Negative electrode material and preparation method therefor, negative electrode plate and battery
Patent Information
- Application Number
- IN202337075181
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-02-25
- Filing Date
- 2023-11-03
- Publication Date
- 2026-10-01
- Estimated Expiration
- 2042-07-20
AI Technical Summary
Existing lithium-ion battery negative electrode materials face challenges in balancing energy density and rate performance, particularly with silicon-based materials experiencing high volume expansion and poor structural stability, leading to suboptimal performance in fast charging systems and high costs.
A negative electrode material comprising boron-doped graphite with a shell of porous titanium oxide, amorphous carbon, and a conductive agent, where the porosity of the titanium oxide is between 5% to 50% and the average pore size is 10nm to 500nm, enhancing ion/electron transfer and structural stability.
The proposed solution significantly improves the rate performance and cycling stability of lithium-ion batteries by optimizing ion intercalation/deintercalation and reducing irreversible capacity loss, while maintaining high energy density.
Smart Images

Figure 00000021_0000 
Figure 00000021_0001
Abstract
Description
TECHNICAL FIELDThe present application relates to the technical field of battery negative electrodematerials, specifically to a negative electrode material and its preparation method, a negativeelectrode plate, and a battery.BACKGROUNDAt present, the market-oriented negative electrode materials are mainly made of artificialgraphite, with a theoretical specific capacity of 372mAh / g. With the increasing demand forenergy density in lithium-ion batteries, the development of negative electrode materials withhigh specific capacity has always been a research hotspot in the field of lithium-ion batteries.Although silicon-based materials have a high specific capacity (theoretical capacity of3200mAh / g), they also have fatal drawbacks such as high volume expansion rate and poorstructural stability, resulting in poor rate performance of batteries, making it difficult to meetthe demand for negative electrode materials in fast charging systems, and the cost is high.The doping and coating of negative electrode materials have a certain improvementeffect on their electrochemical performance. The doping and coating of negative electrodematerials mainly involves coating amorphous carbon and conductive agents on the surface ofgraphite to improve the rate performance, increase the graphitization temperature, andincrease the specific capacity of negative electrode materials. However, there are also defectssuch as the first efficiency and capacity per gram decrease, which affect the utilization of thecapacity per gram of the full battery positive electrode material, which in turn affects theoverall energy density of the battery.SUMMARYTherefore, the technical problem to be solved in the present application is to overcomethe defect that the energy density and rate of lithium batteries obtained from the negativeelectrode materials used in the existing technology cannot be balanced, that is, to improve therate performance of the battery while also improving the energy density, thereby providing anegative electrode material and its preparation method.The present application provides a negative electrode material, comprising:a core comprising a boron-doped graphite; anda shell which is coated outside the core, the shell comprising a porous titanium oxide, anamorphous carbon, and a conductive agent.Furthermore, the porosity of the porous titanium oxide is in a range from 5% to 50%, andthe average pore size of the porous titanium oxide is in a range from 10nm to 500nm. Theporosity and average pore size in the present application were measured using the nitrogenadsorption method, specifically using the nitrogen adsorption porosity tester JW-BK300C.Furthermore, a mass ratio of the core to the shell is (90-99):(1-10).Furthermore, a mass ratio of the porous titanium oxide to the amorphous carbon is(1:10):(88-98.5). Optionally, the mass ratio of the porous titanium oxide to the amorphouscarbon is (5-10):(88-95).Furthermore, a mass ratio of the porous titanium oxide to the conductive agent is(1-10):(0.5-2). Optionally, the mass ratio of the porous titanium oxide to the conductive agentis (5-10):(1-2).Furthermore, a doping ratio of boron in the boron-doped graphite is in a range from1wt% to 20wt%;wherein, the doping ratio of boron refers to the percentage of the mass of boron atoms inthe total mass of boron-doped graphite.Furthermore, the conductive agent is selected from at least one of carbon nanotubes,graphene and super carbon black. Super carbon black, also known as super conductive carbonblack (SP), is a conductive carbon black like furnace black. It is formed by aggregating nativeparticles with a diameter of about 40nm into native aggregates of 150-200nm, which are thenprocessed and formed through soft aggregation and artificial compression. Wherein, carbonnanotubes, graphene, and super carbon black can all be selected from conventional carbonnanotubes, graphene, and super carbon black in this field.The present application also provides a method for preparing a negative electrodematerial, comprising the following steps:(1) mixing a porous titanium oxide, an amorphous carbon raw material, a conductiveagent and an organic solvent to prepare a coating solution; mixing and heating a graphiteraw material, a boron-containing compound and a binder, to obtain a precursor material;and(2) mixing the precursor material with the coating solution, drying, carbonizing toprepare the negative electrode material.Furthermore, the method for preparing a negative electrode material also satisfies at leastone of the following 1) to 8):1) the amorphous carbon raw material is a resin, and optionally, the resin is selected fromat least one of phenolic resin, furfural resin and epoxy resin; wherein the carbon contentof phenolic resin, furfural resin, and epoxy resin is 25%, which means that the mass ofamorphous carbon obtained from the resin after drying and carbonization treatmentaccounts for 25% of the mass of its raw resin;2) the organic solvent is selected from at least one of carbon tetrachloride,N-methylpyrrolidone, cyclohexane, tetrahydrofuran and xylene; and / or, the conductiveagent is selected from at least one of carbon nanotube, graphene and super carbon black;and / or, the boron-containing compound is selected from at least one of boron oxide,titanium diboride, magnesium diboride, chromium diboride and boron carbide;3) the graphite raw material is a needle coke, and optionally, the needle coke is selectedfrom at least one of petroleum-based needle coke and coal-based needle coke;4) the binder is asphalt;5) grinding, stirring and / or ultrasonic treatment are conducted after the mixing of step (1)and / or the mixing of step (2);6) in step (1), the heating process involves heating to a temperature ranging from 200 °Cto 300 °C under inert gas and holding for 1 hour to 6 hours within this temperature range,then heating to a temperature ranging from 700°C to 1000 °C under inert gas and holdingfor 1 hour to 6 hours within this temperature range;7) in step (2), the carbonizing is carried out at a temperature ranging from 600 °C to1000 °C for a time period ranging from 1 hour to 6 hours; and8) a mass ratio of the porous titanium oxide to the resin is (10-50):(50-400); and / or, amass ratio of the porous titanium oxide to the conductive agent is (1-10):(0.5-2); and / or, amass ratio of the graphite raw material to the boron-containing compound is 100:(1-10).In the present application, both petroleum-based needle coke and coal-based needle cokecan both use conventional petroleum-based needle coke and coal-based needle coke in thefield, such as, petroleum-based needle coke that meets the standard "GB / T 37308-2019Oil-based Needle Coke" and coal-based needle coke that meets the standard "GB T32158-2015 Coal-based Needle Coke". Phenolic resin, furfural resin, and epoxy resin can allbe selected from various specifications of phenolic resin, epoxy resin, and furfural resin inthis field. Asphalt can be selected from various specifications of petroleum asphalt and coalasphalt in this field.Furthermore, in step (1), the porous titanium oxide is added into a resin-containingorganic solvent, mixed with a conductive agent-containing organic solvent, to obtain a coatingsolution.The mass-volume percentage can be expressed as %(w / v).In some optional embodiments, a mass-volume percentage of the resin in theresin-containing organic solvent is in a range from 1% to 15%; it means that the mass of resincontained in every 100ml of the resin-containing organic solvent is 1-15g.In some optional embodiments, a ratio of a mass of the porous titanium oxide to avolume of the resin-containing organic solvent is (1-10)g: (2000-7600)mL.In some optional embodiments, a mass-volume percentage of the conductive agent in theconductive agent-containing organic solvent is in a range from 0.5% to 2%; it means thatevery 100ml of the conductive agent-containing organic solvent contains 0.5-2g of theconductive agent.In some optional embodiments, a ratio of a mass of the porous titanium oxide to avolume of the conductive agent-containing organic solvent is (1-10)g: (100-500)mL.Furthermore, a process for preparing the porous titanium oxide comprises the followingsteps:heating an aqueous solution of titanate salt, adding an acid solution to adjust the pHvalue, carrying out a reaction, performing solid-liquid separation to keep solid, drying andcarbonizing to prepare the porous titanium oxide.Furthermore, the titanate salt is selected from at least one of calcium titanate, magnesiumtitanate, lithium titanate, aluminum titanate and potassium titanate; and / or, the aqueoussolution of titanate salt is heated at a temperature ranging from 60 °C to 100 °C for at least 1hour (such as 1 hour to 6 hours); and / or, the reaction is carried out for at least 1 hour (such as1 hour to 12 hours); and / or, the carbonizing is performed at a temperature ranging from600 °C to 1000 °C for 1 hour to 6 hours; and / or, the pH value is adjusted to 4 to 6; and / or, theacid solution is a hydrochloric acid solution, a sulfuric acid solution, a citric acid solution, anacetic acid solution, or a phosphoric acid solution. The mass percentage of titanate salt in theaqueous solution of titanate salt is in a range from 1wt% to 10wt%.The present application also provides a negative electrode plate, comprising any one ofthe aforementioned negative electrode material or the negative electrode material prepared byany one of the aforementioned method for preparing a negative electrode material. Thenegative electrode plate can be prepared using conventional methods, such as homogenization,coating, etc.The present application also provides a battery, comprising the negative electrode plateas described above, as well as a battery shell, a positive electrode plate, a separator, and anelectrolyte solution, wherein the battery can be a lithium-ion battery, a sodium-ion battery, apotassium-ion battery, an aluminum-ion battery, etc.The technical solution of the present application has the following advantages:(1) the negative electrode material provided in the present application uses theboron-doped graphite which is coated with a shell containing a porous titanium oxide, anamorphous carbon, and a conductive agent. The various components cooperate with eachother, which not only significantly improves the ion / electron transfer rate and conductivity ofthe negative electrode material, but also enhances the intercalation / deintercalation of lithiumions in the lithium battery formed by the negative electrode material, reduces the irreversiblecapacity loss of the battery, and improves the first efficiency and rate performance of thebattery. Especially the use of the porous titanium oxide makes the negative electrode materialstructure more stable, significantly improving the cycling performance of the battery.(2) the negative electrode material provided in the present application can furtherimprove the first efficiency and rate performance of the battery composed of the negativeelectrode material by controlling the porosity of the porous titanium oxide to 5-50% andaverage pore size to 10-500nm.BRIEF DESCRIPTION OF THE DRAWINGSIn order to provide a clearer explanation of the specific embodiments of the presentapplication or technical solution in the prior art, a brief introduction will be given to thedrawings required for the specific implementation or description of the prior art. It is evidentthat the drawings in the following description are some of the implementation modes of thepresent application. For ordinary technical personnel in the art, other drawings can beobtained based on these drawings without creative labor.Fig. 1 is an SEM electron microscope image of the negative electrode material preparedin Example 1 of the present application;Fig. 2 shows a comparison of the cyclic curve of Example 1 and Comparative Example1.DETAILED DESCRIPTIONThe following examples are provided for a better understanding of the presentapplication, and are not limited to the best implementation mode. They do not constitutelimitations on the content and scope of protection of the present application. Any product thatis the same or similar to the present application obtained from the inspiration of the presentapplication or by combining the features of the present application with other existingtechnologies falls within the scope of protection of the present application.If the specific experimental steps or conditions are not specified in the examples, theycan be carried out according to the conventional experimental steps or conditions described inthe literature in this field. The reagents or instruments used without specifying themanufacturer are all conventional reagents and products that can be obtained throughcommercial procurement. For phenolic resin, all phenolic resins with a solid content of10-90%, free phenol (%) of ≤ 20, and viscosity of 10-1000mPa·s (25 °C) are suitable for thepresent application. For example, in the following examples and comparative examples, thephenolic resin uses phenolic resin from Wuxi Guangming Chemical Co., Ltd., model 2130;Oil-based needle coke was purchased from PetroChina Daqing Petrochemical Company orJinzhou Petrochemical Co., Ltd., both of which meet the standard "GB / T 37308-2019Oil-based Needle Coke". The coal-based needle coke material was purchased from TangshanDongri New Energy Co., Ltd. and meets the standard "GB T 32158-2015 Coal-based NeedleCoke". The carbon nanotubes in the following examples and comparative examples werefrom Jiangsu Cnano Technology Co., Ltd., model LB107-44. Graphene was from JiangsuCnano Technology Co., Ltd., model: LB2G3-85. Asphalt was purchased from Jining superlian new materials Technology Co., Ltd., model: GB / 8175. Furfural resin was purchased fromWuhan Yuancheng Technology Development Co., Ltd., model: FL resin. Epoxy resin waspurchased from Wuxi Aerzi Chemical Co., Ltd., model: 128 epoxy resin.Taking Example 1 as an example, the calculation formulae for the following parametersare as follows:doping ratio = mass of boron atom / (mass of needle coke material + mass of boron atom)x 100%;mass of the core = mass of the precursor material; andmass of the shell = (total mass of the porous titanium oxide + total mass of resin xCarbon content + total mass of carbon nanotubes) / (volume of carbon tetrachloride solutioncontaining phenolic resin + volume of NMP dispersion containing nanotubes) x actualvolume of the coating liquid used for the negative electrode material.EXAMPLE 1This example provides a negative electrode material and a preparation method thereof,wherein the negative electrode material comprises a core and a shell which is coated outsidethe core, and wherein the core is a boron-doped graphite; the doping ratio of boron in theboron-doped graphite is 9.6% (a mass fraction); and the shell includes a porous titanium oxide,an amorphous carbon, and carbon nanotubes. The porosity of the porous titanium oxide is20%, with an average pore size of 100nm. The mass ratio of the core to the shell is 95:5; themass ratio of the porous titanium oxide to the amorphous carbon is 5:94, and the mass ratio ofthe porous titanium oxide to carbon nanotubes is 5:1.The method for preparing the negative electrode material includes:(1) Preparation of the porous titanium oxide: 50g of calcium titanate was added into1,000g of deionized water to prepare a 5% mass concentration of calcium titanate aqueoussolution, which were reacted at 80 °C for 6 hours to obtain a first solution; 5vt% hydrochloricacid solution was added dropwise into the first solution, the pH was adjusted to 4, and let itreact for 3 hours to obtain a second solution. The second solution was filtered to obtain a solidand the solid was vacuum dried, and then the obtained solid was carbonized in a mufflefurnace at 800 °C for 3 hours to obtain the porous titanium oxide;(2) Preparation of the coating solution: 5g of the porous titanium oxide was added into7,520ml of carbon tetrachloride containing 5% (w / v) phenolic resin, then 100ml ofN-methylpyrrolidone (NMP) dispersion containing 1% (w / v) carbon nanotubes was added,and they were mixed evenly to obtain the coating solution;(3) Preparation of the negative electrode material: 92g of petroleum-based needle cokematerial (PetroChina Daqing Petrochemical Company), 31g of titanium diboride, and 5g ofasphalt were weighed and mix evenly. The mixture was ground through a ball mill at arotation rate of 50rpm / min for 48 hours, then heated to 250 °C under an argon inertatmosphere for softening and kept at the temperature for 3h. Then, the temperature wasincreased to 800 °C under an argon inert atmosphere and kept at the temperature for 3 hours.After that, the temperature was naturally cooled down to room temperature followed bycrushing the resultant to obtain a precursor material. Afterwards, 95g of the precursor materialwas added into 381ml of the coating solution, milled, vacuum dried, and carbonized for 3hours under an argon inert atmosphere at a temperature of 800 °C to obtain the negativeelectrode material.EXAMPLE 2This example provides a negative electrode material and a preparation method thereof,wherein the negative electrode material comprises a core and a shell which is coated outsidethe core, and wherein the core is a boron-doped graphite; the doping ratio of boron in theboron-doped graphite is 2% (a mass fraction); and the shell includes a porous titanium oxide,an amorphous carbon, and graphene. The porosity of the porous titanium oxide is 5%, with anaverage pore size of 10nm. The mass ratio of the core to the shell is 99:1; the mass ratio of theporous titanium oxide to the amorphous carbon is 10:89, and the mass ratio of the poroustitanium oxide to the graphene is 10:1.The method for preparing the negative electrode material includes:(1) Preparation of the porous titanium oxide: 20g of lithium titanate was added into2,000g of deionized water to prepare a 1% mass concentration of lithium titanate aqueoussolution, which were reacted at 60 °C for 12 hours to obtain a first solution; 10vt%hydrochloric acid solution was added dropwise into the first solution, the pH was adjusted to4, and let it react for 1 hour to obtain a second solution. The second solution was filtered toobtain a solid and the solid was vacuum dried, and then the obtained solid was carbonized in amuffle furnace at 600 °C for 6 hours to obtain the porous titanium oxide material;(2) Preparation of the coating solution: 10g of the porous titanium oxide material wasadded into 3,560ml of carbon tetrachloride solution containing 10% (w / v) furfural resin, then100ml of NMP solution containing 1% (w / v) graphene was added, and they were mixedevenly to obtain the coating solution;(3) Preparation of the negative electrode material: 92.75g of oil-based needle cokematerial (Jinzhou Petrochemical Co., Ltd.), 6.25g of boron oxide and 1g of asphalt wereweighed and mix evenly. The mixture was ground through a ball mill at a rotation rate of10rpm / min for 72 hours, then heated to 200 °C under an argon inert atmosphere for softeningand kept at the temperature for 6 hours. Then, the temperature was increased to 700 °C underan argon inert atmosphere and kept at the temperature for 6 hours. After that, the temperaturewas naturally cooled down to room temperature followed by crushing the resultant to obtain aprecursor material. Afterwards, 99g of the precursor material was added into 36.8ml of thecoating solution, milled, vacuum dried, and carbonized for 6 hours under an argon inertatmosphere at a temperature of 600 °C to obtain the negative electrode material.EXAMPLE 3This example provides a negative electrode material and a preparation method thereof,wherein the negative electrode material comprises a core and a shell which is coated outsidethe core, and wherein the core is boron-doped graphite; the doping ratio of boron in theboron-doped graphite is 20% (a mass fraction); and the shell includes a porous titanium oxide,an amorphous carbon, and carbon nanotubes. The porosity of the porous titanium oxide is50%, with an average pore size of 500nm. The mass ratio of the core to the shell is 90:10; themass ratio of the porous titanium oxide to the amorphous carbon is 10:88, and the mass ratioof the porous titanium oxide to carbon nanotubes is 10:2.The method for preparing the negative electrode material includes:(1) Preparation of the porous titanium oxide: 20g of aluminum titanate was added into200g of deionized water to prepare a 10% mass concentration of aluminum titanate aqueoussolution, which were reacted at 100 °C for 1 hour to obtain a first solution; 5vt% hydrochloricacid solution was added dropwise into the first solution, the pH was adjusted to 4, and let itreact for 6 hours to obtain a second solution. The second solution was filtered to obtain a solidand the solid was vacuum dried, and then the obtained solid was carbonized in a mufflefurnace at 1,000 °C for 1 hour to obtain the porous titanium oxide material;(2) Preparation of the coating solution: 10g of the porous titanium oxide material wasadded into 2,356ml of cyclohexane solution containing 15% (w / v) epoxy resin, and then200ml of NMP dispersion containing 1% (w / v) graphene was added therein, and they weremixed evenly to obtain the coating solution;(3) Preparation of negative electrode material: 80g of coal-based needle coke material,41.6g of magnesium diboride and 10g of asphalt were weighed and mix evenly. The mixturewas ground through a ball mill at a rotation rate of 100rpm / min for 12 hours, then heated to300 °C under an argon inert atmosphere for softening and kept at the temperature for 1 hour.Then, the temperature was increased to 1,000 °C under an argon inert atmosphere and kept atthe temperature for 1 hour. After that, the temperature was naturally cooled down to roomtemperature followed by crushing the resultant to obtain a precursor material. Then, 90g ofthe precursor material was added into 255ml of the coating solution, ball milled, spray dried,and carbonized for 1 hour in an argon inert atmosphere at a temperature of 1,000 °C to obtainthe negative electrode material.COMPARATIVE EXAMPLE 1This comparative example provides a negative electrode material with the followingpreparation method:95g of the same batch of oil-based needle coke from Example 1 was added into 100mlof carbon tetrachloride organic solvent containing 5% (w / v) phenolic resin. Then, the mixturewas ground through a ball mill to mill at a rotation rate of 50rpm / min for 48 hours, thenvacuum dried. Then, the temperature was increased to 800 °C under an argon inertatmosphere in a tube furnace for carbonization for 3 hours. After that, the temperature wasnaturally cooled down to room temperature followed by crushing the resultant to obtain a hardcarbon-coated graphite composite material.COMPARATIVE EXAMPLE 2This comparative example provides a negative electrode material and its preparationmethod. The negative electrode material includes a core and a shell which is coated outsidethe core, and the core is boron-doped graphite; the doping ratio of boron in the boron-dopedgraphite is 9.6% (a mass fraction); the shell includes an ordinary titanium oxide, anamorphous carbon, and carbon nanotubes. The mass ratio of the core to the shell is 95:5; themass ratio of the ordinary titanium oxide to the amorphous carbon is 5:94, and the mass ratioof the ordinary titanium oxide to carbon nanotubes is 5:1.The method for preparing the negative electrode material includes:(1) Preparation of the coating solution: 5g of the ordinary titanium oxide (purchasedfrom Guangzhou Hongwu Material Technology Co., Ltd.) was added into 7,520ml of carbontetrachloride containing 5% (w / v) phenolic resin, then 100ml of NMP dispersion containing1% (w / v) carbon nanotubes was added, and they were mixed evenly to obtain the coatingsolution;(2) Preparation of the negative electrode material: 92g of petroleum-based needle cokematerial from the same batch as Example 1, 31g of titanium diboride and 5g of asphalt wereweighed and mix evenly. The mixture was ground through a ball mill at a rotation rate of50rpm / min for 48 hours, and then heated to 250 °C under an argon inert atmosphere forsoftening and kept at the temperature for 3 hours. Then, the temperature was increased to800 °C under an argon inert atmosphere and kept at the temperature for 3 hours. After that, thetemperature was naturally cooled down to room temperature followed by crushing theresultant to obtain a precursor material. Afterwards, 95g of the precursor material was addedinto 381ml of the coating solution, milled, vacuum dried, and carbonized for 3 hours under anargon inert atmosphere at a temperature of 800 °C to obtain the negative electrode material.COMPARATIVE EXAMPLE 3This comparative example provides a negative electrode material and a preparationmethod thereof. The negative electrode material includes a core and a shell which is coatedoutside the core, and the core is boron-doped graphite. The doping ratio of boron in theboron-doped graphite is 9.6% (a mass fraction); and the shell includes a porous iron oxide, anamorphous carbon, and carbon nanotubes. The porosity of the porous iron oxide is 30%, withan average pore size of 100nm. The mass ratio of the core to the shell is 95:5; the mass ratioof the porous iron oxide to amorphous carbon is 5:94, and the mass ratio of the porous ironoxide to carbon nanotubes is 5:1.The method for preparing the negative electrode material includes:(1) Preparation of the porous iron oxide: 139g of FeSO4·7H2O was weighed anddissolved into 7,500g of ultrapure water, and stirred to completely dissolve it. The obtainedsolution was transferred into a stainless steel reaction kettle lined with polytetrafluoroethylene,sealed tightly, and placed in an oven. Reaction was conducted at 160 °C for 12 hours. Afterthe reaction is completed, the resulting reaction product was allowed to naturally cool.Afterwards, the obtained reaction products were alternately cleaned with ultrapure water andanhydrous ethanol until the cleaning solution was neutral. Then, the cleaned reaction productwas dried in a vacuum drying oven at 60 °C for 12 hours to obtain a porous iron oxideprecursor. Afterwards, the precursor was placed in a nitrogen atmosphere and calcined at350 °C for 1 hour to obtain the porous iron oxide.(2) Preparation of the coating solution: 5g of the porous iron oxide was added into7,520ml of carbon tetrachloride containing 5% (w / v) phenolic resin, then 100ml of NMPdispersion containing 1% (w / v) carbon nanotubes was added, and they were mixed evenly toobtain the coating solution;(3) Preparation of the negative electrode material: 92g of needle coke material from thesame batch as the examples, 31g of titanium diboride and 5g of asphalt were weighed and mixevenly. The mixture was ground through a ball mill at a rotation rate of 50rpm / min for 48hours, then heated to 250 °C under an argon inert atmosphere for softening and kept at thetemperature for 3 hours. Then, the temperature was increased to 800 °C under an argon inertatmosphere and kept at the temperature for 3 hours. After that, the temperature was naturallycooled down to room temperature followed by crushing the resultant to obtain a precursormaterial. Afterwards, 95g of the precursor material was added into 381ml of the coatingsolution, ball milled, vacuum dried, and carbonized for 3 hours under an argon inertatmosphere at 800 °C to obtain the negative electrode material.COMPARATIVE EXAMPLE 4This comparative example provides a negative electrode material and a preparationmethod thereof. The negative electrode material comprises a core and a shell which is coatedoutside the core, the core is graphite, and the shell includes a porous titanium oxide, anamorphous carbon, and graphene. The porosity of the porous titanium oxide is 5%, with anaverage pore size of 10nm. The mass ratio of the core to the shell is 99:1; the mass ratio of theporous titanium oxide to the amorphous carbon is 10:89, and the mass ratio of the poroustitanium oxide to the graphene is 10:1.The method for preparing the negative electrode material includes:(1) Preparation of the porous titanium oxide: same as Example 2;(2) Preparation of the coating solution: same as Example 2;(3) Preparation of the negative electrode material: 92.75g of oil-based needle coke and1g of asphalt were weighed and mix evenly. The mixture was ground through a ball mill at arotation rate of 10rpm / min for 72 hours, then heated to 200 °C under an argon inertatmosphere for softening and kept at the temperature for 6 hours. Then, the temperature wasincreased to 700 °C under an argon inert atmosphere and kept at the temperature for 6 hours.After that, the temperature was naturally cooled down to room temperature followed bycrushing the resultant to obtain a precursor material. Afterwards, 99g of the precursor materialwas added into 36.8ml of the coating solution, milled, vacuum dried, and carbonized for 6hours under an argon inert atmosphere at 600 °C to obtain the negative electrode material.EXPERIMENTAL EXAMPLE 1: SEM TestingThe negative electrode material prepared in Example 1 was used for SEM testing, andthe test results are shown in Fig. 1. From Fig. 1, it can be seen that the negative electrodematerial prepared in Example 1 has a granular structure with uniform size ranging from 10μmto 18 μm.EXPERIMENTAL EXAMPLE 2According to GB / T 24533-2009 "Graphite-based Negative Electrode Materials forLithium Ion Batteries", the specific surface area and tap density of the negative electrodematerials prepared in each example and comparative example were tested. The test results areshown in Table 1.Table 1 Specific Surface Area Results of Negative Electrode MaterialsFrom Table 1, it can be seen that the specific surface area of the negative electrodematerial prepared in each example of the present application is significantly higher than thatof Comparative Examples 1-4. The reason for this is that the surface of the composite materialis coated with the porous titanium oxide material or the core is made of boron-doped material,which can improve the specific surface area of the material, and the negative electrodematerial obtained has an appropriate tap density.EXPERIMENTAL EXAMPLE 3: Button Battery TestingThe negative electrode materials prepared in each example and comparative examplewas assembled into button batteries a1, a2, a3, b1, b2, b3 and b4, respectively. The assemblymethod is as follows: an adhesive, a conductive agent, and a solvent were added into thenegative electrode material, and stirred to make slurry, then the slurry was coated on thecopper foil, dried, and rolled to obtain the negative electrode plate. The single surface densityof the electrode plate coating is 6mg / cm2; the adhesive used is LA132 adhesive, theconductive agent is SP, and the solvent is secondary distilled water. The ratio of eachcomponent is, negative electrode material: SP: LA132: secondary distilled water = 95g: 1g:4g: 220mL; the electrolyte is LiPF6 / EC+DEC (the concentration of hexafluorophosphateLiPF6 is 1.2mol / L, and the volume ratio of ethylene carbonate EC to diethyl carbonate DEC is1:1), a metal lithium plate is used as the counter electrode and celegard2400 is used as aseparator. The assembly of the button battery was carried out in a glove box filled with argongas, and the electrochemical performance test was conducted on the CT2001A battery testerof Wuhan Land Electronics Co., Ltd. The charging / discharging voltage is in a range from0.005V to 2.0V, and the first discharge capacity and the first efficiency were tested at acharging and discharging rate of 0.1C. The discharge capacity at 3C and 0.2C rates was alsotested, and the rate (3C / 0.2C) was obtained. The test results are shown in Table 2.Table 2. Performance Comparison of Button Batteries Prepared with Negative ElectrodeMaterials of Examples and Comparative ExamplesFrom Table 2, it can be seen that the first discharge capacity, first charge / dischargeefficiency, and rate performance of the lithium battery prepared using the composite materialsof Examples 1-4 of the present application are significantly higher than that of thecomparative examples. The reason for this is that coating the surface of boron-doped graphitecore with porous titanium oxide, amorphous carbon, and conductive agent can better utilizethe structural stability of porous titanium oxide, improve the intercalation / deintercalation oflithium ions, reduce the irreversible capacity loss of the material, and improve the firstefficiency. It can also better utilize the high conductivity of titanium oxide lithium ions toimprove the rate performance of button batteries.EXPERIMENTAL EXAMPLE 4: Pouch Battery TestingThe negative electrode materials prepared in each example and comparative examplewere used to prepare the negative electrode plates separately, and the method and processconditions are the same as those in Experimental Example 3. A ternary material(LiNi1 / 3Co1 / 3Mn1 / 3O2) was used as positive electrode material, LiPF6 solution (solventEC+DEC, volume ratio 1:1, LiPF6 concentration 1.3mol / L) was used as electrolyte solution,and celegard2400 was used as separator, and 5Ah pouch batteries A1, A2, A3, B1, B2, B3,and B4 were prepared, respectively. Afterwards, the cycling performance and rateperformance of the pouch batteries were tested.Test conditions for cycling performance: charging and discharging current of 1C / 1C,voltage range of 2.8-4.2V, and 500 cycles.Test conditions for rate performance: charging rate of 1C / 3C / 5C / 8C, discharging rate of1C, and voltage range of 2.8-4.2V.The test results are shown in Tables 3 and 4.Table 3. Comparison of Cycling Performance of Pouch Batteries Prepared withNegative Electrode Materials of Examples and Comparative Examples.From Table 3, it can be seen that the cycling performance of the pouch batteriesprepared using the composite materials of Examples 1-3 is better than that of the comparativeexamples, especially at 500 cycles. The reason for this is that in terms of 1C / 1C rate cyclingperformance, the deposition of porous titanium oxide, amorphous carbon, and conductiveagent on the surface of boron-doped graphite core can significantly improve the lithium iontransfer rate; at the same time, the structure stability of the porous titanium oxide is utilized toimprove cycling performance.Table 4. Comparison of Rate Charging Performance of Pouch Batteries Prepared withComposite materials of Examples and Comparative ExamplesFrom Table 4, it can be seen that the pouch batteries prepared using the negativeelectrode materials of Examples 1-3 has better constant current charging ratio. The reason forthis is that coating the surface of boron-doped graphite core with porous titanium oxide,amorphous carbon, and conductive agent can better improve the lithium ionintercalation / deintercalation rate of the material during rate charging, thereby improving ratecharging performance.Obviously, the above examples are only for the purpose of clarifying the examplesprovided, rather than limiting the implementation modes. For ordinary technical personnel intheir respective fields, different forms of changes or modifications can be made based on theabove explanations. There is no need and cannot be an exhaustive list of all implementationmodes here. The obvious changes or modifications arising from this are still within the scopeof protection of the present application.
Claims
1. A negative electrode material, comprising: a core comprising a boron-doped graphite; and a shell which is coated outside the core, the shell comprising a porous titanium oxide, an amorphous carbon, and a conductive agent.
2. The negative electrode material of claim 1, wherein the porous titanium oxide has a porosity ranging from 5% to 50% and an average pore size ranging from 10nm to 500nm.
3. The negative electrode material of claim 1 or 2, wherein a mass ratio of the core to the shell is (90-99):(1-10); and / or, a mass ratio of the porous titanium oxide to the amorphous carbon is (1:10):(88-98.5); and / or, a mass ratio of the porous titanium oxide to the conductive agent is (1-10):(0.5-2); and / or, a doping ratio of boron in the boron-doped graphite is in a range from 1wt% to 20wt%; and / or, the conductive agent is selected from at least one of carbon nanotubes, graphene and super carbon black.
4. A method for preparing a negative electrode material, comprising the following steps: (1) mixing a porous titanium oxide, an amorphous carbon raw material, a conductive agent and an organic solvent to prepare a coating solution; and mixing and heating a graphite raw material, a boron-containing compound and a binder to obtain a precursor material; and (2) mixing the precursor material with the coating solution, drying, carbonizing to prepare the negative electrode material.
5. The method for preparing a negative electrode material of claim 4, wherein the method for preparing a negative electrode material satisfies at least one of the following 1) to 8): 1) the amorphous carbon raw material is a resin, and optionally, the resin is selected from at least one of phenolic resin, furfural resin, and epoxy resin; 2) the organic solvent is selected from at least one of carbon tetrachloride, N-methylpyrrolidone, cyclohexane, tetrahydrofuran, and xylene; and / or, the conductive agent is selected from at least one of carbon nanotube, graphene, and super carbon black; and / or, the boron-containing compound is selected from at least one of boron oxide, titanium diboride, magnesium diboride, chromium diboride and boron carbide; 3) the graphite raw material is a needle coke, and optionally, the needle coke is selected from at least one of petroleum-based needle coke and coal-based needle coke; 4) the binder is asphalt; 5) grinding, stirring and / or ultrasonic treatment are conducted after the mixing of step (1) and / or the mixing of step (2); 6) in step (1), the heating process involves heating to a temperature ranging from 200 °C to 300 °C under an inert gas and holding for 1 hour to 6 hours within this temperature range, then heating to a temperature ranging from 700°C to 1000 °C under an inert gas and holding for 1 hour to 6 hours within this temperature range; 7) in step (2), the carbonizing is carried out at a temperature ranging from 600 °C to 1000 °C for a time period ranging from 1 hour to 6 hours; and 8) a mass ratio of the porous titanium oxide to the resin is (10-50):(50-400); and / or, a mass ratio of the porous titanium oxide to the conductive agent is (1-10):(0.5-2); and / or, a mass ratio of the graphite raw material to the boron-containing compound is 100:(1-10).
6. The method for preparing a negative electrode material of claim 4 or claim 5, wherein in step (1), the porous titanium oxide is added into a resin-containing organic solvent, mixed with a conductive agent-containing organic solvent, to obtain a coating solution; optionally, a mass-volume percentage of the resin in the resin-containing organic solvent is in a range from 1% to 15%; optionally, a ratio of a mass of the porous titanium oxide to a volume of the resin-containing organic solvent is (1-10)g: (2000-7600)mL; optionally, a mass-volume percentage of the conductive agent in the conductive agent-containing organic solvent is in a range from 0.5% to 2%; and optionally, a ratio of a mass of the porous titanium oxide to a volume of the conductive agent-containing organic solvent is (1-10)g: (100-500)mL.
7. The method for preparing a negative electrode material of any one of claims 4 to 6, wherein a process for preparing the porous titanium oxide comprises the following steps: heating an aqueous solution of titanate salt, adding an acid solution to adjust the pH value, carrying out a reaction, performing solid-liquid separation to keep solid, drying and carbonizing to prepare the porous titanium oxide.
8. The method for preparing a negative electrode material of claim 7, wherein the titanate salt is selected from at least one of calcium titanate, magnesium titanate, lithium titanate, aluminum titanate and potassium titanate; and / or, the aqueous solution of titanate salt is heated at a temperature ranging from 60 °C to 100 °C for at least 1 hour; and / or, the reaction is carried out for at least 1 hour; and / or, carbonizing is performed at a temperature ranging from 600 °C to 1000 °C for a time period of 1 hour to 6 hours; and / or, the pH value is adjusted to 4 to 6; and / or, the acid solution is a hydrochloric acid solution, a sulfuric acid solution, a citric acid solution, an acetic acid solution, or a phosphoric acid solution.
9. A negative electrode plate, comprising the negative electrode material of any one of claims 1 to 3 or the negative electrode material prepared by the method for preparing a negative electrode material of any one of claims 4-8.
10. A battery, comprising the negative electrode plate of claim 9, and also a battery shell, a positive electrode plate, a separator and an electrolyte solution.