Acrylate adhesive composition for the outer shell of spiral wound membrane filters

A coiled spiral membrane filter with an outer sleeve and acrylate adhesive formulation addresses structural integrity issues by providing strength and rigidity, enhancing durability and filtration efficiency.

SA1120261965A1Pending Publication Date: 2026-10-05HB FULLER CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
SA1120261965
Authority / Receiving Office
SA · SA
Patent Type
Applications
Current Assignee / Owner
Filing Date
2026-03-10
Publication Date
2026-10-05

AI Technical Summary

Technical Problem

Existing coiled spiral membrane filters face challenges in maintaining structural integrity and shape stability, particularly in larger sizes, due to the lack of a robust and efficient outer casing that can withstand pressure and maintain rigidity during filtration processes.

Method used

A coiled spiral membrane filter with an outer sleeve containing a reinforcing material and an acrylate adhesive formulation, which includes multifunctional (meth)acrylates, is developed. The adhesive formulation has a viscosity of no more than 10,000 centipoise at 23°C, and is hardened using energy sources like UV light, visible light, or heat, providing strength and rigidity.

Benefits of technology

The solution enhances the structural integrity and shape stability of the filter, ensuring durability and resistance to bursting, while maintaining efficient filtration performance.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to a spiral wound membrane filter which includes an outer sheath, which includes a reinforcement material and an acrylate adhesive composition which includes multifunctional (meth)acrylate, whereby the adhesive composition has a viscosity not exceeding 10,000 centipoise when measured at 23°C according to the American Society for Testing and Materials (ASTM) D1084 Test Method B.
Need to check novelty before this filing date? Find Prior Art

Description

coiled spiral membrane filter In membrane filtration, filter elements (such as semi-permeable membranes) are used to remove impurities from a liquid. Membrane filtration can be used in a wide range of applications, including selected applications from the group consisting of reverse osmosis, forward osmosis, nanofiltration, ultrafiltration, and microfiltration. The elements of a spiral wound filter are constructed by spirally wound one or more membrane envelopes and optional feed channel spacer sheets around a center-core collection tube. Each membrane envelope preferably includes two roughly rectangular membrane sheets surrounding a permeate channel spacer sheet. This composite structure is held together with an adhesive along three edges, while the fourth edge is firmly in contact with the permeate collection tube, ensuring the permeate spacer is in fluid contact with the permeate tube's permeate openings. The fluid to be filtered enters the membrane module at one end. Once inside the module, filtration occurs when pressure is applied to force the clean fluid across the membrane surface. Upon exiting the module at the other end, the clean fluid flows through the center-core collection tube where it has been collected, while the concentrated waste fluid flows through the membranes.A spiral membrane filter may also include end caps at its ends to help hold the membranes in place. Helical coil membrane filters are available in a variety of sizes. For larger filters, which in some cases may exceed 2-4 inches in diameter, an outer sleeve surrounds the filter's surface to help maintain its shape and protect it. The invention features a coiled spiral membrane filter that includes an outer sleeve. The outer sleeve contains a strengthening material and an acrylate adhesive formulation that includes (meth)acrylate multifunctional, where the adhesive formulation has a viscosity of no more than 10,000 centipoise when measured at 23 degrees Celsius according to the American Society for Testing and Materials Testing Method B D1084. The invention features a coiled spiral membrane filter that includes an outer shell. The outer shell contains a reinforcing material and an acrylate adhesive formulation that includes multifunctional (meth)acrylate in a proportion ranging from 20% by weight to 90% by weight, where the adhesive formulation has a viscosity of no more than 10,000 centipoise when measured at 23°C according to the American Society for Testing and Materials Testing Method B D1084. In one aspect, the invention features a coiled spiral membrane filter that includes an outer sleeve. The outer sleeve includes a reinforcing material, and an acrylate adhesive formulation that includes multifunctional (meth)acrylate in a proportion ranging from 5% by weight to 90% by weight, where the acrylate adhesive formulation has a viscosity not exceeding 10,000 centipoise when measured at 23°C according to the American Society for Testing and Materials Testing Method B D1084. The invention features a coiled spiral membrane filter that includes an outer sleeve. The outer sleeve includes a reinforcing material, an acrylate adhesive formulation that includes multifunctional (meth)acrylates, and a photoinitiator, where the adhesive formulation has a viscosity of no more than 10,000 centipoise when measured at 23 degrees Celsius according to the American Society for Testing and Materials Testing Method B D1084. The invention also features a coiled spiral membrane filter that includes an outer sleeve. The outer sleeve includes a reinforcing material, and an acrylate adhesive formulation that includes 15% by weight to 60% by weight of multifunctional (meth)acrylate oligomer, 30% by weight to 80% by weight of (meth)acrylate monomer, and 0.5% by weight to 5% by weight of photoinitiator, where the adhesive formulation has a viscosity not exceeding 10,000 centipoise when measured at 23°C according to ASTM D1084 Test Method B. This invention presents a new method for forming the outer casing of a coiled spiral membrane filter, a method that is simpler (consisting of one part instead of two), faster, and provides the required strength and rigidity. outer cover The outer casing surrounds the outer periphery of the membrane filter, helping to maintain and protect its shape. The casing contains a reinforcing material and an acrylate adhesive. The acrylate adhesive is hardened within the casing by exposure to an energy source. This energy source can be selected from a range including ultraviolet light, visible light, electron beam radiation, microwave radiation, heat, and a combination thereof. Alternatively, an energy source can be selected from a range including ultraviolet light, visible light, heat, and a combination thereof. Acrylate adhesives can be cured during coating manufacturing, after coating manufacturing, or a combination of both. When the curing process involves exposing the adhesive to light, the adhesive may contain a photo-initiator. When the curing process involves heating the adhesive, the adhesive may contain a thermal initiator. Acrylate adhesives may also contain both a thermal and a photo-initiator. Strengthening material The reinforcing material can be a choice from a range of options including woven braid, mesh fabric, scrim, and non-woven fabric. A woven braid is often the most common reinforcing material. Alternatively, the reinforcing material can be made from fiberglass, carbon fiber, aramid (such as Kevlar), or another material which, when combined with the adhesive, creates a durable, burst-resistant coating to protect the filter. Acrylate adhesive composition The adhesive formulation is a 100% solid, single-component acrylate adhesive. In one formulation, the acrylate adhesive does not functionally contain isocyanate. The acrylate adhesive formulation includes multifunctional methacrylate. The acrylate adhesive formulation can contain 15% to 90% by weight of multifunctional methacrylate. The adhesive formulation can also contain multifunctional methacrylate and a photoinitiator. The adhesive formulation can contain 15% to 60% by weight of multifunctional methacrylate oligomer, 30% to 80% by weight of methacrylate monomer, and 0.5% to 5% by weight of a photoinitiator. Acrylate adhesive formulations possess sufficient hardness to provide a robust filter coating. Acrylate adhesive formulations can have a Shore D hardness greater than 60, greater than 65, greater than 70, from 50, 55, 60, 65 to 85, 90, 95, 100, or any two values ​​in between. The adhesive formulation of acrylates may have a viscosity of no more than 10,000 centipoise, no more than 7,500 centipoise, no more than 5,000 centipoise, no more than 2,500 centipoise, no more than 1,500 centipoise, from 10 centipoise to 10,000 centipoise, from 10 centipoise to 7,500 centipoise, from 10 centipoise to 2,500 centipoise, from 10 centipoise to 1,500 centipoise, from 50 centipoise to 1,200 centipoise, or even from 250 centipoise to 1,200 centipoise, when measured at 23°C using ASTM D1084 Test Method B. Low viscosity is particularly useful when the reinforcing material is a braid coated with an acrylate adhesive formulation and wrapped around the outer surface of the film. (Meth) Multifunctional Acrylates Multifunctional methacrylates (MMCs) contain at least two ethylenically unsaturated functional groups. Ideally, at least two of these ethylene-unsaturated functional groups are located at the terminals of the MMC. MMCs can be selected from a range consisting of oligomers, monomers, and combinations thereof. The adhesive formulation of acrylates may contain a multifunctional (meth)acrylate content ranging from 5% by weight, 10% by weight, 15% by weight, 20% by weight, 25% by weight, 30% by weight, 35% by weight, 40% by weight, 45% by weight, 70% by weight, 75% by weight, 80% by weight, 85% by weight, 90% by weight, 95% by weight or any two values ​​in between. Oligomer (meth) multifunctional acrylates The adhesive formulation of acrylates includes a multifunctional (meth)acrylate oligomer. An acrylate adhesive formulation can contain more than one (meth)acrylate oligomer. The multifunctional (meth)acrylate oligomer can be selected from a group consisting of urethane / ester / epoxy / butadiene (meth)acrylate oligomers. In one aspect of the present invention, the acrylate meth oligomer is a polyether / polyester urethane acrylate oligomer. A functionalized polyether / polyester urethane component can be synthesized using the diisocyanate reaction with the polyether / polyester polyol to produce isocyanate-terminated urethane. The isocyanate-terminated urethane is then reacted with hydroxy-terminated acrylate to provide acrylate groups at the oligomer ends. The functionalized acrylate meth oligomer can be fully reacted so that no free isocyanate groups are present. Alternatively, if the terminal isocyanates do not fully react with the hydroxy acrylate, the isocyanate groups will remain in the structure as reactive groups in addition to the acrylate terminal groups.This may be useful if additional power is needed. Multifunctional acrylate (meth) oligomers are commercially available under various trade names, including, for example: GENOMER4316, GENOMER4215, GENOMER4267, GENOMER2235, GENOMER2281, GENOMER2263, and GENOMER3486, all available from RAHN USA Corp (Aurora, Illinois), and EBERCRYL 8465 and EBERCRYL 8411, available from Allnex Netherlands BV The adhesive formulation of acrylates includes 5% by weight, 10% by weight, 15% by weight, 20% by weight, 25% by weight, 30% by weight, 35% by weight to 40% by weight, 50% by weight, 55% by weight, 60% by weight, 65% by weight, 70% by weight, 75% by weight, or any two values ​​in between, of an acrylates (meth) oligomer based on the weight of the components of the adhesive formulation of acrylates. (meth)acrylate monomer Acrylates (meth) monomers can be multifunctional (difunctional, trifunctional, etc.) or monofunctional. Acrylates (meth) monomers can act as diluents and can be used to adjust the viscosity of acrylate adhesive formulations. Acrylate adhesive formulations can contain more than one acrylates (meth) monomer; for example, an adhesive formulation can contain a mixture of multifunctional and monofunctional monomers. The (meth)acrylate monomer includes at least one ethylene-unsaturated functional group, or at least two ethylene-unsaturated functional groups. Suitable monofunctional (meth)acrylate monomers include, for example, methyl (meth)acrylate, isopropyl (meth)acrylate, isobutyl (meth)acrylate, tert-butyl (meth)acrylate, steryl (meth)acrylate, 2-hexyl (meth)acrylate, octyl (meth)acrylate, isooctyl (meth)acrylate, decyl (meth)acrylate, and isodecyl (meth)acrylate. (meth)acrylate, dodecyl (meth)acrylate, tetradecyl (meth)acrylate, phenoxyethyl (meth)acrylate, tetrahydrofurfuryl (meth)acrylate, glycidyl (meth)acrylate, hydroxyethyl (meth)acrylate, hydroxypropyl (meth)acrylate, hydroxybutyl (meth)acrylatehydroxybutyl (meth)acrylate, benzyl (meth)acrylate, dicyclopentyl (meth)acrylate, and combinations thereof. Suitable multifunctional (meth)acrylate monomers include, for example, ethylene glycol di(meth)acrylate, diethylene glycol di(meth)acrylate, triethylene glycol di(meth)acrylate, dipropylene glycol di(meth)acrylate, 1,3-butylene glycol di(meth)acrylate, 1,4-butanediol di(meth)acrylate, and 1,6-hexanediol di(meth)acrylate. 1,6-Hexanediol di(meth)acrylate, neopentyl glycol di(meth)acrylate, cyclohexane dimethanol di(meth)acrylate, dicyclopentyl di(meth)acrylate, glyceryl tri(meth)acrylate, trimethylolpropane tri(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, pentaerythritol dipentaerythritol penta(meth)acrylate, hexafunctional aliphatic acrylate monomer, tris(2-hydroxyethyl)isocyanurate tri(meth)acrylate, and alkoxylated versions thereof, and synthesis thereof. The monomer (meth)acrylate can be an aliphatic acrylate. Aliphatic acrylates can be useful in improving the water resistance of acrylate adhesive formulations, and therefore of coatings. The monomer (meth)acrylate can be selected from a group that includes isobornyl acrylate, polyether acrylate, tricyclodecane dimethanol diacrylate, and hexafunctional aliphatic acrylate. (Meth)acrylate monomer can exhibit a viscosity of no more than 1500 centipoise, no more than 1000 centipoise, no more than 500 centipoise, no more than 150 centipoise, from 5 centipoise to 1500 centipoise, or even from 5 centipoise to 1000 centipoise at a temperature of 25 degrees Celsius. Acrylates (meth) monomers are commercially available under multiple trade names, including, for example: GENOMER 1121Y, GENOMER 7302, MIRAMER M262, and MIRAMER M600, all of which are available from RAHN USA Corp (Aurora, Illinois). The adhesive formulation of acrylates includes 5% by weight, 10% by weight, 15% by weight, 20% by weight, 25% by weight, 30% by weight, 35% by weight to 40% by weight, 50% by weight, 55% by weight, 60% by weight, 65% by weight, 70% by weight, 75% by weight or any two values ​​there are between the (meth)acrylate monomer on a weight basis of the components in the adhesive formulation of acrylates. The initiator Acrylic adhesive formulations optionally include a primer. Useful primers include thermal primers, photo-primers, and mixtures of both. Useful thermal starters have a half-life of ten hours at a temperature not exceeding 70°C, not exceeding 60°C, not exceeding 50°C, not exceeding 40°C, not exceeding 30°C, or even from about 30°C to about 70°C. Useful classes of thermodynamic precursors include, for example, organic peroxides (such as di(4-tert-butylcyclohexyl)peroxydicarbonate, tert-butyl peroxyneodecanoate, di(2-ethylhexyl)peroxydicarbonate), benzoyl peroxide, lauroyl peroxide, 2,2-azo-bisisobutyronitrile, t-butyl peroxypivalate, α,α'-bis(neodecanoyl peroxy)diisopropylbenzeneα'-Bis(neodecanoyl peroxy) diisopropyl benzene, cumyl peroxynedecanoate, t-hexyl peroxypivalate, 1,1,3,3-tetramethylbutyl peroxynedecanoate, 1,1,3,3-tetramethylbutyl peroxynedecanoate, 1,1,3,3-tetramethylbutyl peroxy-2-ethylhexanoate, t-amyl peroxypivalate, t-amyl peroxynedecanoate, isobutyryl peroxide, succinic peroxide, peroxide 3,5,5-trimethylhexanoyl peroxide, di-methoxybutyl peroxydicarbonate, di-(sec-butyl)peroxydicarbonate, t-butyl peroxyneoheptanoate, di-(3,5,5-trimethylhexanoyl) peroxide, di(sec-butyl) peroxydicarbonate, and combinations thereof. Suitable thermal primers are commercially available under various trade names, including, for example, PERKADOX 16di(4-tert-butylcyclohexyl)peroxydicarbonate and TRIGONOX 23tert-butylperoxynedecanoate, both available from Nouryon Chemical (Chicago, Illinois), PEROXAN EPCdi(2-ethylhexyl)peroxydicarbonate from Pergan Marshall LLC (Marshall, Texas), under the VAZO series of trade names from DowDuPont (Wilmington, Delaware), and under the CHEMEX series from Hosung Chemex Co., Ltd. (Seoul, Korea), including CHEMEX 2EHPC, BND series, BPV series, CND70(IP), OND, TMPO, AND, and APV. The adhesive formulation of acrylates includes a proportion ranging from 0% by weight to no more than 10% by weight, with a proportion of at least 1% by weight, no more than 5% by weight, no more than 3% by weight, from about 1% by weight to about 5% by weight, or even from about 2% by weight to about 4.5% by weight of the thermal initiator. It may be beneficial to add more than one, or even two, photo-initiators to the acrylic adhesive formulation. Useful photochemical precursors include, for example: 2-hydroxy-2-methyl-1-phenyl-propan-1-one, 2,2-dimethoxy-1,2-diphenylethan-1-one, 1-hydroxycyclohexylphenylketone, 2,4,6-trimethylbenzoyl-diphenylphosphineoxide, benzophenone, benzoin, benzoin ethers (such as benzoin methyl ether and benzoin isopropyl ether). Substituted benzoin ethers (such as anisoin methyl ether), substituted acetophenones (such as 2,2-diethoxyacetophenone and 2,2-dimethoxy-2-phenylacetophenone)2-dimethoxy-2-phenylacetophenone), substituted alpha-ketols (such as 2-methyl-2-hydroxypropiophenone), aromatic sulfonyl chlorides (such as 2-naphthalenesulfonyl chloride), photoactive oximes (such as 1-phenyl-1,2-propanedione-2-(O-ethoxycarbonyl)oxime), methylbenzoylformate and mixtures thereof. Commercially available light-emitting primers are available under various brand names, including, for example: the OMNIRAD series from IGM Resins (Waalwijk, The Netherlands), which includes OMNIRAD 73 (2-hydroxy-2-methyl-1-phenylpropanone); the DAROCUR series from BASF (Florham Park, New Jersey), which includes DAROCUR TPO (2,4,6-trimethylbenzoyl-diphenylphosphine oxide); the IRGACURE series from BASF, which includes, for example, IRGACURE 651 and IRGACURE TPO; the ESACURE series from IGM Resin (Waalwijk, The Netherlands), which includes ESACURE KB-1 benzyl dimethyl ketal; and the GENOCURE series from RAHN USA Corp (Aurora, Illinois), which includes GENOCURE BAPO, GENOCURE TPO-L, and GENOCURE MBF. The adhesive formulation of acrylates includes a percentage ranging from 0% by weight to no more than 10% by weight, no more than 5% by weight, no more than 3% by weight, from 0.2% by weight to about 5% by weight, or even from 0.5% by weight to 5% by weight of a photoinitiator. additives Various additives may be included in the formulation of acrylates adhesives, including, for example: adhesion promoters (such as silane adhesion promoters), antioxidants, rheology modifiers, inhibitors, defoamers, optical brighteners, antioxidants, dyes, pigments, and combinations thereof. Useful adhesion enhancers include, for example, silanes, isocyanate-containing compounds, titanates, zirconates, phosphates, epoxy-containing compounds, epoxy(meth)acrylate hybrid monomers / oligomers, and combinations thereof. Examples of useful epoxy-based compounds include: silsesquioxane, epoxy silane, epoxy resins (such as bisphenol A / Diglycidyl ether and bisphenol F / Diglycidyl ether), epoxy phenolic novolac resins, epoxy cresol novolac resins, cycloaliphtic epoxies, and combinations thereof. Useful epoxy silane adhesion promoters are available under the SILQUEST brand from Momentive Performance Materials Inc.(Waterford, New York), including the alkoxysilane epoxy adhesion promoter SILQUEST A187. Additional materials The adhesive composition of acrylates may also include additives. These additives may be liquid or solid at room temperature. The additives include other polymers, oligomers and monomers (such as meth acrylate polymers) that are unreactive (i.e., those that do not contain a residual meth acrylate functional group), vinyl acetate polymers, core-shell polymers, synthetic rubber polymers (such as polybutadiene and polybutadiene / butadiene-acrylonitrile copolymers) containing a functional group of carboxyl-, amino-, vinyl-, meth acrylic-, or epoxy-, or a combination of these functional groups or any other compatible polymer, etc.) and plasticizers. Additional useful polymers are available under the trade name ELVACITE from Mitsubishi Chemical UK Ltd and under the trade name DEGALAN from Roehm America LLC. How to make a coiled spiral filter housing The invention features a method for making the outer casing of a coiled spiral membrane filter that includes the following steps: obtaining an acrylate adhesive formulation that includes multifunctional acrylates (meth) and an initiator, passing at least one continuous strand of reinforcing material through the acrylate adhesive formulation, wrapping the continuous strand around the outer perimeter of the coiled spiral membrane filter along its full length, and exposing the continuous strand of reinforcing material coated with the acrylate adhesive formulation to an energy source at a time chosen from among during the wrapping, after the wrapping, and a combination of both. The invention also features a method for manufacturing the outer sheath of a coiled spiral membrane filter, which includes the following steps: obtaining an acrylate adhesive formulation that includes multifunctional acrylate (meth) and a photoinitiator, passing at least one connected strand of reinforcing material through the acrylate adhesive formulation, winding at least one connected strand around the outer perimeter of a coiled spiral membrane filter in full length, and exposing the connected strand of reinforcing material coated with the acrylate adhesive formulation to an energy source at a specified time during winding, after winding, and a combination of both. This method involves coating at least one continuous strand of reinforcing material with an acrylic adhesive. To improve speed, any number of strands (e.g., more than one, even 2 to 20, or even 2 to 10) can be coated and wrapped simultaneously. Optionally, this method can include removing excess acrylic adhesive either immediately after coating, after lamination, or after both. The energy source can be chosen from a group consisting of ultraviolet light, visible light, electron beam radiation, microwave radiation, heat, and a combination thereof. Alternatively, the energy source can be chosen from a range consisting of ultraviolet light, visible light, heat, and a combination thereof. The invention will now be described through the following examples. All parts, percentages, and quantities mentioned in the examples are by weight unless otherwise stated. Examples Testing procedures The testing procedures used in the examples include the following. All percentages are by weight unless otherwise stated. Procedures are performed at room temperature (i.e., an ambient temperature of approximately 20°C to approximately 25°C) unless otherwise stated. How to prepare a test sample The samples were prepared as follows: The oligomers were heated at 60°C for two hours and then added to a clean mixing vessel. An upper shear blade was lowered into the oligomer and run at a medium speed for 10 minutes. The monomer was then weighed and slowly added to the oligomer. The sample was then mixed under medium to high shear for two hours or until homogeneous. In a separate container, the powdered photoinitiator was added to the diluent (monofunctional) monomer and mixed under another mixer for 15 minutes. The diluent monomer / photoinitiator mixture was then added to the original container. The combined mixture was mixed for 30 minutes. A second photoinitiator was added and mixed for 15 minutes. The mixture was tested for viscosity, and the diluent monomer was added again to make any necessary adjustments. Viscosity was tested according to Test Method B of the American Society for Testing and Materials D1084. Shore D hardness was tested according to the American Society for Testing and Materials D2240. The liquid acrylate adhesive was poured into a 5.08 cm (2 in) x 5.08 cm (2 in) weighing dish to a depth of 0.635 cm (0.25 in). The sample was then cured under an ultraviolet A (UVA) lamp for 30 seconds and allowed to cool before testing. Moisture absorption was tested according to the American Society for Testing and Materials D570. Six grams of liquid acrylate adhesive were poured into a 50.8 mm diameter metal weight dish. It was then cured under UVA light for 30 seconds. After cooling, it was removed from the dish. The cured thickness was at least 3.2 mm. The sample was left at room temperature for 24 hours before testing. The tensile properties were tested according to the American Society for Testing and Materials D638 in the following manner: Liquid acrylate adhesive was poured into Type IV Teflon molds according to ASTM D638 to form samples approximately 2 mm thick. The samples were cured under a UV-A lamp for 30 seconds and then left to stand under ambient conditions for at least 24 hours prior to testing. Samples were withdrawn using an Instron device set to an expansion rate of 5 mm / min. An average of 5–8 samples was reported. Table 1 Example 1 Example 2 Example 3 Example 4 Example 5 Example 6 Example 7 Example 8 Example 9 EBECRYL 8411 Aliphatic urethane diacrylate oligomer 48.25 GENOMER 4215 Aliphatic polyester urethane diacrylate oligomer 34.3 GENOMER 4267 Aliphatic Diacrylate Urethane Oligomer 41.01 17.1 GENOMER 4316 Aliphatic Polyacrylate Polyurethane Oligomer 41.3 40.3 EBECRYL 8465 Aliphatic urethane triacrylate oligomer 7 GENOMER 2235 Aliphatic epoxy acrylate oligomer 44.6 GENOMER 2281 Epoxy Acrylate Oligomer 43.2 GENOMER 2263 Epoxy Acrylate Oligomer 39.2 25.6 GENOMER 3486 Polyester Acrylate Oligomer 37.6 GENOMER 1121Y Isobornyl acrylate monomer (function = 1) 29.7 24.7 40.47 42.8 32.76 21 37.5 33 18.6 GENOMER 7302 Polyether acrylate monomer (function = 3) 8.7 15 8.3 MIRAMER M262 Tricyclodecane dimethanol diacrylate monomer (function = 2) 17.4 7 15.62 14 16.09 14.4 16.4 16.6 15.3 MIRAMER M600 Hexafunctional aliphatic acrylate monomer 10 GENOCURE BAPO phosphine oxide photo initiator 0.9 0.9 0.9 0.9 0.9 0.9 0.9 0.9 GENOCURE MBF Methylbenzoylformate Photoinitiator 1.0 GENOCURE TPO-L Phosphine Oxide Photoinitiator 2.0 2.0 2.0 1.0 2.0 2.0 2.0 2.0 2.0 Viscosity at 23°C (centipoise) 900 800 1000 1100 900 900 800 900 900 Shore hardness D 74 81 75 74 64 78 82 75 75 Moisture absorption (% by weight) 2.6 1.9 2.7 1.7 1.8 4.7 1.6 1.2 2.4 Automatic Young's Modulus (MPa) 1081 730 1055 637 918 1373 2145 1908 1692 Tensile Stress at Break (MPa) 41 33 43 26 34 9.5 14.8 13.2 11.7 Tensile Strain at Break (%) 7.3 12 9.8 12.9 7.9 8.1 9.1 4.7 4.3

Claims

1. A spiral wound membrane filter with an outer casing. The outer casing contains: a. a reinforcement material, and b. an acrylate adhesive composition containing multifunctional (meth)acrylate. The acrylate adhesive composition has a viscosity not exceeding 10,000 centipoise when measured at 23°C according to ASTM D1084 Test Method B.

2. A spiral wound membrane filter according to protection element 1. The acrylate adhesive composition contains: (1) 15% by weight to 60% by weight of multifunctional (meth)acrylate oligomer, (2) 30% wt. to 80% wt. of (meth)acrylate monomer, and (3). 0.2% wt. to 5% wt. of photoinitiator. 3.The spiral wound membrane filter, according to any of the aforementioned protection criteria, has an acrylate adhesive composition with a viscosity not exceeding 2500 centipoise when measured at 23°C according to the American Society for Testing and Materials (ASTM) Test Method B D1084.

4. The spiral wound membrane filter, according to any of the aforementioned protection criteria, has an acrylate adhesive composition with a viscosity not exceeding 1500 centipoise when measured at 23°C according to the American Society for Testing and Materials (ASTM) Test Method B D1084.

5. The spiral wound membrane filter, according to any of the aforementioned protection criteria, has an acrylate adhesive composition with a Shore D hardness of 60 to 100, as tested according to the Shore D hardness test. 6.The spiral wound membrane filter, according to protection element 1, uses a multifunctional (meth)acrylate oligomer from a group consisting of meth)acrylate oligomer, meth)acrylate monomer, and combinations thereof.

7. The spiral wound membrane filter, according to protection element 2, uses a multifunctional (meth)acrylate oligomer from a group consisting of urethane acrylate, epoxy acrylate, polyester acrylate, acrylic acrylate, polyether acrylates, polybutadiene acrylate, and combinations thereof.

8. The spiral wound membrane filter, according to protection element 2, incorporates a multifunctional (meth) acrylate oligomer containing aliphatic urethane acrylate. 9.The spiral wound membrane filter, according to protection element 2, contains a meth acrylate monomer that includes an isobornyl acrylate monomer.

10. The spiral wound membrane filter, according to protection element 2, contains a meth acrylate monomer that includes at least two meth acrylate monomers.

11. The spiral wound membrane filter, according to protection element 10, contains two meth acrylate monomers, at least one monofunctional monomer and one multifunctional monomer.

12. The spiral wound membrane filter, according to any of the previous protection elements, has a reinforcement material consisting of a continuous fiberglass strand. 13.The spiral wound membrane filter, according to any of the aforementioned protection elements, uses an acrylate adhesive composition consisting of a single part, 100% solids.

14. A method for manufacturing the outer casing of a spiral wound membrane filter, including the following steps: a. Obtain an acrylate adhesive composition containing multifunctional (meth)acrylate and an initiator, with a viscosity not exceeding 10,000 centipoise when measured at 23°C according to American Society for Testing and Materials (ASTM) Method D1084; b. Pass at least one continuous strand of reinforcement material through the acrylate adhesive composition; c. Wrap the continuous strand around the outer perimeter, along the entire length of the spiral wound membrane filter; and d.

15. The continuous strand of reinforcement material coated with an acrylate adhesive composition is exposed to an energy source at a time chosen from among those during winding, after winding, and a combination thereof. The method is in accordance with protection element 14, where the continuous strand of reinforcement material is fiberglass, and the energy source is chosen from a group consisting of ultraviolet light, visible light, heat, and a combination thereof.