Synergistic approach to develop resilient cement systems for long term wellbore integrity of oil, gas and geothermal wells
By adding slip ring and additional polymers to cement mortar, the cement shields in oil and gas wells gain improved elasticity and reduced Young's modulus, addressing stress-induced cracking and maintaining well integrity.
Patent Information
- Application Number
- SA1020253044
- Authority / Receiving Office
- SA · SA
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2025-04-30
- Publication Date
- 2026-10-05
AI Technical Summary
Cement shields in oil and gas wells fail due to stress from pressure and temperature changes, leading to cracking and loss of mechanical integrity, which can compromise well safety and production.
Incorporating a slip ring polymer and an additional polymer into cement mortar formulations to enhance elasticity and reduce Young's modulus, allowing the cement to withstand higher stresses without cracking.
The enhanced cement formulations exhibit increased elasticity and lower Young's modulus, enabling them to withstand greater axial deformation and maintain integrity under wellbore conditions, thus ensuring long-term zone isolation and safety.
Smart Images

Figure 12D77801-25E9-4E78-9240-DACEE15AE7FE 
Figure 173B6159-84F1-4635-BC4B-B68F5A10C458 
Figure 239577CE-05E6-4053-A7F4-3ABAED35EF84
Abstract
Description
Cementing an oil and gas well is a critical process during oil well drilling and completion. The primary function of the initial cementing is to support the casing and provide effective zone insulation for the well's lifetime. To achieve this, the entire wellbore ring should be filled with an effective cementitious component / sealant that meets both short-term and long-term well requirements. The two main phases in the life of an oil, gas, or geothermal well are (1) well construction and (2) operation. During the well construction phase, the continuously varying stresses around the wellbore (exploration well) caused by the oscillation of the fluid within the wellbore affect the residual stresses in the cemented casing. During the well operation phase, inactivity, depletion, and human intervention (pressure testing, drilling, fracturing, production, or injection) can cause stresses on the sealant. The cement shield must protect the well behind the casing and provide long-term zone isolation to ensure safety and prevent environmental problems. The cement in the ring between the casing and the formations (or between the casings) is subject to stress in wellbore conditions, particularly with changes in pressure and temperature or their circulation with the movement of fluids and equipment. As such, cracking can occur due to compression, traction, or micro-ring formation. Physical degradation of the cement over time can lead to deterioration of both its mechanical structure and its chemical adhesion to the casing, tubing, or wellbore wall. This degradation can negatively impact production, increase costs, and reduce the profit margin for safe well operation. Cement shield failure is often caused by stresses arising from the pressure or temperature inherent in well operations. In such cases, axial deformation of the cement shield may occur, during which the shield can be compressed, causing its length to change along the axial plane due to stresses arising from the pressure or temperature inherent in well operations. In particular, cracking can occur at early axial deformation due to the tensile stress of cement with a high Young's modulus (e.g., the cement system shown in Figure 1a). This indicates low elasticity and toughness under thermal and / or mechanical stressful conditions downhole compared to a cement system with a lower Young's modulus, as shown in Figure 1b. Low elasticity and toughness indicate a failure in cement integrity (e.g., cracking), which can create a pathway for formation fluids to enter the annulus, potentially stressing the well and rendering it unsafe to operate. This failure can also cause premature water production, which can limit the economic life of the well.Therefore, if the cemented shield fails during its active service life, the goal of hydrocarbon production may not be achieved safely and economically. The cemented shield must have optimal properties to withstand the stresses caused by well operations. It is generally understood, based on well history data and experimental studies such as finite elemental analysis (FEA), that the long-term mechanical integrity of a cemented shield in a wellbore depends on the mechanical properties of the cemented shield, such as Young's modulus, tensile strength, and elasticity. Specifically, the long-term mechanical properties of a cohesive (firmly constructed) cemented system should include a Young's modulus of 1.5 × 10⁶ psi or less and a high elasticity. High elasticity of the cemented shield may indicate the magnitude of deformation the cement can withstand at an increasing stress level before failing. Thus, the higher the elasticity of the cemented shield, the longer its lifespan. For example, a highly elastic cemented shield will remain intact in the wellbore for a longer period than a low-elasticity cemented shield when subjected to numerous high-stress cycles.The Young's modulus of a high-elasticity cementitious shield whose formulation is based on one or more embodiments may be at least 25% lower than the Young's modulus of a cementitious shield prepared from pure cement. The present invention relates to formulations and methods for producing a cementitious shield with enhanced stress resistance over time. Specifically, a slip ring polymer and an additional polymer are mixed into cementitious mortar and distributed throughout the cement mold during the cement hardening process. The hardened cement obtained from this mortar exhibits higher elasticity compared to cement containing only one of the two polymers, or cement without either the slip ring polymer or the additional polymer. Cement mortar composition In one aspect, embodied cementitious mortar formulations include an aqueous fluid, a cementitious raw material, a slip ring polymer, and an additional polymer. Embodied cementitious mortars may also include one or more silica powders, a cement retarder (hardening agent), a dispersant, and a fluid loss control agent. Embodimental mortars contain a cementitious raw material. The cementitious raw material may be any suitable material that can harden and become cement when mixed with water. The cementitious raw material may be hydraulic or non-hydraulic. A hydraulic or non-hydraulic cementitious raw material may be chosen based on the desired application of the cementitious mortar to which the present invention relates. In some embodiments, the cementitious mortar contains a hydraulic cementitious raw material. Hydraulic cementitious raw materials are materials that refer to a mixture of limestone, clay (slaw), and gypsum burned together under extreme temperatures such that the mixture begins to mature (set and harden) immediately or within a few minutes upon contact with water. In some specific formulations, the cementitious precursor may be a Portland cement precursor, such as Class A, Class B, Class C, Class G, or Class H Portland cement. The Portland cement precursor is a hydraulic cement precursor (a cementitious precursor that not only hardens upon reaction with water but also forms a water-resistant product) produced by grinding un-powdered cement containing hydraulic calcium silicates and one or more forms of calcium sulfate as a semi-powdered additive. In other formulations, the cementitious precursor may be a Saudi cementitious precursor, which is a mixture of Portland cement precursor and crystalline silica. Crystalline silica is also known as quartz. In some variations of cementitious raw material composition, a non-hydraulic cementitious raw material is used. A non-hydraulic cementitious raw material refers to a mixture of lime, gypsum, plaster, and oxychloride. While non-hydraulic cementitious raw materials may take longer to harden or require specific drying conditions for proper setting, they are often more economical. In some other embodiments of the cementitious raw material composition, the cementitious raw material may include additional materials. Cementitious raw materials may include, but are not limited to, calcium hydroxide, silicates, oxides, belite (Ca2SiO5), alite (Ca3SiO4), tricalcium aluminate (Ca3Al2O6), tetracalcium aluminoferrite (Ca4Al2Fe2O10), brown milleriate (4CaOAl2O3·Fe2O3), gypsum (CaO4·2H2O), sodium oxide, potassium oxide, limestone, lime (calcium oxide), hexavalent chromium, calcium aluminate, silica sand, silica flour, hematite, manganese tetroxide. And unions of them.Cementitious raw materials may include, but are not limited to, fly ash, calcined fly ash, slag cement, silica fume (fumigated silica), quartz, any other known cementitious raw material, or combinations of any of these materials. In some formulations, cement mortar includes silica flour. Silica flour is finely ground crystalline silica with the molecular formula silicon dioxide (SiO2) and a particle size ranging from about 1 to about 500 microns, for example, 10 to 500 microns, 10 to 100 microns, 10 to 80 microns, 10 to 50 microns, 10 to 20 microns, 20 to 100 microns, 20 to 80 microns, 20 to 50 microns, 50 to 100 microns, 50 to 80 microns, and 80 to 100 microns. When used, silica powder is present in cement mortar in an amount ranging from about 25% to about 75% of the weight of the cement raw material.Concrete cementitious mortars may include a quantity of setting retarder(s) with a minimum value of any of the values 25, 30, 35, 40, 50, and 55% of the weight of the cementitious raw material and a maximum value of any of the values 50, 60, 65, 70, and 75% of the weight of the cementitious raw material, where any of the lower limits may be used in conjunction with any of the mathematically compatible higher limits. Cementitious mortars, in one or more of their forms, contain an aqueous fluid. The aqueous fluid includes water. This water can be distilled water, deionized water, tap water, fresh water from surface or groundwater sources, production water, formation water, natural and artificial brine solutions, brackish water, natural and artificial seawater, black water (wastewater), brown water, grey water, blue water, potable water, non-potable water, and other types of water, or combinations thereof, suitable for use in a well-hole environment. In one or more of their forms, the water used may naturally contain contaminants such as salts, ions, minerals, organic matter, or combinations thereof, provided that these contaminants do not interfere with the hardening of the cementitious mortar or the mechanical properties of the cementitious mortar. Embodimental mortars may contain sufficient water to harden the previously described cementitious raw material. In some embodiments, the mortar may contain water in quantities ranging from approximately 30% to 320% of the cementitious raw material by weight. Embodimental cementitious mortars, or both, may contain water in quantities with a minimum value of 30%, 35%, 40%, 45%, 50%, 75%, 100%, and 200% of the cementitious raw material by weight and a maximum value of 75%, 200%, 225%, 250%, 275%, 300%, and 320% of the cementitious raw material by weight, where any lower limit may be used in conjunction with any mathematically compatible upper limit. The embodied mortars contain a slip ring polymer. The slip ring polymer may be a polyrotaxane polymer. Slip ring polymers may be of one or more embodiments as described in US Patent Application No. 2020 / 0325070, the contents of which are incorporated in their entirety herein for reference. In some embodiments, the slip ring polymer is Rotamach, which can be obtained from Saudi Arabian Oil Company (Aramco). Embodimental cementitious mortars may contain a slip ring polymer in an amount that has a minimum value of any of the values 0.025, 0.05, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5 or 3.0% by weight of the cementitious raw material and a maximum value of any of the values 5.5, 5.0, 4.5, 4.0 or 3.5 by weight% of the cementitious raw material, where any of the lower limits may be used in conjunction with any of the mathematically compatible higher limits. Embossed mortars contain an additional polymer. This additional polymer may be a thermoplastic polymer. It may also be a styrene-butadiene copolymer. In some embodiments, the styrene-butadiene copolymer contains at least 65% styrene units and less than 35% butadiene units. For example, a styrene-butadiene copolymer may contain 70% styrene units and 30% butadiene units. In certain embodiments, the additional polymer may be Calprene® 411 (e.g., Calprene® C411 M), which can be obtained from Dynasol. In some embodiments, the cement mortar may contain approximately 0.05% to approximately 35.0% by weight of the additional polymer as a percentage of the cementitious raw material. The additional embodied polymers may be present in quantities with a minimum of 0.05, 0.10, 0.25, 0.5, 1.0, 2.0, 2.5, 3.0, 5.0, 7.5, 10, 15, 20 or 25.0 by weight% of the cementitious raw material and a maximum of 35.0, 30.0, 25.0, 20, 15, 12.5, 10, or 7.5 by weight % of the cementitious raw material, where any lower limit may be used in conjunction with any mathematically compatible higher limit. Cement mortar may, in one or more formulations, contain one or more setting retarders or setting-retarding agents. Setting retarders may include, but are not limited to, lignosulfonates, organic acids, phosphonic acid derivatives, synthetic polymers (such as copolymers of 2-acrylamido-2-methylpropane sulfonic acid (“AMPS”), and unsaturated carboxylic acids, including, but not limited to, acrylic acid (AA)), inorganic borate salts, and combinations thereof. In some formulations, the cement setting retarder includes one or more selected compounds from the group consisting of sodium lignosulfonate, calcium lignosulfonate, a copolymer of acrylic acid and 2-acrylamido-2-methylpropanesulfonic acid, and combinations thereof.Setting retarders may include the commercially available PCR-3 retarder from Economy Polymers & Chemicals. When used, these retarders may be present in the cement mortar, the hardened cement mix, or both, in amounts ranging from approximately 0.009% to approximately 10.2% by weight of the cementitious raw material. Concrete cementitious mortars may include a setting retarder(s) in a quantity that has a minimum limit of any of the values 0.009, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5, 3.0, or 5.0% of the weight of the cementitious raw material and a maximum limit of any of the values 5.0, 5.5, 6.0, 7.0, 7.5, 8.0, 9.0, 9.5, 9.9, 10.0, or 10.2% of the weight of the cementitious raw material, where any of the lower limits may be used in conjunction with any of the mathematically compatible higher limits. In one or more formulations, cement mortar contains one or more dispersing agents. The dispersing agent(s) may control the flowability / rheology of the cement mortar. Dispersing agents may include, but are not limited to, lignosulfonates and polyacrylic acid polymer (PAA). The dispersing agent(s) may include the commercially available SC-9 dispersant from Economy Polymers & Chemicals. When used, dispersing agents may be present in cement mortars in amounts ranging from approximately 0.009% to approximately 5.2% by weight of the cementitious raw material. Concrete cementitious mortars may include dispersant(s) in a quantity that has a minimum limit of any of the values 0.009, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5, or 3.0% of the weight of the cementitious raw material and a maximum limit of any of the values 3.0, 3.5, 4.0, 4.5, 5.0, or 5.2% of the weight of the cementitious raw material, where any of the lower limits may be used in conjunction with any of the mathematically compatible higher limits. Cementitious mortar may contain one or more fluid loss control agents in one or more formulations. These agents may include, but are not limited to, hydroxyethylcellulose, a tertiary polymer of 2-acrylamido-2-methylpropanesulfonic acid, acrylic acid, and N,N-dimethylacetamide (NNDMA). In some formulations, the fluid loss control agent(s) may include one or more selected compounds from the group consisting of hydroxyethylcellulose, a tertiary polymer of 2-acrylamido-2-methylpropanesulfonic acid, acrylic acid, and N,N-dimethylacetamide, or combinations thereof. The fluid loss control agent(s) may include the commercially available Polytrol® FL-24 from BASF. When in use, the fluid loss control agent(s) in cement mortar may be present in amounts ranging from approximately 0.009% to approximately 5.2% of the weight of the cementitious raw material.Concrete cementitious mortars may include a fluid loss control factor(s) with a minimum value of any of the values 0.009, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5, or 3.0% of the cementitious raw material weight and a maximum value of any of the values 3.0, 3.5, 4.0, 4.5, 5.0, or 5.2% of the cementitious raw material weight, where any of the lower limits may be used in conjunction with any of the mathematically compatible higher limits. hardened cement composition In one respect, embodied cement formulations refer to a cementitious cement containing a slip ring polymer and an additional polymer distributed throughout the cementitious cement. Embodied cementitious cement is manufactured by hardening the cementitious mortars described previously. Cementitious formulations in one or more embodiments may be capable of axial deformation without cracking when compressive stress is applied. Conversely, cementitious cement prepared in the absence of the slip ring polymer, the additional polymer, or both, has a tendency to crack under compressive stress, setting stresses, setting temperatures, or a combination of these factors. A cement formulation hardened in one or more formulations may have an increased ability to withstand deformation stresses compared to cement hardened without the slip ring polymer, the additional polymer, or both. In some formulations, a cement formulation hardened in one or more formulations may undergo greater axial deformation under stress without cracking compared to cement hardened without the slip ring polymer, the additional polymer, or both. For example, a cement formulation hardened according to one or more formulations may be able to withstand axial stress of 10% or more, 12.5% or more, 15% or more, 20% or more, or 25% or more compared to cement hardened without the slip ring polymer, the additional polymer, or both. Hardened cement that has the composition according to one or more of the embodiments may be able to withstand a greater axial stress than hardened cement prepared in the absence of the slip ring polymer, or the additional polymer, or both, where this amount falls within a range that has a minimum of any of the values 10%, 12.5%, 15%, 25%, 30%, 35%, and 40%, and a higher limit which is any of the values 45%, 50%, 55%, 60%, 70%, 80%, 90%, 95%, and 99%, where any of the lower limits can be combined with any of the higher limits that are mathematically compatible. Embodimental hardening cement formulations may include a slip ring polymer in sufficient quantities to improve the cement's mechanical properties. In some embodiments, the cement may contain a slip ring polymer at a concentration of approximately 0.025 to approximately 5.5 wt% of the cement weight (bwoc). Embodimental slip ring polymers may have a minimum of 0.025, 0.05, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5, or 3.0 wt% of the cement weight and a maximum of 5.5, 5.0, 4.5, 4.0, or 3.5 wt% of the cement weight, where any lower limit can be used in conjunction with any mathematically compatible higher limit. Embodimental hardening cement formulations may include an additional polymer in sufficient quantities to improve the cement's mechanical properties. In some embodiments, the cement may contain the additional polymer at a concentration of approximately 0.05 to approximately 35.0 wt% of the cement weight. Embodimental additive polymers may have a minimum limit of 0.05, 0.10, 0.25, 0.5, 1.0, 2.0, 2.5, 3.0, 5.0, 7.5, 10, 15, 20, or 25.0 wt% of the cement weight and a maximum limit of 35.0, 30.0, 25.0, 20, 15, 12.5, 10, or 7.5 wt% of the cement weight, where any lower limit can be used in conjunction with any mathematically compatible higher limit. When used, silica powder may be present in the hardened cement composition in amounts ranging from approximately 25% to approximately 75% of the cement weight. Embodimentary cementitious mortars may contain silica powder in amounts with a minimum of any of the following values: 25%, 30%, 35%, 40%, 50%, and 55% of the cement weight, and a maximum of any of the following values: 50%, 60%, 65%, 70%, and 75% of the cement weight. Any lower limit may be used in conjunction with any mathematically compatible upper limit. Concrete hardening cement formulations may include one or more fluid loss control agents in amounts ranging from approximately 0.05 to approximately 5.5 wt% of the additional cement weight. Concrete fluid loss control agents may have a minimum limit of 0.05, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5, or 3.0 wt% of the cement weight and a maximum limit of 5.5, 5.0, 4.5, 4.0, or 3.5 wt% of the cement weight, where any lower limit may be used in conjunction with any mathematically compatible higher limit. Concrete-hardened cement formulations may include one or more dispersing agents in amounts ranging from approximately 0.05 to approximately 5.5 wt% of the additional cement weight. The concrete dispersing agent(s) may have a minimum limit of 0.05, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5, or 3.0 wt% of the cement weight and a maximum limit of 5.5, 5.0, 4.5, 4.0, or 3.5 wt% of the cement weight, where any lower limit may be used in conjunction with any mathematically compatible higher limit. Concrete hardening cement formulations may include one or more cement retarders in amounts ranging from approximately 0.05 to approximately 5.5 wt% of the additional cement weight. Concrete cement retarders may have a minimum limit of 0.05, 0.1, 0.25, 0.5, 0.75, 1.0, 2.0, 2.5, or 3.0 wt% of the cement weight and a maximum limit of 5.5, 5.0, 4.5, 4.0, or 3.5 wt% of the cement weight, where any lower limit may be used in conjunction with any mathematically compatible higher limit. Embodied hardened cement formulations may achieve improved mechanical properties compared to cement without an additional polymer and a slip ring polymer. These improvements may include a decrease in free compressive strength, a decrease in compressive strength, and a decrease in Young's modulus when compared to cement without the embodiment of both a slip ring polymer and an additional polymer. For example, the Young's modulus of hardened cement formulated with one or more embodiments may be at least 25% lower than the Young's modulus of hardened cement prepared without the slip ring polymer, the additional polymer, or both. The Young's modulus of cement hardened to which the formulation is made according to one or more embodiments may be at least 25%, at least 28%, at least 30%, at least 35%, at least 40%, at least 45%, or at least 50% lower than the Young's modulus of cement hardened to which cement hardened to which cement prepared in the absence of the slip ring polymer, the additional polymer, or both.The Young's modulus of cement hardened to one or more embodiments may be lower than that of cement hardened to the absence of the slip ring polymer, the additional polymer, or both, and within a range with a lower limit of any of the following values: 25%, 28%, 30%, 35%, and 40%, and a higher limit of any of the following values: 45%, 50%, 55%, 60%, 70%, 80%, 90%, 95%, and 99%, where any lower limit can be combined with any mathematically compatible upper limit. These improved properties may reduce the physical deformation of embodied cement-hardened formulations (such as cement shields) when subjected to temperature and pressure changes, such as those found in subsurface formations. A method for manufacturing cement mortar In one respect, the embodiments presented here relate to a method for manufacturing the cementitious mortar described previously. Figure 2 is a mass flow diagram of an embodied method for manufacturing mortar 200. The method may involve blending a slip ring polymer and an additive polymer with a cementitious raw material to form a mixture for cementitious raw material 202. If available, a fluid loss control agent, dispersant, or setting retarder may be blended with the slip ring polymer, the additive polymer, and the cementitious raw material to form a mixture for cementitious raw material. In some embodiments, dry admixtures are premixed with the powdered cementitious raw material. The dry admixtures and cementitious raw material may be blended using a pneumatic conveying method between tanks 3 to 4 times to form a dry mix. The dry mix can then be mixed with water and any remaining liquid additives and blended at the drill bit site to form a cement slurry using a large-scale, real-time metering mixer. The cement slurry can then be pumped down the well immediately after formation. Implementation methods may also include introducing water into the cementitious raw mix (204). The water can be introduced at a mixing speed within a range of values: a lower limit of 3000, 3500, 3800, and 4000 rpm (revolutions per minute), and a higher limit of 4000, 4200, 4500, 4800, and 5000 rpm. Any lower limit can be combined with any higher limit that is mathematically compatible. In some implementations, the amount of water added to the dry mix is determined based on the target density of the cement slurry. After the water is introduced into the cementitious raw mix, the resulting slurry can be blended for a period of time at a suitable mixing speed to achieve a homogeneous slurry.The embodied mixing times may have a minimum of 10, 20, 30, 35, or 40 seconds and a maximum of 60, 55, 50, or 45 seconds, where any lower limit can be used in conjunction with any mathematically compatible upper limit. The embodied mixing speeds may have a minimum of 500, 1000, 2000, 5000, or 8000 rpm and a maximum of 20000, 18000, 15000, or 12000 rpm, where any lower limit can be used in conjunction with any mathematically compatible upper limit. In some embodiments, mortar can be mixed for approximately 35 seconds at a speed of about 12000 rpm. In some embodiments, water can be introduced into the dry mix at a mixing speed of about 4000 rpm for 15 seconds. The mortar can then be mixed at a speed of 12,000 rpm for 35 seconds. A method for cementing one of the formations In one aspect, the reported embodiments relate to a method for forming a cement shield in a wellbore. The embodiment methods involve introducing the previously described slurry composition into wellbore 206. The composition may include the previously described slip ring polymer and additional polymer, evenly distributed throughout the cement slurry. Figure 3 is a schematic depiction of cementing Composition 300 (cementation). Slurry 308 can be pumped down the wellbore through casing 302. Slurry 308 is then pushed upwards to ring 304 between Composition 306 and casing 302. The direction of cement flow is indicated by arrows (no reference number). Once cement is introduced into the composition, the method may also involve maintaining the cement slurry in the wellbore so that a shield is formed. The cement shield may contain the embodied slip ring polymer and the previously described additional polymer, evenly distributed throughout the cement mold. As previously described, embodiment methods may include introducing the previously described mortar into the borehole 206 (for example, introducing the previously described mortar into the area between the casing and the formation rock of the borehole) and maintaining the cement mortar in the borehole so that a hardened cement shield 208 is formed. Embodimentation methods may involve maintaining the cementitious mortar so that the cement hardens in the borehole. Embodimental mortars can harden at any suitable time, temperature, and pressure for the cement to set. Embodimental cement may begin to harden upon initial contact with water. Embodimental setting times may range from several hours to several days. These times may have a minimum of 3, 4, 5, 10, 12, or 24 hours and a maximum of 90, 50, 30, 7, 5, 4, 3, or 2 days, where any lower limit can be used in conjunction with any mathematically compatible upper limit. Skilled drillers understand that such conditions may vary due to differences in the composition of embodimental cementitious mortars and the conditions downhole. Embodimental cementitious mortars may harden under specific formation conditions, such as temperatures ranging from approximately 25°C to approximately 260°C and pressures ranging from ambient pressure to approximately 45,000 psi. Embodimental formation temperatures may have a lower limit of 25°C, 50°C, 65°C, or 75°C, and a higher limit of 260°C, 200°C, 150°C, or 95°C, where any lower limit can be used in conjunction with any mathematically compatible upper limit. The embodied formation pressures may have a lower limit of 15, 100, 1000, 3000 or 5000 psi, and a higher limit of 45000, 30000, 20000, 15000 or 10000 psi, where any lower limit may be used in conjunction with any mathematically compatible higher limit. Concrete cement can be used in various underground formations for primary and secondary cementing processes. Examples The following examples are merely illustrative and should not be interpreted as limiting the scope of the present invention. Five cement slurry formulations are designed according to Table 1 below. Each cement slurry is mixed according to API RP 10B2, the Recommended Practice for Testing Well Cements. For each cement slurry formulation listed in Table 1, water is introduced into a dry mix of ingredients at a mixing speed of approximately 4000 rpm (rpm) for 15 seconds. The slurry is then mixed at a speed of 12000 rpm for 35 seconds. Table 1: Mortar Compositions Mortar number A B C D E Materials: Cement only (g) Cement + 0.5% RM (g) Cement + 15% EM (g) Cement + 15% EM + 0.25% RM (g) Cement + 15% EM + 0.5% RM (g) Cement Class Z 595.49 594.32 603.05 602.45 601.85 Silica powder 208.42 208.01 211.07 210.86 210.65 FL-24 4.22 4.21 4.27 4.27 4.26 SC-9 2.4 2.4 2.43 2.43 2.43 PCR-3 1 1 1,01 1,01 1,01 RotaMach (RM) 0 2.97 0 1.51 3.01 Calprene 441M Calprene 441M (EM) 0 0 90,46 90,37 90,28 Water 296.24 296 300 300 Density 15.8 lbs per gallon 15.8 lbs per gallon 15.8 lbs per gallon 15.8 lbs per gallon The materials listed in Table 1 include a Class G cementitious raw material, silica flour, BASF Polytrol® FL-24 fluid loss control agent, Economy Polymers & Chemicals SC-9 dispersant, Economy Polymers & Chemicals PCR-3 setting delay agent, Saudi Aramco Rotamach slip ring polymer, and a styrene-butadiene copolymer such as Dynasol Calprene® 411M (EM) copolymer. The test is performed on several 1-inch x 2-inch cylindrical cement samples, which are cured at 300°F and a pressure of 3000 psi for 7 days. The three-axis mechanical properties (e.g., Young's modulus of each sample) are measured using a New England Research (NER 300) instrument with a confined pressure of 1500 psi and a temperature of 100°F. Table 3: Young's modulus and compressive strength for different cementitious systems Mortar number, system, Young's modulus (lb / in²), compressive strength (lb / in²), percentage decrease in Young's modulus A comparative example (cement only) 2.32 × 610 12328 - B Cement + 0.5% RM 2.17 × 610 10878 6.5 Cement + 15% EM 1.94 × 610 8068 16.4 Cement + 15% EM + 0.25% RM 1.51 × 610 7040 34.9 Cement + 15% EM + 0.5% RM 1.29 × 610 6515 44.4 It was determined that the comparable cement system (System A) without a mechanical enhancer has a large Young's modulus (i.e., 2.32 × 10⁶ psi) and a lower axial deformation capacity under stress. System B, containing 0.5% by weight of slip ring polymer (RotaMach (RM)), has a slightly lower Young's modulus and a slightly higher axial deformation capacity under stress compared to System A. System C, containing 15% by weight of additional polymer (i.e., Calprene 411M), has a Young's modulus of 1.94 × 10⁶ psi and a slightly higher axial deformation capacity under stress compared to System A. It was determined that systems D and E, which incorporate a combination of Calperin 411M and Rotamach, possess lower Young's modulus values compared to system A. Specifically, systems D and E were found to have Young's modulus values of approximately 1.5 × 10⁶ psi or less, indicating a very high capacity for axial deformation under stress compared to system A. Figure 4 is a graph of the axial stress versus tensile (strain) (deformation) for the different cement systems listed in Table 2. Figure 5 is a graph of the axial tensile capacity (deformation versus Young's modulus) for systems A–E. As shown in Table 2 and Figures 4 and 5, systems D and E have been found to have a higher deformability capacity, as evidenced by their ability to achieve high tensile values. Therefore, the lower Young's modulus of systems D and E compared to systems A–C indicates that the cementitious shield of such a system can withstand higher stresses for a longer period. Consequently, the combined approach of incorporating an additional polymer (e.g., Calperen 411M) and a relatively small amount of slip ring polymer (e.g., Rotamak) can lead to excellent synergy in providing the elastic mechanical properties in the hardened cement required for long-term zone insulation of oil and gas wells and geothermal wells for the lifetime of the well. Although only a few of the representational figures are described in detail above, skilled artists readily recognize that many modifications can be made to these representations without actually going outside the scope of this invention. Accordingly, all such modifications are intended to fall within the scope of the present invention as defined in the following elements of protection.
Claims
1. Cement slurry includes: water; cement precursor; sliding ring polymer; and additional polymer.
2. Cement slurry according to protection factor 1, where the additional polymer is a thermoplastic copolymer of styrene and butadiene.
3. Cement slurry according to protection factor 2, where the additional polymer is present in an amount ranging from 0.1% to 30% of the weight of the cement precursor.
4. Cement slurry according to protection factor 2, where the styrene-butadiene copolymer comprises 70% butadiene units and 30% styrene units.
5. Cement slurry according to protection element 1, where the amount of water, sliding ring polymer, and additional polymer ranges from 35 to 300% of the weight of the cement precursor, and from 0.0.5 to 5% of the weight of the cement precursor, and 0.1 to 30% of the weight of the cement precursor, respectively.
6. Cement slurry: According to protection element 1, it shall additionally include silica flour in an amount ranging from 30 to 70% by weight of the cement precursor, and a cement retarder in an amount ranging from 0.1 to 10% by weight of the cement precursor, where the cement retarder includes one or more selected compounds from the group consisting of sodium lignosulfonate, calcium lignosulfonate, acrylic acid (AA) copolymer, and 2-acrylamido-2-methylpropane sulfonic acid (AMPS), and combinations thereof.
7. Cement slurry: According to protection element 1, it shall additionally include a dispersant in an amount ranging from 0.1% to 5% of the weight of the cement precursor, where the dispersing agent includes one or more selected compounds from the group consisting of lignosulfonates, polyacrylic acid polymers, and combinations thereof.
8. Cement slurry: According to protection element 1, it also includes a fluid loss control agent in an amount ranging from 0.1% to 5% of the weight of the cement precursor, where the fluid loss control agent includes one or more selected compounds from the group consisting of hydroxyethylcellulose, 2-acrylamido-2-methylpropane sulfonic acid tertiary polymer, acrylic acid, and N,N-dimethyl acetamide (NNDMA), and combinations thereof.
9. Cement composition: A hardened cement slurry prepared according to the protection element 1. 10.
11. Cement composition hardened according to protection element 9, where the cement composition hardened has a Young's modulus less than the Young's modulus of cement prepared in the absence of the sliding ring polymer and the additional polymer.
12. Cement composition hardened according to protection element 10, where the Young's modulus of the cement composition hardened is at least 25% less than the Young's modulus of cement prepared in the absence of the sliding ring polymer, the additional polymer, or both.
13. Cement composition hardened according to protection element 10, where the Young's modulus of the cement composition hardened is 1.5 × 10⁶ psi or less.
14. Cement composition hardened according to protection element 10, where the cement composition hardened is capable of axial deformation under compressive stress.
15. A cement composition hardened according to Protection Element 12, where the cement composition is capable of withstanding axial stress 10% or more compared to cement hardened in the absence of a sliding ring polymer, an additional polymer, or both.
16. A cement composition hardened according to Protection Element 10, where the compressive strength of the cement composition is 8000 psi or less.
17. A method for providing cement shielding in a wellbore, which involves introducing cement slurry into the area between the casing and the formation rock of the wellbore, where the cement slurry includes: water; a cement precursor; a polyrotaxane polymer; and an additional copolymer. The cement slurry injected into the area between the casing and the formation rock of the wellbore hardens, thus forming the cement shield in the wellbore. 17.The method according to Protection Element 16, in addition to cement slurry preparation, involves mixing cement, polyrotaxane polymer, additional copolymer, and water.
18. The method according to Protection Element 16, where the Young's modulus of the cement shield is 1.5 × 10⁶ psi or less.
19. The method according to Protection Element 16, where the cement shield is capable of axial deformation under compressive stress.
20. The method according to Protection Element 16, in addition to cement slurry preparation, involves mixing the cement precursor, polyrotaxane polymer, and additional copolymer to form a dry mix before introducing the cement slurry into the wellbore; and adding water to the dry mix to form the cement slurry.