Catalyst for reducing sox and NOX in flue gas and preparation method thereof, and method for removing sox and NOX from flue gas

IN604959BActive Publication Date: 2026-10-05CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
IN202447027544
Authority / Receiving Office
IN · IN
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-09-09
Filing Date
2024-04-03
Publication Date
2026-10-05

AI Technical Summary

Technical Problem

Current desulfurization and denitrification technologies are unable to simultaneously remove nitrogen oxides (NOx) and sulfur oxides (SOx) from catalytic cracking regeneration flue gas, leading to increased costs and potential impacts on product distribution due to the need for higher additive amounts.

Method used

A catalyst comprising a support with rare earth metals, Group VIII non-precious metals, and precious metals, specifically formulated to achieve simultaneous reduction of NOx and SOx emissions, utilizing a method that includes coprecipitation and impregnation processes to optimize the catalyst's composition and activity.

Benefits of technology

The catalyst effectively reduces both NOx and SOx emissions in catalytic cracking regeneration flue gas, enhancing emission reduction efficiency while minimizing the amount of additives required, thus reducing costs and improving the competitive advantage of additive technology.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to a catalyst for simultaneously reducing SOx and NOx in flue gas, a preparation method therefor and an application thereof, and a method for simultaneously removing SOx and NOx from flue gas.
Need to check novelty before this filing date? Find Prior Art

Description

Technical fieldThe present invention relates to a catalyst for simultaneously reducing both SOx and NOxin flue gas and a preparation method and use thereof, a nd a method for simultaneouslyreducing both SOx and NOx from flue gas.BackgroundDuring the catalytic cracking reaction, coke is deposited on the catalyst due to the reactionof hydrocarbons, which reduces the catalyst activity. After the coke-containing catalyst isseparated from the hydrocarbons adsorbed on the catalyst through the stripping section, itis transported to the regenerator. In the regenerator, the coke-containing catalyst is fullycontacted with the air at high temperature, and the coke on the catalyst surface is burnedoff, allowing the catalyst activity to be restored. When the coke is burned off the catalyst,SOx and NOx are generated, and these gases are emitted into the air and cause atmosphericpollution. As environmental protection requirements become more and more stringent,emission standards for flue gas pollutants are becoming more and more stringent.At present, the main technical measures to reduce the emission of flue gas pollutants fromcatalytic cracking regeneration include: regenerator optimization, use of additives and fluegas post-treatment. Among them, the method of adding the additive is widely used becauseof its advantages of flexible operation and no need to invest in facilities. At present,desulfurization or denitrification additives mainly remove one type of flue gas pollutantalone. For example: CN1334316A discloses a sulfur transfer agent comprising a magnesiaaluminaspinel-containing composition and a Ce / V oxide, which is used to remove SOxfrom the catalytic cracking flue gas; CN104399478A discloses a sulfur transfer agent andits preparation and evaluation method, which is used to remove SOx from the catalyticcracking flue gas; CN101311248B provides a composition capable of reducing theemission of NOx in the catalytic cracking regeneration flue gas, which is used to reduceNOx in the catalytic cracking flue gas.The above-mentioned patent documents have good removal effects when separatelyremoving SOx or NOx in the regeneration flue gas, but they cannot remove nitrogen oxidesand sulfur oxides at the same time / simultaneously. This results in a larger total demand foradditives if SOx and NOx need to be removed at the same time. On the one hand, itincreases the cost of removing flue gas pollutants; on the other hand, a larger amount ofadditives will affect the distribution of catalytic cracking products.In order to reduce the total addition amount of additives, enhance the emission reductioneffect of additives, and improve the competitive power of the additive technology, startingfrom the purpose of removing SOx and NOx in combination, the present invention developsa new catalyst for removing the flue gas pollutants in combination.Summary of the InventionThe purpose of the present invention is to overcome the shortcomings of the existingdesulfurization and denitrification technology that it is unable to simultaneously removenitrogen oxides and sulfur oxides and that the cost is too high, and to provide a catalyst forsimultaneously reducing both SOx and NOx in flue gas (especially catalytic crackingregeneration flue gas) and a preparation method and use thereof, and a method forsimultaneously removing both SOx and NOx from flue gas (especially catalytic crackingregeneration flue gas). The catalyst provided by the present invention has high activity andcan effectively reduce the emission of SOx and NOx in flue gas, and the method ofpreparing the catalyst provided by the present invention is simple.In order to achieve the above object, in a first aspect of the present invention there isprovided a catalyst for (simultaneously) reducing NOx and SOx emissions in flue gas,which catalyst comprises a support and, loaded on the support, a first active componentselected from rare earth metals, a second active component selected from Group VIII nonpreciousmetals and a precious metal component; based on the total weight of the catalyst,the content of the support is 25-95 wt%, the content of the first active component as oxideis 4-60 wt%, the content of the second active component (as_oxide) is 2-12 wt%, and thecontent of the precious metal component as element is 0.01-2 wt%;as metal oxides, the molar ratio of the first active component to the second activecomponent is (0.5-15):1; for example (1-10):1, or (2-5):1.In the present invention, in the absence of contrary teaching, "based on the total weight ofthe catalyst" means that the total weight of the catalyst is 100wt%; when referring to theconstitution and content of a component, in the absence of a definitive basis, the basis isestablished on that the total weight of said component is 100 wt%.In order to achieve the above object, in a second aspect of the present invention there isprovided a (simultaneous) desulfurization and denitrification catalyst, based on the totalweight of the catalyst, the catalyst comprises by weight percent:25-92 wt%, or 40-85 wt%, or 45-80 wt% of an inorganic oxide matrix as oxide;6-70 wt%, or 12-60 wt%, or 12-48 wt% of a rare earth metal component as oxide (preferably,the rare earth metal component is selected from one or more of La, Ce, Pr and Nd, morepreferably La);1-12 wt%, or 2-10 wt%, or 2-8 wt% of a non-precious metal component(s) selected fromGroups VB, VIII, IB, and IIB as oxide (preferably, the non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB is one or more of Fe, Co, Ni, Cu, Zn and V,more preferably Co);1-10 wt%, or 1-8 wt%, or 2-5 wt% of Group VIIB non-precious metal component as oxide(preferably the Group VIIB non-precious metal component is Mn);0.01-1.5 wt%, or 0.02-1.2 wt%, or 0.02-1.0 wt% of a precious metal component as element(preferably the precious metal component is selected from one or more of Ru, Rh, Re, Pt,Pd, Ag, Ir and Au, more preferably one or more of Pt, Pd and Rh, most preferably Pd).In order to achieve the above object, in a third aspect of the present invention there isprovided a catalyst capable of / for simultaneously reducing both SOx and NOx in flue gas,the catalyst comprises a support and, loaded on the support, a first active componentselected from rare earth metals, a second active component selected from non-preciousmetals of Groups VB, VIII, IB, and IIB, a third active component selected from Group IIAmetals, and a precious metal component; based on the total weight of the catalyst, thecontent of the support is 25-93 wt%, the content of the first active component as oxide is4-60 wt%, the content of the second active component (as_oxide) is 2-30 wt%, the contentof the third active component (as_oxide) is 1-30 wt%, and the content of the precious metalcomponent as element is 0.01-2 wt%. Preferably, as metal oxides, the molar ratio of thefirst active component to the second active component is (0.4-12):1, preferably (0.5-8):1,further preferably (1-4):1.In order to achieve the above object, in a fourth aspect of the present invention there isprovided a catalyst for simultaneously reducing both SOx and NOx in flue gas, based onthe total weight of the catalyst, the catalyst contains 25-95 wt% of inorganic oxide matrix;2-70 wt% of rare earth metal component as oxide; 1-30 wt% of Group IIA metal componentas oxide; 1-15 wt% of non-precious metal component(s) selected from Groups VB, VIII,IB, and IIB as oxide; 1-10 wt% of Group VIIB non-precious metal component as oxide;and 0.01-1.5 wt% of precious metal component as element. Preferably, as metal element,the molar ratio of the rare earth metal component to the non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB is (0.4-18):1, for example (0.5-12):1, or (1-6):1.In order to achieve the above object, in a fifth aspect of the present invention there isprovided a method for preparing the catalyst for (simultaneously) reducing NOx and SOxemissions in flue gas according to the first aspect, which method comprises:(1) providing a precursor solution containing a precursor of a first active componentselected from rare earth metals, and a precursor of a second active component selected fromGroup VIII non-precious metals;(2) carrying out a coprecipitation reaction between the precursor solution and acoprecipitant, then drying and calcining;(3) mixing and slurrifying the solid product obtained in step (2) and a support and / or aprecursor of a support to produce a slurry, then drying and calcining the slurry;(4) impregnating the solid product obtained in step (3) with a solution containing aprecursor of precious metal component as impregnation solution, then drying and / orcalcining.In a sixth aspect of the present invention there is provided a method for preparing adesulfurization and denitrification catalyst, which comprises the steps of:S1. Preparation of active metal precursor: using the co-precipitation method or the sol-gelmethod;S2. Preparation of semi-finished catalyst product: mixing and slurrifying an active metalprecursor and an inorganic oxide matrix and / or a precursor of inorganic oxide matrix andoptionally a precursor of precious metal component to produce a slurry, drying andcalcining the slurry;the method also optionally comprises: S3. impregnating the semi-finished catalyst productobtained in step S2 with a solution containing a precursor of precious metal component asimpregnation solution to produce a solid product, and drying and calcining the solidproduct;wherein the active metal in the active metal precursor comprises a rare earth metalcomponent, non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and a Group VIIB non-precious metal component;the active metal precursor, the inorganic oxide matrix and / or the precursor of inorganicoxide matrix, and the precursor of precious metal component are used in such amounts thatthe prepared catalyst, based on the total weight of the catalyst, comprises by weight percent:as oxide: 25-92 wt% of inorganic oxide matrix, 6-70 wt% of rare earth metal component,1-12 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,1-10 wt% of Group VIIB non-precious metal component; and0.01-1.5 wt% of precious metal component as element.In a seventh aspect of the present invention there is provided a method for preparing acatalyst capable of simultaneously reducing SOx and NOx in flue gas, which methodcomprises the steps of:(1) providing a precursor solution containing a precursor of a first active componentselected from rare earth metals, a precursor of a second active component selected fromnon-precious metals of Groups VB, VIII, IB, and IIB, and a precursor of a third activecomponent selected from Group IIA metals;(2) carrying out a coprecipitation reaction between the precursor solution and acoprecipitant, then drying and calcining;(3) mixing and slurrifying the solid product obtained in step (2) and a support and / or aprecursor of a support and optionally a precursor of precious metal component to producea slurry, then drying and calcining the slurry;the method also optionally comprises: (4) impregnating the solid product obtained in step(3) with a solution containing a precursor of precious metal component as impregnationsolution, then drying and / or calcining;the precursor of first active component, the precursor of second active component, theprecursor of third active component, the support and / or the precursor of support, and theprecursor of precious metal component are used in such amounts that in the preparedcatalyst, based on the total weight of the catalyst, the content of the support is 25-93 wt%,the content of the first active component as oxide is 4-60 wt%, the content of the secondactive component (as_oxide) is 2-30 wt%, the content of the third active component(as_oxide) is 1-30 wt%, and the content of the precious metal component as element is0.01-2 wt%.In an eighth aspect of the present invention there is provided a method for preparing acatalyst for simultaneously reducing both SOx and NOx in flue gas, which methodcomprises the steps of:(1) a co-precipitation method or a sol-gel method is used to produce an active metalprecursor;(2) mixing and slurrifying an active metal precursor and an inorganic oxide matrix and / ora precursor of inorganic oxide matrix and optionally a precursor of precious metalcomponent to produce a slurry, drying and / or calcining the slurry to produce a composition;the method also optionally comprises: (3) impregnating the composition obtained in step(2) with a solution containing a precursor of precious metal component as impregnationsolution to produce a solid product, and then drying and / or calcining the soild product;wherein the active metal in the active metal precursor comprises rare earth metalcomponent, Group IIA metal component, non-precious metal component(s) selected fromGroups VB, VIII, IB, and IIB, and Group VIIB non-precious metal component;the active metal precursor, the inorganic oxide matrix and / or the precursor of inorganicoxide matrix, and the precursor of precious metal component are used in such amounts thatthe prepared catalyst, based on the total weight of the catalyst, comprises 25-95 wt% ofinorganic oxide matrix; 2-70 wt% of rare earth metal component as oxide; 1-30 wt% ofGroup IIA metal component as oxide; 1-15 wt% of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB as oxide; 1-10 wt% of Group VIIB non15precious metal component as oxide; and 0.01-1.5 wt% of precious metal component aselement.In a ninth aspect of the present invention there is provided the use of the catalyst accordingto any one of the preceding aspects in simultaneously removing SOx and NOx in flue gas.Specifically, the present invention provides a method for simultaneously removing SOxand NOx from a flue gas containing SOx and NOx, and the method comprises:contacting the flue gas containing SOx and NOx with the catalyst according to any one ofthe preceding aspects in a condition for simultaneously removing SOx and NOx. Preferably,the condition for simultaneously removing SOx and NOx comprises: the temperature is500-800°C, the pressure is 0.02-4MPa, the volumetric hourly space velocity of flue gas is100-50000 h-1. Preferably, the flue gas has a SOx content of 0.001-0.5 vol%, and an NOxcontent of 0.001-0.3 vol%.The present inventors discovered during the research that using specific amounts of rareearth metal element(s) (e.g. La) and Group VIII non-precious metal(s) (e.g. Co) incombination with at least one precious metal element (such as Pt) as active componentswith a specific ratio of rare earth metal(s) to Group VIII non-noble metal(s) can effectivelyreduce the emissions of SOx and NOx in flue gas at the same time. On this basis, theintroduction of Group IIA metal components (e.g. Mg) and / or the introduction of GroupVIIB metal components (e.g. Mn) can further improve the ability of the catalyst to removeNOx and SOx in combination. When contacting the catalyst of the present invention withSO2, it is believed that the sulfur element can be converted into different valence states, inwhich the low-valence sulfur element is beneficial to the conversion of NOx in the flue gas,so that the entire process can promote the conversion of SOx and NOx in a direction thatis conducive to reducing the pollution.The catalyst provided by the invention is simply prepared and easy to implement, and caneffectively reduce the emissions of SOx and NOx in the catalytic cracking regenerationflue gas.Detailed Description of the InventionThe endpoints of ranges and any values disclosed herein are not limited to such preciseranges or values. Still, these ranges or values should be understood to include valuesapproaching such ranges or values. For numerical ranges, a combination between any twoof the endpoint values of ranges, a combination between one of the endpoint values ofranges and an individual point value, or a combination between any two of individual pointvalues can be made to obtain one or more new numerical ranges. These numerical rangesshall be deemed to be specifically disclosed herein.In the present invention, unless otherwise stated, pressure refers to gauge pressure.In the present invention, the catalyst capable of simultaneously reducing SOx and NOx influe gas means that the catalyst can be used to simultaneously remove SOx and NOx in fluegas and reduce the contents of SOx and NOx in flue gas.In the present invention, SOx refers to a mixture of sulfur oxides (e.g. a mixture of SO2and SO3, the molar ratio of oxides is not particularly limited, e.g. 1:10 to 10:1), NOx refersto a mixture of nitrogen oxides (e.g. a mixture of NO2 and NO, the molar ratio of oxidesis not particularly limited, e.g. 1:10 to 10:1).In the present invention, expressions such as "catalyst for reducing the emission of NOxand SOx in flue gas", "catalyst for (simultaneously) reducing NOx and SOx emissions influe gas", "desulfurization and denitrification catalyst", "catalyst capable of simultaneouslyreducing SOx and NOx in flue gas", "catalyst for simultaneously reducing both SOx andNOx in flue gas" have the same meaning, which means that these catalysts can be used tosimultaneously remove SOx and NOx in flue gas and reduce the contents of SOx and NOxin flue gas.According to the first aspect of the present invention, the present invention provides acatalyst for reducing the emission of NOx and SOx in flue gas, the catalyst comprises asupport and, loaded on the support, a first active component selected from rare earth metals,a second active component selected from Group VIII non-precious metals and a preciousmetal component; based on the total weight of the catalyst, the content of the support is 25-95 wt%, the content of the first active component as oxide is 4-60 wt%, the content of thesecond active component (as_oxide) is 2-12 wt%, and the content of the precious metalcomponent as element is 0.01-2 wt%;as metal oxides, the molar ratio of the first active component to the second activecomponent is (0.5-15):1, e.g. (1-10):1, or (1-6):1, (2-5):1, or (2.5-3.5):1, or (2.6-3.4):1, or(2.7-3.3):1, or (2.8-3.2):1, or (2.9-3.1):1, or (2.95-3.05):1.In the catalyst provided by the invention, the support can be selected in a relatively widerange. Preferably, the support is at least one of alumina, silica-alumina, zeolite, spinel,kaolin, diatomaceous earth, perlite, and perovskite, further preferably alumina.The present invention has no special limitation on the crystal form of alumina, includingbut not limited to γ-alumina, δ-alumina, η-alumina, ρ-alumina, κ-alumina and χ-alumina.According to the present invention, conventionally defined Group rare earth componentsare used in the present invention, the first active component is La and / or Ce, preferably La.This method can further improve the SOx and NOx removal performance of the catalyst.The second active component can be at least one of Group VIII metals, preferably Co and / orFe, more preferably Co.According to the present invention, the precious metal has a conventional meaning in theart. Preferably, the precious metal component is one or more of Pt, Pd and Rh, mostpreferably Pd. The present inventors discovered during the research that using the preciousmetal element Pd and other active components in combination can greatly improve theremoval effect of SOx and NOx in flue gas.According to the present invention, the first active component and the second activecomponent are used in the molar ratio of (0.5-15):1. At the special ratio, the first activecomponent and the second active component synergize to improve the removal effect ofSOx and NOx in flue gas.According to a preferable embodiment of the present invention, as metal oxides, the molarratio of the first active component to the second active component is (1-10):1, preferably(2-5):1. The effect of the catalyst in removing SOx and NOx in flue gas can be furtherimproved by optimizing the ratio of the first active component to the second activecomponent.According to a preferable embodiment of the present invention, based on the total weightof the catalyst, the content of the support is 40-90 wt%, the content of the first activecomponent as oxide is 8-50 wt%, the content of the second active component (as_oxide) is2-12 wt%, and the content of the precious metal component as element is 0.02-1.5 wt%.Preferably, based on the total weight of the catalyst, the content of the support is 50-88wt%, the content of the first active component as oxide is 8-40 wt%, the content of thesecond active component (as_oxide) is 2-10 wt%, and the content of the precious metalcomponent as element is 0.03-1.2 wt%.According to the second aspect of the present invention, the present invention provides adesulfurization and denitrification catalyst, based on the total weight of the catalyst, whichcomprises by weight percent:as oxide: 25-92 wt% of inorganic oxide matrix, 6-70 wt% of rare earth metal component,1-12 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,1-10 wt% of Group VIIB non-precious metal component; and0.01-1.5 wt% of precious metal component as element.According to the present invention, preferably, based on the total weight of the catalyst,which comprises by weight percent:as oxide: 40-85 wt% of inorganic oxide matrix, 12-60 wt% of rare earth metal component,2-10 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 1-8 wt% of Group VIIB non-precious metal component;as element: 0.02-1.2 wt% of precious metal component.more preferably, based on the total weight of the catalyst, which comprises by weightpercent:as oxide: 45-80 wt% of inorganic oxide matrix, 12-48 wt% of rare earth metal component,2-8 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 2-5 wt% of Group VIIB non-precious metal component;as element: 0.02-1.0 wt% of precious metal component;most preferably, based on the total weight of the catalyst, which comprises by weightpercent:as oxide: 50-80 wt% of inorganic oxide matrix, 12-43 wt% of rare earth metal component,2-5 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 2-5 wt% of Group VIIB non-precious metal component;as element: 0.02-0.05 wt% of precious metal component.By using the above technical solution, different types of metals are selected for synergisticcoordination within a specific content range, so that different types of metals can exert asynergistic effect, and the used amount of precious metal can be reduced and the cost canbe reduced.According to the present invention, all rare earth metal components can be used in thepresent invention. In order to further improve the SOx and NOx removal performance ofthe catalyst, preferably the rare earth metal component is one or more of La, Ce, Pr and Nd,more preferably La.In an embodiment, Group VB non-precious metal component can be one or more of V, Nband Ta; Group VIII non-precious metal component can be one or more Fe, Co and Ni;Group IB non-precious metal component can be Cu; Group IIB non-precious metalcomponent can be one or more of Zn, Cd and Hg.In a preferred embodiment, the non-precious metal component(s) selected from Groups VB,VIII, IB, and IIB comprise one or more of Fe, Co, Ni, Cu, Zn and V, more preferably Co.In a preferred embodiment, the Group VIIB non-precious metal component is Mn.In a preferred embodiment, the precious metal component is one or more of Ru, Rh, Re, Pt,Pd, Ag, Ir and Au, more preferably one or more of Pt, Pd and Rh, most preferably Pd.According to the desulfurization and denitrification catalyst obtained from the preparationof the present invention, the inorganic oxide matrix comprises various inorganic oxidematrices conventionally used in the art, and is for example one or more of alumina, silica30alumina, zeolite, spinel, kaolin, diatomaceous earth, perlite and perovskite. In the presentinvention, the spinel can be various spinels conventionally used in the art, for example oneor more of magnesia-alumina spinel, ZnO-alumina spinel and titania-alumina spinel.In a preferred embodiment of the present invention, the inorganic oxide matrix is alumina.In a preferred embodiment, alumina is one or more of γ-alumina, δ-alumina, η-alumina, ρ-alumina, κ-alumina and χ-alumina, the present invention has no special limitation thereto.In a preferred embodiment of the present invention, as metal element, the molar ratio ofthe rare earth metal component to the non-precious metal component(s) selected fromGroups VB, VIII, IB, and IIB is (0.6-18):1, further preferably (2-12):1, further morepreferably (3-6):1, e.g. (1-10):1, or (1-6):1, (2-5):1, or (2.5-3.5):1, or (2.6-3.4):1, or (2.7-3.3):1, or (2.8-3.2):1, or (2.9-3.1):1, or (2.95-3.05):1.In a particularly preferabe embodiment of the present invention, based on the total weightof the catalyst, by weight percent, alumina: 50-80 wt%, as oxide, La 12-43 wt%, Co 2-5wt%, Mn 2-5 wt%; as element, Pd 0.02-0.05 wt%; more preferably, the molar ratio of La:Cois (3-6):1 or (1-6):1, (2-5):1, or (2.5-3.5):1, or (2.6-3.4):1, or (2.7-3.3):1, or (2.8-3.2):1, or(2.9-3.1):1, or (2.95-3.05):1.The present inventors discovered during the research that in a particularly preferableembodiment, selecting the rare earth metal element La and the non-precious metal elementscontaining Co and Mn together with at least one element of the precious metal elements asthe active component and using the active component in the desulfurization anddenitrification catalyst can be particularly effective in reducing the emission of NOx andSOx in flue gas.According to the third aspect of the present invention, the present invention provides acatalyst capable of / for simultaneously reducing both SOx and NOx in flue gas, the catalystcomprises a support and, loaded on the support, a first active component selected from rareearth metals, a second active component selected from non-precious metals of Groups VB,VIII, IB, and IIB, a third active component selected from Group IIA metals, and a preciousmetal component; based on the total weight of the catalyst, the content of the support is 25-93 wt%, the content of the first active component as oxide is 4-60 wt%, the content of thesecond active component (as_oxide) is 2-30 wt%, the content of the third active component(as_oxide) is 1-30 wt%, and the content of the precious metal component as element is0.01-2 wt%.According to the present invention, conventionally defined rare earth metal componentscan be used in the present invention. Preferably, the first active component is one or moreof La, Ce, Pr and Nd, more preferably La and / or Ce, most preferably La. This manner canfurther improve the SOx and NOx removal performance of the catalyst.The Group VB non-precious metal component can be one or more V, Nb and Ta; the GroupVIII non-precious metal component can be at least one of Fe, Co and Ni; the Group IB nonpreciousmetal component can be Cu; the Group IIB non-precious metal component can beat least one of Zn, Cd and Hg.Preferably, the second active component is one or more of Fe, Co, Ni, Cu, Zn, and V, morepreferably Co and / or Fe, most preferably Co.In the present invention, the third active component can be one or more of Be, Mg, Ca, Srand Ba, more preferably Mg.The precious metal component can be one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir and Au,preferably one or more of Pt, Pd and Rh, most preferably Pd. The present inventorsdiscovered during the research that using Pd together with other active components incombination is more conducive to removing SOx and NOx in flue gas.In the catalyst provided by the invention, the support can be selected in a relatively widerange. Preferably, the support is at least one of alumina, silica-alumina, zeolite, spinel,kaolin, diatomaceous earth, perlite, and perovskite, further preferably alumina.The present invention has no special limitation on the crystal form of alumina, includingbut not limited to γ-alumina, δ-alumina, η-alumina, ρ-alumina, κ-alumina and χ-alumina.According to a preferable embodiment of the present invention, based on the total weightof the catalyst, the content of the support is 40-87 wt%, the content of the first activecomponent as oxide is 8-50 wt%, the content of the second active component (as_oxide) is3-20 wt%, the content of the third active component (as_oxide) is1-20 wt%, and the contentof the precious metal component as element is 0.02-1.5 wt%;Preferably, based on the total weight of the catalyst, the content of the support is 45-80wt%, the content of the first active component as oxide is 8-40 wt%, the content of thesecond active component (as_oxide) is 3-15 wt%, the content of the third active component(as_oxide) is2-15 wt%, and the content of the precious metal component as element is 0.03-1.2 wt%.According to the present invention, preferably, as metal oxides, the molar ratio of the firstactive component to the second active component is (0.4-12):1, preferably (0.5-8):1,further preferably (1-4):1, e.g. (1-6):1, (2-5):1, or (2.5-3.5):1, or (2.6-3.4):1, or (2.7-3.3):1,or (2.8-3.2):1, or (2.9-3.1):1, or (2.95-3.05):1. The present inventors discovered during theresearch that Combining the two at a special ratio can achieve a better synergistic effectand is more conducive to removing SOx and NOx in flue gas.According to the fourth aspect of the present invention, the present invention provides acatalyst for simultaneously reducing both SOx and NOx in flue gas, which is characterizedin that, based on the total weight of the catalyst, the catalyst comprises 25-95 wt% ofinorganic oxide matrix; 2-70 wt% of rare earth metal component as oxide; 1-30 wt% ofGroup IIA metal component as oxide; 1-15 wt% of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB as oxide; 1-10 wt% of Group VIIB nonpreciousmetal component as oxide; and 0.01-1.5 wt% of precious metal component aselement.According to the present invention, preferably, based on the total weight of the catalyst,the catalyst comprises 40-90 wt% of inorganic oxide matrix; 4-50 wt% of rare earth metalcomponent as oxide; 1-20 wt% of Group IIA metal component as oxide; 2-12 wt% of nonpreciousmetal component(s) selected from Groups VB, VIII, IB, and IIB as oxide; 1-8 wt%of Group VIIB non-precious metal component as oxide; 0.02-1.2 wt% of precious metalcomponent as element; more preferably, based on the total weight of the catalyst, thecatalyst comprises 50-80 wt% of inorganic oxide matrix; 4-40 wt% of rare earth metalcomponent as oxide; 2-15 wt% of Group IIA metal component as oxide; 2-10 wt% of nonpreciousmetal component(s) selected from Groups VB, VIII, IB, and IIB as oxide; 2-5 wt%of Group VIIB non-precious metal component as oxide; 0.02-1.0 wt% of precious metalcomponent as element; most preferably, based on the total weight of the catalyst, thecatalyst comprises 50-80 wt% of inorganic oxide matrix; 7-38 wt% of rare earth metalcomponent as oxide; 2-8 wt% of Group IIA metal component as oxide; 2-7 wt% of nonpreciousmetal component(s) selected from Groups VB, VIII, IB, and IIB as oxide; 2-5 wt%of Group VIIB non-precious metal component as oxide; 0.02-0.05 wt% of precious metalcomponent as oxide. Based on the above preferable embodiment, using specific contentsof the above metals in combination can greatly reduce the used amounts of precious metalsand reduce the cost.According to the present invention, conventionally defined rare earth metal componentscan be used in the present invention. In order to further improve the SOx and NOx removalperformance of the catalyst, the rare earth metal component is preferably one or more ofLa, Ce, Pr and Nd, more preferably La and / or Ce, most preferably La.According to the present invention, said Group IIA metal component is one or more of Be,Mg, Ca, Sr and Ba, more preferably Mg.The Group VB non-precious metal component can be one or more V, Nb and Ta; the GroupVIII non-precious metal component can be at least one of Fe, Co and Ni; the Group IB non10precious metal component can be Cu; the Group IIB non-precious metal component can beat least one of Zn, Cd and Hg.Preferably, the non-precious metal component(s) selected from Groups VB, VIII, IB, andIIB is one or more of Fe, Co, Ni, Cu, Zn, and V, more preferably Co and / or Fe, mostpreferably Co.Preferably, the Group VIIB non-precious metal component is Mn.Preferably, said precious metal component is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir andAu, more preferably one or more of Pt, Pd and Rh, most preferably Pd.According to the catalyst provided by the present invention, the inorganic oxide matrix canbe various inorganic oxide matrices conventionally used in the art, for example at least oneof alumina, silica-alumina, zeolite, spinel, kaolin, diatomaceous earth, perlite, andperovskite. In the present invention, the spinel can be various spinels conventionally usedin the art, and for example can be at least one of magnesia-alumina spinel, ZnO-aluminaspinel and titania-alumina spinel.According to a preferable embodiment of the present invention, the inorganic oxide matrixis alumina.In the present invention, alumina can be one or more of γ-alumina, δ-alumina, η-alumina,ρ-alumina, κ-alumina and χ-alumina. The present invention has no special limitationthereto.According to a preferable embodiment of the present invention, as metal element, the molarratio of the rare earth metal component to the non-precious metal component(s) selectedfrom Groups VB, VIII, IB, and IIB is (0.4-18):1, further preferably (0.5-12):1, further morepreferably (1-6):1, e.g. (2-5):1, or (2.5-3.5):1, or (2.6-3.4):1, or (2.7-3.3):1, or (2.8-3.2):1,or (2.9-3.1):1, or (2.95-3.05):1.According to a particularly preferable embodiment of the present invention, based on thetotal weight of the catalyst, the catalyst comprises 50-80 wt% of alumina; 7-38 wt% of Laas oxide; 2-8 wt% of Mg as oxide; 2-7 wt% of Co as oxide; 2-5 wt% of Mn as oxide; 0.02-0.05 wt% of Pd as element; more preferably, the molar ratio of La:Co is (1-6):1, e.g. (2-5):1, or (2.5-3.5):1, or (2.6-3.4):1, or (2.7-3.3):1, or (2.8-3.2):1, or (2.9-3.1):1, or (2.95-3.05):1.The present inventors discovered during the research that using the Group rare earthelement La, the Group IIA element Mg, and the transitional non-precious metal elementscontaining Co and Mn, together with at least one of precious metal elements as activecomponent can be particularly effective in reducing the emission of NOx and SOx incatalytic cracking regeneration flue gas.According to the fifth aspect of the present invention, the present invention provides amethod for preparing a catalyst for reducing the emission of NOx and SOx in flue gasaccording to the first aspect of the present invention, which method comprises:(1) providing a precursor solution containing a precursor of a first active componentselected from rare earth metals, and a precursor of a second active component selected fromGroup VIII non-precious metals;(2) carrying out a coprecipitation reaction between the precursor solution and acoprecipitant, then drying and calcining;(3) mixing and slurrifying the solid product obtained in step (2) and a support and / or aprecursor of a support to produce a slurry, then drying and calcining the slurry;(4) impregnating the solid product obtained in step (3) with a solution containing aprecursor of precious metal component as impregnation solution, then drying and / orcalcining.According to the method of the present invention, the selection ranges for specific types ofthe first active component, the second active component, the precious metal componentand the support have been mentioned in the first aspect above, and will not be described indetail again here.In the present invention, there is no particular limitation on the method of providing theprecursor solution in step (1), as long as the precursors of metal components are mixedevenly. For example, the precursors of metal components can be dissolved in water andstirred thoroughly.According to the method of the present invention, preferably, the precursor of first activecomponent and the precursor of second active component can be each independentlyselected from water-soluble salts such as nitrates, chlorides, chlorates and sulfates,preferably nitrates and / or chlorides of metal components.According to the method of the present invention, preferably, the precursor of the preciousmetal component is at least one of palladium nitrate, palladium chloride, platinum chlorateand rhodium chloride, preferably palladium nitrate and / or palladium chloride.According to the present invention, the co-precipitation method is used to carry out thecoprecipitation reaction of the precursor solution. The present invention has no particularlimitation on the type and amount of the coprecipitant, as long as the coprecipitationreaction can proceed smoothly.The type of the coprecipitant can be conventionally selected in the art, preferably, thecoprecipitant is a carbonate salt, further preferably at least one of ammonium carbonate,potassium carbonate and sodium carbonate, more preferably ammonium carbonate.In step (2), the coprecipitant can be introduced in the form of solution to carry out acoprecipitation reaction with the precursor solution. The present invention has no particularlimitation on the concentration of the solution formed from the precursor solution and thecoprecipitant, as long as the concentration of the formed solution is less than the solubilityduring preparation, thereby ensuring that the coprecipitation reaction can fully occur.Preferably, the coprecipitation reaction is carried out at pH=8-10, preferably 8.5-9.5. ThepH of the coprecipitation reaction can be adjusted by adding acids and / or bases, the specifictypes of which are not particularly limited, for example, ammonia water.According to the present invention, the method also includes the reaction product obtainedby the coprecipitation reaction is subjected to a solid-liquid separation (for example,filtering or centrifugal separation) to produce the solid product, followed by drying andcalcining.Preferably, the condition for calcining in step (2) includes: the temperature is 300-800°C,the time is 1-8h.In the present invention, the precursor of support can be any substance that can beconverted into the support through subsequent calcining. Those skilled in the art can makean appropriate selection based on the specific type of support, which will not be describedin detail again here. For example, the precursor of aluminum can be various sols or gels ofaluminum, or aluminium hydroxide. The aluminium hydroxide can be at least one ofgibbsite, bayerite, nordshandite, diaspore, boehmite and pseudo-boehmite.According to the method of the present invention, the support is alumina, preferably, beforeslurrifying, the support and / or the precursor of support are subjected to acidificationtreatment. The acidification treatment can be performed according to the conventionaltechnical means in the art. Further preferably, the acid used in acidification treatment ishydrochloric acid.The present invention has a relatively wide selection range for the condition of acidificationtreatment., preferably, the condition of acidification treatment includes: the acid / aluminaratio is 0.12-0.22:1, the time is 20-40min.In the present invention, unless otherwise specified, the acid / alumina ratio refers to themass ratio of hydrochloric acid based on 36 wt% of concentrated hydrochloric acid to theprecursor of alumina based on dry basis.The specific implementation mode of acidification treatment can be as follows: adding theprecursor of alumina to water, and slurrifying and dispersing.According to the present invention, the method of mixing and slurrifying the solid productobtained in step (2), and the support and / or the precursor of support is not particularlylimited, and the addition order of the above-mentioned substances is also not limited, aslong as the above-mentioned substances and water can be contacted and mixed evenly.According to the method of the present invention, preferably, in step (3), the slurry has asolid content of 7-35 wt%.According to the method of the present invention, in step (3), the drying is preferably spraydrying. In the present invention, the spray drying can be performed according toconventional technical means in the art, and the present invention has no special limitationthereto. Those skilled in the art can select an appropriate condition for spray drying basedon the average particle size of the target catalyst. The preferred condition for spray dryingis such that the particles obtained by spray drying have an average particle size of 60-80μm with the particle size distribution being mainly in the range of 20-100 μm.According to the method of the present invention, in step (3), the slurry obtained aftermixing and slurrifying may be calcined, preferably, in step (3), the condition for calciningincludes: the temperature is 300-800°C, the time is 1-5h.According to the method of the present invention, in step (4), the impregnation is notparticularly limited, and can be carried out according to conventional technical means inthe art. It can be saturation impregnation or over-impregnation, preferably overimpregnation.Those skilled in the art can select appropriate operations based on the contentof precious metal in the target product.According to the present invention, preferably, in step (4), the precursor of precious metalcomponent is hydrolyzed in an acid solution to provide the impregnation solution.Specifically, after the hydrolysis, the dilution (e.g. by adding water) or the concentration(e.g. by evaporation), and then the impregnation can be performed to provide a catalystwith a specific loading amount of the precious metal component.Preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,preferably at least one of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid.According to the present invention, preferably, the acid is used in such an amount that thepH value of the impregnation solution is less than 5.0, preferably 2-5. Adopting thispreferred embodiment is more conducive to the uniform dispersion of active componentsand can improve the wear resistance of the finished catalyst.In the present invention, the solid product can be obtained by filtering the mixture obtainedafter impregnation. The filtering can be carried out according to conventional technicalmeans in the art.According to the present invention, in step (4), the solid product can be only dried, or onlycalcined, or dried and then calcined, and the present invention has no special limitationthereto. Preferably, the solid product is dried and then calcined.The drying conditions in step (2), step (3) and step (4) of the present invention are notparticularly limited and the drying can be carried out according to conventional technicalmeans in the art. For example, the conditions for drying can each independently include:the temperature is 60-200°C, the time is 2-10h.The present invention has no special limitation on the condition for calcining, and thecalcining can be carried out according to conventional technical means in the art. Thecalcining can be performed in an air or inert atmosphere (including but not limited tonitrogen), preferably, the condition for calcining in step (4) includes: the temperature is300-700°C, the time is 0.1-5h.According to the sixth aspect of the present invention, the present invention provides amethod for preparing the desulfurization and denitrification catalyst according to thesecond aspect of the present invention, which method comprises the steps of:S1. Preparation of active metal precursor: using the co-precipitation method or the sol-gelmethod;S2. Preparation of semi-finished catalyst product: mixing and slurrifying an active metalprecursor and an inorganic oxide matrix and / or a precursor of inorganic oxide matrix andoptionally a precursor of precious metal component to produce a slurry, drying andcalcining the slurry;the method also optionally comprises: S3. impregnating the semi-finished catalyst productobtained in step S2 with a solution containing a precursor of precious metal component asimpregnation solution to produce a solid product, and drying and calcining the solidproduct;wherein the active metal in the active metal precursor comprises a rare earth metalcomponent, non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and a Group VIIB non-precious metal component;the active metal precursor, the inorganic oxide matrix and / or the precursor of inorganicoxide matrix, and the precursor of precious metal component are used in such amounts thatthe prepared catalyst, based on the total weight of the catalyst, comprises by weight percent:as oxide: 25-92 wt% of inorganic oxide matrix, 6-70 wt% of rare earth metal component,1-12 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,1-10 wt% of Group VIIB non-precious metal component; and0.01-1.5 wt% of precious metal component as element.According to the present invention, preferably, the active metal precursor, the inorganicoxide matrix and / or the precursor of inorganic oxide matrix, and the precursor of preciousmetal component are used in such amounts that the prepared catalyst, based on the totalweight of the catalyst, comprises by weight percent:as oxide: 40-85 wt% of inorganic oxide matrix, 12-60 wt% of rare earth metal component,2-10 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 1-8 wt% of Group VIIB non-precious metal component;as element: 0.02-1.2 wt% of precious metal component;preferably, the active metal precursor, the inorganic oxide matrix and / or the precursor ofinorganic oxide matrix, and the precursor of precious metal component are used in suchamounts that the prepared catalyst, based on the total weight of the catalyst, comprises byweight percent:as oxide: 45-80 wt% of inorganic oxide matrix, 12-48 wt% of rare earth metal component,2-8 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 2-5 wt% of Group VIIB non-precious metal component;as element: 0.02-1.0 wt% of precious metal component;most preferably, the active metal precursor, the inorganic oxide matrix and / or the precursorof inorganic oxide matrix, and the precursor of precious metal component are used in suchamounts that the prepared catalyst, based on the total weight of the catalyst, comprises byweight percent:as oxide: 50-80 wt% of inorganic oxide matrix, 12-43 wt% of rare earth metal component,2-5 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 2-5 wt% of Group VIIB non-precious metal component;as element: 0.02-0.05 wt% of precious metal component.Preferably, in said active component precursor, as metal element, the molar ratio of the rareearth metal component to the non-precious metal component(s) selected from Groups VB,VIII, IB, and IIB is (0.6-18):1, further preferably (2-12):1, further more preferably (3-6):1,e.g. (1-10):1, or (1-6):1, (2-5):1, or (2.5-3.5):1, or (2.6-3.4):1, or (2.7-3.3):1, or (2.8-3.2):1,or (2.9-3.1):1, or (2.95-3.05):1.According to the preparation method of the present invention, the selection ranges forspecific types of the rare earth metal component, the non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB, the Group VIIB non-precious metal component,the precious metal component, and the inorganic oxide matrix have been mentioned in thesecond aspect above, and will not be described in detail again here.According to the preparation method of the present invention, either a co-precipitationmethod may be used, or a sol-gel method may be used. More preferably, the coprecipitationmethod is used. In step S1, the co-precipitation method is used to produce anactive metal precursor.Preferably, the co-precipitation method comprises:S11. Preparing a first solution containing a precursor of rare earth metal component, aprecursor of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and a precursor of Group VIIB non-precious metal component;S12. Subjecting a first solution and a coprecipitant to carry out a coprecipitation reaction;S13. Drying and / or calcining a solid product obtained in the coprecipitation reaction.In the present invention, there is no particular limitation on the method of producing thefirst solution in step S11, as long as the precursors of metal components are mixed evenly.For example, the precursors of metal components in step S11 can be dissolved in water andstirred thoroughly.According to the present invention, preferably, the precursor of rare earth metal component,the precursor of non-precious metal component(s) selected from Groups VB, VIII, IB, andIIB, the precursor of Group VIIB non-precious metal component, and the precursor ofprecious metal component can be each independently selected from water-soluble saltssuch as nitrates, chlorides, chlorates and sulfates, preferably nitrates and / or chlorides ofmetal components. Further preferably, the precursor of Mn is potassium permanganateand / or manganese chloride.The present invention has no particular limitation on the type and amount of thecoprecipitant, as long as the coprecipitation reaction can proceed smoothly. Thecoprecipitant can be those conventionally selected in the art, preferably, the coprecipitantis a carbonate salt, further preferably one or more of ammonium carbonate, potassiumcarbonate, and sodium carbonate, more preferably ammonium carbonate.In step S12, the coprecipitant can be introduced in the form of solution to carry out acoprecipitation reaction with the first solution. The present invention has no particularlimitation on the concentration of the solution formed from the first solution and thecoprecipitant, as long as the concentration of the formed solution is less than the solubilityduring preparation, thereby ensuring that the coprecipitation reaction can fully occur.Preferably, the coprecipitation reaction is carried out at pH=8-10, preferably 8.5-9.5. ThepH of the coprecipitation reaction can be adjusted by adding acids and / or bases, the specifictypes of which are not particularly limited, for example, ammonia water.According to the present invention, the method also includes the reaction product obtainedby the coprecipitation reaction is subjected to a solid-liquid separation to produce the solidproduct. The present invention has no limitation on the solid-liquid separation method, aslong as the solid-liquid separation of the reaction product can be fulfilled. For example, thesolid-liquid separation method can be filtering or centrifugation.Preferably, the condition for drying in step S13 includes: the temperature is 60-300°C, thetime is 0.5-6h.Preferably, the condition for calcining in step S13 includes: the temperature is 300-800°C,the time is 1-8h.According to the present invention, the precious metal component may be introduced instep S2, or in step S3, or a part thereof is introduced in step S2 and the other part isintroduced in step S3. Preferably it is introduced in step S3, and this preferable embodimentis more conducive to the dispersion of precious metal.In the present invention, the precursor of inorganic oxide matrix can be any substance thatcan be converted into the oxide matrix through subsequent calcining. Those skilled in theart can make an appropriate selection based on the specific type of inorganic oxide matrix,which will not be described in detail again here. For example, the precursor of aluminumcan be various sols or gels of aluminum, or aluminium hydroxide. The aluminiumhydroxide can be one or more of gibbsite, bayerite, nordshandite, diaspore, boehmite, andpseudo-boehmite. Most preferably, the precursor of alumina is pseudo-boehmite.According to the preparation method provided by the present invention, the inorganic oxidematrix is alumina, preferably, before slurrifying, the inorganic oxide matrix and / or theprecursor of inorganic oxide matrix need to be subjected to acidification treatment. Theacidification treatment can be performed according to the conventional technical means inthe art. Further preferably, the acid used in acidification treatment is hydrochloric acid.The present invention has a relatively wide selection range for the condition of acidificationtreatment, preferably, the condition of acidification treatment includes: the acid / aluminaratio is (0.12-0.22):1, the time is 20-40min.In the present invention, unless otherwise specified, the acid / alumina ratio refers to themass ratio of hydrochloric acid based on 36 wt% of concentrated hydrochloric acid to theprecursor of alumina based on dry basis.The specific implementation mode of acidification treatment can be as follows: adding theprecursor of alumina to water, and slurrifying and dispersing.According to the present invention, the method of mixing and slurrifying the active metalprecursor, and the inorganic oxide matrix and / or the precursor of inorganic oxide matrixand optionally the precursor of precious metal component is not particularly limited, andthe addition order of the active metal precursor, and the inorganic oxide matrix and / or theprecursor of inorganic oxide matrix and optionally the precursor of precious metalcomponent is also not limited, as long as the active metal precursor, and the inorganic oxidematrix and / or the precursor of inorganic oxide matrix and optionally the precursor ofprecious metal component, and water can be contacted. In case that the slurrifying processfurther involves the precursor of precious metal component, the specific mixing andslurrifying process may include: adding the precursor of precious metal component (whichcan be introduced in form of solution) to the acidified inorganic oxide matrix and thenmixing and slurrifying, then adding the active metal precursor, and then drying and / orcalcining the slurry to produce the finished catalyst.According to the present invention, preferably, in step S2, the slurry has a solid content of5-40 wt%.In step S2, the drying is preferably spray drying. In the present invention, the spray dryingcan be performed according to conventional technical means in the art, and the presentinvention has no special limitation thereto. Those skilled in the art can select an appropriatecondition for spray drying based on the average particle size of the target catalyst. Thepreferred condition for spray drying is such that the particles obtained by spray drying havean average particle size of 60-80 μm with the particle size distribution being mainly in therange of 20-100 μm.Preferably, in step S2, the condition for calcining includes: the temperature is 300-800°C,the time is 1-5h.According to the preparation method of the present invention, in step S3, the impregnationcan be carried out according to conventional technical means in the art. The presentinvention has no special limitation thereto. For example, the impregnation can be saturationimpregnation or over-impregnation, preferably over-impregnation.According to the present invention, preferably, in step S3, the precursor of precious metalcomponent is hydrolyzed in an acid solution to provide the impregnation solution.Specifically, after the hydrolysis, the dilution (e.g. by adding water) or the concentration(e.g. by evaporation), and then the impregnation can be performed to provide adesulfurization and denitrification catalyst with a specific loading amount of the preciousmetal component.Preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,preferably one or more of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid.According to the present invention, preferably, the acid is used in such an amount that thepH value of the impregnation solution is less than 6.0, preferably less than 5. Adopting thispreferred embodiment is more conducive to the uniform dispersion of active componentsand can improve the wear resistance of the finished catalyst.In the present invention, the solid product can be obtained by filtering the mixture obtainedafter impregnation. The filtering can be carried out according to conventional technicalmeans in the art.According to present invention, in step S3, the solid product can be only dried, or onlycalcined, or dried and then calcined, and the present invention has no special limitationthereto. Preferably, the solid product is dried and then calcined. The present invention hasno special limitation on the conditions for drying and calcining, and drying and calciningcan be carried out according to conventional technical means in the art. For example, thecondition for drying can include: the temperature is 60-150°C, the time is 2-10h. Thepresent invention has no special limitation on the condition f or calcining. The calciningcan be performed in an air or inert atmosphere (e.g. nitrogen), and the present inventionhas no special limitation thereto. Preferably, the condition for calcining in step S3 is: thetemperature is 300-800°C, the time is 0.1-5h.According to the seventh aspect of the present invention, the present invention provides amethod for preparing a catalyst capable of simultaneously reducing SOx and NOx in fluegas according to the third aspect of the present invention, which method comprises thesteps of:(1) providing a precursor solution containing a precursor of a first active componentselected from rare earth metals, a precursor of a second active component selected fromnon-precious metals of Groups VB, VIII, IB, and IIB, and a precursor of a third activecomponent selected from Group IIA metals;(2) carrying out a coprecipitation reaction between the precursor solution and acoprecipitant, then drying and calcining;(3) mixing and slurrifying the solid product obtained in step (2) and a support and / or aprecursor of a support and optionally a precursor of precious metal component to producea slurry, then drying and calcining the slurry;the method also optionally comprises: (4) impregnating the solid product obtained in step(3) with a solution containing a precursor of precious metal component as impregnationsolution, then drying and / or calcining;the precursor of first active component, the precursor of second active component, theprecursor of third active component, the support and / or the precursor of support, and theprecursor of precious metal component are used in such amounts that in the preparedcatalyst, based on the total weight of the catalyst, the content of the support is 25-93 wt%,the content of the first active component as oxide is 4-60 wt%, the content of the secondactive component (as_oxide) is 2-30 wt%, the content of the third active component(as_oxide) is 1-30 wt%, and the content of the precious metal component as element is0.01-2 wt%.According to the method of the present invention, preferably, the precursor of first activecomponent, the precursor of second active component, the precursor of third activecomponent, the support and / or the precursor of support, and the precursor of precious metalcomponent are used in such amounts that in the prepared catalyst, based on the total weightof the catalyst, the content of the support is 40-87 wt%, the content of the first activecomponent as oxide is 8-50 wt%, the content of the second active component (as_oxide) is3-20 wt%, the content of the third active component (as_oxide) is1-20 wt%, and the contentof the precious metal component as element is 0.02-1.5 wt%;preferably, the precursor of first active component, the precursor of second activecomponent, the precursor of third active component, the support and / or the precursor ofsupport, and the precursor of precious metal component are used in such amounts that inthe prepared catalyst, based on the total weight of the catalyst, the content of the supportis 45-80 wt%, the content of the first active component as oxide is 8-40 wt%, the contentof the second active component (as_oxide) is 3-15 wt%, the content of the third activecomponent (as_oxide) is2-15 wt%, and the content of the precious metal component aselement is 0.03-1.2 wt%.According to the method of the present invention, the selection ranges for specific types ofthe first active component, the second active component, the third active component andthe precious metal component and the support have been mentioned in the third aspectabove, and will not be described in detail again here.According to a preferable embodiment of the present invention, as metal element, the molarratio of the precursor of first active component to the precursor of second active componentis (0.4-12):1, preferably (0.5-8):1, further preferably (1-4):1.In the present invention, there is no particular limitation on the method of providing theprecursor solution in step (1), as long as the precursors of metal components are mixedevenly. For example, the precursors of metal components may be dissolved in water andstirred thoroughly.According to the present invention, preferably, the precursor of first active component, theprecursor of second active component and the precursor of third active component can beeach independently selected from water-soluble salts such as nitrates, chlorides, chloratesand sulfates, preferably nitrates and / or chlorides of metal components.According to the present invention, preferably, the precursor of the precious metalcomponent is at least one of palladium nitrate, palladium chloride, platinum chlorate andrhodium chloride, preferably palladium nitrate and / or palladium chloride.The present invention has no particular limitation on the type and amount of thecoprecipitant, as long as the coprecipitation reaction can proceed smoothly.The type of thecoprecipitant can be conventionally selected in the art, preferably, the coprecipitant is acarbonate salt, further preferably at least one of ammonium carbonate, potassium carbonateand sodium carbonate, more preferably ammonium carbonate.In step (2), the coprecipitant can be introduced in the form of solution to carry out acoprecipitation reaction with the precursor solution. The present invention has no particularlimitation on the concentration of the solution formed from the precursor solution and thecoprecipitant, as long as the concentration of the formed solution is less than the solubilityduring preparation, thereby ensuring that the coprecipitation reaction can fully occur.Preferably, the coprecipitation reaction is carried out at pH=8-10, preferably 8.5-9.5. ThepH of the coprecipitation reaction can be adjusted by adding acids and / or bases, the specifictypes of which are not particularly limited, for example, ammonia water.According to the present invention, the method also includes the reaction product obtainedby the coprecipitation reaction is subjected to a solid-liquid separation (for example,filtering or centrifugal separation) to produce the solid product, followed by drying andcalcining.According to the present invention, the precious metal component may be introduced instep (3), or in step (4), or a part thereof is introduced in step (3) and the other part isintroduced in step (4). Preferably it is introduced in step (4), and this preferableembodiment is more conducive to the dispersion of precious metal.The support precursor can be any substance that can be converted into the support throughsubsequent calcining. Those skilled in the art can make an appropriate selection based onthe specific type of support, which will not be described in detail again here.For example,the precursor of aluminum can be various sols or gels of aluminum, or aluminiumhydroxide. The aluminium hydroxide can be at least one of gibbsite, bayerite, nordshandite,diaspore, boehmite and pseudo-boehmite.According to the method of the present invention, the support is alumina, preferably, beforeslurrifying, the support and / or the precursor of support are subjected to acidificationtreatment. The acidification treatment can be performed according to the conventionaltechnical means in the art. Further preferably, the acid used in acidification treatment ishydrochloric acid.The present invention has a relatively wide selection range for the condition of acidificationtreatment., preferably, the condition of acidification treatment includes: the acid / aluminaratio is 0.12-0.22:1, the time is 20-40min.In the present invention, unless otherwise specified, the acid / alumina ratio refers to themass ratio of hydrochloric acid based on 36 wt% of concentrated hydrochloric acid to theprecursor of alumina based on dry basis.The specific implementation mode of acidification treatment can be as follows: adding theprecursor of alumina to water, and slurrifying and dispersing.According to the present invention, the method of mixing and slurrifying the solid productobtained in step (2), and the support and / or the precursor of support, and optionally theprecursor of precious metal component is not particularly limited, and the addition orderof the above-mentioned substances is also not limited, as long as the above-mentionedsubstances and water can be contacted and mixed evenly. In case that the slurrifying processfurther involves the precursor of precious metal component, the specific mixing andslurrifying process may include: adding the precursor of precious metal component (whichcan be introduced in form of solution) to the acidified support and then mixing andslurrifying, then adding the solid product obtained in step (2), and then drying and / orcalcining the slurry.According to the present invention, preferably, in step (3), the slurry has a solid content of6-38 wt%.According to the method of the present invention, in step (3), the drying is preferably spraydrying, In the present invention, the spray drying can be performed according toconventional technical means in the art, and the present invention has no special limitationthereto. Those skilled in the art can select an appropriate condition for spray drying basedon the average particle size of the target catalyst. The preferred condition for spray dryingis such that the particles obtained by spray drying have an average particle size of 60-80μm with the particle size distribution being mainly in the range of 20-100 μm.According to the method of the present invention, in step (4), the impregnation is notparticularly limited and can be carried out according to conventional technical means inthe art. The impregnation can be saturation impregnation or over-impregnation, preferablyover-impregnation. Those skilled in the art can select appropriate operations based on thecontent of precious metal in the target product.According to the present invention, preferably, in step (4), the precursor of precious metalcomponent is hydrolyzed in an acid solution to provide the impregnation solution.Specifically, after the hydrolysis, the dilution (e.g. by adding water) or the concentration(e.g. by evaporation), and then the impregnation can be performed to provide a catalystwith a specific loading amount of the precious metal component.Preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,preferably at least one of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid.According to the present invention, preferably, the acid is used in such an amount that thepH value of the impregnation solution is less than 6.0, preferably 2-5. Adopting thispreferred embodiment is more conducive to the uniform dispersion of active componentsand can improve the wear resistance of the finished catalyst.In the present invention, the solid product can be obtained by filtering the mixture obtainedafter impregnation. The filtering can be carried out according to conventional technicalmeans in the art.According to the present invention, in step (4), the solid product can be only dried, or onlycalcined, or dried and then calcined, and the present invention has no special limitationthereto. Preferably, the solid product is dried and then calcined. The present invention hasno special limitation on the conditions for drying and calcining, and drying and calciningcan be carried out according to conventional technical means in the art. For example, thecondition for drying can include: the temperature is 60-200°C, the time is 2-10h.According to the method of the present invention, each step may have the same or differentcondition for calcining, preferably, in step (2), step (3) and step (4), the conditions forcalcining may each independently include: the temperature is 300-800°C, the time is 0.5-8h. The calcining can be carried out in air or an inert atmosphere (e.g. nitrogen). Thepresent invention has no special limitation thereto. Preferably the calcining is carried outin an air atmosphere.According to the eighth aspect of the present invention, the present invention provides amethod for preparing a catalyst for simultaneously reducing both SOx and NOx in flue gasaccording to the fourth aspect of the present invention, which method comprises the stepsof:(1) a co-precipitation method or a sol-gel method is used to produce an active metalprecursor;(2) mixing and slurrifying an active metal precursor and an inorganic oxide matrix and / ora precursor of inorganic oxide matrix and optionally a precursor of precious metalcomponent to produce a slurry, drying and / or calcining the slurry to produce a composition;the method also optionally comprises: (3) impregnating the composition obtained in step(2) with a solution containing a precursor of precious metal component as impregnationsolution to produce a solid product, and then drying and / or calcining the soild product;wherein the active metal in the active metal precursor comprises rare earth metalcomponent, Group IIA metal component, non-precious metal component(s) selected fromGroups VB, VIII, IB, and IIB, and Group VIIB non-precious metal component;the active metal precursor, the inorganic oxide matrix and / or the precursor of inorganicoxide matrix, and the precursor of precious metal component are used in such amounts thatthe prepared catalyst, based on the total weight of the catalyst, comprises 25-95 wt% ofinorganic oxide matrix; 2-70 wt% of rare earth metal component as oxide; 1-30 wt% ofGroup IIA metal component as oxide; 1-15 wt% of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB as oxide; 1-10 wt% of Group VIIB nonpreciousmetal component as oxide; and 0.01-1.5 wt% of precious metal component aselement.According to the present invention, preferably, the active metal precursor, the inorganicoxide matrix and / or the precursor of inorganic oxide matrix, and the precursor of preciousmetal component are used in such amounts that the prepared catalyst, based on the totalweight of the catalyst, comprises 40-90 wt% of inorganic oxide matrix; 4-50 wt% of rareearth metal component as oxide; 1-20 wt% of Group IIA metal component as oxide; 2-12wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB asoxide; 1-8 wt% of Group VIIB non-precious metal component as oxide; 0.02-1.2 wt% ofprecious metal component as element; more preferably, the active metal precursor, theinorganic oxide matrix and / or the precursor of inorganic oxide matrix, and the precursor ofprecious metal component are used in such amounts that the prepared catalyst, based onthe total weight of the catalyst, comprises 5-80 wt% of inorganic oxide matrix; 4-40 wt%of rare earth metal component as oxide; 2-15 wt% of Group IIA metal component as oxide;2-10 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIBas oxide; 2-5 wt% of Group VIIB non-precious metal component as oxide; 0.02-1.0 wt%of precious metal component as element; most preferably, based on the total weight of thecatalyst, comprises 50-80 wt% of inorganic oxide matrix; 7-38 wt% of rare earth metalcomponent as oxide; 2-8 wt% of Group IIA metal component as oxide; 2-7 wt% of nonpreciousmetal component(s) selected from Groups VB, VIII, IB, and IIB as oxide; 2-5 wt%of Group VIIB non-precious metal component as oxide; 0.02-0.05 wt% of precious metalcomponent as oxide.Preferably, in said active component precursor, as metal element, the molar ratio of the rareearth metal component to the non-precious metal component(s) selected from Groups VB,VIII, IB, and IIB is (0.4-18):1, further preferably (0.5-12):1, further more preferably (1-6):1.According to the method of the present invention, the selection ranges for specific types ofthe rare earth metal component, the Group IIA metal component, the non-precious metalcomponent(s) selected from Groups VB, VIII, IB, and IIB, the Group VIIB non-preciousmetal component and the precious metal component and the inorganic oxide matrix havebeen mentioned in the fourth aspect above, and will not be described in detail again here.According to the method of the present invention, either a co-precipitation method may beused, or a sol-gel method may be used. More preferably, the co-precipitation method isused. Preferably, in step (1), the co-precipitation method is used to produce the active metalprecursor; more preferably, the co-precipitation method comprises:(1-1) providing a first solution containing a precursor of rare earth metal component, aprecursor of Group IIA metal component, a precursor of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB, and a precursor of Group VIIB non-preciousmetal component;(1-2) subjecting the first solution and a coprecipitant to carry out a coprecipitation reaction;(1-3) drying and / or calcining a solid product obtained in the coprecipitation reaction.In the present invention, there is no particular limitation on the method of providing thefirst solution in step (1-1), as long as the precursors of metal components are mixed evenly.For example, the precursors of metal components can be dissolved in water and stirredthoroughly.According to the present invention, preferably, the precursor of rare earth metal component,the precursor of Group IIA metal component, the precursor of non-precious metalcomponent(s) selected from Groups VB, VIII, IB, and IIB, and the precursor of Group VIIBnon-precious metal component can be each independently selected from water-soluble saltssuch as nitrates, chlorides, chlorates and sulfates, preferably nitrates and / or chlorides ofmetal components. In particular, the precursor of Mn can be potassium permanganateand / or manganese chloride.According to the present invention, the precursor of the precious metal component can beany water-soluble compound containing the precious metal component, preferably, theprecursor of the precious metal component is at least one of palladium nitrate, palladiumchloride, platinum chlorate and rhodium chloride, further preferably palladium nitrateand / or palladium chloride.The present invention has no particular limitation on the type and amount of thecoprecipitant, as long as the coprecipitation reaction can proceed smoothly.The type of thecoprecipitant can be conventionally selected in the art, preferably, the coprecipitant is acarbonate salt, further preferably at least one of ammonium carbonate, potassium carbonateand sodium carbonate, more preferably ammonium carbonate.In step (1-2), the coprecipitant can be introduced in the form of solution to carry out acoprecipitation reaction with the first solution. The present invention has no particularlimitation on the concentration of the solution formed from the first solution and thecoprecipitant, as long as the concentration of the formed solution is less than the solubilityduring preparation, thereby ensuring that the coprecipitation reaction can fully occur.Preferably, the coprecipitation reaction is carried out at pH=8-10, preferably 8.5-9.5. ThepH of the coprecipitation reaction can be adjusted by adding acids and / or bases, the specifictypes of which are not particularly limited, for example, ammonia water.According to the present invention, the method also includes the reaction product obtainedby the coprecipitation reaction is subjected to a solid-liquid separation (for example,filtering or centrifugal separation) to produce the solid product.Preferably, the condition for drying in step (1-3) includes: the t emperature is 60-150°C, thetime is 4-12h.Preferably, the condition for calcining in step (1-3) includes: the temperature is 300-800°C,the time is 1-8h.According to the present invention, the precious metal component may be introduced instep (2), or in step (3), or a part thereof is introduced in step (2) and the other part isintroduced in step (3). Preferably it is introduced in step (3), and this preferableembodiment is more conducive to the dispersion of precious metal.The precursor of inorganic oxide matrix can be any substance that can be converted intothe oxide matrix through subsequent calcining. Those skilled in the art can make anappropriate selection based on the specific type of inorganic oxide matrix, which will notbe described in detail again here.For example, the precursor of aluminum can be various sols or gels of aluminum, oraluminium hydroxide. The aluminium hydroxide can be at least one of gibbsite, bayerite,nordshandite, diaspore, boehmite and pseudo-boehmite. Most preferably, the precursor ofalumina is pseudo-boehmite.According to the preparation method provided by the present invention, the inorganic oxidematrix is alumina, preferably, before slurrifying, the inorganic oxide matrix and / or theprecursor of inorganic oxide matrix is subjected to acidification treatment. Theacidification treatment can be performed according to the conventional technical means inthe art. Further preferably, the acid used in acidification treatment is hydrochloric acid.The present invention has a relatively wide selection range for the condition of acidificationtreatment., preferably, the condition of acidification treatment includes: the acid / aluminaratio is 0.12-0.22:1, the time is 20-40min.In the present invention, unless otherwise specified, the acid / alumina ratio refers to themass ratio of hydrochloric acid based on 36 wt% of concentrated hydrochloric acid to theprecursor of alumina based on dry basis.The specific implementation mode of acidification treatment can be as follows: adding theprecursor of alumina to water, and slurrifying and dispersing.According to the present invention, the method of mixing and slurrifying the active metalprecursor, the inorganic oxide matrix and / or the precursor of inorganic oxide matrix andoptionally the precursor of precious metal component is not particularly limited, and theaddition order of the active metal precursor, and the inorganic oxide matrix and / or theprecursor of inorganic oxide matrix and optionally the precursor of precious metalcomponent is also not limited, as long as the active metal precursor, and the inorganic oxidematrix and / or the precursor of inorganic oxide matrix and optionally the precursor ofprecious metal component, and water can be contacted. In case that the slurrifying processfurther involves the precursor of precious metal component, the specific mixing andslurrifying process may include: adding the precursor of precious metal component (whichcan be introduced in form of solution) to the acidified inorganic oxide matrix and thenmixing and slurrifying, then adding the active metal precursor, and then drying and / orcalcining the slurry to produce the finished catalyst.According to the present invention, preferably, in step (2), the slurry has a solid content of5-40 wt%.In step (2), the drying is preferably spray drying. In the present invention, the spray dryingcan be performed according to conventional technical means in the art, and the presentinvention has no special limitation thereto. Those skilled in the art can select an appropriatecondition for spray drying based on the average particle size of the target catalyst. Thepreferred condition for spray drying is such that the particles obtained by spray drying havean average particle size of 60-80 μm with the particle size distribution being mainly in therange of 20-100 μm.Preferably, the condition for calcining in step (2) includes: the temperature is 300-800°C,the time is 1-5h.According to the preparation method of the present invention, in step (3), the impregnationis not particularly limited and can be carried out according to conventional technical meansin the art. The impregnation can be saturation impregnation or over-impregnation,preferably over-impregnation.According to the present invention, preferably, in step (3), the precursor of precious metalcomponent is hydrolyzed in an acid solution to provide the impregnation solution.Specifically, after the hydrolysis, the dilution (e.g. by adding water) or the concentration(e.g. by evaporation), and then the impregnation can be performed to provide a catalystwith a specific loading amount of the precious metal component.Preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,preferably at least one of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid.According to the present invention, preferably, the acid is used in such an amount that thepH value of the impregnation solution is less than 6.0, preferably less than 5.0. Adoptingthis preferred embodiment is more conducive to the uniform dispersion of activecomponents and can improve the wear resistance of the finished catalyst.In the present invention, the solid product can be obtained by filtering the mixture obtainedafter impregnation. The filtering can be carried out according to conventional technicalmeans in the art.According to the present invention, in step (3), the solid product can be only dried, or onlycalcined, or dried and then calcined, and the present invention has no special limitationthereto. Preferably, the solid product is dried and then calcined. The present invention hasno special limitation on the conditions for drying and calcining, and drying and calciningcan be carried out according to conventional technical means in the art. For example, thecondition for drying can include: the temperature is 60-150°C, the time is 2-10h. Thepresent invention has no special limitation on the condition for calcining. The calciningcan be performed in an air or inert atmosphere (e.g. nitrogen), and the present inventionhas no special limitation thereto. The condition for calcining in step (3) preferablycomprises: the temperature is 300-800°C, the time is 0.1-5h.According to the method of the present invention, with respect to the method for providingthe active metal component precursor, either a co-precipitation m ethod may be used, or asol-gel method may be used. More preferably, the co-precipitation method is used.However it should be understood that the sol-gel method is also within the protection scopeof the present invention.The catalyst provided by the present invention is suitable for the treatment of any flue gascontaining SOx and NOx, and is particularly suitable for removing SOx and NOx incatalytic cracking regeneration flue gas.Thus according to the ninth aspect of the present invention, the present invention providesa method for simultaneously reducing both SOx and NOx from flue gas, which comprisescontacting a flue gas containing SOx and NOx with the catalyst of the present invention ina condition for simultaneously removing SOx and NOx.According to a preferable embodiment of the present invention, the condition forsimultaneously removing SOx and NOx comprises:the temperature is 500-800°C, e.g. 550-780°C, 550-750°C,the pressure is 0.01-4MPa, e.g. 0.02-4MPa, 0.02-1MPa, 0.03-2MPa, 0.02-0.1MPa,the volumetric hourly space velocity of flue gas is 100-50000h-1, e.g. 200-20000h-1, 500-10000h-1.In the present invention, unless otherwise specified, the pressure is gauge pressure.Preferably, in the flue gas, the SOx content is 0.001-0.5 vol%, 0.002-0.2 vol%, the NOxcontent is 0.001-0.3 vol%, 0.002-0.2 vol%, 0.001-0.03 vol%.Preferably, in the flue gas, the volume content ratio of SOx and NOx is 1-1.4:1, preferably1-1.2:1. This preferred embodiment is more conducive to improving the removal efficiencyof both.The present invention has a relatively wide selection range for the flue gas, and the methodof the present invention is suitable for any flue gas containing both SOx and NOx at thesame time.The flue gas (e.g. catalytic cracking regeneration flue gas) may contain the componentsCO, CO2, and H2O besides SOx and NOx.Preferably, the flue gas is a catalytic cracking regeneration flue gas.In an aspect of the present invention, the present invention provides the following technicalsolutions:1. A catalyst for simultaneously reducing both SOx and NOx in flue gas, which ischaracterized in that, based on the total weight of the catalyst, the catalyst comprises 25-95 wt% of inorganic oxide matrix; 2-70 wt% of rare earth metal component as oxide; 1-30wt% of Group IIA metal component as oxide; 1-15 wt% of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB as oxide; 1-10 wt% of Group VIIB nonpreciousmetal component as oxide; and 0.01-1.5 wt% of precious metal component aselement.2. The catalyst according to technical solution 1, wherein, based on the total weight of thecatalyst, the catalyst contains 40-90 wt% of inorganic oxide matrix; 4-50 wt% of rare earthmetal component as oxide; 1-20 wt% of Group IIA metal component as oxide; 2-12 wt%of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB as oxide;1-8 wt% of Group VIIB non-precious metal component as oxide; 0.02-1.2 wt% of preciousmetal component as element;preferably, based on the total weight of the catalyst, the catalyst contains 50-80 wt% ofinorganic oxide matrix; 4-40 wt% of rare earth metal component as oxide; 2-15 wt% ofGroup IIA metal component as oxide; 2-10 wt% of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB as oxide; 2-5 wt% of Group VIIB non-preciousmetal component as oxide; 0.02-1.0 wt% of precious metal component as element.3. The catalyst according to technical solution 1, wherein, the rare earth metal componentis one or more of La, Ce, Pr and Nd, more preferably La and / or Ce;said Group IIA metal component is one or more of Be, Mg, Ca, Sr and Ba, more preferablyMg;the non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB is one ormore of Fe, Co, Ni, Cu, Zn, and V, more preferably Co and / or Fe;the Group VIIB non-precious metal component is Mn;said precious metal component is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir and Au, morepreferably one or more of Pt, Pd and Rh, most preferably Pd;the inorganic oxide matrix is at least one of alumina, silica-alumina, zeolite, spinel, kaolin,diatomaceous earth, perlite, and perovskite, preferably alumina.4. The catalyst according to any one of technical solutions 1-3, wherein, as metal element,the molar ratio of the rare earth metal component to the non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB is (0.4-18):1, further preferably (0.5-12):1,further more preferably (1-6):1.5. A method for preparing a catalyst for simultaneously reducing both SOx and NOx in fluegas, which method comprises the steps of:(1) a co-precipitation method or a sol-gel method is used to produce an active metalprecursor;(2) mixing and slurrifying an active metal precursor and an inorganic oxide matrix and / ora precursor of inorganic oxide matrix and optionally a precursor of precious metalcomponent to produce a slurry, drying and / or calcining the slurry to produce a composition;the method also optionally comprises: (3) impregnating the composition obtained in step(2) with a solution containing a precursor of precious metal component as impregnationsolution to produce a solid product, and then drying and / or calcining the soild product;wherein the active metal in the active metal precursor comprises rare earth metalcomponent, Group IIA metal component, non-precious metal component(s) selected fromGroups VB, VIII, IB, and IIB, and Group VIIB non-precious metal component;the active metal precursor, the inorganic oxide matrix and / or the precursor of inorganicoxide matrix, and the precursor of precious metal component are used in such amounts thatthe prepared catalyst, based on the total weight of the catalyst, comprises 25-95 wt% ofinorganic oxide matrix; 2-70 wt% of rare earth metal component as oxide; 1-30 wt% ofGroup IIA metal component as oxide; 1-15 wt% of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB as oxide; 1-10 wt% of Group VIIB nonpreciousmetal component as oxide; and 0.01-1.5 wt% of precious metal component aselement.6. The preparation method according to technical solution 5, wherein the active metalprecursor, the inorganic oxide matrix and / or the precursor of inorganic oxide matrix, andthe precursor of precious metal component are used in such amounts that the preparedcatalyst, based on the total weight of the catalyst, comprises 40-90 wt% of inorganic oxidematrix; 4-50 wt% of rare earth metal component as oxide; 1-20 wt% of Group IIA metalcomponent as oxide; 2-12 wt% of non-precious metal component(s) selected from GroupsVB, VIII, IB, and IIB as oxide; 1-8 wt% of Group VIIB non-precious metal component asoxide; 0.02-1.2 wt% of precious metal component as element;preferably, the active metal precursor, the inorganic oxide matrix and / or the precursor ofinorganic oxide matrix, and the precursor of precious metal component are used in suchamounts that the prepared catalyst, based on the total weight of the catalyst, comprises 50-80 wt% of inorganic oxide matrix; 4-40 wt% of rare earth metal component as oxide; 2-15wt% of Group IIA metal component as oxide; 2-10 wt% of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB as oxide; 2-5 wt% of Group VIIB non-preciousmetal component as oxide; 0.02-1.0 wt% of precious metal component as element;preferably, in said active component precursor, as metal element, the molar ratio of the rareearth metal component to the non-precious metal component(s) selected from Groups VB,VIII, IB, and IIB is (0.4-18):1, further preferably (0.5-12):1, further more preferably (1-6):1.7. The preparation method according to technical solution 5 or 6, wherein the rare earthmetal component is one or more of La, Ce, Pr and Nd, more preferably La and / or Ce;said Group IIA metal component is one or more of Be, Mg, Ca, Sr and Ba, more preferablyMg;the non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB is one ormore of Fe, Co, Ni, Cu, Zn, and V, more preferably Co and / or Fe;the Group VIIB non-precious metal component is Mn;said precious metal component is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir and Au, morepreferably one or more of Pt, Pd and Rh, most preferably Pd;the inorganic oxide matrix is at least one of alumina, silica-alumina, zeolite, spinel, kaolin,diatomaceous earth, perlite, and perovskite, preferably alumina.8. The preparation method according to any one of technical solutions 5-7, wherein in step(1), the co-precipitation method is used to produce the active metal precursor; preferably,the co-precipitation method comprises:(1-1) providing a first solution containing a precursor of rare earth metal component, aprecursor of Group IIA metal component, a precursor of non-precious metal component(s)selected from Groups VB, VIII, IB, and IIB, and a precursor of Group VIIB non-preciousmetal component;(1-2) subjecting the first solution and a coprecipitant to carry out a coprecipitation reaction;(1-3) drying and / or calcining a solid product obtained in the coprecipitation reaction.9. The preparation method according to technical solution 8, wherein, the precursor of rareearth metal component, the precursor of Group IIA metal component, the precursor of nonpreciousmetal component(s) selected from Groups VB, VIII, IB, and IIB, and the precursorof Group VIIB non-precious metal component can be each independently selected fromnitrate and / or chloride of each metal component;preferably, the coprecipitant is a carbonate salt, further preferably at least one ofammonium carbonate, potassium carbonate and sodium carbonate;preferably, the coprecipitation reaction is carried out at pH=8-10;preferably, the condition for calcining in step (1-3) includes: the temperature is 300-800°C,the time is 1-8h.10. The preparation method according to any one of technical solutions 5-9, wherein, instep (2), the slurry has a solid content of 5-40 wt%;preferably, the condition for calcining in step (2) includes: the temperature is 300-800°C,the time is 1-5h.11. The preparation method according to any one of technical solutions 5-10, wherein, instep (3), the precursor of precious metal component is hydrolyzed in an acid solution toprovide the impregnation solution;preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,preferably at least one of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid;preferably, the acid is used in such an amount that the pH value of the impregnation solutionis less than 6.0, preferably less than 5.0;preferably, the condition for calcining in step (3) includes: the temperature is 300-800°C,the time is 0.1-5h.12. Use of the catalyst according to any one of technical solutions 1-4 or the catalystprepared with the preparation method according to any one of technical solutions 5-11 insimultaneously removing both SOx and NOx in catalytic cracking regeneration flue gas.13. A method for simultaneously reducing both SOx and NOx from flue gas, whichcomprises contacting a flue gas containing SOx and NOx with the catalyst according to anyone of technical solutions 1-4 or the catalyst prepared with the preparation methodaccording to any one of technical solutions 5-11 under a condition for removing SOx andNOx,preferably, the condition for removing SOx and NOx includes: the temperature is 500-800°C, the pressure is 0.02-4MPa, the volumetric hourly space velocity of flue gas is 100-50000h-1;preferably, in the flue gas, the SOx content is 0.001-0.5 vol%, the NOx content is 0.001-0.3 vol%;preferably, the flue gas is a catalytic cracking regeneration flue gas.In an aspect of the present invention, the present invention provides the following technicalsolutions:1. A desulfurization and denitrification catalyst, which is characterized in that, based onthe total weight of the catalyst, the catalyst comprises by weight percent:as oxide: 25-92 wt% of inorganic oxide matrix, 6-70 wt% of rare earth metal component,1-12 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,1-10 wt% of Group VIIB non-precious metal component; and0.01-1.5 wt% of precious metal component as element.2. The desulfurization and denitrification catalyst according to technical solution 1,wherein, based on the total weight of the catalyst, which comprises by weight percent:as oxide: 40-85 wt% of inorganic oxide matrix, 12-60 wt% of rare earth metal component,2-10 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 1-8 wt% of Group VIIB non-precious metal component;as element: 0.02-1.2 wt% of precious metal component;preferably, based on the total weight of the catalyst, which comprises by weight percent:as oxide: 45-80 wt% of inorganic oxide matrix, 12-48 wt% of rare earth metal component,2-8 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 2-5 wt% of Group VIIB non-precious metal component;as element: 0.02-1.0 wt% of precious metal component.3. The desulfurization and denitrification catalyst according to technical solution 1,wherein, the rare earth metal component is selected from one or more of La, Ce, Pr and Nd,more preferably La;the non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB is one ormore of Fe, Co, Ni, Cu, Zn and V, more preferably Co;the Group VIIB non-precious metal component is Mn;the precious metal component is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir and Au, morepreferably one or more of Pt, Pd and Rh, most preferably Pd;the inorganic oxide matrix is one or more alumina, silica-alumina, zeolite, spinel, kaolin,diatomaceous earth, perlite, and perovskite, preferably alumina.4. The desulfurization and denitrification catalyst according to any one of technicalsolutions 1-3, wherein as element, the molar ratio of the rare earth metal component to thenon-precious metal component(s) selected from Groups VB, VIII, IB, and IIB is (0.6-18):1,further preferably (2-12):1, further more preferably (3-6):1.5. A method for preparing a desulfurization and denitrification catalyst, which comprisesthe steps of:S1. Preparation of active metal precursor: using the co-precipitation method or the sol-gelmethod;S2. Preparation of semi-finished catalyst product: mixing and slurrifying an active metalprecursor and an inorganic oxide matrix and / or a precursor of inorganic oxide matrix andoptionally a precursor of precious metal component to produce a slurry, drying andcalcining the slurry;the method also optionally comprises: S3. impregnating the semi-finished catalyst productobtained in step S2 with a solution containing a precursor of precious metal component asimpregnation solution to produce a solid product, and drying and calcining the solidproduct;wherein the active metal in the active metal precursor comprises a rare earth metalcomponent, non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and a Group VIIB non-precious metal component;the active metal precursor, the inorganic oxide matrix and / or the precursor of inorganicoxide matrix, and the precursor of precious metal component are used in such amounts thatthe prepared catalyst, based on the total weight of the catalyst, comprises by weight percent:as oxide: 25-92 wt% of inorganic oxide matrix, 6-70 wt% of rare earth metal component,1-12 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,1-10 wt% of Group VIIB non-precious metal component; and0.01-1.5 wt% of precious metal component as element.6. The preparation method according to technical solution 5, wherein the active metalprecursor, the inorganic oxide matrix and / or the precursor of inorganic oxide matrix, andthe precursor of precious metal component are used in such amounts that the preparedcatalyst, based on the total weight of the catalyst, comprises by weight percent:as oxide: 40-85 wt% of inorganic oxide matrix, 12-60 wt% of rare earth metal component,2-10 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 1-8 wt% of Group VIIB non-precious metal component;as element: 0.02-1.2 wt% of precious metal component;preferably, the active metal precursor, the inorganic oxide matrix and / or the precursor ofinorganic oxide matrix, and the precursor of precious metal component are used in suchamounts that the prepared catalyst, based on the total weight of the catalyst, comprises byweight percent:as oxide: 45-80 wt% of inorganic oxide matrix, 12-48 wt% of rare earth metal component,2-8 wt% of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and 2-5 wt% of Group VIIB non-precious metal component;as element: 0.02-1.0 wt% of precious metal component;preferably, in said active component precursor, as metal element, the molar ratio of the rareearth metal component to the non-precious metal component(s) selected from Groups VB,VIII, IB, and IIB is (0.6-18):1, further preferably (2-12):1, further more preferably (3-6):1.7. The preparation method according to technical solution 5 or 6, wherein the rare earthmetal component is selected from one or more of La, Ce, Pr and Nd, more preferably La;the non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB is one ormore of Fe, Co, Ni, Cu, Zn and V, more preferably Co;the Group VIIB non-precious metal component is Mn;said precious metal component is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir and Au, morepreferably one or more of Pt, Pd and Rh, most preferably Pd;the inorganic oxide matrix is one or more alumina, silica-alumina, zeolite, spinel, kaolin,diatomaceous earth, perlite, and perovskite, preferably alumina.8. The preparation method according to any one of technical solutions 5-7, wherein in stepS1, the co-precipitation method is used to produce an active metal precursor,preferably, the co-precipitation m ethod comprises:S11. Preparing a first solution containing a precursor of rare earth metal component, aprecursor of non-precious metal component(s) selected from Groups VB, VIII, IB, and IIB,and a precursor of Group VIIB non-precious metal component;S12. Subjecting a first solution and a coprecipitant to carry out a coprecipitation reaction;S13. Drying and / or calcining a solid product obtained in the coprecipitation reaction.9. The preparation method according to technical solution 8, wherein, the precursor of rareearth metal component, the precursor of non-precious metal component(s) selected fromGroups VB, VIII, IB, and IIB, the precursor of Group VIIB non-precious metal component,and the precursor of precious metal component are each independently selected fromnitrates and / or chlorides of metal components;preferably, the coprecipitant is a carbonate salt, preferably one or more of ammoniumcarbonate, potassium carbonate, and sodium carbonate;preferably, the coprecipitation reaction is carried out at pH=8-10;preferably, the condition for calcining in step S13 is: the temperature is 300-800°C, thetime is 1-8h.10. The preparation method according to any one of technical solutions 5-9, wherein, instep S2, the slurry has a solid content of 5-40 wt%;preferably, the condition for calcining in step S2 is: the temperature is 300-800°C, the timeis 1-5h.11. The preparation method according to any one of technical solutions 5-10, wherein, instep S3, the precursor of precious metal component is hydrolyzed in an acid solution toprovide the impregnation solution;preferably, the acid is a water-soluble inorganic acid and / or organic acid, preferably one ormore of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid.preferably, the acid is used in such an amount that the pH value of the impregnation solutionis less than 6.0, preferably less than 5.0;preferably, the condition for calcining in step S3 is: the temperature is 300-800°C, the timeis 0.1-5h.12. Use of the desulfurization and denitrification catalyst according to any one of technicalsolutions 1-4 or the desulfurization and denitrification catalyst prepared with thepreparation method according to any one of technical solutions 5-11 in simultaneouslyremoving both SOx and NOx in flue gas.13. Use according to technical solution 12, wherein the desulfurization and denitrificationcatalyst is contacted with a flue gas containing SOx and NOx;wherein the condition for removing SOx and NOx is: the temperature is 500-800°C, thepressure is 0.02-4MPa, the volumetric hourly space velocity of flue gas is 100-50000h-1;preferably, the flue gas has a SOx content of 0.001-0.5 vol%, and an NOx content of 0.001-0.3 vol%;preferably, the flue gas is a catalytic cracking regeneration flue gas.In an aspect of the present invention, the present invention provides the following technicalsolutions:1. A catalyst for reducing the emission of NOx and SOx in flue gas, the catalyst comprisesa support and, loaded on the support, a first active component selected from rare earthmetals, a second active component selected from Group VIII non-precious metals and aprecious metal component; based on the total weight of the catalyst, the content of thesupport is 25-95 wt%, the content of the first active component as oxide is 4-60 wt%, thecontent of the second active component (as_oxide) is 2-12 wt%, and the content of theprecious metal component as element is 0.01-2 wt%;as metal oxides, the molar ratio of the first active component to the second activecomponent is (0.5-15):1.2. The catalyst according to technical solution 1, wherein, based on the total weight of thecatalyst, the content of the support is 40-90 wt%, the content of the first active componentas oxide is 8-50 wt%, the content of the second active component (as_oxide) is 2-12 wt%,and the content of the precious metal component as element is 0.02-1.5 wt%;preferably, based on the total weight of the catalyst, the content of the support is 50-88wt%, the content of the first active component as oxide is 8-40 wt%, the content of thesecond active component (as_oxide) is 2-10 wt%, and the content of the precious metalcomponent as element is 0.03-1.2 wt%.3. The catalyst according to technical solution 1 or 2, wherein, as metal oxides, the molarratio of the first active component to the second active component is (1-10):1, furtherpreferably (2-5):1.4. The catalyst according to any one of technical solutions 1-3, wherein,the first active component is La and / or Ce, preferably La;the second active component is at least one of Group VIII metals, preferably Co and / or Fe,more preferably Co;the precious metal component is one or more of Pt, Pd and Rh, most preferably Pd;the support is at least one of alumina, silica-alumina, zeolite, spinel, kaolin, diatomaceousearth, perlite, and perovskite, preferably alumina.5. A method for preparing the catalyst for reducing the emission of NOx and SOx in fluegas according to any one of technical solutions 1-4, which method comprises:(1) providing a precursor solution containing a precursor of a first active componentselected from rare earth metals, and a precursor of a second active component selected fromGroup VIII non-precious metals;(2) carrying out a coprecipitation reaction between the precursor solution and acoprecipitant, then drying and calcining;(3) mixing and slurrifying the solid product obtained in step (2) and a support and / or aprecursor of a support to produce a slurry, then drying and calcining the slurry;(4) impregnating the solid product obtained in step (3) with a solution containing aprecursor of precious metal component as impregnation solution, then drying and / orcalcining.6. The preparation method according to technical solution 5, wherein the precursor of firstactive component and the precursor of second active component are each independentlyselected from nitrate and / or chloride of each metal component;the precursor of the precious metal component is at least one of palladium nitrate, palladiumchloride, platinum chlorate and rhodium chloride, preferably palladium nitrate and / orpalladium chloride.7. The preparation method according to technical solution 5 or 6, wherein in step (2), thecoprecipitant is a carbonate salt, further preferably at least one of ammonium carbonate,potassium carbonate and sodium carbonate;preferably, the coprecipitation reaction is carried out at pH=8-10;preferably, the condition for calcining in step (2) includes: the temperature is 300-800°C,the time is 1-8h.8. The preparation method according to any one of technical solutions 5-7, wherein in step(3), the slurry has a solid content of 7-35 wt%;preferably, the condition for calcining in step (3) includes: the temperature is 300-800°C,the time is 1-5h.9. The preparation method according to any one of technical solutions 5-8, wherein, in step(4), the precursor of precious metal component is hydrolyzed in an acid solution to providethe impregnation solution;preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,preferably at least one of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid;preferably, the acid is used in such an amount that the pH value of the impregnation solutionis less than 5.0, preferably 2-5;preferably, the condition for calcining in step (4) includes: the temperature is 300-700°C,the time is 0.1-5h.10. A method for simultaneously reducing both SOx and NOx from flue gas, which methodcomprises: contacting a flue gas containing SOx and NOx with the catalyst for reducingthe emission of NOx and SOx in flue gas according to any one of technical solutions 1-4under a condition for simultaneously removing SOx and NOx;preferably, the condition for simultaneously removing SOx and NOx comprises: thetemperature is 500-800°C, the pressure is 0.01-4MPa, the volumetric hourly space velocityof flue gas is 100-50000h-1;preferably, in the flue gas, the SOx content is 0.001-0.5 vol%, the NOx content is 0.001-0.3 vol%;preferably, the flue gas is a catalytic cracking regeneration flue gas.In an aspect of the present invention, the present invention provides the following technicalsolutions:1. A catalyst capable of / for simultaneously reducing both SOx and NOx in flue gas, whereinthe catalyst comprises a support and, loaded on the support, a first active componentselected from rare earth metals, a second active component selected from non-preciousmetals of Groups VB, VIII, IB, and IIB, a third active component selected from Group IIAmetals, and a precious metal component; based on the total weight of the catalyst, thecontent of the support is 25-93 wt%, the content of the first active component as oxide is4-60 wt%, the content of the second active component (as_oxide) is 2-30 wt%, the contentof the third active component (as_oxide) is 1-30 wt%, and the content of the precious metalcomponent as element is 0.01-2 wt%.2. The catalyst according to technical solution 1, wherein,as metal oxides, the molar ratio of the first active component to the second activecomponent is (0.4-12):1, preferably (0.5-8):1, further preferably (1-4):1.3. The catalyst according to technical solution 1, wherein,based on the total weight of the catalyst, the content of the support is 40-87 wt%, thecontent of the first active component as oxide is 8-50 wt%, the content of the second activecomponent (as_oxide) is 3-20 wt%, the content of the third active component (as_oxide)is1-20 wt%, and the content of the precious metal component as element is 0.02-1.5 wt%;preferably, based on the total weight of the catalyst, the content of the support is 45-80wt%, the content of the first active component as oxide is 8-40 wt%, the content of thesecond active component (as_oxide) is 3-15 wt%, the content of the third active component(as_oxide) is2-15 wt%, and the content of the precious metal component as element is 0.03-1.2 wt%.4. The catalyst according to any one of technical solutions 1-3, wherein,the support is at least one of alumina, silica-alumina, zeolite, spinel, kaolin, diatomaceousearth, perlite, and perovskite, preferably alumina;the first active component is La and / or Ce, preferably La;the second active component is at least one of Group VIII metals, preferably Co and / or Fe,more preferably Co;the third active component is one or more of Be, Mg, Ca, Sr and Ba, preferably Mg;the precious metal component is one or more of Pt, Pd and Rh, most preferably Pd.5. A method for preparing a catalyst capable of simultaneously reducing SOx and NOx influe gas, which method comprises the steps of:(1) providing a precursor solution containing a precursor of a first active componentselected from rare earth metals, a precursor of a second active component selected fromnon-precious metals of Groups VB, VIII, IB, and IIB, and a precursor of a third activecomponent selected from Group IIA metals;(2) carrying out a coprecipitation reaction between the precursor solution and acoprecipitant, then drying and calcining;(3) mixing and slurrifying the solid product obtained in step (2) and a support and / or aprecursor of a support and optionally a precursor of precious metal component to producea slurry, then drying and calcining the slurry;the method also optionally comprises: (4) impregnating the solid product obtained in step(3) with a solution containing a precursor of precious metal component as impregnationsolution, then drying and / or calcining;the precursor of first active component, the precursor of second active component, theprecursor of third active component, the support and / or the precursor of support, and theprecursor of precious metal component are used in such amounts that in the preparedcatalyst, based on the total weight of the catalyst, the content of the support is 25-93 wt%,the content of the first active component as oxide is 4-60 wt%, the content of the secondactive component (as_oxide) is 2-30 wt%, the content of the third active component(as_oxide) is 1-30 wt%, and the content of the precious metal component as element is0.01-2 wt%.6. The method according to technical solution 5, wherein, as metal element, the molar ratioof the precursor of first active component to the precursor of second active component is(0.4-12):1, preferably (0.5-8):1, further preferably (1-4):1.7. The method according to technical solution 5 or 6, wherein, the precursor of first activecomponent, the precursor of second active component, the precursor of third activecomponent, the support and / or the precursor of support, and the precursor of precious metalcomponent are used in such amounts that in the prepared catalyst, based on the total weightof the catalyst, the content of the support is 40-87 wt%, the content of the first activecomponent as oxide is 8-50 wt%, the content of the second active component (as_oxide) is3-20 wt%, the content of the third active component (as_oxide) is1-20 wt%, and the contentof the precious metal component as element is 0.02-1.5 wt%;preferably, the precursor of first active component, the precursor of second activecomponent, the precursor of third active component, the support and / or the precursor ofsupport, and the precursor of precious metal component are used in such amounts that inthe prepared catalyst, based on the total weight of the catalyst, the content of the supportis 45-80 wt%, the content of the first active component as oxide is 8-40 wt%, the contentof the second active component (as_oxide) is 3-15 wt%, the content of the third activecomponent (as_oxide) is2-15 wt%, and the content of the precious metal component aselement is 0.03-1.2 wt%.8. The method according to any one of technical solutions 5-7, wherein,the support is at least one of alumina, silica-alumina, zeolite, spinel, kaolin, diatomaceousearth, perlite, and perovskite, preferably alumina;the first active component is La and / or Ce, preferably La;the second active component is at least one of Group VIII metals, preferably Co and / or Fe,more preferably Co;the third active component is one or more of Be, Mg, Ca, Sr and Ba, preferably Mg;the precious metal component is one or more of Pt, Pd and Rh, most preferably Pd.9. The method according to any one of technical solutions 5-8, wherein,in step (2), the coprecipitant is a carbonate salt, preferably at least one of ammoniumcarbonate, potassium carbonate, and sodium carbonate;preferably, in step (2), the coprecipitation reaction is carried out at pH=8-10;preferably, in step (3), the slurry has a solid content of 6-38 wt%.10. The method according to any one of technical solutions 5-9, wherein,in step (4), the precursor of precious metal component is hydrolyzed in an acid solution toprovide the impregnation solution;preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,preferably at least one of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid;preferably, the acid is used in such an amount that the pH value of the impregnation solutionis less than 6.0, preferably 2-5.11. The method according to any one of technical solutions 5-10, wherein, in step (2), step(3) and step (4), the conditions for calcining may each independently include: thetemperature is 300-800°C, the time is 0.5-8h.12. The catalyst capable of simultaneously reducing SOx and NOx in flue gas preparedwith the method according to any one of technical solutions 5-11.13. Use of the catalyst capable of simultaneously reducing SOx and NOx in flue gasaccording to any one of technical solutions 1-4 and 12 in simultaneously removing bothSOx and NOx in a flue gas containing SOx and NOx.14. A method for simultaneously reducing both SOx and NOx from flue gas, which methodcomprises:contacting a flue gas with the catalyst capable of simultaneously reducing SOx and NOxin flue gas according to any one of technical solutions 1-4 and 12;preferably, the condition for contacting includes: the temperature is 500-800°C, thepressure is 0.01-4MPa, the volumetric hourly space velocity of catalytic crackingregeneration flue gas is 200-20000h-1;preferably, in the flue gas, the SOx content is 0.001-0.5 vol%, the NOx content is 0.001-0.3 vol%.In an aspect of the present invention, the present invention provides the following technicalsolutions:1. A catalyst capable of / for simultaneously reducing both SOx and NOx in flue gas, whichis characterized in that, the catalyst comprises the following components or essentiallyconsists of the following components, wherein the active component is components (2) to(6):(1) a support or inorganic oxide matrix, (2) a rare earth metal, (3) a non-precious metalselected from Group VIII, or non-precious metal(s) selected from Groups VB, VIII, IB, andIIB, (4) a precious metal, (5) optionally, a Group VIIB non-precious metal, (6) optionally,a Group IIA metal,wherein on the basis that the total weight of the catalyst is 100 wt%,the content of the support or inorganic oxide matrix of component (1) as oxide is 25-95wt%, e.g., 25-93 wt%, or 25-92 wt%, or 40-90 wt%, or 40-87 wt%, or 40-85 wt%, or 45-80 wt%, or 50-88 wt%, or 50-80 wt%;the content of the rare earth metal(s) of component (2) as oxide is 2-70 wt%, e.g., 4-60wt%, or 4-50 wt%, or 4-40 wt%, or 6-70 wt%, or 8-50 wt%, or 8-40 wt%, or 12-60 wt%,or 12-48 wt%;the content of the non-precious metal selected from Group VIII or said non-preciousmetal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 1-30wt%, e.g., 1-15 wt%, or 1-12 wt%, or 2-30 wt%, or 2-12 wt%, or 2-10 wt%, or 2-8 wt%,or 3-20 wt%, or 3-15 wt%;the content of the precious metal of component (4) as element is 0.01-2 wt%, e.g., 0.01-1.5wt%, or 0.01-2 wt%, or 0.02-1.5 wt%, or 0.02-1.2 wt%, or 0.02-1.0 wt%; or 0.03-1.2 wt%;the content of the Group VIIB non-precious metal of component (5) as oxide is: 0 or 1-10wt%, 0 or 1-8 wt%, 0 or 2-5 wt%;the content of the Group IIA metal of component (6) as oxide is 0 or 1-30 wt%, 0 or 1-20wt%, 0 or 2-15 wt%;wherein, as metal element, the molar ratio of component (2) to component (3) is (0.4-18):1,for example (0.4-12):1, or (0.5-15):1, or (0.5-12):1, or (0.5-8):1, or (0.6-18):1, or (1-10):1,or (1-6):1, or (1-4):1, or (2-12):1, or (2-5):1, or (3-6):1;preferably, the sum of the content of the Group VIIB non-precious metal of component (5)as oxide and the content of the Group IIA metal of component (6) as oxide is not zero.2. The catalyst according to technical solution 1, wherein,the support or inorganic oxide matrix of component (1) is at least one of alumina, silicaalumina,zeolite, spinel, kaolin, diatomaceous earth, perlite, and perovskite, preferablyalumina; and / orthe rare earth metal of component (2) is one or more of La, Ce, Pr and Nd, more preferablyLa and / or Ce; most preferably La; and / orthe non-precious metal selected from Group VIII of component (3) is Co and / or Fe, morepreferably Co; or said non-precious metal(s) selected from Groups VB, VIII, IB, and IIBof component (3) is one or more of Fe, Co, Ni, Cu, Zn, and V, more preferably Co and / orFe, most preferably Co; and / orthe precious metal of component (4) is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir, and Au,more preferably one or more of Pt, Pd and Rh, most preferably Pd; and / orthe Group VIIB non-precious metal of component (5) is Mn; and / orthe Group IIA metal of component (6) is one or more of Be, Mg, Ca, Sr and Ba, morepreferably Mg.3. The catalyst according to any one of the preceding technical solutions, whereinthe catalyst comprises (1) a support and, loaded on the support, (2) a rare earth metal, (3)a non-precious metal selected from Group VIII, and (4) a precious metal, wherein the activecomponent is components (2) to (4);wherein on the basis that the total weight of the catalyst is 100 wt%,the content of the support of component (1) is 25-95 wt%;the content of the rare earth metal(s) of component (2) as oxide is 4-60 wt%;the content of the non-precious metal selected from Group VIII of component (3) as oxideis 2-12 wt%;the content of the precious metal of component (4) as element is 0.01-2 wt%;orthe content of the support of component (1) is 40-90 wt%;the content of the rare earth metal(s) of component (2) as oxide is 8-50 wt%;the content of the non-precious metal selected from Group VIII of component (3) as oxideis 2-12 wt%;the content of the precious metal of component (4) as element is 0.02-1.5 wt%;orthe content of the support or inorganic oxide matrix of component (1) as oxide is 50-88wt%;the content of the rare earth metal(s) of component (2) as oxide is 8-40 wt%;the content of the non-precious metal selected from Group VIII of component (3) as oxideis 2-10 wt%;the content of the precious metal of component (4) as element is 0.03-1.2 wt%;wherein, as metal element, the molar ratio of component (2) to component (3) is (0.5-15):1,or (1-10):1, or (2-5):1.4. The catalyst according to any one of the preceding technical solutions, wherein thecatalyst comprises (1) a support and, loaded on the support, (2) a rare earth metal, (3) nonpreciousmetal(s) selected from Groups VB, VIII, IB, and IIB, (4) a precious metal, and (6)a Group IIA metal,wherein the active component is components (2) to (4) and (6);wherein on the basis that the total weight of the catalyst is 100 wt%,the content of the support or inorganic oxide matrix of component (1) as oxide is 25-93wt%;the content of the rare earth metal(s) of component (2) as oxide is 4-60 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 2-30 wt%;the content of the precious metal of component (4) as element is 0.01-2 wt%;the content of the Group IIA metal of component (6) as oxide is 1-30 wt%;orthe content of the support or inorganic oxide matrix of component (1) as oxide is 40-87wt%;the content of the rare earth metal(s) of component (2) as oxide is 8-50 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 3-20 wt%;the content of the precious metal of component (4) as element is 0.02-1.5 wt%;the content of the Group IIA metal of component (6) as oxide is 1-20 wt%;orthe content of the support or inorganic oxide matrix of component (1) as oxide is 40-85wt%;the content of the rare earth metal(s) of component (2) as oxide is 8-40 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 3-15 wt%;the content of the precious metal of component (4) as element is 0.03-1.2 wt%;the content of the Group IIA metal of component (6) as oxide is 2-15 wt%;wherein, as metal element, the molar ratio of component (2) to component (3) is (0.4-18):1,for example (0.4-12):1, or (0.5-8):1, or (1-4):1.5. The catalyst according to any one of the preceding technical solutions, whereinthe catalyst comprises the following components or essentially consists of the followingcomponents, wherein the active component is components (2) to (5):(1) a support or inorganic oxide matrix, (2) a rare earth metal, (3) non-precious metal(s)selected from Groups VB, VIII, IB, and IIB, (4) a precious metal, and (5) a Group VIIBnon-precious metal,wherein on the basis that the total weight of the catalyst is 100 wt%,the content of the support or inorganic oxide matrix of component (1) as oxide is 25-92wt%;the content of the rare earth metal(s) of component (2) as oxide is 6-70 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 1-12 wt%;the content of the precious metal of component (4) as element is 0.01-1.5 wt%;the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-10 wt%;orthe content of the support or inorganic oxide matrix of component (1) as oxide is 40-85wt%;the content of the rare earth metal(s) of component (2) as oxide is 12-60 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 2-10 wt%;the content of the precious metal of component (4) as element is 0.02-1.2 wt%;the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-8 wt%;orthe content of the support or inorganic oxide matrix of component (1) as oxide is 40-85wt%;the content of the rare earth metal(s) of component (2) as oxide is 12-48 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 2-8 wt%;the content of the precious metal of component (4) as element is 0.02-1.0 wt%;the content of the Group VIIB non-precious metal of component (5) as oxide is: 2-5 wt%;wherein, as metal element, the molar ratio of component (2) to component (3) is (0.6-18):1,e.g. (2-12):1, or (3-6):1.6. The catalyst according to any one of the preceding technical solutions, whereinthe catalyst comprises the following components or essentially consists of the followingcomponents, wherein the active component is components (2) to (6):(1) a support or inorganic oxide matrix, (2) a rare earth metal, (3) non-precious metal(s)selected from Groups VB, VIII, IB, and IIB, (4) a precious metal, (5) a Group VIIB nonpreciousmetal, and (6) a Group IIA metal,wherein on the basis that the total weight of the catalyst is 100 wt%,the content of the support or inorganic oxide matrix of component (1) as oxide is 25-95wt%;the content of the rare earth metal(s) of component (2) as oxide is 2-70 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 1-15 wt%;the content of the precious metal of component (4) as element is 0.01-1.5 wt%;the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-10 wt%;the content of the Group IIA metal of component (6) as oxide is 1-30 wt%;orthe content of the support or inorganic oxide matrix of component (1) as oxide is 40-90wt%;the content of the rare earth metal(s) of component (2) as oxide is 4-50 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 2-12 wt%;the content of the precious metal of component (4) as element is 0.02-1.2 wt%;the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-8 wt%;the content of the Group IIA metal of component (6) as oxide is 1-20 wt%;orthe content of the support or inorganic oxide matrix of component (1) as oxide is 50-80wt%;the content of the rare earth metal(s) of component (2) as oxide is 4-40 wt%;the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB ofcomponent (3) as oxide is 2-10 wt%;the content of the precious metal of component (4) as element is 0.02-1.0 wt%;the content of the Group VIIB non-precious metal of component (5) as oxide is: 2-5 wt%;the content of the Group IIA metal of component (6) as oxide is 2-15 wt%;wherein, as metal element, the molar ratio of component (2) to component (3) is (0.4-18):1,for example (0.5-12):1, or (1-6):1.7. The catalyst according to any one of the preceding technical solutions, wherein thecatalyst is a catalyst that has been exposed to an atmosphere containing SO2;for example, the catalyst is a catalyst that has been exposed to an atmosphere containingSO2, wherein the atmosphere containing SO2 has a temperature of 350-1000°C, a pressureof 0-8 MPa, and an SO2 content of 0.001-100 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 400-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 450-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 500-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 550-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 600-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 650-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 400-800°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 450-800°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 500-800°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 550-800°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 600-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 650-900°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 400-750°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 450-750°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 500-750°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 550-750°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 600-750°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 650-750°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 400-700°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 450-700°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 500-700°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 550-700°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 600-700°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for at least1 minute, wherein the atmosphere containing SO2 has a temperature of 650-700°C, apressure of 0-5 MPa, and an SO2 content of 0.001-5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 400-900°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 450-900°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 500-900°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 550-900°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 600-900°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 650-900°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 400-800°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 450-800°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 500-800°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 550-800°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 600-800°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 650-800°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 400-750°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 450-750°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 500-750°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 550-750°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 600-750°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 650-750°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 400-700°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 450-700°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 500-700°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 550-700°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 600-700°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 30-480minutes, wherein the atmosphere containing SO2 has a temperature of 650-700°C, apressure of 0-2 MPa, and an SO2 content of 0.01-1 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 400-900°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 450-900°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 500-900°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 550-900°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 600-900°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 650-900°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 400-800°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 450-800°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 500-800°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 550-800°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 600-800°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 650-800°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 400-750°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 450-750°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 500-750°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 550-750°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 600-750°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 650-750°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 650-750°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 400-700°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 450-700°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 500-700°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 550-700°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 600-700°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%; orthe catalyst is a catalyst that has been exposed to an atmosphere containing SO2 for 60-120minutes, wherein the atmosphere containing SO2 has a temperature of 650-700°C, apressure of 0-0.5 MPa, and an SO2 content of 0.02-0.5 vol%.8. The catalyst according to any one of the preceding technical solutions, whereinthe rare earth metal(s) of component (2) comprises La;the non-precious metal selected from Group VIII or said non-precious metal(s) selectedfrom Groups VB, VIII, IB, and IIB of component (3) comprises Co;the precious metal of component (4) comprises Pd;the Group VIIB non-precious metal of component (5), if any, comprises Mn;the Group IIA metal of component (6), if any, comprises Mg.9. The catalyst according to any one of the preceding technical solutions, whereinthe rare earth metal(s) of component (2) is La;the non-precious metal selected from Group VIII or said non-precious metal(s) selectedfrom Groups VB, VIII, IB, and IIB of component (3) is Co;the precious metal of component (4) is Pd;the Group VIIB non-precious metal of component (5), if any, is Mn;the Group IIA metal of component (6), if any, is Mg.10. The catalyst according to any one of the preceding technical solutions, wherein thecatalyst is a catalyst that has been exposed to an atmosphere containing SO2, the catalysthas characteristic peaks at 2θ=28.6°±0.1°, 30.0°±0.1° and 50.4°±0.1° in the powder XRDspectrum.11. The catalyst according to any one of the preceding technical solutions, wherein thecatalyst (fresh) has characteristic peaks at 2θ=33.0°±0.1°, 33.5°±0.1°, and 47.5°±0.1°, aswell as 27.0°±0.1°, 28.0°±0.1°, and 39.5°±0.1° in the powder XRD spectrum.12. A method for preparing the catalyst according to any one of the preceding technicalsolutions, which method comprises:(I) a co-precipitation method or a sol-gel method is used to produce an active metalprecursor,wherein the active metal in the active metal precursor comprises (2) a rare earth metal, (3)a non-precious metal selected from Group VIII, or non-precious metal(s) selected fromGroups VB, VIII, IB, and IIB, (5) optionally, a Group VIIB non-precious metal, and (6)optionally, a Group IIA metal; and(II) the active metal precursor and (1) the support or inorganic oxide matrix or a precursorthereof, and optionally a precursor of (4) the precious metal are mixed and slurrified toproduce a slurry, the resulting slurry is dried and / or calcined to produce a catalyst; orthe active metal precursor and (1) the support or inorganic oxide matrix or aprecursor thereof, and optionally a precursor of (4) the precious metal are mixed andslurrified to produce a slurry, the resulting slurry is dried and / or calcined to produce a semifinishedcatalyst product; then the semi-finished catalyst product is impregnated with asolution containing a precursor of (4) the precious metal as impregnation solution toproduce a solid product, and then the solid product is dried and / or calcined to produce acatalyst;wherein the active metal precursor, the support or inorganic oxide matrix or the precursorthereof, and the precursor of the precious metal are used in such amounts that the producedcatalyst has the composition of the catalyst of any of the preceding technical solutions.13. The preparation method according to any of the preceding technical solutions, whereinin step (I), the co-precipitation method is used to produce the active metal precursor;preferably, the co-precipitation method comprises:(I-1) providing a first solution containing a precursor of (2) rare earth metal(s), a precursorof (3) non-precious metal selected from Group VIII or non-precious metal(s) selected fromGroups VB, VIII, IB, and IIB, optionally a precursor of (5) Group VIIB non-precious metal,and optionally a precursor of (6) Group IIA metal;preferably, each precursor is independently selected from nitrate and / or chloride of eachmetal;(I-2) subjecting the first solution and a coprecipitant to carry out a coprecipitation reaction;preferably, the coprecipitant is a carbonate salt, further preferably at least one ofammonium carbonate, potassium carbonate and sodium carbonate;preferably, the coprecipitation reaction is carried out at pH=8-10;(I-3) drying and / or calcining a soild product obtained in the coprecipitation reaction toproduce an active metal precursor;preferably, the condition for calcining in step (I-3) includes: the temperature is 300-800°C,e.g., 300-700°C, the time is 0.5-8h, e.g., 1-8h or 1-5h,wherein, the support or inorganic oxide matrix or a precursor thereof, the precursor of rareearth metal(s), the precursor of non-precious metal selected from Group VIII or non30precious metal(s) selected from Groups VB, VIII, IB, and IIB, the precursor of preciousmetal, optionally the precursor of Group VIIB non-precious metal, and optionally theprecursor of Group IIA metal are used in such amounts that the produced catalyst has thecomposition of the catalyst of any of the preceding technical solutions.14. The preparation method according to any one of the preceding technical solutions,whereinin step (II), the precursor of the precious metal component is at least one of nitrates,chlorides, and / or chlorates, e.g. at least one of palladium nitrate, palladium chloride,platinum chlorate and rhodium chloride, preferably palladium nitrate and / or palladiumchloride; and / orin step (II), the slurry has a solid content of 5-40 wt%, e.g., 6-38 wt%, or 7-35 wt%; and / orin step (II), the condition for calcining the slurry includes: the temperature is 300-800°C,e.g., 300-700°C, the time is 0.5-8h, e.g., 1-8h or 1-5h; and / orin step (II), the precursor of precious metal is hydrolyzed in an acid solution to provide theimpregnation solution;preferably, the acid is selected from water-soluble inorganic acids and / or organic acids,more preferably, at least one of hydrochloric acid, nitric acid, phosphoric acid, and aceticacid;preferably, the acid is used in such an amount that the pH value of the impregnationsolution is less than 6.0, preferably less than 5.0, e.g. 2.0-5.0;preferably, the condition for calcining the solid product includes: the temperature is300-800°C, e.g., 300-700°C, the time is 0.5-8h, e.g., 1-8h or 1-5h.15. A method for simultaneously reducing both SOx and NOx from flue gas, whichcomprises, under a condition for removing SOx and NOx, contacting the flue gas with acatalyst according to any one of the preceding technical solutions or a catalyst prepared bya preparation method according to any one of the preceding technical solutions;preferably, the condition for removing SOx and NOx includes: the temperature is 300-1000°C, e.g. 500-800°C, or 600-750°C, or 625-750°C, or 650-750°C, or 675-750°C, or700-750°C, or 725-750°C, or 600-725°C, or 625-725°C, or 650-725°C, or 675-725°C, or700-725°C, or 600-700°C, or 625-700°C, or 650-700°C, or 675-700°C, or 600-675°C, or625-675°C, or 650-675°C, or 600-650°C, or 625-650°C, or 600-625°C; the pressure is 0-4MPa, e.g. 0.01-4 MPa, or 0.02-4 MPa, or 0-0.5 MPa; the volumetric hourly space velocityof flue gas is 100-50000 h-1 or 200-20000h-1; and / orpreferably, in the flue gas, the SOx content is 0.001-0.5 vol%, the NOx content is 0.001-0.3 vol%; or the volume fractions of SOx and NOx in the flue gas are respectively 1-3000μL / L, and the molar ratio of SOx to NOx is 0.5:1-2:1; and / orpreferably, the flue gas is a flue gas containing a certain concentration of SOx and NOx atthe same time, e.g. catalytic cracking regeneration flue gas; preferably, contacting thecatalytic cracking regeneration flue gas with the catalyst is carried out in a flue gas passwayprovided after a catalytic cracking cyclone separator and / or after a CO incinerator.In the present invention, the contents of components in a catalyst with regular structure aredetermined using the X-ray fluorescence spectroscopy (Petrochemical Analysis Methods(RIPP Experimental Methods), edited by Yang Cuiding et al., published by Science Pressin 1990).In the present invention, a Siemens D5005 diffractometer is used to perform powder X-raydiffraction (XRD) analysis on the catalyst sample, in which CuKα (λ=0.15418nm) radiationis generated under the conditions of 40 kV, 40 mA and filtered by Ni. Diffraction signalsare recorded in the range of 2θ 5-70° with a step of 0.02°.In the present invention, the condition for calcining is not particularly limited. For example,the calcining can be performed in an air or inert atmosphere (e.g. nitrogen); the conditionfor calcining may be: the temperature is 300-900°C, e.g. 400, 500, 600, 700, 800°C and atemperature range formed from any two of these points, the time is 0.1-12h, e.g. 0.1-5h,and the pressure can be below atmospheric pressure, atmospheric pressure, or aboveatmospheric pressure (e.g. 0-5MPa).In the present invention, the condition for drying is not particularly limited. For example,the condition for drying may be: the temperature is 25-250°C, the time is 0.1-12h, and thepressure may be in vacuum (for example the absolute pressure is 0-1kPa, 0-5kPa, 0-10kPa,0-20kPa, 0-30kPa, 0-40kPa, 0-50kPa, 0-60kPa, 0-70kPa, 0-80kPa, 0-90kPa, 0-100kPa) oratmospheric pressure (the absolute pressure is 0.1MPa). In the present invention, in casethat the dying followed by the calcining is performed, the drying temperature is lower thanthe calcining temperature.In the present invention, the ppm refers to the volume concentration unless otherwisespecified.The following describes the implementation process and the beneficial effects of thepresent invention in detail through specific examples, which are intended to help readersunderstand the spirit and essence of the present invention more clearly, but do not limit theimplementation scope of the present invention in any way.The raw materials used in the following examples and comparative examples are allcommercially available products. The specific manufacturers and grades are shown in Table1 below:Table 1 Manufacturers and grades of raw materials used in Examples and ComparativeExamplesIn the following examples, the contents of the components in a catalyst are determined byX-ray fluorescence spectroscopy (XRF). For details, see Petrochemical Analysis Methods(RIPP Experimental Methods), edited by Yang Cuiding et al., published by Science Pressin 1990.In the following examples, a Siemens D5005 diffractometer was used to perform powderX-ray diffraction (XRD) analysis on the catalyst sample, in which CuKα (λ=0.15418nm)radiation was generated under the conditions of 40 kV, 40 mA and filtered by Ni.Diffraction signals were recorded in the range of 2θ 5-70° with a step of 0.02°.Example A1350mL of deionized water was added to a beaker, and then 30g as the mass of La2O3 oflanthanum nitrate, 5g as the mass of Co2O3 of cobalt nitrate were added under stirring untilcompletely dissolved. Ammonium carbonate (52.5g) was added to deionized water(210mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9. Thecompletely precipitated mixture was suction-filtered and rinsed with deionized water. Thefilter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°C inan air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofhydrochloric acid (36 wt%) were added. The resulting mixture was slurrified. 20g of theactive metal precursor was weighed and added to the acidified support and the resultingmixture was stirred. The slurry was dried at 200°C, then calcined in an air atmosphere at700°C for 4 hours to produce a semi-finished catalyst microsphere product. The non20precious metal active component comprised 33wt% of the prepared semi-finished catalystmicrosphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at 1:1, and the resultingmixture was diluted with deionized water to produce a palladium chloride solution havinga concentration of 5.6g / L and pH=2. 15g of the semi-finished catalyst microsphere productwas taken, and a certain amount (the Pd equivalent mass of 0.0045g) of the palladiumchloride solution was taken. The Pd-containing solution as impregnation solution wasimpregnated to the above-mentioned semi-finished catalyst product to produce a solidproduct, then the solid product was dried at 120°C, then calcined in an air atmosphere at700°C for 4 hours to produce catalyst A1.XRD analysis was performed on fresh catalyst A1. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst A1 was exposed to an atmosphere containing SO2 for 5 mins, wherein theatmosphere containing SO2 had a temperature of 400°C, a pressure of 0 MPa, and an SO2content of 0.001 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst A1. In the XRD spectrum of catalyst A1, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example A2125mL of deionized water was added to a beaker, and then 10g as the mass of La2O3 oflanthanum nitrate, 2.5g as the mass of Co2O3 of cobalt nitrate were added under stirringuntil completely dissolved. Ammonium carbonate (18.75g) was added to deionized water(75mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 330mL of water and 6g ofhydrochloric acid (36 wt%) were added. The resulting mixture was slurrified. 10g of theactive metal precursor was weighed and added to the acidified support and the resultingmixture was stirred. The slurry was dried at 200°C, then calcined in an air atmosphere at700°C for 4 hours to produce a semi-finished catalyst microsphere product. The nonpreciousmetal active component comprised 20wt% of the prepared semi-finished catalystmicrosphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at 1:1, and the resultingmixture was diluted with deionized water to produce a palladium chloride solution havinga concentration of 5.6g / L and pH=2. 15g of the semi-finished catalyst microsphere productwas taken, and a certain amount (the Pd equivalent mass of 0.003g) of the palladiumchloride solution was taken. The Pd-containing solution as impregnation solution wasimpregnated to the above-mentioned semi-finished catalyst product to produce a solidproduct, then the solid product was dried at 120°C, then calcined in an air atmosphere at700°C for 4 hours to produce catalyst A2.XRD analysis was performed on fresh catalyst A2. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst A2 was exposed to an atmosphere containing SO2 for 5 mins, wherein theatmosphere containing SO2 had a temperature of 400°C, a pressure of 0 MPa, and an SO2content of 0.001 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst A2. In the XRD spectrum of catalyst A2, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example A3331mL of deionized water was added to a beaker, and then 30g as the mass of La2O3 oflanthanum nitrate, 3.1g as the mass of Co2O3 of cobalt nitrate were added under stirringuntil completely dissolved. Ammonium carbonate (49.65g) was added to deionized water(200mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofhydrochloric acid (36 wt%) were added. The resulting mixture was slurrified. 20g of theactive metal precursor was weighed and added to the acidified support and the resultingmixture was stirred. The slurry was dried at 200°C, then calcined in an air atmosphere at700°C for 4 hours to produce a semi-finished catalyst microsphere product. The nonpreciousmetal active component comprised 33wt% of the prepared semi-finished catalystmicrosphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at 1:1, and the resultingmixture was diluted with deionized water to produce a palladium chloride solution havinga concentration of 5.6g / L and pH=2. 15g of the semi-finished catalyst microsphere productwas taken, and a certain amount (the Pd equivalent mass of 0.003g) of the palladiumchloride solution was taken. The Pd-containing solution as impregnation solution wasimpregnated to the above-mentioned semi-finished catalyst product to produce a solidproduct, then the solid product was dried at 120°C, then calcined in an air atmosphere at700°C for 4 hours to produce catalyst A3.XRD analysis was performed on fresh catalyst A3. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst A3 was exposed to an atmosphere containing SO2 for 5 mins, wherein theatmosphere containing SO2 had a temperature of 400°C, a pressure of 0 MPa, and an SO2content of 0.001 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst A3. In the XRD spectrum of catalyst A3, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example A4Example A1 was repeated except that the used amount of bauxite was reduced so that thenon-precious metal active component comprised 50wt% of the prepared semi-finishedcatalyst microsphere product. Specifically, 20g as the mass of Al2O3 of bauxite and 20g ofthe active metal precursor were used to produce catalyst A4.XRD analysis was performed on fresh catalyst A4. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst A4 was exposed to an atmosphere containing SO2 for 5 mins, wherein theatmosphere containing SO2 had a temperature of 400°C, a pressure of 0 MPa, and an SO2content of 0.001 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst A4. In the XRD spectrum of catalyst A4, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example A5350mL of deionized water was added to a beaker, and then 34g as the mass of La2O3 oflanthanum nitrate, 1g as the mass of Co2O3 of cobalt nitrate were added under stirring untilcompletely dissolved. Ammonium carbonate (52.5g) was added to deionized water(210mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofhydrochloric acid (36 wt%) were added. The resulting mixture was slurrified. 20g of theactive metal precursor was weighed and added to the acidified support and the resultingmixture was stirred. The slurry was dried at 200°C, then calcined in an air atmosphere at700°C for 4 hours to produce a semi-finished catalyst microsphere product. The nonpreciousmetal active component comprised 33wt% of the prepared semi-finished catalystmicrosphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at 1:1, and the resultingmixture was diluted with deionized water to produce a palladium chloride solution havinga concentration of 5.6g / L and pH=2. 15g of the semi-finished catalyst microsphere productwas taken, and a certain amount (the Pd equivalent mass of 0.003g) of the palladiumchloride solution was taken. The Pd-containing solution as impregnation solution wasimpregnated to the above-mentioned semi-finished catalyst product to produce a solidproduct, then the solid product was dried at 120°C, then calcined in an air atmosphere at700°C for 4 hours to produce catalyst A5.XRD analysis was performed on fresh catalyst A5. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst A5 was exposed to an atmosphere containing SO2 for 5 mins, wherein theatmosphere containing SO2 had a temperature of 400°C, a pressure of 0 MPa, and an SO2content of 0.001 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst A5. In the XRD spectrum of catalyst A5, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example A6440mL of deionized water was added to a beaker, and then 22g as the mass of La2O3 oflanthanum nitrate, 22g as the mass of Co2O3 of cobalt nitrate were added under stirringuntil completely dissolved. Ammonium carbonate (66g) was added to deionized water(264mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofhydrochloric acid (36 wt%) were added. The resulting mixture was slurrified. 20g of theactive metal precursor was weighed and added to the acidified support and the resultingmixture was stirred. The slurry was dried at 200°C, then calcined in an air atmosphere at700°C for 4 hours to produce a semi-finished catalyst microsphere product. The non-precious metal active component comprised 33wt% of the prepared semi-finished catalystmicrosphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at 1:1, and the resultingmixture was diluted with deionized water to produce a palladium chloride solution havinga concentration of 5.6g / L and pH=2. 15g of the semi-finished c atalyst microsphere productwas taken, and a certain amount (the Pd equivalent mass of 0.003g) of the palladiumchloride solution was taken. The Pd-containing solution as impregnation solution wasimpregnated to the above-mentioned semi-finished catalyst product to produce a solidproduct, then the solid product was dried at 120°C, then calcined in an air atmosphere at700°C for 4 hours to produce catalyst A6.XRD analysis was performed on fresh catalyst A6. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst A6 was exposed to an atmosphere containing SO2 for 5 mins, wherein theatmosphere containing SO2 had a temperature of 400°C, a pressure of 0 MPa, and an SO2content of 0.001 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst A6. In the XRD spectrum of catalyst A6, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example A7Example A1 was repeated except that the palladium chloride solution was replaced withthe equal concentration of a ruthenium chloride solution, and the content of precious metalin the prepared catalyst remained unchanged to produce Catalyst A7.Example A8Example A1 was repeated except that as oxide, lanthanum nitrate was replaced with theequal mass of cerium nitrate; and as oxide, cobalt nitrate was replaced with the equal massof ferric nitrate to produce Catalyst A8.Comparative Example 130g as the mass of La2O3 of lanthanum nitrate was dissolved in a beaker. 45g of ammoniumcarbonate was completely dissolved in another beaker. The lanthanum nitrate solutionunder stirring was added to the ammonium carbonate solution under stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9. Theresulting mixture was suction-filtered. The filter cake mixture obtained by suction filteringwas dried at 120°C, calcined at 700°C in an air atmosphere for 6 hours, and then ground toobtain an active metal precursor L.5g as the mass of Co2O3 of cobalt nitrate was dissolved in a beaker. 7.5g of ammoniumcarbonate was completely dissolved in another beaker. The cobalt nitrate solution understirring was added to the ammonium carbonate solution under stirring, and a certain amountof ammonia water was added to maintain the pH value of the solution at 9. The resultingmixture was suction-filtered. The filter cake mixture obtained by suction filtering was driedat 120°C, calcined at 700°C in an air atmosphere for 6 hours, and then ground to obtain anactive metal precursor C.The active metal precursor L and the active metal precursor C obtained in the first twosteps were fully mechanically mixed to produce a mixed precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the mixed precursor was weighed and added to the acidified inorganic oxide matrixand the resulting mixture was stirred. The slurry was dried at 120°C, then calcined in anair atmosphere at 700°C for 4 hours to produce Catalyst E1.Comparative Example 2The catalyst was prepared as follows: 15g of OX50 (SiO2) powder was weighed, and acertain amount (the Pd equivalent mass of 0.0045g) of the palladium chloride solutionprepared in Example A1 was taken. The palladium chloride solution was added to the OX50powder and mixed evenly by stirring continuously. The resulting mixture was placed in anoven at 120°C until dry, and calcined at 700°C in an air atmosphere for 4 hours to produceCatalyst E2.Comparative Example 330g of La2O3 and 5g of Co2O3 were fully and mechanically mixed to obtain a mixedprecursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the mixed precursor was weighed and added to the acidified inorganic oxide matrixand the resulting mixture was stirred. The slurry was dried at 120°C, then calcined in anair atmosphere at 700°C for 4 hours to produce Catalyst E3.Comparative Example 4A comparative catalyst was prepared according to the method described in CN110787834A.Alumina, kaolin, Mg, B, La, Pt, Ti, alumina sol, and ethyl acetate were weighed accordingto the proportions in Table 2 and mixed. 5 fold water was added and the mixture wasimpregnated at 85°C for more than 3 hours. After impregnation, the mixture was stirred for3 hours at 85°C to disperse evenly. The above slurry was spray-dried at 300°C, and sievedto obtain particles of ≤ 200 μm. The obtained particles were calcined at 500°C for 4 hoursto obtain an active metal precursor. The resulting active metal precursor was fully ground,pressed into tablets, and sieved to produce the final catalyst, marked as E4.Table 2: Mass percentage of each raw material in Comparative Example 4Example B1S1. Preparation of active metal precursor: 360mL of deionized water was added to a beaker,and then 30g as the mass of La2O3 of lanthanum nitrate, 3.5g as the mass of Co2O3 ofcobalt nitrate and 2.5g as the mass of MnO of manganese chloride were added under stirringuntil completely dissolved. Ammonium carbonate54g was added to deionized water(215mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.S2. Preparation of semi-finished catalyst product: 40g as the mass of Al2O3 of bauxite wasweighed, and 380mL of water and 6g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 20g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 33wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Pd was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a palladiumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Pd equivalent mass of0.0045g) of the palladium chloride solution having a concentration of 5.6g / L was taken.The Pd-containing solution as impregnation solution was impregnated to the above25mentioned semi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B1.XRD analysis was performed on fresh catalyst B1. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst B1 was exposed to an atmosphere containing SO2 for 30mins, wherein theatmosphere containing SO2 had a temperature of 650°C, a pressure of 0.05 MPa, and anSO2 content of 0.01 vol%. After exposure to SO2 treatment, XRD analysis was performedon catalyst B1. In the XRD spectrum of catalyst B1, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example B2S1. Preparation of active metal precursor: 150mL of deionized water was added to a beaker,and then 10g as the mass of La2O3 of lanthanum nitrate, 1.6g as the mass of Co2O3 ofcobalt nitrate and 3.4g as the mass of MnO of manganese chloride were added under stirringuntil completely dissolved. Ammonium carbonate (22.5g) was added to deionized water(90mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.S2. Preparation of semi-finished catalyst product: 40g as the mass of Al2O3 of bauxite wasweighed, and 330mL of water and 6g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 10g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 20wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Pd was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a palladiumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Pd equivalent mass of0.0030g) of the palladium chloride solution having a concentration of 5.6g / L was taken.The Pd-containing solution as impregnation solution was impregnated to the above20mentioned semi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B2.Example B3S1. Preparation of active metal precursor: 360mL of deionized water was added to a beaker,and then 30g as the mass of La2O3 of lanthanum nitrate, 2.6g as the mass of Co2O3 ofcobalt nitrate and 3.4g as the mass of MnO of manganese chloride were added under stirringuntil completely dissolved. Ammonium carbonate54g was added to deionized water(215mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.S2. Preparation of semi-finished catalyst product: 40g as the mass of Al2O3 of bauxite wasweighed, and 380mL of water and 6g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 20g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 33wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Pd was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a palladiumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Pd equivalent mass of0.0030g) of the palladium chloride solution having a concentration of 5.6g / L was taken.The Pd-containing solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B3.XRD analysis was performed on fresh catalyst B3. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst B3 was exposed to an atmosphere containing SO2 for 30mins, wherein theatmosphere containing SO2 had a temperature of 650°C, a pressure of 0.05 MPa, and anSO2 content of 0.01 vol%. After exposure to SO2 treatment, XRD analysis was performedon catalyst B3. In the XRD spectrum of catalyst B3, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example B4Example B1 was repeated except that the used amount of bauxite was reduced so that thenon-precious metal active component comprised 50wt% of the prepared semi-finishedcatalyst microsphere product.Specifically, S1. Preparation of active metal precursor: 360mL of deionized water wasadded to a beaker, and then 30g as the mass of La2O3 of lanthanum nitrate, 3.5g as themass of Co2O3 of cobalt nitrate and 2.5g as the mass of MnO of manganese chloride wereadded under stirring until completely dissolved. Ammonium carbonate54g was added todeionized water (215mL), and the mixture was stirred until completely dissolved. Themetal nitrate mixed solution was added to the ammonium carbonate solution while stirring,and a certain amount of ammonia water was added to maintain the pH value of the solutionat 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.S2. Preparation of semi-finished catalyst product: 20g as the mass of Al2O3 of bauxite wasweighed, and 240mL of water and 3g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 20g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 50wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Pd was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a palladiumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Pd equivalent mass of0.0060g) of the palladium chloride solution having a concentration of 5.6g / L was taken.The Pd-containing solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B4.XRD analysis was performed on fresh catalyst B4. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst B4 was exposed to an atmosphere containing SO2 for 30mins, wherein theatmosphere containing SO2 had a temperature of 650°C, a pressure of 0.05 MPa, and anSO2 content of 0.01 vol%. After exposure to SO2 treatment, XRD analysis was performedon catalyst B4. In the XRD spectrum of catalyst B4, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example B5S1. Preparation of active metal precursor: 340mL of deionized water was added to a beaker,and then 30g as the mass of La2O3 of lanthanum nitrate, 1g as the mass of Co2O3 of cobaltnitrate and 3g as the mass of MnO of manganese chloride were added under stirring untilcompletely dissolved. Ammonium carbonate51g was added to deionized water (205mL),and the mixture was stirred until completely dissolved. The metal nitrate mixed solutionwas added to the ammonium carbonate solution while stirring, and a certain amount ofammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.S2. Preparation of semi-finished catalyst product: 40g as the mass of Al2O3 of bauxite wasweighed, and 380mL of water and 6g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 20g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 33wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Pd was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a palladiumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Pd equivalent mass of0.0030g) of the palladium chloride solution having a concentration of 5.6g / L was taken.The Pd-containing solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B5.Example B6S1. Preparation of active metal precursor: 330mL of deionized water was added to a beaker,and then 15g as the mass of La2O3 of lanthanum nitrate, 15g as the mass of Co2O3 of cobaltnitrate and 3g as the mass of MnO of manganese chloride were added under stirring untilcompletely dissolved. Ammonium carbonate (49.5g) was added to deionized water(200mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.S2. Preparation of semi-finished catalyst product: 40g as the mass of Al2O3 of bauxite wasweighed, and 380mL of water and 6g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 20g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 33wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Pd was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a palladiumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Pd equivalent mass of0.0045g) of the palladium chloride solution having a concentration of 5.6g / L was taken.The Pd-containing solution as impregnation solution was impregnated to the above25mentioned semi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B6.XRD analysis was performed on fresh catalyst B6. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst B6 was exposed to an atmosphere containing SO2 for 30mins, wherein theatmosphere containing SO2 had a temperature of 650°C, a pressure of 0.05 MPa, and anSO2 content of 0.01 vol%. After exposure to SO2 treatment, XRD analysis was performedon catalyst B6. In the XRD spectrum of catalyst B6, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example B7S1. Preparation of active metal precursor: 365mL of deionized water was added to a beaker,and then 30g as the mass of La2O3 of lanthanum nitrate, 3.5g as the mass of Co2O3 ofcobalt nitrate and 3g as the mass of MnO of manganese chloride were added under stirringuntil completely dissolved. Ammonium carbonate (54.75g) was added to deionized water(220mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an a ctive metal precursor.S2. Preparation of semi-finished catalyst product: 40g as the mass of Al2O3 of bauxite wasweighed, and 380mL of water and 6g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 20g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 33wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Ru was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a rutheniumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Ru equivalent mass of0.0045g) of the ruthenium chloride solution having a concentration of 5.6g / L was taken.The Ru-containing solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B7.Example B8S1. Preparation of active metal precursor: 365mL of deionized water was added to a beaker,and then 30g as the mass of CeO2 of cerium nitrate, 3.5g as the mass of Fe2O3 of ferricnitrate and 3g as the mass of MnO of manganese chloride were added under stirring untilcompletely dissolved. Ammonium carbonate (54.75g) was added to deionized water(220mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.S2. Preparation of semi-finished catalyst product: 40g as the mass of Al2O3 of bauxite wasweighed, and 380mL of water and 6g of concentrated hydrochloric acid (36 wt%) wereadded. The resulting mixture was slurrified. 20g of the active metal precursor was weighedand added to the acidified inorganic oxide matrix and the resulting mixture was stirred. Theslurry was dried at 200°C, then calcined in an air atmosphere at 700°C for 4 hours toproduce a semi-finished catalyst microsphere product. The non-precious metal activecomponent comprised 33wt% of the prepared semi-finished catalyst microsphere product.S3. Preparation of Catalyst: A precursor of Pd was dissolved in a diluted hydrochloric acidat 1:1, and the resulting mixture was diluted with deionized water to produce a palladiumchloride solution having a concentration of 5.6g / L and pH=2. 15g of the semi-finishedcatalyst microsphere product was taken, and a certain amount (the Pd equivalent mass of0.0045g) of the palladium chloride solution having a concentration of 5.6g / L was taken.The Pd-containing solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst product to produce a solid product, then the solid productwas dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hours to producecatalyst B8.Example C1390mL of deionized water was added to a beaker, and then 30g as the mass of La2O3 oflanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 5.5g as the mass of Co2O3of cobalt nitrate were added under stirring until completely dissolved. Ammoniumcarbonate (59.25g) was added to deionized water (250mL), and the mixture was stirreduntil completely dissolved. The metal nitrate mixed solution was added to the ammoniumcarbonate solution while stirring, and a certain amount of ammonia water was added tomaintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semi25finished catalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0045g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst C1.XRD analysis was performed on fresh catalyst C1. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst C1 was exposed to an atmosphere containing SO2 for 240 minutes, wherein theatmosphere containing SO2 had a temperature of 750°C, a pressure of 0.1 MPa, and an SO2content of 0.02 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst C1. In the XRD spectrum of catalyst C1, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example C2220mL of deionized water was added to a beaker, and then 10g as the mass of La2O3 oflanthanum nitrate, 7g as the mass of MgO of magnesium nitrate, 5g as the mass of Co2O3of cobalt nitrate and were added under stirring until completely dissolved. Ammoniumcarbonate (33g) was added to deionized water (150mL), and the mixture was stirred untilcompletely dissolved. The metal nitrate mixed solution was added to the ammoniumcarbonate solution while stirring, and a certain amount of ammonia water was added tomaintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 330mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.10g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 20wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0030g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst C-2.Example C3390mL of deionized water was added to a beaker, and then 30g as the mass of La2O3 oflanthanum nitrate, 5g as the mass of MgO of magnesium nitrate, 4g as the mass of Co2O3of cobalt nitrate were added under stirring until completely dissolved. Ammoniumcarbonate (58.5g) was added to deionized water (250mL), and the mixture was stirred untilcompletely dissolved. The metal nitrate mixed solution was added to the ammoniumcarbonate solution while stirring, and a certain amount of ammonia water was added tomaintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0030g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst C-3.XRD analysis was performed on fresh catalyst C3. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst C3 was exposed to an atmosphere containing SO2 for 240mins, wherein theatmosphere containing SO2 had a temperature of 750°C, a pressure of 0.1 MPa, and an SO2content of 0.02 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst C3. In the XRD spectrum of catalyst C3, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example C4Example C1 was repeated except that the used amount of bauxite was reduced, so that thenon-precious metal active component comprised 50wt% of the prepared semi-finishedcatalyst microsphere product, i.e., 20g as the mass of Al2O3 of bauxite and 20g of the activemetal precursor, were used to produce catalyst C4.XRD analysis was performed on fresh catalyst C4. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst C4 was exposed to an atmosphere containing SO2 for 240mins, wherein theatmosphere containing SO2 had a temperature of 750°C, a pressure of 0.1 MPa, and an SO2content of 0.02 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst C4. In the XRD spectrum of catalyst C4, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example C5390mL of deionized water was added to a beaker, and then 34g as the mass of La2O3 oflanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 1g as the mass of Co2O3of cobalt nitrate were added under stirring until completely dissolved. Ammoniumcarbonate (58.5g) was added to deionized water (250mL), and the mixture was stirred untilcompletely dissolved. The metal nitrate mixed solution was added to the ammoniumcarbonate solution while stirring, and a certain amount of ammonia water was added tomaintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an a ctive metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0030g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst C5.Example C6480mL of deionized water was added to a beaker, and then 22g as the mass of La2O3 oflanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 22g as the mass of Co2O3of cobalt nitrate were added under stirring until completely dissolved. Ammoniumcarbonate (72g) was added to deionized water (300mL), and the mixture was stirred untilcompletely dissolved. The metal nitrate mixed solution was added to the ammoniumcarbonate solution while stirring, and a certain amount of ammonia water was added tomaintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0045g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst C6.XRD analysis was performed on fresh catalyst C6. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst C6 was exposed to an atmosphere containing SO2 for 240mins, wherein theatmosphere containing SO2 had a temperature of 750°C, a pressure of 0.1 MPa, and an SO2content of 0.02 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst C6. In the XRD spectrum of catalyst C6, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example C7Example C1 was repeated except that the palladium chloride solution was replaced withthe equal concentration of a ruthenium chloride solution, and the content of precious metalin the prepared catalyst remained unchanged to produce Catalyst C7.Example C8Example C1 was repeated except that as oxide, lanthanum nitrate was replaced with theequal mass of cerium nitrate; and as oxide, cobalt nitrate was replaced with the equal massof ferric nitrate to produce Catalyst C8.Example D1420mL of deionized water was added to a beaker, and then 30g as the mass of La2O3 oflanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 5g as the mass of Co2O3of cobalt nitrate and 3g as the mass of MnO of manganese chloride were added understirring until completely dissolved. Ammonium carbonate63g was added to deionized water(250mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0045g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst D1.XRD analysis was performed on fresh catalyst D1. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst D1 was exposed to an atmosphere containing SO2 for 480mins, wherein theatmosphere containing SO2 had a temperature of 800°C, a pressure of 0.2 MPa, and an SO2content of 0.02 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst D1. In the XRD spectrum of catalyst D1, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example D2250mL of deionized water was added to a beaker, and then 10g as the mass of La2O3 oflanthanum nitrate, 7g as the mass of MgO of magnesium nitrate, 5g as the mass of Co2O3of cobalt nitrate and 3g as the mass of MnO of manganese chloride were added understirring until completely dissolved. Ammonium carbonate (37.5g) was added to deionizedwater (150mL), and the mixture was stirred until completely dissolved. The metal nitratemixed solution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.10g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 20wt% of the prepared semi35finished catalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0030g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the above-mentioned semi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst D-2.Example D3410mL of deionized water was added to a beaker, and then 30g as the mass of La2O3 oflanthanum nitrate, 5g as the mass of MgO of magnesium nitrate, 2.6g as the mass of Co2O3of cobalt nitrate and 3.4g as the mass of MnO of manganese chloride were added understirring until completely dissolved. Ammonium carbonate (61.5g) was added to deionizedwater (250mL), and the mixture was stirred until completely dissolved. The metal nitratemixed solution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0030g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst D-3.Example D4Example D1 was repeated except that the used amount of bauxite was reduced, so that thenon-precious metal active component comprised 50wt% of the prepared semi-finishedcatalyst microsphere product.Specifically: 420mL of deionized water was added to a beaker, and then 30g as the mass ofLa2O3 of lanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 5g as the massof Co2O3 of cobalt nitrate and 3g as the mass of MnO of manganese chloride were addedunder stirring until completely dissolved. Ammonium carbonate63g was added to deionizedwater (250mL), and the mixture was stirred until completely dissolved. The metal nitratemixed solution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.20g as the mass of Al2O3 of bauxite was weighed, and 240mL of water and 3g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 50wt% of the prepared semi10finished catalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0060g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst D4.XRD analysis was performed on fresh catalyst D4. In the XRD spectrum, there werecharacteristic peaks at 2θ=about 33.0°, about 33.5° and about 47.5° as well as at 2θ=about27.0°, about 28.0° and about 39.5°.Catalyst D4 was exposed to an atmosphere containing SO2 for 480mins, wherein theatmosphere containing SO2 had a temperature of 800°C, a pressure of 0.2 MPa, and an SO2content of 0.02 vol%. After exposure to SO2 treatment, XRD analysis was performed oncatalyst D4. In the XRD spectrum of catalyst D4, there were characteristic peaks at2θ=about 28.6°, about 30.0° and about 50.4°.Example D5420mL of deionized water was added to a beaker, and then 34g as the mass of La2O3 oflanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 1g as the mass of Co2O3of cobalt nitrate and 3g as the mass of MnO of manganese chloride were added understirring until completely dissolved. Ammonium carbonate63g was added to deionized water(250mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid a t a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0030g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst D5.Example D6510mL of deionized water was added to a beaker, and then 22g as the mass of La2O3 oflanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 22g as the mass of Co2O3of cobalt nitrate and 3g as the mass of MnO of manganese chloride were added understirring until completely dissolved. Ammonium carbonate (76.5g) was added to deionizedwater (300mL), and the mixture was stirred until completely dissolved. The metal nitratemixed solution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0045g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst D6.Example D7420mL of deionized water was added to a beaker, and then 30g as the mass of La2O3 oflanthanum nitrate, 4g as the mass of MgO of magnesium nitrate, 5g as the mass of Co2O3of cobalt nitrate and 3g as the mass of MnO of manganese chloride were added understirring until completely dissolved. Ammonium carbonate63g was added to deionized water(250mL), and the mixture was stirred until completely di ssolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Ru was dissolved in a diluted hydrochloric acid at 1:1, and the resultingmixture was diluted with deionized water to produce a ruthenium chloride solution havinga concentration of 5.6g / L. 15g of the semi-finished catalyst microsphere product was taken,and a certain amount (the Ru equivalent mass of 0.0045g) of the ruthenium chloridesolution having a concentration of 5.6g / L was taken. The Ru-containing solution asimpregnation solution was impregnated to the above-mentioned semi-finished catalystproduct to produce a solid product, then the solid product was dried at 120°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce catalyst D7.Example D8420mL of deionized water was added to a beaker, and then 30g as the mass of CeO2 ofcerium nitrate, 4g as the mass of MgO of magnesium nitrate, 5g as the mass of Fe2O3 offerric nitrate and 3g as the mass of MnO of manganese chloride were added under stirringuntil completely dissolved. Ammonium carbonate63g was added to deionized water(250mL), and the mixture was stirred until completely dissolved. The metal nitrate mixedsolution was added to the ammonium carbonate solution while stirring, and a certainamount of ammonia water was added to maintain the pH value of the solution at 9.The completely precipitated mixture was suction-filtered and rinsed with deionized water.The filter cake mixture obtained by suction filtering was dried at 120°C, calcined at 700°Cin an air atmosphere for 6 hours, and then ground to obtain an active metal precursor.40g as the mass of Al2O3 of bauxite was weighed, and 380mL of water and 6g ofconcentrated hydrochloric acid (36 wt%) were added. The resulting mixture was slurrified.20g of the active metal precursor was weighed and added to the acidified inorganic oxidematrix and the resulting mixture was stirred. The slurry was dried at 200°C, then calcinedin an air atmosphere at 700°C for 4 hours to produce a semi-finished catalyst microsphereproduct. The non-precious metal active component comprised 33wt% of the prepared semifinishedcatalyst microsphere product.A precursor of Pd was dissolved in a diluted hydrochloric acid at a mass ratio of 1:1, andthe resulting mixture was diluted with deionized water to produce a palladium chloridesolution having a concentration of 5.6g / L and pH=2. 15g of the semi-finished catalystmicrosphere product was taken, and a certain amount (the Pd equivalent mass of 0.0045g)of the palladium chloride solution having a concentration of 5.6g / L was taken. Thepalladium chloride solution as impregnation solution was impregnated to the abovementionedsemi-finished catalyst microsphere product to produce a solid product, then thesolid product was dried at 120°C, then calcined in an air atmosphere at 700°C for 4 hoursto produce catalyst D8.Performance TestingDetermination of the contents of components: the contents of components in catalystsprepared in Examples were determined using the X-ray fluorescence spectroscopy (XRF).For details, see Petrochemical Analysis Methods (RIPP Experimental Methods), edited byYang Cuiding et al., published by Science Press in 1990. The specific results are shown inTable 3 below.Table 3: Compositions of catalysts (weight percentage, %)Activity evaluation: in the present invention, the evaluation standard of the catalyst activitywas the concentration changes of SOx and NOx in the reaction product. The SOx and NOxcontents in the product were measured using an FT-IR Fourier transform infrared flue gasanalyzer. A fixed-bed micro-reactor was used as the experimental device for the evaluation.The evaluation results for the catalyst activity were expressed as conversion rate.Calculation method for the conversion rate:X=[Cinlet-Coutlet] / Cinletx100%wherein, Cinlet refers to the concentration of SOx or NOx at the inlet of the experimentaldevice; Coutlet refers to the concentration of SOx or NOx at the outlet of the experimentaldevice.The catalysts provided in the above examples and comparative examples were evaluatedfor their effects in simultaneously reducing the emissions of both NO and SO2 in flue gas.The catalytic cracking reaction-regeneration evaluation was carried out on a small fixedbedsimulated flue gas device. The catalyst was loaded in an amount of 1.5g, and placed ina quartz tube fixed-bed reactor with an inner diameter of 16.8mm. the catalyst bed wasfilled with quartz fiber and quartz sand (20-40 mesh) at both ends so that the catalyst bedwas fixed in the constant temperature section in the middle of the reactor. The reactiontemperature was 680°C, and the reaction pressure was 0.03MPa. The feedstock gas had avolume flow rate (STP, standard temperature and pressure) of 1500 mL / min, and avolumetric hourly space velocity of about 15000 h-1. After the reactor temperaturestabilized, the catalyst was first pre-treated in an N2 atmosphere for 30min to fully removeadsorbed species on the catalyst surface. At the beginning of the reaction, the feedstock gascontained 1200 ppm vol% of NO, 1200 ppm vol% of SO2, and the balance of N2. The gasproducts were analyzed by an online infrared to obtain the concentrations of SO2 and NOafter the reaction. The results with the evaluation time of 0.5h are listed in Table 4. Theresults with the evaluation time of 1.5h are listed in Table 5. In Tables 4 and 5, Alone-NOand Alone-SO2 referred to that the feedstock gas only contained 1200 ppm vol% of NO or1200 ppm vol% of SO2 respectively.Table 4: Performance comparison of different catalysts within 0.5hTable 5: Performance comparison of different catalysts within 1.5hThe preferred embodiments of the present invention have been described in detail above,but the present invention is not limited thereto. Within the scope of the technical conceptof the present invention, a variety of simple modifications can be made to technicalsolutions of the present invention, including combinations of various technical features inany other suitable manner. These simple modifications and combinations should also beregarded as the disclosed content of the present invention. All belong to the protectionscope of the present invention.

Claims

1. A catalyst capable of / for simultaneously reducing both SOx and NOx in flue gas, which is characterized in that the catalyst comprises the following components: (1) a support or inorganic oxide matrix, (2) a rare earth metal, (3) a non-precious metal selected from Group VIII, or non-precious metal(s) selected from Groups VB, VIII, IB, and IIB, (4) a precious metal, (5) optionally, a Group VIIB non-precious metal, (6) optionally, a Group IIA metal, wherein, based on the total weight of the catalyst, the content of the support or inorganic oxide matrix of component (1) as oxide is 25-95 wt%, e.g., 25-93 wt%, or 25-92 wt%, or 40-90 wt%, or 40-87 wt%, or 40-85 wt%, or 45- 80 wt%, or 50-88 wt%, or 50-80 wt%; the content of the rare earth metal(s) of component (2) as oxide is 2-70 wt%, e.g., 4-60 wt%, or 4-50 wt%, or 4-40 wt%, or 6-70 wt%, or 8-50 wt%, or 8-40 wt%, or 12-60 wt%, or 12-48 wt%; the content of the non-precious metal selected from Group VIII or said non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 1-30 wt%, e.g., 1-15 wt%, or 1-12 wt%, or 2-30 wt%, or 2-12 wt%, or 2-10 wt%, or 2-8 wt%, or 3-20 wt%, or 3-15 wt%; the content of the precious metal of component (4) as element is 0.01-2 wt%, e.g., 0.01-1.5 wt%, or 0.01-2 wt%, or 0.02-1.5 wt%, or 0.02-1.2 wt%, or 0.02-1.0 wt%; or 0.03-1.2 wt%; the content of the Group VIIB non-precious metal of component (5) as oxide is: 0 or 1-10 wt%, 0 or 1-8 wt%, 0 or 2-5 wt%; the content of the Group IIA metal of component (6) as oxide is 0 or 1-30 wt%, 0 or 1-20 wt%, 0 or 2-15 wt%; wherein, as metal element, the molar ratio of component (2) to component (3) is (0.4-18):1, for example (0.4-12):1, or (0.5-15):1, or (0.5-12):1, or (0.5-8):1, or (0.6-18):1, or (1-10):1, or (1-6):1, or (1-4):1, or (2-12):1, or (2-5):1, or (3-6):1; preferably, the sum of the content of the Group VIIB non-precious metal of component (5) as oxide and the content of the Group IIA metal of component (6) as oxide is not zero.

2. The catalyst according to claim 1, wherein, the support or inorganic oxide matrix of component (1) is at least one of alumina, silicaalumina, zeolite, spinel, kaolin, diatomaceous earth, perlite, and perovskite, preferably alumina; and / or the rare earth metal of component (2) is one or more of La, Ce, Pr and Nd, more preferably La and / or Ce; most preferably La; and / or the non-precious metal selected from Group VIII of component (3) is Co and / or Fe, more preferably Co; or said non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) is one or more of Fe, Co, Ni, Cu, Zn, and V, more preferably Co and / or Fe, most preferably Co; and / or the precious metal of component (4) is one or more of Ru, Rh, Re, Pt, Pd, Ag, Ir, and Au, more preferably one or more of Pt, Pd and Rh, most preferably Pd; and / or the Group VIIB non-precious metal of component (5) is Mn; and / or the Group IIA metal of component (6) is one or more of Be, Mg, Ca, Sr and Ba, more preferably Mg.

3. The catalyst according to any one of the preceding claims, wherein the catalyst comprises (1) a support and, loaded on the support, (2) a rare earth metal, (3) a non-precious metal selected from Group VIII, and (4) a precious metal; wherein, based on the total weight of the catalyst, the content of the support of component (1) is 25-95 wt%; the content of the rare earth metal(s) of component (2) as oxide is 4-60 wt%; the content of the non-precious metal selected from Group VIII of component (3) as oxide is 2-12 wt%; the content of the precious metal of component (4) as element is 0.01-2 wt%; or the content of the support of component (1) is 40-90 wt%; the content of the rare earth metal(s) of component (2) as oxide is 8-50 wt%; the content of the non-precious metal selected from Group VIII of component (3) as oxide is 2-12 wt%; the content of the precious metal of component (4) as element is 0.02-1.5 wt%; or the content of the support or inorganic oxide matrix of component (1) as oxide is 50-88 wt%; the content of the rare earth metal(s) of component (2) as oxide is 8-40 wt%; the content of the non-precious metal selected from Group VIII of component (3) as oxide is 2-10 wt%; the content of the precious metal of component (4) as element is 0.03-1.2 wt%; wherein, as metal element, the molar ratio of component (2) to component (3) is (0.5-15):1, or (1-10):1, or (2-5):1.

4. The catalyst according to any one of the preceding claims, wherein the catalyst comprises (1) a support and, loaded on the support, (2) a rare earth metal, (3) non-precious metal(s) selected from Groups VB, VIII, IB, and IIB, (4) a precious metal, and (6) a Group IIA metal, wherein, based on the total weight of the catalyst, the content of the support or inorganic oxide matrix of component (1) as oxide is 25-93 wt%; the content of the rare earth metal(s) of component (2) as oxide is 4-60 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 2-30 wt%; the content of the precious metal of component (4) as element is 0.01-2 wt%; the content of the Group IIA metal of component (6) as oxide is 1-30 wt%; or the content of the support or inorganic oxide matrix of component (1) as oxide is 40-87 wt%; the content of the rare earth metal(s) of component (2) as oxide is 8-50 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 3-20 wt%; the content of the precious metal of component (4) as element is 0.02-1.5 wt%; the content of the Group IIA metal of component (6) as oxide is 1-20 wt%; or the content of the support or inorganic oxide matrix of component (1) as oxide is 40-85 wt%; the content of the rare earth metal(s) of component (2) as oxide is 8-40 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 3-15 wt%; the content of the precious metal of component (4) as element is 0.03-1.2 wt%; the content of the Group IIA metal of component (6) as oxide is 2-15 wt%; wherein, as metal element, the molar ratio of component (2) to component (3) is (0.4-18):1, for example (0.4-12):1, or (0.5-8):1, or (1-4):1.

5. The catalyst according to any one of the preceding claims, wherein the catalyst comprises the following components: (1) a support or inorganic oxide matrix, (2) a rare earth metal, (3) non-precious metal(s) selected from Groups VB, VIII, IB, and IIB, (4) a precious metal, and (5) a Group VIIB non-precious metal, wherein, based on the total weight of the catalyst, the content of the support or inorganic oxide matrix of component (1) as oxide is 25-92 wt%; the content of the rare earth metal(s) of component (2) as oxide is 6-70 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 1-12 wt%; the content of the precious metal of component (4) as element is 0.01-1.5 wt%; the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-10 wt%; or the content of the support or inorganic oxide matrix of component (1) as oxide is 40-85 wt%; the content of the rare earth metal(s) of component (2) as oxide is 12-60 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 2-10 wt%; the content of the precious metal of component (4) as element is 0.02-1.2 wt%; the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-8 wt%; or the content of the support or inorganic oxide matrix of component (1) as oxide is 40-85 wt%; the content of the rare earth metal(s) of component (2) as oxide is 12-48 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 2-8 wt%; the content of the precious metal of component (4) as element is 0.02-1.0 wt%; the content of the Group VIIB non-precious metal of component (5) as oxide is: 2-5 wt%; wherein, as metal element, the molar ratio of component (2) to component (3) is (0.6-18):1, e.g. (2-12):1, or (3-6):1.

6. The catalyst according to any one of the preceding claims, wherein the catalyst comprises the following components: (1) a support or inorganic oxide matrix, (2) a rare earth metal, (3) non-precious metal(s) selected from Groups VB, VIII, IB, and IIB, (4) a precious metal, (5) a Group VIIB nonprecious metal, and (6) a Group IIA metal, wherein, based on the total weight of the catalyst, the content of the support or inorganic oxide matrix of component (1) as oxide is 25-95 wt%; the content of the rare earth metal(s) of component (2) as oxide is 2-70 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 1-15 wt%; the content of the precious metal of component (4) as element is 0.01-1.5 wt%; the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-10 wt%; the content of the Group IIA metal of component (6) as oxide is 1-30 wt%; or the content of the support or inorganic oxide matrix of component (1) as oxide is 40-90 wt%; the content of the rare earth metal(s) of component (2) as oxide is 4-50 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 2-12 wt%; the content of the precious metal of component (4) as element is 0.02-1.2 wt%; the content of the Group VIIB non-precious metal of component (5) as oxide is: 1-8 wt%; the content of the Group IIA metal of component (6) as oxide is 1-20 wt%; or the content of the support or inorganic oxide matrix of component (1) as oxide is 50-80 wt%; the content of the rare earth metal(s) of component (2) as oxide is 4-40 wt%; the content of the non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) as oxide is 2-10 wt%; the content of the precious metal of component (4) as element is 0.02-1.0 wt%; the content of the Group VIIB non-precious metal of component (5) as oxide is: 2-5 wt%; the content of the Group IIA metal of component (6) as oxide is 2-15 wt%; wherein, as metal element, the molar ratio of component (2) to component (3) is (0.4-18):1, for example (0.5-12):1, or (1-6):1.

7. The catalyst according to any one of the preceding claims, wherein the catalyst is a catalyst that has been exposed to an atmosphere containing SO2.

8. The catalyst according to any one of the preceding claims, wherein the rare earth metal(s) of component (2) comprises La; the non-precious metal selected from Group VIII or said non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) comprises Co; the precious metal of component (4) comprises Pd; the Group VIIB non-precious metal of component (5), if any, comprises Mn; the Group IIA metal of component (6), if any, comprises Mg.

9. The catalyst according to any one of the preceding claims, wherein the rare earth metal(s) of component (2) is La; the non-precious metal selected from Group VIII or said non-precious metal(s) selected from Groups VB, VIII, IB, and IIB of component (3) is Co; the precious metal of component (4) is Pd; the Group VIIB non-precious metal of component (5), if any, is Mn; the Group IIA metal of component (6), if any, is Mg.

10. The catalyst according to any of the preceding claims 7-9, wherein the catalyst is a catalyst that has been exposed to an atmosphere containing SO2, the catalyst has characteristic peaks at 2θ=28.6°±0.1°, 30.0°±0.1° and 50.4°±0.1° in the powder XRD spectrum.

11. The catalyst according to any of the preceding claims 8-9, wherein the catalyst has characteristic peaks at 2θ=33.0°±0.1°, 33.5°±0.1°, and 47.5°±0.1°, as well as 27.0°±0.1°, 28.0°±0.1°, and 39.5°±0.1° in the powder XRD spectrum.

12. A method for preparing a catalyst of any one of the preceding claims, which method comprises: (I) a co-precipitation method or a sol-gel method is used to produce an active metal precursor, wherein the active metal in the active metal precursor comprises (2) a rare earth metal, (3) a non-precious metal selected from Group VIII, or non-precious metal(s) selected from Groups VB, VIII, IB, and IIB, (5) optionally, a Group VIIB non-precious metal, and (6) optionally, a Group IIA metal; and (II) the active metal precursor and (1) the support or inorganic oxide matrix or a precursor thereof, and optionally a precursor of (4) the precious metal are mixed and slurrified to produce a slurry, the resulting slurry is dried and / or calcined to produce a catalyst; or the active metal precursor and (1) the support or inorganic oxide matrix or a precursor thereof, and optionally a precursor of (4) the precious metal are mixed and slurrified to produce a slurry, the resulting slurry is dried and / or calcined to produce a semi35 finished catalyst product; then the semi-finished catalyst product is impregnated with a solution containing a precursor of (4) the precious metal as impregnation solution to produce a solid product, and then the solid product is dried and / or calcined to produce a catalyst; wherein the active metal precursor, the support or inorganic oxide matrix or the precursor thereof, and the precursor of the precious metal are used in such amounts that the produced catalyst has the composition of the catalyst of any of the preceding claims.

13. The preparation method according to any of the preceding claims, wherein in step (I), the co-precipitation method is used to produce the active metal precursor; preferably, the co-precipitation method comprises: (I-1) providing a first solution containing a precursor of (2) rare earth metal(s), a precursor of (3) non-precious metal selected from Group VIII or non-precious metal(s) selected from Groups VB, VIII, IB, and IIB, optionally a precursor of (5) Group VIIB non-precious metal, and optionally a precursor of (6) Group IIA metal; preferably, each precursor is independently selected from nitrate and / or chloride of each metal; (I-2) subjecting the first solution and a coprecipitant to carry out a coprecipitation reaction; preferably, the coprecipitant is a carbonate salt, further preferably at least one of ammonium carbonate, potassium carbonate and sodium carbonate; preferably, the coprecipitation reaction is carried out at pH=8-10; (I-3) drying and / or calcining a soild product obtained in the coprecipitation reaction to produce an active metal precursor; preferably, the condition for calcining in step (I-3) includes: the temperature is 300-800°C, e.g., 300-700°C, the time is 0.5-8h, e.g., 1-8h or 1-5h, wherein, the support or inorganic oxide matrix or a precursor thereof, the precursor of rare earth metal(s), the precursor of non-precious metal selected from Group VIII or non20 precious metal(s) selected from Groups VB, VIII, IB, and IIB, the precursor of precious metal, optionally the precursor of Group VIIB non-precious metal, and optionally the precursor of Group IIA metal are used in such amounts that the produced catalyst has the composition of the catalyst of any of the preceding claims.

14. The preparation method according to any one of the preceding claims, wherein in step (II), the precursor of the precious metal component is at least one of nitrates, chlorides, and / or chlorates, e.g. at least one of palladium nitrate, palladium chloride, platinum chlorate and rhodium chloride, preferably palladium nitrate and / or palladium chloride; and / or in step (II), the slurry has a solid content of 5-40 wt%, e.g., 6-38 wt%, or 7-35 wt%; and / or in step (II), the condition for calcining the slurry includes: the temperature is 300-800°C, e.g., 300-700°C, the time is 0.5-8h, e.g., 1-8h or 1-5h; and / or in step (II), the precursor of precious metal is hydrolyzed in an acid solution to provide the impregnation solution; preferably, the acid is selected from water-soluble inorganic acids and / or organic acids, more preferably, at least one of hydrochloric acid, nitric acid, phosphoric acid, and acetic acid; preferably, the acid is used in such an amount that the pH value of the impregnation solution is less than 6.0, preferably less than 5.0, e.g. 2.0-5.0; preferably, the condition for calcining the solid product includes: the temperature is 300- 800°C, e.g., 300-700°C, the time is 0.5-8h, e.g., 1-8h or 1-5h.

15. A method for simultaneously reducing both SOx and NOx from flue gas, which comprises, under a condition for removing SOx and NOx, contacting the flue gas with a catalyst according to any one of the preceding claims or a catalyst prepared by a preparation method according to any one of the preceding claims; preferably, the condition for removing SOx and NOx includes: the temperature is 300- 1000°C, e.g. 500-800°C, or 600-750°C, or 625-750°C, or 650-750°C, or 675-750°C, or 700-750°C, or 725-750°C, or 600-725°C, or 625-725°C, or 650-725°C, or 675-725°C, or 700-725°C, or 600-700°C, or 625-700°C, or 650-700°C, or 675-700°C, or 600-675°C, or 625-675°C, or 650-675°C, or 600-650°C, or 625-650°C, or 600-625°C; the pressure is 0-4 MPa, e.g. 0.01-4 MPa, or 0.02-4 MPa, or 0-0.5 MPa; the volumetric hourly space velocity of flue gas is 100-50000 h-1 or 200-20000h-1; and / or preferably, in the flue gas, the SOx content is 0.001-0.5 vol%, the NOx content is 0.001- 0.3 vol%; or the volume fractions of SOx and NOx in the flue gas are respectively 1-3000 μL / L, and the molar ratio of SOx to NOx is 0.5:1-2:1; and / or preferably, the flue gas is a flue gas containing a certain concentration of SOx and NOx at the same time, e.g. catalytic cracking regeneration flue gas; preferably, contacting the catalytic cracking regeneration flue gas with the catalyst is carried out in a flue gas passway provided after a catalytic cracking cyclone separator and / or after a CO incinerator.