A method for concentrating carbon from direct reduced iron (DRI) char fines
Patent Information
- Application Number
- IN202331006362
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-01-31
- Publication Date
- 2026-10-05
Abstract
Description
TECHNICAL FIELDThe present disclosure relates to a beneficiation process for recovering carbon values fromDirect Reduced Iron (DRI) char fines. Particularly, the present disclosure relates to a methodfor concentrating carbon from DRI char fines to yield a carbon concentrate product having ahigh amount of Fixed Carbon content and low ash content and which can be used as a feed forsinter or pellet plant.BACKGROUND OF THE DISCLOSURESponge iron is the final product of coal fired rotary kilns. The schematic diagram in Figure 1describes the unit processes involved in a sponge iron production plant. The major rawmaterials used in sponge iron production include iron ore (hematite or Fe2O3), non-coking coal,and limestone / dolomite. The iron ore and non-coking coal are reduced to the required size incrushers. Iron ore, coal, and dolomite of required proportion are fed into the kiln continuouslyfrom the feed end. The raw materials move along the length of the kiln with the preset rotation.Secondary air is blown into the kiln through air pipes located along the kiln length. Thetemperatures of different heating zones are measured and controlled using thermocouplesmounted on the kiln. Fine coal is injected at the discharge end of the kiln to meet additionalcarbon requirements for the reactions. As the charge moves along the kiln length, it graduallygoes through three zones: Pre-heating zone, which accounts for about 30% of the kiln length,wherein both moisture and volatile matter present in feed mixture are removed; Reduction zone(at 900-1050 degree) wherein reduction is carried out by picking up heat from the hot gasesflowing in the opposite direction of the charge (3rd zone is soaking zone). The product of kiln(Direct Reduced Iron (DRI) and char mix) is then cooled in a rotatory cooler with externalcooling system and sent to a product separation area where vibratory screens and magneticseparators are used. The product is first screened in a double deck screen having 20 mm and 3mm screens. The particles having size greater than 20mm are removed first and sent to amagnetic separator to get lump DRI product. The particles having size less than 20 mm screenare screened in the 3 mm screen and then each fraction is passed through magnetic separator.The magnetic portion of each fraction is DRI.The non-magnetic fraction of above 3 mm size is mostly char which can be recycled to the kilnif desired or can be used in power plant boiler as fuel. The non-magnetic fraction of -3 mmwhich is composed mostly of spent calcined dolomite, ash and fine char is usually discarded.Among them, char fines (-3 mm size) display complex liberation characteristics with respectto carbon values due to following reasons: [1] high temperatures change the physical propertyof carbon particles (no role of hydrophobicity during beneficiation); [2] carbon particles getentrapped inside the fused iron particles during reduction; [3] liberation of carbon particlesneed fine grinding at suitable size and then beneficiation. In view of this, there is a need todevelop a process for recovering carbon values or concentrating carbon from DRI char fines,such that they may be used for different applications, for instance, as a feed for sinter / pelletmaking processes.There are prior studies that disclose concentrating carbon from different raw materials:US20080047880A1 describes a system and method for beneficiating, or "cleaning", ultra-fineraw coal with spiral concentrators.US3770213A reaches separation of carbon particles from iron oxide particles and other gangueparticles contained in blast furnace flue dust using froth flotation technology.US 5456363A describes an improved froth flotation method for the removal and recovery ofan ultra-fine constituent such as carbon from tailings such as fly ash.US 8051985B2A describes a method to remove unburned carbon from coal ash, comprisingthe steps of; mechanically separating the unburned carbon from the coal ash using a dry typeclassifying unit; and grinding or crushing the coal ash from which the unburned carbon hasbeen partially removed by means of a dry type grinding unit.KR 20030016555A describes a separation apparatus and a separating method in order toseparate unburned carbon powders in fly ash by a complex corona-electrostatic field.However, there are no studies on concentrating carbon from DRI char fines in order to increasetheir value and use them for further applications rather than merely discarding them. Thepresent disclosure addresses this need.STATEMENT OF THE DISCLOSUREThe present disclosure relates to a method for concentrating carbon from Direct Reduced Iron(DRI) char fines, comprising: a. grinding DRI char fines to a size less than 0.5 mm to provideground char fines, b. mixing the ground char fines with water to prepare a slurry, c. feeding theslurry into a concentrator to separate the slurry into three fractions: a light fraction (topfraction), a middle fraction (middling), and a heavy fraction (reject), d. drying the middle andthe light fractions to obtain dried fractions and e. combining the dried fractions to provide acarbon concentrate product.BRIEF DESCRIPTION OF THE ACCOMPANYING FIGURESIn order that the disclosure may be readily understood and put into practical effect, referencewill now be made to exemplary embodiments as illustrated with reference to the accompanyingfigures. The figures together with detailed description below, are incorporated in and form partof the specification, and serve to further illustrate the embodiments and explain variousprinciples and advantages, in accordance with the present disclosure where:Figure 1 is a general schematic diagram describing the unit processes involved in a spongeiron production plant.Figure 2 depicts the SEM analysis of char fines sample with element concentration at variouspoints.Figures 3a-3d depict the specific gravity curves plotted at different size fractions of char fines(-1 mm, -0.5 mm, -0.250 mm and 0.150mm, respectively).Figure 4 is a block diagram showing an exemplary embodiment of the char fines beneficiationprocess according to the present disclosure.DETAILED DESCRIPTION OF THE DISCLOSUREWith respect to the use of substantially any plural and / or singular terms herein, those havingskill in the art can translate from the plural to the singular and / or from the singular to the pluralas is appropriate to the context and / or application. The various singular / plural permutationsmay be expressly set forth herein for sake of clarity. The use of the expression "at least" or "atleast one" suggests the use of one or more elements or ingredients or quantities, as the use maybe in the embodiment of the disclosure to achieve one or more of the desired objects or results.Throughout this specification, the word "comprise", or variations such as "comprises" or"comprising" or "containing" or "has" or "having", or "including but not limited to" whereverused, will be understood to imply the inclusion of a stated element, integer or step, or group ofelements, integers or steps, but not the exclusion of any other element, integer or step, or groupof elements, integers or steps.Reference throughout this specification to "some embodiments", "one embodiment" or "anembodiment" means that a particular feature, structure or characteristic described in connectionwith the embodiment may be included in at least one embodiment of the present disclosure.Thus, the appearances of the phrases "in some embodiments", "in one embodiment" or "in anembodiment" in various places throughout this specification may not necessarily all refer tothe same embodiment. It is appreciated that certain features of the disclosure, which are, forclarity, described in the context of separate embodiments, may also be provided in combinationin a single embodiment. Conversely, various features of the disclosure, which are, for brevity,described in the context of a single embodiment, may also be provided separately or in anysuitable sub-combination.The term "about" as used herein encompasses variations of + / -5% and more preferably + / -2.5%, as such variations are appropriate for practicing the present invention.As used herein, the term 'Direct Reduced Iron (DRI) char fines' refers to a non-magneticfraction of less than 3 mm (-3 mm) obtained as a by-product after separation of other fractionsfrom the product of a sponge iron manufacturing plant or a DRI plant.The terms "method" and "process" are used interchangeably throughout the present disclosure.An objective of the present invention is to improve the efficiency of a sponge ironmanufacturing plant by enabling utilization of DRI char fines which are generally discarded aswaste.Another objective of the present invention is to improve the properties of DRI char fines byconcentrating carbon from the char fines to prepare a carbon concentrate product having lowash content such that may be used in various applications, such as, but not limiting to, feeds insinter and pellet plants.Accordingly, the present disclosure provides a method for concentrating carbon from DirectReduced Iron (DRI) char fines, comprising:a. grinding DRI char fines to a size less than 0.5 mm to provide ground char fines;b. mixing the ground char fines with water to prepare a slurry;c. feeding the slurry into a concentrator to separate the slurry into three fractions: alight fraction, a middle fraction (middling), and a heavy fraction (reject);d. drying the middle and the light fractions to obtain dried fractions; ande. combining the dried fractions to provide a carbon concentrate product.In some embodiments, the DRI char fines comprise about 50-55% ash and about 45-50% FixedCarbon (FC), including values and ranges therebetween.For example, in some embodiments of the present disclosure, the DRI char fines comprise ashat a concentration of about 50-54%, about 50-53%, about 50-52%, about 51-55%, about 51-54%, about 51-53%, about 52-55%, about 52-54%, about 53-55%, about 50%, about 50.5%,about 51%, about 51.5%, about 52%, about 52.6%, about 53%, about 53.5%, about 54%, about54.5% or about 55%; and wherein the DRI char fines comprise fixed carbon at a concentrationof about 45%, about 45.4%, about 45%, about 45.6%, about 46%, about 46.5%, about 47%,about 47.5%, about 48%, about 48.5%, about 49%, about 49.5% or about 50%.In some non-limiting embodiments of the present disclosure, the DRI char fines comprise about50-53% ash and about 45-47% Fixed Carbon.DRI char fines are ground to a size less than 0.5 mm to provide ground char fines. In someembodiments, the DRI char fines are ground in a ball mill at a speed of about 50-55 rpm forabout 30-40 minutes.In some embodiments, the char fines are ground at a speed of about 50-54 rpm, 50-53 rpm, 50-52 rpm, 51-55 rpm, 51-54 rpm, 51-53 rpm, 52-55 rpm, 52-54 rpm, 53-55 rpm, about 50 rpm,about 51 rpm, about 52 rpm, about 53 rpm, about 54 rpm or about 55 rpm for a time period ofabout 30-38 minutes, about 30-35 minutes, about 35-40 minutes, about 30 minutes, about 31minutes, about 32 minutes, about 33 minutes, about 34 minutes, about 35 minutes, about 36minutes, about 37 minutes, about 38 minutes, about 39 minutes or about 40 minutes.In some embodiments, the char fines are ground in a ball mill with a weight of grinding mediain the range of about 25-30 Kg.In some embodiments, the weight of the grinding media is about 25 kg, about 26 kg, about 27kg, about 28 kg, about 29 kg or about 30 kg.In some exemplary, non-limiting embodiments of the present disclosure, the char fines areground in a ball mill at a speed of about 50 rpm for about 40 minutes and media weight ofabout 30 kg.The ground char fines are mixed with water to prepare a slurry. In some embodiments, theground char fines are mixed with water to prepare a slurry having a pulp density of about 14-16% solids by weight, including values and ranges therebetween.For example, in some embodiments of the present disclosure, the ground char fines are mixedwith water to prepare a slurry having a pulp density of about 14%, about 14.5%, about 15%,about 15.5% or about 16% solids by weight.In some exemplary, non-limiting embodiments of the present disclosure, the ground char finesare mixed with water to prepare a slurry having a pulp density of about 15%.In some embodiments, the ground char fines are mixed with water in a mixer for about 10minutes to prepare the slurry. In some embodiments, the mixing is carried out by stirring.The slurry of ground char fines is fed into a concentrator. In some embodiments, theconcentrator is a flowing film concentrator, table concentrator or spiral concentrator.In some embodiments, the concentrator is operated at a wash water flow rate of about 1.5-3litres per minute (LPM), including values and ranges therebetween.For example, in some embodiments of the present disclosure, the concentrator is operated at awash water flow rate of about 1.5, about 2, about 2.5 or about 3 litres per minute.In some preferred, non-limiting embodiments of the present disclosure, the concentrator isoperated at a wash water flow rate of about 2 litres per minute.Subjecting the slurry of ground fines to a concentrator separates the slurry into three fractions:a light fraction, a middle fraction (middling), and a heavy fraction (reject). The light fractionand the middle fraction are collected and dried. The dried fractions are combined to obtain acarbon concentrate product.In some embodiments, the carbon concentrate product comprises about 35-40% ash and about57-62% Fixed Carbon, including values and ranges therebetween.For example, in some embodiments of the present disclosure, the carbon concentrate productcomprises about 35% ash, about 35.5% ash, about 36% ash, about 36.5% ash, about 37% ash,about 37.5% ash, about 38% ash, about 38.5% ash, about 39% ash, about 39.5% ash or about40% ash; and about 57% Fixed Carbon, about 57.5% Fixed Carbon, about 58% Fixed Carbon,about 58.3% Fixed Carbon, about 58.5 Fixed Carbon, about 59% Fixed Carbon, about 59.5%Fixed Carbon, about 60% Fixed Carbon, about 60.5% Fixed Carbon, about 61% Fixed Carbon,about 61.5% Fixed Carbon or about 62% Fixed Carbon.In some embodiments, the method of the present disclosure concentrates carbon by about 35-40%.In some embodiments, the method concentrates carbon by about 35%, about 36%, about 37%,about 38%, about 39% or about 40%.In some exemplary non-limiting embodiments, the method of the present disclosureconcentrates carbon by about 37-40%.It is to be understood that the foregoing descriptive matter is illustrative of the disclosure andnot a limitation. While considerable emphasis has been placed herein on the particular featuresof this disclosure, it will be appreciated that various modifications can be made, and that manychanges can be made in the preferred embodiments without departing from the principles ofthe disclosure. It is to be understood that the phraseology or terminology employed herein isfor the purpose of description and not of limitation. Those skilled in the art will recognize thatthe embodiments herein can be practiced with modification within the spirit and scope of theembodiments as described herein. Similarly, additional embodiments and features of thepresent disclosure will be apparent to one of ordinary skill in art based upon descriptionprovided herein.Descriptions of well-known / conventional methods / steps and techniques are omitted so as tonot unnecessarily obscure the embodiments herein. Further, the disclosure herein provides forexamples illustrating the above-described embodiments, and in order to illustrate theembodiments of the present disclosure certain aspects have been employed. The examples usedherein for such illustration are intended merely to facilitate an understanding of ways in whichthe embodiments herein may be practiced and to further enable those of skill in the art topractice the embodiments herein. Accordingly, the following examples should not be construedas limiting the scope of the embodiments herein.EXAMPLESExample 1: Chemical Analysis of Feed Sample Obtained from DRI PlantFeed sample (char fines of -3 mm size) was collected from the DRI plant and analysed for bulkchemistry, size wise chemical analysis and SEM. The bulk chemistry of sample is shown inTable 1 below:Table 1: Bulk chemistry of as received char fines sampleThe table above shows that the sample collected contained 46.5% Fixed carbon (FC) and 52.6%Ash along with other constituents. Additionally, the size wise chemical analysis of the receivedsample was carried out and results are shown in Table 2 below:Table 2: Size wise chemical analysis of as received char fines sampleThe above table shows that about 80 wt% material is finer than 2.6 mm.It was also found that the sample had difficult liberation characteristics as ash was distributedthroughout in all the size fractions as evident from table 2. Additionally, SEM analysis wasalso conducted on the feed sample which corroborated the above. Figure 2 depicts the SEManalysis of the feed sample which shows C, Al, Si and O were combined together even in below micron size. This explains that C, AL, Si and O are interlocked even in below 30 micronsize so liberation of DRI fines in ultrafine size is difficult.Table 3 shows the elemental analysis of the SEM images.Table 3This therefore showed that there was a need to develop a method to concentrate carbon fromDRI char fines.Example 2: Washability Characteristics of the Feed SamplePost the chemical analysis carried out in Example 1, the washability characteristics of the charfines sample was studied. The char fines sample was ground to different sizes such as 1 mm,0.5 mm, 0.25 mm and 0.15 mm and sink-float test was conducted at the different ground sizesand at different specific gravity such as 1.7, 1.8, 1.9 and 2.0. Floatability of the ground materialsat different specific gravities was determined by plotting specific gravity curves (Figures 3(ad)). Based on the plots, it was found that fractions of 0.5 mm size showed highest float yieldand thereby highest carbon value (Figure 3(b)). Based on this, 0.5 mm was selected andfinalized as the ideal fraction size for beneficiation to recover carbon values or concentratecarbon from char fines.Example 3: Method for Beneficiation or Concentration of Carbon from DRI Char FinesThe char fines of -3 mm size obtained from the DRI plant was ground using a laboratory ballmill in dry mode to achieve a ground product size of below 0.5 mm. During the ball milloperation, operating parameters such as rotation speed, grinding time and media weight werevaried. Specifically, rotation speed was varied between 50-55 rpm, grinding time was variedbetween 30-40 minutes and media weight was varied between 25-30 kg during theexperimentation as shown in Table 4 below:Table 4. Result of ball mill testAs can be seen from the above table, the size of less than 0.5 mm was obtained at a rotationspeed of about 50 rpm, grinding time of about 40 minutes and media weight of about 30 kg.Grinding energy consumption was found to be 6.5 KWH / ton using these parameters.The ground product of size less than 0.5 mm was then mixed with water to achieve feed pulpdensity of about 15% solid by weight and stirred for about 10 minutes using a rotating mixerto make the slurry uniform. This slurry was then fed into a laboratory scale Wilfley Table(model 15S) which is a flowing film concentrator that separates particles based on gravity.Several tests were carried out by varying the deck tilt angle, wash water flow rate and splitterposition by keeping the other variables such as the feed pulp density (15% solids by weight)and shake amplitude (15 mm) constant as shown in Tables 5a-d given below:2 LPM wash water, 8 degree deck angle and splitter position @ 8 nonotchTable 5a3 LPM wash water, 5 degree deck angle and splitter position @ 7 nonotchTable 5b3 LPM wash water, 40 degree deck angle and splitter position @ 7 nonotchTable 5c2.5 LPM, 5 degree deck angle and splitter position@ 8 nonotchesTable 5dTable 5a-d Wilfley Table Results at different Operating ConditionsAs can be seen from the above tables, concentration at different operating conditions, resultedin concentrates having Fixed Carbon (FC) content between 45-59% and ash content between35-47%. Of these, the concentration conditions of about 2 litres per minute (LPM) of washwater flow rate, about 8° of deck tilt angle and splitter position of about 8 nos. notches (Table5a) provided optimum results. After optimizing the operation conditions, three fractions ofproducts, namely, heavy, middlings and light were collected, dried and analysed for weights,fixed carbon and ash analysis. Middling and light fractions were found high in fixed carboncontent and therefore, these two fractions were combined to form the final concentrate product.The overall process produced about 40% concentrate product with 58.3% Fixed Carbon andabout 36% Ash which may be used as feed for sinter or pellet. A Block Flow diagram of thechar fines beneficiation process as demonstrated in this example is presented in Figure 4.Any discussion of documents, acts, materials, devices, articles and the like that has beenincluded in this specification is solely for the purpose of providing a context for the disclosure.It is not to be taken as an admission that any or all of these matters form a part of the prior artbase or were common general knowledge in the field relevant to the disclosure as it existedanywhere before the priority date of this application.
Claims
1. A method for concentrating carbon from Direct Reduced Iron (DRI) char fines, comprising: a. grinding DRI char fines to a size less than 0.5 mm to provide ground char fines; b. mixing the ground char fines with water to prepare a slurry; c. feeding the slurry into a concentrator to separate the slurry into three fractions: a light fraction, a middle fraction (middling), and a heavy fraction (reject); d. drying the middle and the light fractions to obtain dried fractions; and e. combining the dried fractions to provide a carbon concentrate product.
2. The method as claimed in claim 1, wherein the DRI char fines comprise about 50-55% ash and about 45-50% Fixed Carbon.
3. The method as claimed in claim 1 or 2, wherein the DRI char fines are ground in a ball mill at a speed of about 50-55 rpm for about 30-40 minutes.
4. The method as claimed in claim 3, wherein the DRI char fines are ground in a ball mill with a weight of grinding media in the range of about 25-30 Kg.
5. The method as claimed in any one of claims 1-4, wherein the ground char fines are mixed with water to prepare a slurry having a pulp density of about 14-16% solids by weight.
6. The method as claimed in any one of claims 1-5, wherein the ground char fines are mixed with water in a mixer for about 10 minutes to prepare the slurry.
7. The method as claimed in any one of claims 1-6, wherein the concentrator is a flowing film concentrator, table concentrator or spiral concentrator.
8. The method as claimed in claim 7, wherein the concentrator is operated at a wash water flow rate of about 1.5-3 litres per minute.
9. The method as claimed in any one of claims 1-8, wherein the carbon concentrate product comprises about 35-40% ash and about 57-62% Fixed Carbon.
10. The method as claimed in any one of claims 1-9, wherein the method concentrates carbon by about 35-40%.