A method for producing copper target metal for thin film coating using the sputtering method in the hot extrusion process.

TH1701005862APending Publication Date: 2026-11-02ORIENTAL COPPER CO LTD
0 Cites 0 Cited by

Patent Information

Application Number
TH1701005862
Authority / Receiving Office
TH · TH
Patent Type
Applications
Current Assignee / Owner
Filing Date
2017-09-29
Publication Date
2026-11-02
Patent Text Reader

Abstract

------February 17, 2022------(OCR) The production of copper target metal begins with the melting and casting of copper rods with a copper purity of at least 99.99% by weight and an oxygen content of no more than 5 ppm. It is then shaped using hot extrusion and cold drawing processes. The variables controlling the copper grain size to be no more than 100 μm are: 1) the size reduction ratio during hot extrusion, 2) the temperature of the copper rod before hot extrusion, and 3) the hot extrusion blade speed. The study found that the variables with the greatest effect on grain size are the size reduction ratio during hot extrusion and the temperature of the copper rod before hot extrusion. The production conditions that result in a copper grain size not exceeding 100 Jm are: 1) Hot extrusion using a 10-inch diameter copper pipe: 1.1) Temperature of the copper pipe before hot extrusion = 750°C; 1.2) Hot extrusion speed = 5-20 mm / sec. 2) Hot extrusion using a 12-inch diameter copper pipe: 2.1) Temperature of the copper pipe before hot extrusion = 750-800°C.2) Hot extrusion speed is 5-20 mm / sec. The hot-extruded copper is further reduced in size by cold drawing at a reduction percentage not exceeding 30% to obtain copper with a surface hardness of 85 HV (not exceeding 100 HV). The above process makes the copper suitable as a target metal for thin film coating technology by the sputtering method, which improves the quality of thin films.
Need to check novelty before this filing date? Find Prior Art

Claims

16 / 10 / 2569 1. Method for producing a copper target for thin-film coating using the sputtering method. (Sputtering method) From the hot extrusion process to obtain the grain size of... Copper must not exceed 100 micrometers and surface hardness must not exceed 100 HV. The assembly procedure is as follows: a. Selecting copper pipes b. Under-water hot extrusion and c. Cold Drawing 2. The method under Claim 1, whereby the selection of copper pipes is made from copper pipes of a certain diameter. 10-12 inches in diameter, with at least 99.99% copper purity by weight, and oxygen content not exceeding 5 ppm.

3. The method under claim 1 or 2 where hot-pressure rolling in water is further incorporated with the application of... Heat the copper pipe to a temperature of 750-800 degrees Celsius before hot extrusion.

4. Any of the methods under claims 1 through 3, in which water-cooled hot extrusion is incorporated. The process of rapidly cooling (quenching) a copper pipe without contact with air, after it has been compressed through a channel. The mold (Extrusion Die) moves through water at a temperature not exceeding 40 degrees Celsius.

5. Method under claim 4 where the hot extrusion speed is 5-20 mm / sec.

6. Method under Claim 1 where the percentage reduction during cold drawing (% Cold Drawing) The reduction (or deduction) must not exceed 30%.