Hot-stamped component and method for manufacturing same

IN604880BActive Publication Date: 2026-10-01HYUNDAE STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202317041900
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-12-09
Filing Date
2023-06-23
Publication Date
2026-10-01
Patent Text Reader

Abstract

A method for manufacturing a hot-stamped component, according to one embodiment of the present invention, comprises: a step of inserting a blank having a plating layer formed on at least one surface of a base material into a heating furnace having a plurality of sections having different temperature increase rate ranges; and a multi-stage heating step of heating the blank step by step through the plurality of sections, wherein the plurality of sections include: a first heating section having a first average temperature increase rate change rate; a second heating section, after the first heating section, having a second average temperature increase rate change rate different from the first average temperature increase rate change rate; and a third heating section, after the second heating section, having a third average temperature increase rate change rate different from the first average temperature increase rate change rate and the second average temperature increase rate change rate, the third average temperature increase rate change rate including a section in which a positive value changes to a negative value.
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELDThe present disclosure relates to a hot stamping component and a method ofmanufacturing the hot stamping component.BACKGROUNDAccording to the reinforcement of environmental regulations and safety standards in theautomobile industry, the need for high-strength and light-weight vehicle materials is increasing.As a method of manufacturing such high-strength and light-weight vehicle materials, hot stampingtechnology receives attention, and R&D on hot stamping materials is being actively conducted.The hot stamping process generally includes heating / forming / cooling / trimming, and mayutilize changes in microstructure, such as phase transformation of materials and alloying of platingduring the process. In this case, in the hot stamping process, there may be problems in that anamount of hydrogen mixed during heating or heat treatment is increased, and the performance ofcomponents, such as poor weldability according to the structure of the plating layer may bedeteriorated. In particular, microstructure characteristics of the hot stamping material are changedaccording to the heating or heat treatment temperature, and accordingly, hydrogen embrittlementand welding performance may be changed.Therefore, for the component performance of the hot stamping material, a precise controlusing the hot stamping heat treatment temperature condition is required. As a related technology,there is Korean Patent Laid-Open Publication No. 10-2013-0136565 (Title of the Invention: Steelplate for hot stamping member and manufacturing method thereof).SUMMARYTechnical ProblemProvided are a hot stamping component with improved component performance, such asstrength characteristics, hydrogen embrittlement according to an amount of hydrogen mixed, andweldability according to a structure of a plating layer by controlling a hot stamping heatingtemperature, and a method of manufacturing the hot stamping component.Technical SolutionAccording to an exemplary embodiment of the present disclosure, a method ofmanufacturing a hot stamping component, the method includes: inserting a blank including aplating layer formed on at least one surface of a base material into a heating furnace having aplurality of sections having different temperature increase rate ranges; and multi-stage heating theblank by gradually heating while passing through the plurality of sections, wherein the plurality ofsections includes: a first heating section having a first average temperature increase rate changerate; after the first heating section, a second heating section having a second average temperatureincrease rate change rate different from the first average temperature increase rate change rate; andafter the second heating section, a third heating section having a third average temperature increaserate change rate different from the first average temperature increase rate change rate and thesecond average temperature increase rate change rate, wherein the third average temperatureincrease rate change rate includes a section in which a positive value is changed to a negative value.Between the first heating section and the second heating section, the change from the firstaverage temperature increase rate change rate to the second average temperature increase ratechange rate may be discontinuous.The third heating section may include a 3-1 heating section having a 3-1 averagetemperature increase rate change rate and a 3-2 heating section having a 3-2 average temperatureincrease rate change rate, wherein the 3-1 average temperature increase rate change rate may havea positive value, and the 3-2 average temperature increase rate change rate may have a negativevalue, and an absolute value of the 3-1 average temperature increase rate change rate may be lessthan an absolute value of the 3-2 average temperature increase rate change rate.The first average temperature increase rate change rate and the second averagetemperature increase rate change rate each may have a negative value, and an absolute value of thefirst average temperature increase rate change rate may be greater than an absolute value of thesecond average temperature increase rate change rate.The plurality of sections, after the third heating section, may further include a fourthheating section having a fourth average temperature increase rate change rate different from thefirst average temperature increase rate change rate, the second average temperature increase ratechange rate, and the third average temperature increase rate change rate, and an absolute value ofthe fourth average temperature increase rate change rate may be less than the absolute value ofeach of the first average temperature increase rate change rate, the second average temperatureincrease rate change rate, and the third average temperature increase rate change rate.The 3-1 average temperature increase rate change rate may have a value of 0 or greaterand 0.25 °C / s2 or less, and the 3-2 average temperature increase rate change rate may have a valueof -0.3 °C / s2 or greater and 0 or less.The first average temperature increase rate change rate may have a value of -0.5 °C / s2 orgreater and 0 or less, and the second average temperature increase rate change rate may have avalue of -0.25 °C / s2 or greater and 0 or less.The plating layer may be alloyed in the second heating section, and the base material mayhave a phase transformation in the third heating section.According to an exemplary embodiment of the present disclosure, a hot stampingcomponent manufactured according to the method described above, the hot stamping componentincludes an amount of mixed hydrogen of 0 or greater and less than 0.21 ppm, and a dynamicresistance value of greater than 0 and 0.8 mΩ or less.Advantageous EffectsAccording to embodiments of the present disclosure, by controlling a temperature increaserate by section in a hot stamping heating process, the component performance of the hot stampingcomponent, such as strength characteristics, hydrogen embrittlement according to an amount ofmixed hydrogen, and weldability according to the structure of a plating layer, may be improvedBRIEF DESCRIPTION OF DRAWINGSFIG. 1 shows a flowchart illustrating a method of manufacturing a hot stampingcomponent according to an exemplary embodiment of the present disclosure;FIG. 2 shows a graph showing a temperature change of a blank when the blank is singleheated by the method of related art;FIG. 3 shows a graph illustrating a temperature change when a blank is heated in multiplestages and soaking-heated in a method of manufacturing a hot stamping component according toan exemplary embodiment of the present disclosure;FIG. 4 shows a graph showing a temperature increase rate change rate in a plurality ofsections according to a heating time in the method of manufacturing a hot stamping componentaccording to an exemplary embodiment of the present disclosure;FIG. 5 shows a scanning electron microscope (SEM) image showing a cross section of ahot stamping component according to an exemplary embodiment of the present disclosure;FIG. 6 shows an SEM image showing a cross-section of a hot stamping componentaccording to a comparative example of the present disclosure;FIG. 7 shows a schematic plan view illustrating a blank used in a method of manufacturinga hot stamping component according to an exemplary embodiment of the present disclosure; andFIG. 8 shows is a schematic plan view illustrating a blank inserted into a heating furnacein a method of manufacturing a hot stamping component according to an exemplary embodimentof the present disclosure.DETAILED DESCRIPTIONAs the present disclosure allows for various changes and numerous embodiments,particular embodiments will be illustrated in the drawings and described in detail in the writtendescription The advantages, features, and methods of achieving the advantages of the presentdisclosure may be clear when referring to the embodiments described below together with thedrawings. However, the present disclosure may have different forms and should not be construedas being limited to the descriptions set forth herein.It will be understood that, although the terms "first", "second", "third", etc., may be usedherein to describe various elements, these elements should not be limited by these terms. Theseterms are only used to distinguish one element from another.In the following embodiments, the singular forms include the plural forms unless thecontext clearly indicates otherwise.It will be further understood that the terms "comprises" and / or "comprising," when usedin this specification, specify the presence of stated features or constituent elements but do notpreclude the presence or addition of one or more other features or constituent elements.It will also be understood that when a film, a region, a constituent element is referred toas being "on" or "above" another element, the film, the region, or the constituent element may bein direct contact with the other element or other intervening film, region, or constituent elementmay be present.In the drawings, thicknesses of layers and regions may be exaggerated or reduced forconvenience of explanation. For example, the sizes and thicknesses of elements in the drawingsare arbitrarily expressed for convenience of explanation, and thus, the current inventive concept isnot limited to the drawings.When a certain embodiment may be implemented differently, a specific process order maybe performed differently from the described order. For example, two consecutively describedprocesses may be performed substantially at the same time or performed in an order opposite tothe described order.Hereafter, the present disclosure will be described more fully with reference to theaccompanying drawings. In describing the present disclosure with reference to drawings, likereference numerals are used for elements that are substantially identical or correspond to eachother.FIG. 1 shows a flowchart illustrating a method of manufacturing a hot stampingcomponent according to an exemplary embodiment of the present disclosure. Hereinafter, amethod of manufacturing a hot stamping component will be described with reference to FIG. 1.The method of manufacturing a hot stamping component according to an exemplaryembodiment of the present disclosure may include inserting a blank (S100) and multi-stage heating(S200), and after the multi-stage heating (S200), may further include transferring (S300), forming(S400), and cooling (S500).First, the operation of inserting a blank (S100 may be an operation of introducing a blankinto a heating furnace having a plurality of sections having different temperature increase rateranges. The blank may be provided in a form in which a plating layer is formed on at least onesurface of a base material.The blank inserted into the heating furnace may be formed by cutting a plate (or a basematerial) for forming a hot stamping component. The plate material may be manufactured byperforming hot rolling or cold rolling on a steel slab, followed by annealing heat treatment. Inaddition, after the annealing heat treatment, an Al-Si-based plating layer or a Zn plating layer maybe formed on at least one surface of the annealed sheet material, and the type of the plating layerformed on one surface of the base material is not limited thereto.After the operation of inserting a blank (S100), an operation of multi-stage heating (S200)may be performed. The operation of multi-stage heating (S200) may be an operation in which theblank passes through a plurality of sections provided in the heating furnace and is heated step bystep. The operation of multi-stage heating (S200) will be described in more detail below usinggraphs of FIGS. 2 to 4.After the operation of multi-stage heating (S200), operations of the transferring (S300),the forming (S400), and the cooling (S500) may be further performed.The operation of transferring (S300) may be an operation of transferring a blank that issoaking-heated during the multi-stage heating from the heating furnace to a press mold. In theoperation of transferring the soaking-heated blank from the heating furnace to the press mold, thesoaking-heated blank may be air-cooled for 7 seconds to 15 seconds, preferably, it may be aircooled for 10 seconds to 15 seconds.The operation of forming (S400) may be an operation of hot stamping the transferredblank to form a molded body. The operation of cooling (S500) may be an operation of cooling theformed molded body.After being molded into a final component shape in a press mold, a final product may beformed by cooling the molded body. A cooling channel through which a refrigerant circulates maybe provided in the press mold. The heated blank may be rapidly cooled at the same time as moldingby the circulation of the refrigerant supplied through the cooling channel provided in the pressmold. At this time, in order to prevent a spring back phenomenon of the plate material and maintaina desired shape, a rapid cooling may be performed while pressing the press die in a closed state.In the forming and cooling of the heated blank, the heated blank may be cooled at an averagecooling rate of at least 10 °C / s or greater to a martensite end temperature. The blank may be heldfor 3 to 20 seconds in the press mold. If the holding time in the press mold is less than 3 seconds,a sufficient amount of martensite may not be generated and mechanical properties may not besecured. In addition, when the holding time in the press mold exceeds 20 seconds, the holding timein the press mold becomes long, and thus, productivity may decrease.FIG. 2 shows a graph showing a temperature change of the blank when the blank is singleheated by the method of the related art. Specifically, FIG. 2 shows a graph showing the temperaturechange of blanks with time when a blank with a thickness of 1.2 mm and a blank with a thicknessof 1.6 mm are simultaneously single heated (310, 320) after setting the temperature of the furnaceso that the internal temperature of the furnace is maintained equal to a target temperature Tt of theblank.In this case, the target temperature Tt of the blank may be equal to or greater than Ac3 (atemperature at which the transformation from ferrite to austenite is completed). Preferably, thetarget temperature Tt of the blank may be about 930 °C. More preferably, the target temperature Ttof the blank may be about 950 °C. However, the present disclosure is not limited thereto. Inaddition, the single heating is not heating by putting a blank having a thickness of 1.2 mm and ablank having a thickness of 1.6 mm into the heating furnace, respectively, but means a case inwhich a blank having a thickness of 1.2 mm and a blank having a thickness of 1.6 mm aresimultaneously introduced into the furnace and heated after setting the temperature of the furnaceto a single temperature.Referring to FIG. 2, after setting the temperature inside the heating furnace to the sametemperature as the target temperature Tt of the blank, when a blank having a thickness of 1.2 mmand a blank having a thickness of 1.6 mm are single heated at the same time, it may be seen thatthe blank having a thickness of 1.2 mm reaches the target temperature Tt earlier than the blankhaving a thickness of 1.6 mm.That is, the blank having a thickness of 1.2 mm first reaches the target temperature Tt, andis soaking-heated for a first time S1 (310), and the blank having a thickness of 1.6 mm may besoaking-heated for a second time S2 (320) that is shorter than the first time S1 (310). Because thesoaking heating time is adjusted based on the blank reaching the target temperature late, the blankwith a thickness of 1.2 mm that has reached the target temperature first may be overheated, andthus, hydrogen-delayed rupture of the blank having a thickness of 1.2 mm increases, andweldability may be reduced.In addition, when a control range is set based only on the target temperature Tt and timeof the hot stamping process, there is a problem in that the performance of the component may notbe effectively controlled. For example, a component including an Al-Si plating layer may beaccompanied by an alloying of the plating layer and a phase transformation operation of a basematerial during the hot stamping process. At this time, depending on the temperature historyapplied to the component and the control of the hot stamping process, the structure of a platinglayer, the thickness of an interdiffusion layer, peeling of a plating layer, the formability, hydrogenembrittlement, and weldability are determined differently. The conventional hot stamping processmay be controlled based on the above-mentioned final target temperature Tt or an overalltemperature increase rate. Because there is a limit to precisely controlling the performance ofcomponents by simply controlling the process using only the target temperature and time,hereinafter, in the embodiments of the present disclosure, the component performance is easilyand precisely controlled by controlling the temperature increase rate change rate for a blank.Hereinafter, with reference to FIGS. 3 and 4, a plurality of sections in which a blank passesand is heated step by step in the operation of multi-stage heating will be described.FIG. 3 shows a graph illustrating a temperature change when a blank is heated in multiplestages and soaking-heated in the method of manufacturing a hot stamping component accordingto an exemplary embodiment of the present disclosure. More specifically, FIG. 3 is a graphshowing a temperature change according to time, that is, shows a temperature change accordingto time in an exemplary embodiment of the present invention in the case when a blank having athickness of 1.2 mm is multi-stage heated 510 and a blank having a thickness of 1.6 mm is multistage heated 520.Referring to FIG. 3, a heating furnace according to an exemplary embodiment may includea plurality of heating sections P1, P2, P3, and P4 having different temperature ranges. Morespecifically, the heating furnace may include a first heating section P1 having a first temperaturerange T1, a second heating section P2 having a second temperature range T2, a third heatingsection P3 having a third temperature range T3, and a fourth heating section P4 having a fourthtemperature range T4. In this case, the third heating section T3 may include two sections havingdifferent temperature ranges. The third heating section T3 may include a 3-1 heating section P3-1having a 3-1 temperature range T3-1, and a 3-2 heating section P3-2 having a 3-2 temperaturerange T3-2. According to an exemplary embodiment, the second heating section T2 may includea plurality of sections having different temperature ranges. The second heating section T2 mayinclude a 2-1 heating section P2-1 having a 2-1 temperature range T2-1 to a 2-n heating sectionP2-n having a 2-n temperature range T2-n. Also, the first heating section P1 may include a pluralityof sections having different temperature ranges. The first heating section P1 may include a 1-1heating section P1-1 having a 1-1 temperature range T1-1 to a 1-n heating section P1-n having a1-n temperature range T1-n.The first heating section P1 to the fourth heating section P4 may be sequentially arrangedin the heating furnace. The first heating section P1 may be adjacent to an inlet of the heatingfurnace into which the blank is placed, and the fourth heating section P4 may be adjacent to anoutlet of the heating furnace through which the blank is discharged. Accordingly, the first heatingsection P1 having the first temperature range T1 may be the first section of the heating furnace,and the fourth heating section P4 having the fourth temperature range T4 may be the last sectionof the heating furnace. As will be described later, the fourth heating section P4, which is the lastsection among the plurality of sections of the heating furnace, may be a section in which soakingheating is performed, not a section in which multi-stage heating is performed.The temperature of a plurality of sections provided in the heating furnace, for example,the temperature of the first heating section P1 to the fourth heating section P4 may increase in adirection towards the outlet of the heating furnace from which the blank is discharged from theinlet of the heating furnace through which the blank is placed. In addition, a temperature differencebetween two adjacent sections among the plurality of sections provided in the heating furnace maybe greater than 0 °C and less than or equal to 100 °C. For example, the temperature differencebetween the first heating section P1 and the second heating section P2 may be greater than 0 °Cand equal to or less than 100 °C.In an exemplary embodiment, the first temperature range T1 of the first heating sectionP1 may be in a range from about 840 °C to about 860 °C, and in a range from about 835 °C toabout 865 °C. The second temperature range T2 of the second heating section P2 may be in a rangefrom about 870 °C to about 920 °C, and in a range from about 865 °C to about 925 °C. The 3-1temperature range T3-1 of the 3-1 heating section P3-1 may be in a range from about 920 °C toabout 940 °C, and in a range from about 915 °C to about 945 °C. The 3-2 temperature range T3-2of the 3-2 heating section P3-2 may be in a range from about 940 °C to about 960 °C, and in a rangefrom about 935 °C to about 965 °C. The fourth temperature range T4 of the fourth heating sectionP4 may be in a range from about Ac3 to about 1,000 °C. Preferably, the fourth temperature rangeT4 of the fourth heating section P4 may be 930 °C or greater and 1,000 °C or less. More preferably,the fourth temperature range T4 of the fourth heating section P4 may be 950 °C or greater and1,000 °C or less.According to an exemplary embodiment, when the second heating section P2 includes the2-1 heating section P2-1 and the 2-2 heating section P2-2 having different temperature ranges asdescribed above, the 2-1 temperature range T2-1 may be in a range from about 870 °C to about890 °C, and may be in a range from about 865 °C to about 895 °C, and the 2-2 temperature rangeT2-2 of the 2-2 heating section P2-2 may be in a range from about 900 °C to about 920 °C, and ina range from about 895 °C to about 925 °C.Boundary values defining the plurality of sections described above will be described. Theboundary values represent the heating time range (sec) as the horizontal axis of the graph. First, afirst boundary value e1 positioned between the first heating section P1 and the second heatingsection P2 may be in a range from about 30 sec to about 50 sec, and may be about 40 sec. Thesecond boundary value e2 positioned between the second heating section P2 and the third heatingsection P3 may be in a range from about 80 sec to about 130 sec, and may be about 85 sec. Thethird boundary value e3 positioned between the 3-1 heating section P3-1 and the 3-2 heatingsection P3-2 may be in a range from about 110 sec to about 180 sec, and may be about 120 sec.The fourth boundary value e4 positioned between the 3-2 heating section P3-2 and the fourthheating section P4 may be in a range from about 140 sec to about 230 sec, and may be about 150sec.According to an exemplary embodiment, when the second heating section P2 includes the2-1 heating section P2-1 and the 2-2 heating section P2-2 having different temperature ranges asdescribed above, a 2-1 boundary value e2' positioned between the 2-1 heating section P2-1 and the2-2 heating section P2-2 may be in a range from about 50 sec to about 110 sec, and may be about60 sec.In FIG. 3, the heating furnace according to an exemplary embodiment of the presentdisclosure is illustrated as having five sections P1, P2, P3-1, P3-2, and P4 having differenttemperature ranges, but the present disclosure is not limited thereto. Five, seven, or eight sectionshaving different temperature ranges may be provided in the heating furnace.FIG. 4 is a graph showing a temperature increase rate change rate in a plurality of sectionsaccording to heating time in the method of manufacturing a hot stamping component according toan exemplary embodiment of the present disclosure, that is, a graph showing a temperatureincrease rate (°C / s) of a blank according to heating time (s). The plurality of sections and boundaryvalues illustrated in FIG. 4 have the same contents as those described above in FIG. 3, anddescriptions may be simplified or omitted.Referring to FIG. 4, the distribution of the temperature increase rate (°C / s) or thetemperature increase rate change rate (°C / s2) in a plurality of sections in which the multi-stageheating of a blank is performed is as described below. Hereinafter, the term "temperature increaserate change rate" refers to an average slope of each section of the graph shown in FIG. 4, and maybe described as 'average temperature increase rate change rate'. Hereinafter, the 'averagetemperature increase rate change rate' in one section may be defined as, for example, a valueobtained by dividing a difference between the initial temperature increase rate and the finaltemperature increase rate in the corresponding section by the time of the corresponding section.FIG. 4 shows a temperature increase rate first control curve 610 (hereinafter, a first control curve610) according to an exemplary embodiment of the present disclosure and a temperature increaserate second control curve 620 (hereinafter, a second control curve 620) according to a comparativeexample.First, the first control curve 610 according to an exemplary embodiment of the presentdisclosure will be described.The first heating section P1 may have a first average temperature increase rate change rater1. The second heating section P2 positioned after the first heating section P1 may have a secondaverage temperature increase rate change rate r2 different from the first average temperatureincrease rate change rate r1. The third heating section P3 positioned after the second heatingsection P2 may have a third average temperature increase rate change rate r3 different from thefirst and second average temperature increase rate change rates r1 and r2. In this case, the thirdaverage temperature increase rate change rate r3 may include a section in which a positive valueis changed to a negative value. The fourth heating section (P4) positioned after the third heatingsection P3 may have a fourth average temperature increase rate change rate r4 different from thefirst, second, and third average temperature increase rate change rates r1, r2, and r3.The first heating section P1 may be a general temperature rising section, and in the secondheating section P2, the temperature increase rate is gently decreased (|r1|>|r2|) compared to thefirst heating section P1, and thus, alloying of a plating layer may be performed. The third heatingsection P3 is a phase transformation section in which a base material of a blank undergoes phasetransformation, and the 3-1 heating section P3-1 may have a positive (+) temperature increase ratechange rate, and the 3-2 heating section P3-2 may have a negative (-) temperature increase ratechange rate. The fourth heating section P4 may be a stabilization section in which a blank issoaking-heated with a uniform temperature.Referring to the first control curve 610, the first average temperature increase rate changerate r1 and the second average temperature increase rate change rate r2 respectively have a negativevalue, an absolute value of the first average temperature increase rate change rate r1 may be greaterthan an absolute value of the second average temperature increase rate change rate r2 (|r1|>|r2|).The first average temperature increase rate change rate r1 may be about -0.5 °C / s2or greater and 0 or less, for example, about -0.3 °C / s2. The second average temperature increase rate change rate r2 may be greater than or equal to about -0.25 °C / s2 and less than or equal to 0, for example, about -0.07 °C / s2.Between the first heating section P1 and the second heating section P2, that is, in thevicinity of the first boundary value e1, the change from the first average temperature increase ratechange rate r1 to the second average temperature increase rate change rate r2 is discontinuous.More specifically, a temperature increase rate v1 in the first boundary value e1 defining the firstaverage temperature increase rate change rate r1 in the first heating section P1 and a temperatureincrease rate v2 in the first boundary value e1 defining the average temperature increase ratechange rate r2 in the second heating section P2 may have different values. In other words, the finaltemperature increase rate v1 of the first average temperature increase rate change rate r1 and theinitial temperature increase rate v2 of the second average temperature increase rate change rate r2may be different values. When the temperature increase rate change rate discontinuously changesin the vicinity of the first boundary value e1 (r1 -> r2) (610), the weldability of a hot stampingcomponent may be improved when compared to the case when the temperature increase ratechange rate continuously changes (620).The discontinuous change of the average temperature increase rate change rate betweenthe first heating section P1 and the second heating section P2 is because a lot of energy is requiredto a plating layer change. In order for Fe of a base material to be diffused into an Al plating layerand an Al-Fe phase is initially generated and grown in the plating layer, the supply of necessaryenergy is needed. In addition, Fe diffused into the base material generates an Al-Fe-Si alloy layerover time, and the more discontinuous the change in the temperature increase rate change rate nearthe first boundary value e1, the more uniform diffusion to a surface, and thus, favorable weldabilitymay be obtained. On the other hand, when the change in the temperature increase rate change rateis continuous, because the diffusion of Al-Fe-Si to the surface is fast and non-uniform, phases withhigh welding resistance presents on the surface, resulting in poor weldability.The third heating section P3 may include a 3-1 heating section P3-1 having a 3-1temperature increase rate change rate r3-1, and a 3-2 heating section P3-2 having a 3-2 temperatureincrease rate change rate r3-2. The 3-1 average temperature increase rate change rate r3-1 has apositive value, the 3-2 average temperature increase rate change rate r3-2 has a negative value, andthe third average temperature increase rate change rate r3 may have a section in which a positivevalue changes to a negative value. In this case, an absolute value of the 3-1 average temperatureincrease rate change rate r3-1 may be less than an absolute value of the 3-2 average temperatureincrease rate change rate r3-2 (|r3-1|<|r3-2|). The 3-1 average temperature increase rate change rater3-1 may be 0 or greater and about 0.25 °C / s2 or less, and for example, the 3-1 average temperatureincrease rate change rate r3-1 may be about 0.07 °C / s2 . The 3-2 average temperature increase ratechange rate r3-2 may be about -0.3 °C / s2 or greater and 0 or less, for example, about -0.08 °C / s2.As the third average temperature increase rate change rate r3 in the 3-1 heating sectionP3-1 is smaller and as the slope of the first control curve 610 is gentle, the amount of mixedhydrogen decreases, and thus, hydrogen embrittlement is improved. However, the second controlcurve 620 has a form in which the temperature increase rate change rate rapidly increases ordiscontinuously increases in the 3-1 heating section P3-1. In this case, the amount of mixedhydrogen increases, and thus, hydrogen embrittlement may be reduced. In this way, unlike betweenthe first heating section P1 and the second heating section P2, in the third heating section P3, as asection in which a phase transformation of the base material is performed, if there is a rapidtemperature change, there may be problems, such as hydrogen embrittlement and delayed rupture,thus, the lower the temperature increase rate change rate, the more advantageous.Between the second heating section P2 and the 3-1 heating section P3-1, that is, in thevicinity of the second boundary value e2, the change from the second average temperature increaserate change rate r2 to the 3-1 average temperature increase rate change rate r3-1 is a change froma negative value to a positive value. That is, as the temperature increase rate decreases and thenincreases, a phase transformation of a base material may occur. For example, during the phasetransformation of the base material, when transforming to austenite in the corresponding section,an endothermic reaction occurs. Because energy supply is required for the endothermic reaction,the temperature increase rate must be increased again in the 3-1 heating section P3-1 to induce areasonable level of phase transformation into austenite.Between the 3-1 heating section P3-1 and the 3-2 heating section P3-2, that is, in thevicinity of the third boundary value e3, the change from the 3-1 average temperature increase ratechange rate r3-1 the 3-2 average temperature increase rate change rate r3-2 is a change from apositive value to a negative value. That is, as the temperature increase rate increases and thendecreases again, a phase transformation of a base material may occur. As the phase transformationprogresses, the endothermic reaction requires a large amount of thermal energy, and thus, thetemperature increase rate increases, but as the phase transformation progresses, the amount ofaustenite increases, and accordingly, the thermal energy required for the endothermic reaction maygradually decrease in the 3-2 heating section P3-2, and thus, the temperature increase rate maydecrease.An absolute value of the fourth average temperature increase rate change rate r4 may beless than an absolute value of each of the first average temperature increase rate change rate r1,the second average temperature increase rate change rate r2, and the third average temperatureincrease rate change rate r3. For example, the fourth average temperature increase rate change rater4 is a value close to zero, and the fourth heating section P4 may be a section soaking-heated witha uniform temperature. In the fourth heating section P4, the heating time t4 of the blank may beabout 50% or less of the total heating time t. This means that the longer the time t4 during whichthe blank is soaking-heated in the fourth heating section P4 compared to the time t1 in which theblank is heated in multiple stages in the first to third heating sections P1, P2, and P3, the componentcharacteristics, such as weldability, hydrogen embrittlement, and bending performance may bereduced. For example, a ratio (t1:t4) of a length of the multi-stage heating sections P1, P2, and P3to a length of the soaking-heating section P4 may satisfy 1:1 to 4:1.Hereinafter, the characteristic of the second control curve 620 compared to the first controlcurve 610 described above will be described, but differences from the first control curve 610 willbe mainly described. Referring to the second control curve 620, a first' average temperatureincrease rate change rate r1' between the first heating section P1 and the second heating section P2is continuously changed. More specifically, a temperature increase rate in the first boundary valuee1 defining the first' average temperature increase rate change rate r1' in the first heating sectionP1, and a temperature increase rate v1' in the first boundary value e1 defining the first' averagetemperature increase rate change rate r1' the in the second heating section P2 may have the samevalue.The first' average temperature increase rate change rate r1' may be about -0.26 °C / s2 or greater and 0 or less, for example, about -0.2 °C / s2. The change characteristics of the temperature increase rate change rates r3', r3-1', and r3-2' in the third heating section P3 of the second control curve 620 may have the same as those described in the first control curve 610. However, the 3-1' temperature increase rate change rate r3-1' may have a discontinuous and unstable value compared to the 3-1 average temperature increase rate change rate r3-1 of the first control curve 610. In this case, the 3-1' temperature increase rate change rate r3-1' may denote a rate of change at a front end in which the temperature increase rate shows an increasing trend during the 3-1 heating section P3-1. The 3-1' temperature increase rate change rate r3-1' may be about 0.04 °C / s2 or greater and about 0.16 °C / s2 or less, for example, about 0.1 °C / s2 . The 3-2' temperature increase rate change rate r3-2' may be about -0.16 ° °C / s2 or greater and about -0.04 °C / s2 or less, for example, about - 0.1 °C / s2 . The fourth heating section P4 of the second control curve 620, like the first control curve610, may be a soaking-heating section in which the fourth average temperature increase ratechange rate r4 has a value close to zero.In this way, in the method of manufacturing a hot stamping component according to anexemplary embodiment of the present disclosure, by controlling the temperature increase ratechange rate for each section according to the characteristics of a plurality of sections as describedabove, component characteristics, such as ultra-high strength characteristics of a hot stampingcomponent, weldability, hydrogen embrittlement, and bending performance may be preciselycontrolled and improved. Component characteristics of a hot stamping component according toembodiments will be described in more detail with reference to FIGS. 5 and 6 to be described later.A relationship between the heating time s shown in the horizontal axis of FIG. 4 andboundary values is not limited to that shown in FIG. 4, and various changes may be applied withinthe range of improving the component performance of the hot stamping component according tothe present disclosure. In the above, the plurality of sections has been described as having fivesections, but the plurality of sections may be differently classified according to the distribution ofthe temperature increase rate change rate.FIG. 5 shows a scanning electron microscope (SEM) image showing a cross section of ahot stamping component according to an exemplary embodiment of the present disclosure. Thehot stamping component 1 shown in FIG. 5 may be a hot stamping component manufactured byusing the method of manufacturing a hot stamping component according to an exemplaryembodiment of the present disclosure (e.g., the curve 610 in FIG. 4).Referring to FIG. 5, the hot stamping component 1 may include a base material 10 and aplating layer 20 including a plurality of layers 21, 22, 23, and 24 positioned on the base material10. The base material 10 may be a steel sheet manufactured by performing a hot rolling processand / or a cold rolling process on a steel slab cast to include a predetermined alloying element in apredetermined content. For example, the steel sheet may include carbon (C), silicon (Si),manganese (Mn), phosphorus (P), sulfur (S), titanium (Ti), boron (B), remnant iron (Fe), and otherunavoidable impurities. In addition, the steel sheet may further include one or more componentsof niobium (Nb), molybdenum (Mo), and aluminum (Al).The plating layer 20, as an alloying layer, may be formed on at least one surface of thebase material 10 and may include aluminum (Al), iron (Fe), or the like. The plating layer 20 mayinclude a plurality of layers 21, 22, 23, and 24 sequentially stacked on the base material 10. In thehot stamping component 1 according to an exemplary embodiment of the present disclosure, asshown in FIG. 5, the plating layer 20 may be clearly divided into four layers. For example, theplurality of layers 21, 22, 23, and 24 may sequentially have a α-Fe phase, Fe2Al5 phase, AlFe phase,and Fe2Al5 phase, but the composition of the plurality of layers is not limited thereto. In the hotstamping component 1 shown in FIG. 5, an amount of mixed hydrogen may be 0 ppm or greaterand less than 0.21 ppm, and a dynamic resistance value may be greater than 0 mΩ and 0.8 mΩ orless.FIG. 6 shows a SEM image showing a cross-section of a hot stamping component 1'according to an exemplary embodiment of the present disclosure, and portions that are differentfrom the cross-section of FIG. 5 will be mainly described. The hot stamping component 1' of FIG.6 may be a component manufactured by using the method of manufacturing a hot stampingcomponent according to an exemplary embodiment of the present disclosure (e.g., the secondcontrol curve 620 in FIG. 4).The hot stamping part 1' illustrated in FIG. 6 may include a base material 10 and a platinglayer 30 positioned on the base material 10. Unlike the plating layer 20 of FIG. 5, the plating layer30 may be a single layer rather than a plurality of layers, and may have a thickness less than thatof the plating layer 20. According to an exemplary embodiment, the plating layer 30 may have anunclear boundary even if the plating layer 30 includes a plurality of layers. The plating layer 30may include at least one of Al, Fe, and Si. In the hot stamping component 1' shown in FIG. 6, anamount of mixed hydrogen may be 0 ppm or greater and less than 0.35 ppm, and the dynamicresistance value may be 0.5 mΩ or greater and 1.5 mΩ or less.Hereinafter, using Table 1 together, the characteristics of the hot stamping components 1and 1' according to FIGS. 5 and 6 described above will be compared and described. The evaluationcontents described in the Table 1 below may be relative comparison results.Table 1The plating layer 20 of FIG. 5 includes more layers than the plating layer 30 of FIG. 6,and at this time, boundaries between the plurality of layers may also become clear. Accordingly,a thickness of the plating layer 20 is greater than a thickness of the plating layer 30. Here, referringto FIG. 4 together, thickness characteristics of the plating layer and control characteristics of thefirst control curve 610 may be obtained as a result of mutual influence. For example, when theplating layer has a large thickness, during heating the first heating section P1 and the secondheating section P2, the temperature increase rate change rate between the first and second heatingsections P1 and P2 may be discontinuously changed, and in the third heating section P3, the slopeof the first control curve 610 may be gentle, that is, the temperature increase rate change rate maybe small.On the other hand, as the thickness of the plating layer increases, the amount of mixedhydrogen decreases and the hydrogen embrittlement of the blank becomes excellent. Because thethickness of the plating layer 20 of FIG. 5 is large, as described above, the amount of mixedhydrogen in the component 1 (less than about 0.21 ppm) of FIG. 5 is less than in the component 1'(less than about 0.35 ppm) of FIG. 6, and accordingly, hydrogen embrittlement is higher, and therisk of hydrogen delayed rupture may be reduced.In addition, a surface resistance of the component 1 of FIG. 5 may be less than that of thecomponent 1' of FIG. 6 due to the thickness characteristics described above of the plating layer. Inaddition, the less the dynamic resistance, the better the weldability. As described above, becausethe dynamic resistance value of the component 1 of FIG. 5 (about 0.8 mΩ or less) is less than thatof the component 1' of FIG. 6 (about 0.8 mΩ or less), it may be seen that the component 1 of FIG.5 has superiority in weldability.As described above, according to the method of manufacturing a hot stamping componentaccording to an exemplary embodiment of the present disclosure, precise control of a componentis possible by controlling the temperature increase rate change rate for each section, and thereby,there is an advantage of improving component performance, such as weldability, hydrogenembrittlement, and ultra-high strength of the hot stamping component.FIG. 7 shows a plan view schematically illustrating a blank 200 used in a method ofmanufacturing a hot stamping component according to an exemplary embodiment of the presentdisclosure.Referring to FIG. 7, the blank 200 according to an exemplary embodiment may include atleast one of a blank 210 having a single thickness, a taylor welded blank (TWB) 220 obtained bycutting and welding different shapes of plates having different thicknesses into a required shape, atailor rolled blank (TRB) 230 having different thicknesses by rolling a single-thickness plate, anda patchwork 240 manufactured by welding a small patch blank to a large blank.The TWB 220 may be manufactured by welding a first plate material 221 and a secondplate material 223 having different thicknesses from each other. A B-pillar, which is an importantcomponent for collision members of a vehicle, is a form in which plates of different strengths arecombined in an upper collision supporter and a lower shock absorber, and is manufactured bywelding the two plates and then forming them. A TWB method, which is mainly used at this time,refers to a series of processes for manufacturing components by cutting and welding different typesof sheets with different thicknesses, strengths, and materials to a required shape, and then pressforming to manufacture components. By manufacturing blanks having different thicknesses bywelding plates having different thicknesses, it is possible to have different properties for each partof the blank. For example, an ultra-high-strength plate of 120 to 150K grade is used for thecollision supporter of an upper part of the B-pillar, and a plate with good shock absorptionperformance is connected to a lower part of the B-pillar where stress is concentrated to improveshock absorption ability in the event of a vehicle collision.The TRB 230 may be manufactured by rolling a cold-rolled steel material to have aspecific thickness profile, and when manufacturing a hot stamping component using the TRB 230,light-weight effect is excellent. For example, the thickness profile may be performed by using amethod of the related art. For example, when the cold-rolled steel material is cold-rolled, the TRB230 including a first region 231 having a first thickness, a second region 232 having a secondthickness, a third region 233 having a third thickness, and a fourth region 234 having a fourththickness may be formed. In this case, the first thickness, the second thickness, the third thickness,and the fourth thickness may be different from each other, and a transition period 235 may existbetween the first region 231 and the second region 232, between the second region 232 and thethird region 233, and between the third region 233 and the fourth region 234, respectively.However, in FIG. 2, it is illustrated that the TRB 230 includes the first to fourth regions 231 to234, the present disclosure is not limited thereto. The TRB 230 may be formed to include a firstregion 231, a second region 232, . . . , and an nth region.The patchwork 240 is a method of partially reinforcing a base material using at least twoor more plate materials, and the patch is bonded to the base material before molding process sothat the base material and the patch may be formed at the same time. For example, after welding apatch 243 having a second size less than a first size to a base material 241 having the first size,they may be simultaneously molded.FIG. 8 is a schematic plan view illustrating a blank inserted into a heating furnace in amethod of manufacturing a hot stamping component according to an exemplary embodiment ofthe present disclosure. Hereinafter, the method will be described with reference to FIG. 1.In the operation of inserting a blank (S100), at least two blanks 200 different from eachother in at least one of a thickness and a size may be simultaneously introduced into a heatingfurnace.For example, FIG. 8 shows two first blanks 250 and two second blanks 260 that aresimultaneously introduced into the heating furnace. In this case, the first blank 250 and the secondblank 260 may have different sizes and different thicknesses. For example, the first blank 250 mayhave a thickness of about 1.2 mm, and the second blank 260 may have a thickness of about 1.6mm. However, the present disclosure is not limited thereto, and one first blank 250 and one secondblank 260 may be simultaneously introduced into the heating furnace. In addition, the first blank250 and the second blank 260 have the same size but different thicknesses, or are formed to havedifferent sizes with the same thickness, and various modifications are possible.In another embodiment, in the operation of inserting a blank (S100), at least two blanks200 having a single thickness may be simultaneously introduced into the heating furnace. Forexample, at least two or more blanks 240 having a thickness of 1.2 mm may be simultaneouslyinput, or at least two or more blanks 250 having a thickness of 1.6 mm may be simultaneouslyintroduced into the heating furnace. In addition, in the operation of inserting a blank (S100), theTWB 220 (refer to FIG. 7) or the TRB (230, refer to FIG. 7) may be introduced into the heatingfurnace.A blank introduced into the heating furnace may be transported along a transport directionafter being mounted on a roller (S300).After the operation of inserting a blank (S100), an operation of multi-stage heating (S200)may be performed. The operation of multi-stage heating (S200) may be an operation in which theblank passes through a plurality of sections provided in the heating furnace and is heated gradually,and may include at least one section in which soaking-heating is performed.As described above, while the present disclosure has been described with reference toexemplary embodiments shown in the drawings. However, it will be understood by those ofordinary skill in the art that various changes in form and details may be made therein withoutdeparting from the spirit and scope of the inventive concept. Accordingly, the scope of the presentdisclosure is defined not by the detailed description of the invention but by the appended claims.

Claims

1. A method of manufacturing a hot stamping component, the method comprising: inserting a blank comprising a plating layer formed on at least one surface of a base material into a heating furnace having a plurality of sections having temperature increase rate ranges different from each other; and multi-stage heating the blank by gradually heating while passing through the plurality of sections, wherein the plurality of sections comprise: a first heating section having a first average temperature increase rate change rate; after the first heating section, a second heating section having a second average temperature increase rate change rate different from the first average temperature increase rate change rate; and after the second heating section, a third heating section having a third average temperature increase rate change rate different from the first average temperature increase rate change rate and the second average temperature increase rate change rate, wherein the third average temperature increase rate change rate comprises a section in which a positive value is changed to a negative value.

2. The method of claim 1, wherein between the first heating section and the second heating section, a change from the first average temperature increase rate change rate to the second average temperature increase rate change rate is discontinuous.

3. The method of claim 1, wherein the third heating section comprises a 3-1 heating section having a 3-1 average temperature increase rate change rate and a 3-2 heating section having a 3-2 average temperature increase rate change rate, wherein the 3-1 average temperature increase rate change rate has a positive value, and the 3-2 average temperature increase rate change rate has a negative value, and an absolute value of the 3-1 average temperature increase rate change rate is less than an absolute value of the 3-2 average temperature increase rate change rate.

4. The method of claim 1, wherein the first average temperature increase rate change rate and the second average temperature increase rate change rate each have a negative value, and an absolute value of the first average temperature increase rate change rate is greater than an absolute value of the second average temperature increase rate change rate.

5. The method of claim 1, wherein the plurality of sections, after the third heating section, further comprises a fourth heating section having a fourth average temperature increase rate change rate different from the first average temperature increase rate change rate, the second average temperature increase rate change rate, and the third average temperature increase rate change rate, and an absolute value of the fourth average temperature increase rate change rate is less than the absolute value of each of the first average temperature increase rate change rate, the second average temperature increase rate change rate, and the third average temperature increase rate change rate.

6. The method of claim 3, wherein the 3-1 average temperature increase rate change rate has a value of 0 or greater and 0.25 °C / s2 or less, and the 3-2 average temperature increase rate change rate has a value of -0.3 °C / s2 or greater and 0 or less.

7. The method of any one of claims 4 and 6, wherein the first average temperature increase rate change rate has a value of -0.5 °C / s2 or greater and 0 or less, and the second average temperature increase rate change rate has a value of -0.25 °C / s2 or greater and 0 or less.

8. The method of claim 1, wherein the plating layer is alloyed in the second heating section, and the base material has a phase transformation in the third heating section.

9. A hot stamping component manufactured according to any one of claims 1 to 8, the hot stamping component comprising an amount of mixed hydrogen of 0 or greater and less than 0.21 ppm, and a dynamic resistance value of greater than 0 and 0.8 mΩ or less.