Process for decontamination of petrochemical compositions obtained from chemical recycling of polymer materials
Patent Information
- Application Number
- SA1120263078
- Authority / Receiving Office
- SA · SA
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2026-04-13
- Publication Date
- 2026-10-05
AI Technical Summary
Existing hydrocarbon formulations used in chemical and refining processes often exhibit undesirable viscosity or volatility, leading to process disturbances, and contain impurities such as chlorine and nitrogen that can cause corrosion and settling issues.
A hydrocarbon formulation with controlled boiling points and specific compositions, combined with a pyrolysis process using zeolite catalysts, is used to produce a hydrocarbon stream with reduced impurities, followed by water washing and adsorption using cerium beta zeolite to remove chlorine.
The process achieves a hydrocarbon stream suitable for refining operations with minimal process disturbances and significantly reduces chlorine content, enhancing stability and safety.
Abstract
Description
According to the present invention, a hydrocarbon formulation, as used here, can be defined, for example, by its boiling point range. Hydrocarbon formulations are typically products of a hydrocarbon nature, usually mixtures of compounds with varying boiling points. For processing in process runs, as is commonly used in the chemical and refining industry, formulations may not be highly viscous or highly volatile. A typical boiling point range for suitable formulations may include an initial boiling point ≥ 25°C and a final boiling point ≤ 350°C. The boiling points may be determined according to the method described in ASTM D86 (2012). The initial boiling point reflects the lowest temperature at which the chemical compounds in a hydrocarbon oil mixture boil, and thus indicates the temperature at which the most volatile compounds, usually those with lower molecular weights, begin to boil under atmospheric pressure. The final boiling point reflects the highest temperature achievable in boiling a hydrocarbon oil mixture, and thus indicates the temperature at which the compounds with the highest boiling points, usually those with higher molecular weights, will also boil under atmospheric conditions. Ideally, the hydrocarbon formulation A, as used in the present invention, should have an initial boiling point ≥ 30°C, preferably ≥ 50°C. Ideally, the hydrocarbon formulation A should also have a final boiling point ≤ 325°C, preferably ≤ 300°C, preferably ≤ 250°C, preferably ≤ 225°C, or even ≤ 200°C. In particular, suitable hydrocarbon formulations may have an initial boiling point ≥ 30°C and a final boiling point ≤ 300°C, preferably an initial boiling point ≥ 30°C and a final boiling point ≤ 250°C, preferably also an initial boiling point ≥ 50°C and a final boiling point ≤ 200°C. Formulations with such a range of initial and final boiling points are suitable for processing in chemical and refining operations, including allowing the application of appropriate transfer, heating, cooling and separation processes, without undesirable process disturbances. Furthermore, a hydrocarbon composition that could be considered suitable for use in the present invention may include, for example, quantities of n-paraffins, isoparaffins, olefins, naphthenes, and / or aromatic compounds. The composition may include, for example, quantities of n-paraffins, isoparaffins, olefins, naphthenes, and aromatic compounds. In the context of the present invention, n-paraffins present in formulation A may include, for example, n-alkanes with 3 to 40 carbon atoms. Isoparaffins present in formulation A may also include, for example, 3 to 40 carbon atoms. Naphthenes present in formulation A may also include, for example, 3 to 40 carbon atoms. Aromatic compounds present in hydrocarbon formulation A may also include, for example, 6 to 40 carbon atoms. Hydrocarbon composition A may include, for example, ≥ 25.0 and ≤ 95.0% by weight of n-paraffins, relative to the total weight of hydrocarbon composition A. Ideally, hydrocarbon composition A should include ≥ 25.0 and ≤ 80.0% by weight of n-paraffins, even more preferable ≥ 25.0 and ≤ 70.0% by weight, and even more preferable ≥ 25.0 and ≤ 50.0% by weight. Hydrocarbon composition A may include, for example, ≥ 5.0 and ≤ 40.0% by weight of iso-paraffins, relative to the total weight of hydrocarbon stream A. Ideally, hydrocarbon composition A should include ≥ 5.0 and ≤ 30.0% by weight of iso-paraffins, and even more preferably ≥ 7.5% by weight and ≤ 25.0% by weight. Hydrocarbon composition A may include, for example, ≤ 50.0% by weight of olefins, relative to the total weight of hydrocarbon composition A. Ideally, hydrocarbon composition A should include ≤ 40.0% by weight of olefins, even more preferably ≤ 35.0% by weight, and even more preferably ≤ 30.0% by weight. Hydrocarbon composition A may include, for example, ≥ 5.0 and ≤ 50.0% by weight of olefins, relative to the total weight of hydrocarbon composition A. Ideally, hydrocarbon composition A should include ≥ 10.0 and ≤ 40.0% by weight of olefins, and even more preferably ≥ 15.0 and ≤ 35.0% by weight. Hydrocarbon composition A may include, for example, ≥ 5.0 and ≤ 20.0% by weight of naphthenes, relative to the total weight of hydrocarbon composition A. Ideally, hydrocarbon composition A should include ≥ 5.0 and ≤ 15.0% by weight of naphthenes, and even more preferably ≥ 7.5% by weight and ≤ 15.0% by weight. Hydrocarbon composition A may include, for example, ≥ 5.0 and ≤ 15.0% by weight of aromatic compounds, relative to the total weight of hydrocarbon composition A. Ideally, hydrocarbon composition A should include ≥ 5.0 and ≤ 12.5% by weight of aromatic compounds, but even more preferably ≥ 7.5% by weight and ≤ 12.5% by weight. The hydrocarbon composition may include, for example: Regarding the total weight of the hydrocarbon composition A. In the context of the present invention, the atomic chlorine content shall be understood as the total weight of chlorine atoms present in the molecules of the hydrocarbon composition as a percentage of the total weight of the hydrocarbon stream. The atomic nitrogen content shall be understood as the total weight of nitrogen atoms present in the molecules of the hydrocarbon stream as a percentage of the total weight of the hydrocarbon stream. Hydrocarbon composition A may, for example, contain a certain amount of pollutants. For instance, hydrocarbon composition A may contain a quantity of compounds containing chlorine atoms. The quantity of compounds containing chlorine atoms may be expressed as the atomic chlorine content of hydrocarbon composition A. For example, hydrocarbon composition A may have an atomic chlorine content of 2000 ppm by weight, as defined by ASTM UOP 779-08, or < 1500 ppm, or < 1000 ppm, preferably < 800 ppm, preferably < 700 ppm, preferably more < 600 ppm, preferably more < 500 ppm, preferably more < 400 ppm. The hydrocarbon composition may include, for example, >150 ppm of atomic chlorine, preferably >200 ppm, preferably more >250 ppm. For example, a hydrocarbon composition may include >200 and <800 ppm of atomic chlorine, preferably >200 and <600 ppm, preferably more >200 and <500 ppm. A hydrocarbon composition A may include a quantity of compounds containing nitrogen atoms. The quantity of compounds containing nitrogen atoms may be expressed as the atomic nitrogen content of the hydrocarbon composition A. For example, a hydrocarbon composition A may have an atomic nitrogen content < 1600 ppm by weight, as defined according to ASTM D5762 (2012), preferably < 1500 ppm, preferably more < 1400 ppm, preferably even more < 1300 ppm, preferably even more < 1200 ppm, or < 1100 ppm, or < 1000 ppm. For example, a hydrocarbon composition A may have an atomic nitrogen content < 100 ppm by weight, as defined according to ASTM D4629 (2017). The hydrocarbon composition may include a quantity of compounds containing olefinic unsaturations. The bromine number of the hydrocarbon stream is an indicator of the quantity of olefinic unsaturations. The bromine number indicates the amount of bromine, in grams, that reacts with 100 grams of the hydrocarbon sample when tested under ASTM D1159-07 (2012) conditions. For example, the hydrocarbon composition as used in the present invention may have a bromine number < 100, preferably < 95, preferably even < 90, and preferably even < 85. The product should ideally contain <100 parts per million, preferably more than <75 parts per million, of atomic chlorine. Hydrocarbon composition A might, for example, be a stream of material obtained by processing waste plastic feedstock. For instance, hydrocarbon composition A might be obtained by processing a waste plastic stream in a pyrolysis unit. This pyrolysis unit may be a continuously operating unit, where a stream of plastic waste is continuously fed into the unit and at least one liquid stream containing the pyrolysis products is continuously obtained from the unit. Alternatively, the pyrolysis unit may be a batch operating unit, where a quantity of plastic waste is fed into the unit, subjected to pyrolysis conditions, and then at least one liquid stream containing the pyrolysis products is obtained from the unit. The pyrolysis process carried out in a pyrolysis unit may be a low-intensity or high-intensity pyrolysis process. In a low-intensity pyrolysis process, the pyrolysis may be carried out at temperatures ≥ 250°C and ≤ 450°C, preferably ≥ 275°C and ≤ 425°C, and even more preferably ≥ 300°C and ≤ 400°C. Alternatively, the pyrolysis process may be a high-intensity process carried out at temperatures ≥ 450°C and ≤ 750°C, preferably ≥ 500°C and ≤ 700°C, and even more preferably ≥ 550°C and ≤ 650°C. The thermal decomposition process may be catalytic. In this thermal decomposition process, for example, a quantity of zeolite catalyst such as ZSM-5 zeolite (Socony Mobile-5). In this thermal decomposition process, for example, a quantity of spent liquid catalytic cracking (FCCfluid) catalyst may be used. Specifically, a combination of Socony Mobile-5 zeolite catalyst and spent liquid catalytic cracking catalyst may be used. For example, a combination of Socony Mobile-5 zeolite catalyst and spent liquid catalytic cracking catalyst may be used, where the weight ratio of the spent liquid catalyst to the Socony Mobile-5 zeolite catalyst is between 0.5 and 5.0, such as between 1.0 and 3.0. The present invention process may include, for example, prior to step (i), a thermal decomposition step of the plastic waste formulation, whereby a hydrocarbon formulation is obtained as a liquid product of thermal decomposition. The feedstock for the waste plastics used to produce the hydrocarbon composition of the current process may include, for example, polyolefins, polyesters, thermoplastic elastomers, polyvinyl chlorides, polystyrenes, or polycarbonates. Plastic waste feedstocks used to produce hydrocarbon composites can be mixtures containing polyolefins, polyesters, thermoplastic elastomers, polyvinyl chlorides, polystyrene, or polycarbonates. Specifically, plastic waste feedstocks used to produce hydrocarbon composites can be mixtures containing <25.0% by weight of polyolefins, relative to the total weight of the plastic waste feedstock. Ideally, the plastic waste feedstock may contain <40.0% by weight of polyolefins, preferably more than <50.0% by weight, preferably even more than <60.0% by weight, or <70.0% by weight. The plastic waste feedstock may also contain a proportion of non-thermoplastic materials. These non-thermoplastic materials may be, for example, hydrocarbon-based materials such as rubber, but they may also include materials such as paper, sand, and soil. One of the advantages of the present invention is that it may be used to feed plastic waste materials containing a maximum of 10% by weight, preferably a maximum of 5.0% by weight, preferably more than a maximum of 2.0% by weight of selected materials such as paper, sand, and soil, and combinations thereof, are used in the process of preparing polypropylene. This allows for the processing of such feedstocks without the need for cleaning operations that might require the use of solvents or detergents. For example, a plastic waste feed material may include ≤ 10.0% by weight of components representing the total content of glass, paper, metals, cardboard, biodegradable waste, wood, stone, textiles, rubber materials and super-absorbent hygiene products, relative to the total weight of the plastic waste feed material. Plastic waste feed material may include, for example, ≥ 90.0% by weight of polymer materials, relative to the total weight of the plastic waste feed material. Plastic waste feedstock may contain, for example, a certain amount of polyester. For instance, plastic waste feedstock may contain <20.0% by weight of polyester, preferably <15.0% by weight, preferably more than <10.0% by weight, preferably even more than <5.0% by weight, preferably even more than <2.0% by weight. In certain formulations, plastic waste feedstock may be polyester-free. A specific type of polyester that may commonly be found in plastic waste feedstocks, such as those used in hydrocarbon stream preparation as in the present process, is polyethylene terephthalate (PET), which may also be referred to as PET. Plastic waste feedstocks may, for example, contain a certain amount of PET. Specifically, plastic waste feedstocks may contain <20.0% by weight of PET, preferably <15.0% by weight, preferably more, <10.0% by weight, preferably even more, <5.0% by weight, preferably even more, and even <2.0% by weight. In certain formulations, plastic waste feedstocks may be PET-free. Polyesters, such as polyethylene terephthalate (PET), contain oxygen atoms in their polymer chains. The presence of compounds containing oxygen atoms in hydrocarbon streams is subject to certain limitations, as an excessive amount of oxygen in the compounds supplied to the thermal cracking furnace can lead to problems including settling and corrosion during the subsequent treatment of the cracked hydrocarbon stream exiting the furnace. Therefore, there is a desire to control or even minimize the amount of oxygen-containing polymers in the plastic waste feedstock used to prepare hydrocarbon streams. Plastic waste feedstock may contain, for example, a certain amount of polyamides. For instance, plastic waste feedstock may contain <20.0% by weight of polyamides, preferably <15.0% by weight, preferably more than <10.0% by weight, preferably even more than <5.0% by weight, preferably even more than <2.0% by weight. In certain formulations, plastic waste feedstock may be polyamide-free. Certain types of polyamide that may be commonly found in plastic waste feedstocks, such as those used in the preparation of hydrocarbon stream A as used in the present process, are polyamide 6 and polyamide 66, also referred to as PA6 and PA66, respectively. Plastic waste feedstock may, for example, contain a certain amount of polyamide 6 or polyamide 66. For instance, plastic waste feedstock may contain <20.0% by weight of total polyamide 6 and polyamide 66, preferably <15.0% by weight, preferably more than <10.0% by weight, preferably even more than <5.0% by weight, preferably even more than <2.0% by weight. In certain formulations, plastic waste feedstock may be completely free of polyamide 6 and / or polyamide 66. Plastic waste feedstock may contain, for example, a quantity of polyvinyl chloride, also known as PVC. For example, plastic waste feedstock may contain <5.0% by weight of PVC, preferably <2.0% by weight, preferably more; <1.0% by weight, preferably even more; <0.5% by weight, preferably even more; and <0.1% by weight, preferably even more. In certain formulations, plastic waste feedstock may be completely PVC-free. Plastic waste feed material may include, for example Regarding the total weight of polymer materials in the plastic waste feed material. The percentages provided for polyesters, polyamides and polyvinyl chlorides in plastic waste feed material are understood as percentages by weight of the total weight of polymer materials present in the plastic waste feed material. Plastic waste feed material may also include a quantity of moisture; for example, plastic waste feed material may contain up to 20.0% by weight of moisture, preferably up to 10.0% by weight, preferably more than up to 5.0% by weight. In the present invention process, the water washing step(i) is preferably carried out at a temperature ≥ 10°C and ≤ 60°C, preferably ≥ 10°C and ≤ 40°C, preferably more ≥ 15°C and ≤ 30°C. Ideally, the water wash treatment should involve subjecting a mixture containing the hydrocarbon formulation and water (preferably deionized water) to a mixing operation. In the water wash treatment step (i), the weight ratio of the hydrocarbon formulation to water should be 1:10 to 10:1, preferably 1:5 to 5:1, preferably greater than 1:3 to 3:1, and preferably greater than 1:2 to 2:1. Using a small amount of water is desirable, as this reduces the amount of wastewater. The mixing operation can be carried out, for example, by stirring for ≥ 5 minutes, preferably ≥ 5 and ≤ 60 minutes. It is preferable that the mixing operation be followed by a sedimentation period during which the phase separation occurs to obtain an aqueous phase and a washed product (b). In the present invention process, step (ii) may involve, for example, supplying a quantity of adsorbent to the washed product. Ideally, the adsorbent should be supplied in a quantity ≥ 1.0 and ≤ 10.0% by weight, preferably more ≥ 2.0 and ≤ 5.0% by weight, relative to the weight of the washed product. The adsorbent may be selected from, for example, alumina, silica, or aluminosilicate adsorbents. For instance, the adsorbent may be a zeolite type of aluminosilicate adsorbent. This zeolite type may be selected from, for example, faujasite (FAU), beta (BEA), mordenite (MOR), Mobil Five (MFI), and ferrierite (FER). In particular, the adsorbent may be beta zeolite, which may also be referred to as beta-zeolite. The adsorbent material may be, for example, an aluminosilicate zeolite containing iron (Fe), germanium (GeGermanium), gallium (Gallium), boron (Boron), zinc (Zinc), tin (Tin), titanium (Titanium), or cerium (Cerium) atoms in its structure. Ideally, the adsorbent material should be a zeolite containing iron, zinc, or cerium atoms in its structure. In particular, a zeolite containing cerium atoms is preferable. For example, the adsorbent material may be a beta-zeolite containing cerium, a beta-zeolite containing iron, or a beta-zeolite containing zinc. Ideally, the adsorbent material should be a beta-zeolite containing cerium. For example, the adsorbent material may have a Brunauer-Emmett-Teller (BET) surface area >100 and <800 m² / g, but >200 and <600 m² / g is preferable. Similarly, the adsorbent material may have an average pore diameter >0.3 and <0.8 nm, but >0.5 and <0.8 nm is preferable. The adsorption material may, for example, be aluminosilicate with a silicon-to-aluminum weight ratio < 3.0, preferably < 2.0, preferably > 1.0 and < 2.0. Step (ii) may, in certain embodiments, include a first step of mixing the washed product with the adsorbent, preferably for >0.5 and <10 hours, preferably more >2 and <6 hours, followed by a separation step, preferably by centrifugation, to remove the adsorbent and obtain the product. Step (ii) may be carried out at a temperature ≥ 10°C and ≤ 60°C, preferably ≥ 10°C and ≤ 40°C, preferably even more ≥ 15°C and ≤ 30°C. The invention will now be illustrated by the following unrestricted examples. For the purpose of illustrating the present invention, as hydrocarbon current A, a plastic-derived oil product with an initial boiling point of 30°C and a final boiling point of 180°C was used. The plastic-derived oil product had a total chlorine content of approximately 350 ppm, a total nitrogen content below 1000 ppm, and a bromine number below 85. The plastic-derived oil comprised 43% by weight of n-paraffins, 17% by weight of isoparaffins, 19% by weight of olefins, 10% by weight of naphthenes, and 11% by weight of aromatic compounds. The plastic-derived oil had a density of approximately 750 kg / m³. Experiment 1: Washing with water to remove oil derived from plastic The washing step was performed by supplying, at room temperature, 100 mL of plastic-derived oil and 100 mL of deionized water into a suitable-sized separation funnel. The funnel was shaken for 20 minutes to form an emulsion. The emulsion was then allowed to settle for 30 minutes to allow for phase separation. The oily and aqueous phases were removed from the funnel separately and characterized. Analysis of the resulting oily product showed that 57.9 wt% of the chlorine was removed from the plastic-derived oil as a result of the water washing step. Experiment 2: Chlorine adsorption from oil derived from plastics The plastic-derived oil underwent an adsorption step. 30 mL of the water-washed oil and 1 g of the adsorbent were added to a spherical-bottom flask. The adsorption step was carried out at room temperature. Several adsorbents were tested, as shown in the table below: The experiment involved the adsorption material. 2a Alumina 2B Silica 2g Beta Cerium Zeolite 2D Beta Iron Zeolite 2H Beta Zinc Zeolite Adsorption experiments were performed by stirring the flasks for 5 hours at room temperature and atmospheric pressure. The contents of the flasks were then transferred to centrifuge tubes and centrifuged at 6000 rpm for 10 minutes. The resulting oil from the decontaminated plastic was collected and further characterized for chlorine content. The results are shown in the table below: The experiment involved the adsorption material removing chlorine (% by weight). 2a Alumina 27.2 2B Silica 22.6 2g Beta Cerium Zeolite 48.9 2D Beta Iron Zeolite 40.4 2H Beta Zinc Zeolite 37.6 As can be seen, the highest efficiency was achieved using cerium beta zeolite adsorption material. Experiment 3: The combination of washing with water and adsorption In addition to the above experiments, an experiment was conducted combining water washing and adsorption. The oily product collected from Experiment 1 was also subjected to an adsorption test carried out according to the method of Experiment 2, using cerium beta zeolite as the adsorbent. This resulted in an oily product obtained after this second decontamination step, in which 80.1% by weight of chlorine was removed, compared to the original chlorine content in the plastic-derived oil. Accordingly, by applying the combination of washing with water and adsorption, more than 80% by weight of chlorine was removed from the plastic-derived oil sample.
Claims
1. A process for removing contamination from petrochemical formulations, where the process involves subjecting a hydrocarbon formulation (A) containing inorganic and / or polar contaminants, preferably where the inorganic and / or polar contaminants are chlorine-containing, to the following steps: (i) washing treatment, and (ii) adsorption treatment.
2. A process in accordance with safeguard element 1, where the process involves the following steps: (i) subjecting a hydrocarbon formulation (A) containing inorganic and / or polar contaminants to washing treatment, preferably where the inorganic and / or polar contaminants are chlorine-containing, to obtain a washed product (B); and (ii) subjecting the product (B) obtained from step (i) to adsorption treatment to obtain product (C).
3. A process in accordance with either safeguard element 1–2, where the hydrocarbon formulation A is an oil-based hydrocarbon product obtained by the decomposition of waste plastics. 4.Process in accordance with any of the safeguards 1–3, where the hydrocarbon composition includes >200 ppm and <600 ppm of atomic chlorine, as defined in accordance with ASTM UOP 779-08.
5. Process in accordance with any of the safeguards 1–4, where the hydrocarbon composition includes: ≥25.0 and ≤95.0% by weight, preferably ≥25.0 and ≤70.0% by weight, preferably more than ≥25.0 and ≤50.0% by weight, of n-paraffins; and / or ≥ 5.0 and ≤ 20.0% by weight, preferably ≥ 5.0 and ≤ 15.0% by weight, preferably more than ≥ 7.5 and ≤ 15.0% by weight, of iso-paraffins; and / or ≥ 5.0 and ≤ 50.0% by weight, preferably ≥ 10.0 and ≤ 40.0% by weight, preferably more than ≥ 15.0 and ≤ 35.0% by weight, preferably more than ≥ 15.0 and ≤ 25.0% by weight, of olefins; and / or ≥ 5.0 and ≤ 20.0% by weight, preferably ≥ 5.0 and ≤ 15.0% by weight, preferably more than ≥ 7.5 and ≤ 15.0% by weight, of naphthenes; and / or ≥ 5.0 and ≤ 15.0% by weight, preferably ≥ 5.0 and ≤ 12.5% by weight, preferably more than ≥ 7.5 and ≤ 12.5% by weight, of aromatic compounds relative to the total weight of the hydrocarbon composition A. 6.
7. A process in accordance with any of the safeguards 1–5, where the water wash treatment is carried out at a temperature ≥ 10°C ≤ 60°C.
8. A process in accordance with any of the safeguards 1–6, where the water wash treatment involves subjecting a formulation containing the hydrocarbon formulation and water, preferably deionized water, to a mixing operation.
9. A process in accordance with any of the safeguards 1–7, where, in the water wash treatment step (i), the weight ratio of the hydrocarbon formulation to water is 1:10 to 10:
1.
10. A process in accordance with any of the safeguards 7–8, where the mixing operation is carried out by stirring for ≥ 5 minutes, preferably ≥ 5 and ≤ 60 minutes.
11. A process in accordance with any of the safeguards 7–9, where the mixing operation is followed by a sedimentation period during which phase separation occurs to obtain an aqueous phase and a washed product (b).
11. A process in accordance with any of the safeguards 1–10, where step (ii) involves supplying a quantity of adsorbent to the washed product. It is preferable that the adsorbent be supplied in a quantity ≥ 1.0 and ≤ 10.0% by weight, relative to the weight of the washed product. 12.A method according to protection element 11, where the adsorbent is chosen from alumina, silica, and zeolite, preferably a β-zeolite adsorbent containing a cerium atom.
13. A process according to any of protection elements 11–12, where step (ii) may include a first step of mixing the washed product B with the adsorbent, preferably for >0.5 and <10 hours, followed by a separation step, preferably by centrifugation, to remove the adsorbent and obtain product C.
14. A process in accordance with any of the safeguards 1–13, where the process includes, prior to step (i), a pyrolysis step of the waste plastics composition, preferably where the waste plastics composition includes <40.0% by weight of polyolefins, preferably more than <50.0% by weight, preferably even more than <60.0% by weight, or <70.0% by weight, where a hydrocarbon composition A is obtained as a liquid product of the pyrolysis. 15.A process in accordance with protection element 14, whereby a low-severity pyrolysis process is carried out, at a temperature ≥ 250°C and ≤ 450°C, preferably ≥ 275°C and ≤ 425°C, preferably more ≥ 300°C and ≤ 400°C; or a high-severity pyrolysis process is carried out at a temperature ≥ 450°C and ≤ 750°C, preferably ≥ 500°C and ≤ 700°C, preferably more ≥ 550°C and ≤ 650°C.