+) and at 783.03 eV and 799.73 eV (Co2+),indicating the coexistence of both oxidation states of cobalt, which is further supportedby the presence of satellite peaks at 787 eV and 804.07 eV (Fig. 4e). The O 1s spectrum(Fig. 4f) reveals peaks at 531.31 eV (M-O), 531.4 eV (M-O-H), and 534.9 eV (hydroxylgroups), suggesting the hydroxide nature of the material. These XPS results confirm thepresence of mixed oxidation states of nickel and cobalt, along with various oxygenspecies of the NiCoLDH structure, providing a comprehensive insight into the material'scomposition and bonding characteristics.The three-electrode system was employed to compare the electrochemical performanceof various electrode materials, including NiCoLDH-7.5mM, NiCoLDH-10mM,NiCoLDH-12.5mM, and DS-NiCoLDH-10mM. Fig. 5a, 5b, and 5c present thecomparison of cyclic voltammetry (CV), galvanostatic charge-discharge (GCD), andelectrochemical impedance spectroscopy (EIS) data of these different electrodes. Thecyclic voltammetry (CV) data shown in Fig. 5a compares the electrochemicalperformance of NiCoLDH electrodes synthesized at different concentrations (7.5mM,10mM, and 12.5mM) and DS-NiCoLDH-10mM at 5mV / s. In the CV curve forNiCoLDH-10mM demonstrates a significantly higher integral area compared to otherconcentrations, indicating superior capacitance and overall electrochemical performance.This result is further supported by the uniform growth observed in the FESEM images,which contributes to the enhanced charge storage capacity and more efficientelectrochemical behaviour of the NiCoLDH-10mM electrode. This is further confirmedby the galvanostatic charge-discharge (GCD) test (Fig. 5b), where NiCoLDH-10mMexhibits the longest discharge time of 3110 seconds, corresponding to its highercapacitance i.e. 6220 mF cm-2at 1 mA / cm2. Electrochemical impedance spectroscopy(EIS) was employed to assess the solution resistance (RS) and charge transfer resistance(RCT) of the synthesized electrode materials. The Nyquist plot, recorded over a frequencyrange of 100 kHz to 10 mHz with a 5 mV amplitude (Fig. 5c), revealed that theNiCoLDH-10mM electrode exhibited the lowest values for both RS and RCT, indicatingminimal resistance and enhanced electrochemical performance. Table 1 summarizes thecomparison of RS and RCT values for all the electrodes.Table 1: Comparison of Solution Resistance and Charge Transfer Resistance ofNiCoLDH synthesized at 7.5mM, 10mM, and 12mM concentrations, as well as DSNiCoLDH-10mM.The Fig. 5d presents the cyclic voltammetry (CV) measurements of NiCoLDH-10mM atvarious scan rates ranging from 2 mV / s to 200 mV / s. Notably, the CV curves maintaintheir distinct shape even at higher scan rates, indicating that the electrode exhibitsexcellent structural stability and is capable of retaining its electrochemical performanceunder varying operating conditions. Fig. 5e displays the galvanostatic charge-discharge(GCD) analysis of NiCoLDH-10mM at multiple current densities (1, 2, 5, and 10mA / cm²). The resulting areal capacitance from these GCD measurements was calculatedand subsequently compared in Fig. 5f. Among the tested samples, NiCoLDH-10mMshows the highest capacitance, followed by NiCoLDH-12.5mM and NiCoLDH-7.5mM.In contrast, DS-NiCoLDH-10mM exhibits the lowest capacitance, highlighting thesuperior electrochemical performance of the NiCoLDH-10mM composite. Table 2presents a detailed comparison of areal capacitance for all the electrode materials atvarious current densities. Interestingly, when Ni foam is directly used as the nickelsource, the resistance is significantly reduced, leading to a threefold increase incapacitance compared to the double salt-based NiCoLDH, where higher resistanceimpedes electrochemical performance.Table 2: Areal Capacitance of NiCoLDH synthesized at 7.5mM, 10mM, and 12mMconcentrations, as well as DS-NiCoLDH-10mM at various current densities.Fig. 6 provides a thorough electrochemical assessment of the NiCoLDH-10mMelectrode in full-cell configurations, demonstrating its potential for energy storageapplications. Fig. 6a presents the cyclic voltammetry (CV) curve for the NiCoLDH10mM / / AC asymmetric cells (ASC) across various potential windows. The curveindicates polarization at 1.9V, with a safe operating window defined at 1.8V, ensuringboth safety and stability of the system. Fig. 6b depicts the corresponding galvanostaticcharge-discharge (GCD) data, confirming the charging plateau at 1.9V, therebyvalidating the selected potential window. Fig. 6c showcases the CV measurements atscan rates ranging from 2mV / s to 200mV / s within the 0-1.8V window, highlighting therobust structural stability of the material. The shape of the curve remains consistent evenat higher scan rates, suggesting that the full cell maintains its electrochemicalperformance under varied operational conditions. Fig. 6d provides GCD data at differentcurrent densities (1, 2, 5, and 10 mA / cm²). From these measurements, key parameterssuch as discharge time, areal capacitance, energy density, and power density arecalculated and summarized in Table 3. The electrochemical performance of theNiCoLDH-10mM / / AC full cell with other published studies are compared in Table 4,emphasizing its superior performance, particularly with the use of Ni foam as both thecurrent collector and active material.Table 3: Table summarizing discharge time, energy density, and power density ofAsymmetric Supercapacitor (NiCoLDH-10mM / / AC) at various current densities.Table 4: Table comparing the energy density, and power density of full cells atvarious current densities with the previous reported literatures.Additionally, the NiCoLDH-10mM / / Zn full cell is analysed, with zinc metal as theanode and NiCoLDH-10mM as the cathode, separated by Whatman filter paper andusing 3M KOH and 10mM Zinc Acetate as the electrolyte. Fig. 6(e) illustrates the CVcurve for this cell, measured at various scan rates within a 0.8V to 1.8V potentialwindow, demonstrating its excellent structural stability. Fig. 6(f) presents GCDmeasurements at different current densities, with Table 5 summarizing the dischargetime, energy density, and power density of Zn ion hybrid supercapacitors. It is importantto note that this area of research and technology is still emerging, with limited studies onZn-ion hybrid supercapacitors. A comparable study on NiCo-LDHs@Co / CoO-CNFsdemonstrated an energy density of 108 Wh kg-1 and a power density of 914.8 W kg-1 at acurrent density of 1 A g-1 and as discussed in Ge, H., Wang, J., Luo, Y., Shi, B., Jiang, J.,Cui, S., Cheng, L., Li, Z., Jiao, Z. (2024). Enhancing heterojunction interface chargetransport efficiency in NiCo-LDHs@Co / CoO-CNFs for high-performance asymmetricand zinc-ion hybrid supercapacitors. Carbon, 229, 119482.https: / / doi.org / 10.1016 / j.carbon.2024.119482.Table 5: Table summarizing discharge time, energy density, and power density ofZinc-Ion Hybrid Supercapacitor (NiCoLDH-10mM / / Zn) at various currentdensities.It is concluded that the present invention successfully demonstrates a novel, binder-freeapproach for synthesizing NiCoLDH directly on Ni foam, addressing key limitations intraditional supercapacitor electrode fabrication. By employing Ni foam as both thecurrent collector and a nickel precursor, this method eliminates the need for binders andexternal coatings, significantly enhancing ion accessibility, electron transport, andinterfacial contact. The comparison between direct Ni foam utilization and the dual-saltsynthesis approach underscores the superior electrochemical performance of thebinder-free method, including higher capacitance, energy density, and power density.This approach leverages the inherent three-dimensional porous structure and high surfacearea of Ni foam, simplifying fabrication processes while delivering high-performance,scalable, and cost-effective supercapacitor electrodes. The results highlight the potentialof this innovation to significantly advance energy storage technology, offering efficient,durable, and environmentally sustainable solutions for modern energy storageapplications.Accordingly, the present invention introduces a transformative approach to fabricatinghigh-performance supercapacitor electrodes by leveraging Ni foam as both the currentcollector and a precursor for nickel. This dual functionality highlights the versatility ofNi foam in synthesizing a range of nickel-based compounds, such as NiCoLDH, withoutthe need for binders or external coatings. The direct use of Ni foam in this mannersimplifies fabrication, enhances material integration, and optimizes electrochemicalproperties, such as capacitance and energy density.This binder-free synthesis method is applicable not only for NiCoLDH but also for othernickel-based materials, expanding the potential for Ni foam in diverse energy storagetechnologies. By harnessing the three-dimensional porous structure and high surface areaof Ni foam, this approach maximizes ion accessibility and minimizes resistance, enablingits use in scalable, cost-effective, and environmentally friendly energy storage devices.The scope of this invention extends to the broader application of Ni foam as a precursorin the synthesis of various nickel compounds, offering significant opportunities foradvancements in supercapacitors, batteries, and other energy storage systems. Thisinnovation paves the way for efficient, sustainable, and high-performance solutions thatmeet the demands of modern energy storage technologies.REFERENCES:1. Yu, Y., Liao, Y., Fan, J., Ding, Y., Fan, Y., Cao, J., Zhou, X., Wang, Y., Yan, J., Li,H., Li, D., Wu, J. (2025). Tip effect of NiCo-LDH with low crystallinity for enhancedenergy storage performance of yarn-shaped supercapacitors. Journal of Colloid andInterface Science, 679, 1242-1252. https: / / doi.org / 10.1016 / j.jcis.2024.10.064.2. Wang, H., Jin, C., Liu, Y., Kang, X., Bian, S., Zhu, Q. (2018). Cotton yarns modifiedwith three-dimensional metallic Ni conductive network and pseudocapacitive Co-Nilayered double hydroxide nanosheet array as electrode materials for flexible yarnsupercapacitors. Electrochimica Acta, 283, 1789-1797.https: / / doi.org / 10.1016 / j.electacta.2018.07.090.3. Wang, Y., Wang, H., Yang, S., Yue, Y., Bian, S. (2019). HierarchicalNiCo2S4@Nickel-Cobalt Layered Double Hydroxide Nanotube Arrays on MetallicCotton Yarns for Flexible Supercapacitors. ACS Applied Materials & Interfaces, 11,30384-30390. https: / / doi.org / 10.1021 / acsami.9b06317.4. Su, W., Wu, F., Fang, L., Hu, J., Liu, L., Guan, T., Long, X., Luo, H., Zhou, M.(2019). NiCo-LDH nanowires@nanosheets core-shell structure grown on carbon fibercloth for high performance flexible supercapacitor electrode. Journal of Alloys andCompounds, 799, 15-25. https: / / doi.org / 10.1016 / j.jallcom.2019.05.305.5. Lu, H., Chen, J., Tian, Q. (2018). Wearable high-performance supercapacitors basedon Ni-coated cotton textile with low-crystalline Ni-Al layered double hydroxidenanoparticles. Journal of Colloid and Interface Science, 513, 342-348.https: / / doi.org / 10.1016 / j.jcis.2017.11.046.6. Gao, L., Surjadi, J. U., Cao, K., Zhang, H., Li, P., Xu, S., Jiang, C., Song, J., Sun, D.,Lu, Y. (2017). Flexible Fiber-Shaped Supercapacitor Based on Nickel-Cobalt DoubleHydroxide and Pen Ink Electrodes on Metallized Carbon Fiber. ACS Applied Materials& Interfaces, 9, 5409-5418. https: / / doi.org / 10.1021 / acsami.6b16101.7. Shahrokhian, S., Naderi, L., Mohammadi, R. (2018). High-Performance Fiber-ShapedFlexible Asymmetric Microsupercapacitor Based on Ni(OH)2Nanoparticles-Decorated Porous Dendritic Ni-Cu Film / Cu Wire and Reduced GrapheneOxide / Carbon Fiber Electrodes. ACS Sustainable Chemistry & Engineering, 6, 14574-14588. https: / / doi.org / 10.1021 / acssuschemeng.8b03196.8. Senthilkumar, S., Fu, N., Liu, Y., Wang, Y., Zhou, L., Huang, H. (2016). Flexiblefiber hybrid supercapacitor with NiCo2O4 nanograss@carbon fiber and bio-wastederived high surface area porous carbon. Electrochimica Acta, 211, 411-419.https: / / doi.org / 10.1016 / j.electacta.2016.06.059.

Claims

1. A method for fabricating high-performance, binder-free supercapacitor electrodes, wherein the method comprises: preparation of Ni(OH)2 precursor from Ni-foam; synthesis of nickel cobalt layered double hydroxides (NiCoLDH) arrays from Ni(OH)2 precursor, Co(NO3)2.6H2O, and urea, wherein nickel cobalt layered double hydroxides (NiCoLDH) arrays act as a supercapacitor positive electrode; preparing an activated carbon (AC) material as negative electrode; and preparing a supercapacitor device by hybridizing the nickel cobalt layered double hydroxides (NiCoLDH) arrays with Activated Carbon (AC).

2. The method as claimed in claim 1, wherein, the preparation of Ni(OH)2 precursor comprises: cutting Ni-foam into small Ni-foam pieces having a size in a range of 1x1 cm2 to 5x5 cm2 ; cleaning the small Ni-foam pieces with HCl solution to get cleaned Ni-foam pieces; washing the cleaned Ni-foam pieces with absolute ethanol for 10 to 20 minutes and deionized water for 10 to 20 minutes to obtain the washed Ni-foam pieces; placing the washed Ni-foam pieces in sealed glass vials for 20 to 28 hours; immersing the washed Ni-foam pieces in a mixture of NaOH and (NH4)2S2O8 at room temperature for 10 to 20 hours; and rinsing the washed Ni-foam pieces in distilled water, followed by vacuum-drying at 140 to 160°C for 5 to 7 hours to prepare the Ni(OH)2 precursor.

3. The method as claimed in claim 1, wherein, cleaning of the small Ni-foam pieces is done by immersing the small Ni-foam pieces in an ultrasonic bath for 20 to 40 minutes to remove the oxide layer, wherein the ultrasonic bath consists of 3 M HCl solution.

4. The method as claimed in claim 1, wherein, the mixture of NaOH and (NH4)2S2O8 comprises 3M NaOH and 1M (NH4)2S2O8 having a volume percentage ratio of 2:1.

5. The method as claimed in claim 1, wherein, synthesis of nickel cobalt layered double hydroxides (NiCoLDH) Arrays comprises: dissolving Co(NO3)2.6H2O in distilled water to obtain a first solution; adding urea in the first solution and stirring the first solution at room temperature for 20 minutes to form a pink solution; immersing Ni(OH)2 precursor in the pink solution and subjecting Ni(OH)2 precursor to hydrothermal treatment at 120 to 140°C for 12 to 18 hours; cooling the pink solution at room temperature to obtain the nickel cobalt layered double hydroxides (NiCoLDH) array samples, followed by washing the NiCoLDH array samples with deionized water; and vacuum-drying the NiCoLDH array samples overnight at 60 to 80°C and labelling the NiCoLDH array samples based on the concentration of cobalt nitrate used.

6. The method as claimed in claim 5, wherein, Co(NO3)2.6H2O is dissolved in distilled water at concentrations of 7.5 mM, 10 mM, and 12.5 mM.

7. The method as claimed in claim 5, wherein, urea and cobalt nitrate are in a weight percentage ratio of 2:1.

8. The method as claimed in claim 1, wherein, the Activated Carbon (AC) material is prepared from cotton material through a process comprising of: washing the cotton material with a soap solution to remove impurities, followed by rinsing with deionized water to obtain a washed cotton material; drying the washed cotton material in a vacuum oven at 50 to 80°C for 12 to 24 hours to obtain a dry cotton material; placing the dry cotton material in a tube furnace and stabilizing the dry cotton material in air at 220 to 300°C for 1 to 2 hours; carbonizing the dry cotton material at a temperature in a range of 800 to 1100°C at a rate of 5°C / min under a nitrogen atmosphere for 1 to 2 hours to obtain a carbonized cotton (CC); soaking the carbonized cotton (CC) in a solution of KOH and distilled water for 30 minutes, followed by heating at 5°C / min at a temperature in a range of 800 to 1000°C for 1 to 2 hours to obtain the activated carbon (AC) material; and washing the activated carbon (AC) material with 1M HCl to neutralize residual KOH, followed by rinsing the activated carbon (AC) with deionized water, and drying at 60 to 80°C for 24 to 48 hours in a vacuum oven.

9. The method as claimed in claim 8, wherein, the cotton material is a waste cotton material.

10. The method as claimed in claim 8, wherein, the KOH and carbonized cotton (CC) are in a ratio of 4:1.